TY - JOUR A1 - Chakraborty, P. A1 - Mouton, I. A1 - Gault, B. A1 - Tehranchi, Ali A1 - Neugebauer, J. A1 - Hickel, Tilmann T1 - Effect of Sn on stacking fault energies in zirconium and its hydrides N2 - Hydrogen embrittlement in Zr-alloy fuel cladding is a primary safety concern for water-based nuclear reactors. Here we investigated the stabilization of planar defects within the forming hydrides by Sn, the primary alloying element of Zircaloy-4 used in the cladding. In order to explain the formation of hydrides and planar defects observed in our experiments, we performed atomic-scale ab initio calculations focusing on the solute interactions with generalized stacking faults in hcp 𝛼-Zr and fcc zirconium hydrides. Our calculations showed that an increase in Sn concentration leads to a stabilization of stacking faults in both the 𝛼-Zr and hydride phases. However, the solution enthalpy of Sn is lower in the 𝛼-Zr as compared to the other hydride phases, indicative of two competing processes of Sn depletion/enrichment at the Zr hydride/matrix interface. This is corroborated by experimental findings, where Sn is less soluble in hydrides and is mostly found trapped at interfaces and planar defects, indicative of stacking faults inside the hydride phases. Our systematic investigation enables us to understand the presence and distribution of solutes in the hydride phases, which provides a deeper insight into the microstructural evolution of such alloy's properties during its service lifetime. KW - Defects KW - First-principles calculations KW - Interface and surface thermodynamics KW - Microstructure KW - Hydrides KW - Structural properties PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-618044 DO - https://doi.org/10.1103/PhysRevMaterials.8.033605 SN - 2475-9953 VL - 8 IS - 3 SP - 1 EP - 9 PB - APS AN - OPUS4-61804 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -