TY - JOUR A1 - Vogel, F. A1 - Cheng, J. A1 - Liang, S. B. A1 - Ke, C. B. A1 - Cao, S. S. A1 - Zhang, X. P. A1 - Zizak, I. A1 - Manzoni, Anna Maria A1 - Yu, J. M. A1 - Wanderka, N. A1 - Li, W. T1 - Formation and evolution of hierarchical microstructures in a Ni-based superalloy investigated by in situ high-temperature synchrotron X-ray diffraction N2 - Hierarchical microstructures are created when additional γ particles form in γ’ precipitates and they are linked to improved strength and creep properties in high-temperature alloys. Here, we follow the formation and evolution of a hierarchical microstructure in Ni86.1Al8.5Ti5.4 by in situ synchrotron X-ray diffraction at 1023 K up to 48 h to derive the lattice parameters of the γ matrix, γ’ precipitates and γ particles and misfits between phases. Finite element method-based computer simulations of hierarchical microstructures allow obtaining each phase's lattice parameter, thereby aiding peak identification in the in situ X-ray diffraction data. The simulations further give insight into the heterogeneous strain distribution between γ’ precipitates and γ particles, which gives rise to an anisotropic diffusion potential that drives the directional growth of γ particles. We rationalize a schematic model for the growth of γ particles, based on the Gibbs-Thomson effect of capillary and strain-induced anisotropic diffusion potentials. Our results highlight the importance of elastic properties, elastic anisotropy, lattice parameters, and diffusion potentials in controlling the behavior and stability of hierarchical microstructures. KW - XRD KW - Superalloy KW - Finite element method KW - Transmission electron microscopy PY - 2022 DO - https://doi.org/10.1016/j.jallcom.2022.165845 SN - 0925-8388 VL - 919 SP - 1 EP - 17 PB - Elsevier CY - Lausanne AN - OPUS4-55394 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gluth, Gregor A1 - Ke, X. A1 - Vollpracht, A. A1 - Weiler, L. A1 - Bernal, S. A. A1 - Cyr, M. A1 - Dombrowski-Daube, K. A1 - Geddes, D. A1 - Grengg, C. A1 - Le Galliard, C. A1 - Nedeljkovic, M. A1 - Provis, J. L. A1 - Valentini, L. A1 - Walkley, B. ED - Jędrzejewska, A. ED - Kanavaris, F. ED - Azenha, M. ED - Benboudjema, F. ED - Schlicke, D. T1 - Carbonation of alkali-activated concretes: effects of compositional parameters and carbonation conditions N2 - The current ability to predict the carbonation resistance of alkali-activated materials (AAMs) is incomplete, partly because of widely varying AAM chemistries and variable testing conditions. To identify general correlations between mix design parameters and the carbonation rate of AAMs, RILEM TC 281-CCC Working Group 6 compiled and analysed carbonation data for alkali-activated concretes and mortars from the literature. For comparison purposes, data for blended Portland cement-based concretes with a high percentage of SCMs (≥66% of the binder) were also included in the database. The results show that the water/CaO ratio is not a reliable indicator of the carbonation rate of AAMs. A better indicator of the carbonation rate of AAMs under conditions approximating natural carbonation is their water/(CaO + MgOeq + Na2Oeq + K2Oeq) ratio, where the index ‘eq’ indicates an equivalent amount based on molar masses. This finding can be explained by the CO2 binding capacity of alkaline-earth and alkali metal ions; the obtained correlation also indicates an influence of the space-filling capability of the binding phases of AAMs, as for conventional cements. However, this ratio can serve only as an approximate indicator of carbonation resistance, as other parameters also affect the carbonation resistance of alkali-activated concretes. In addition, the analysis of the dataset revealed peculiarities of accelerated tests using elevated CO2 concentrations for low-Ca AAMs, indicating that even at the relatively modest concentration of 1% CO2, accelerated testing may lead to inaccurate predictions of their carbonation resistance under natural exposure conditions. T2 - International RILEM Conference on Synergising Expertise towards Sustainability and Robustness of Cement-based Materials and Concrete Structures: SynerCrete 2023 CY - Adamantas, Greece DA - 14.06.2023 KW - Carbonation KW - Alkali-activated materials KW - Mix design PY - 2023 DO - https://doi.org/10.1007/978-3-031-33187-9_94 VL - 2 SP - 1029 EP - 1037 PB - Springer CY - Cham AN - OPUS4-57699 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gluth, Gregor A1 - Ke, X. A1 - Vollpracht, A. A1 - Bernal, S. A. A1 - Cizer, Ö. A1 - Cyr, M. A1 - Dombrowski-Daube, K. A1 - Geddes, D. A1 - Grengg, C. A1 - Le Galliard, C. A1 - Nedeljkovic, M. A1 - Provis, J. L. A1 - Shi, Z. A1 - Valentini, L. A1 - Walkley, B. ED - Escalante-Garcia, J. I. ED - Castro Borges, P. ED - Duran-Herrera, A. T1 - RILEM TC 281-CCC Working Group 6: Carbonation of alkali activated concrete—preliminary results of a literature survey and data analysis N2 - The current understanding of the carbonation of alkali-activated concretes is ham-pered inter alia by the wide range of binder chemistries used. To overcome some of the limitations of individual studies and to identify general correlations between their mix design parameters and carbonation resistance, the RILEM TC 281-CCC working group 6 compiled carbonation data for alkali-activated concretes and mortars from the literature. For comparison purposes, data for blended Portland cement-based concretes with a high percentage of SCMs (≥ 66 % of the binder) were also included in the database. A preliminary analysis of the database indicates that w/CaO ratio and w/b ratio exert an influence on the carbonation resistance of alkali-activated concretes but, contrary to what has been reported for concretes based on (blended) Portland cements, these are not good indicators of their carbonation resistance when considered individually. A better indicator of the carbonation resistance of alkali-activated concretes under conditions approxi-mating natural carbonation appears to be their w/(CaO + Na2O + K2O) ratio. Furthermore, the analysis points to significant shortcomings of tests at elevated CO2 concentrations for low-Ca alkali-activated concretes, indicating that even at a concentration of 1 % CO2, the outcomes may lead to inaccurate predictions of the carbonation coefficient under natural exposure conditions. T2 - 75th RILEM Annual Week CY - Mérida, Yucatán, Mexico DA - 30.08.2021 KW - Alkali-activated materials KW - Durability KW - Carbonation KW - Testing KW - Concrete PY - 2023 SN - 978-3-031-21734-0 SN - 978-3-031-21735-7 DO - https://doi.org/10.1007/978-3-031-21735-7_72 SN - 2211-0852 SN - 2211-0844 VL - 40 SP - 667 EP - 676 PB - Springer CY - Cham AN - OPUS4-57157 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gluth, Gregor A1 - Ke, X. A1 - Vollpracht, A. A1 - Weiler, L. A1 - Bernal, S. A. A1 - Cyr, M. A1 - Dombrowski-Daube, K. A1 - Geddes, D. A. A1 - Grengg, C. A1 - Le Galliard, C. A1 - Nedeljkovic, M. A1 - Provis, J. L. A1 - Valentini, L. A1 - Walkley, B. T1 - Carbonation rate of alkali-activated concretes and high-volume SCM concretes: a literature data analysis by RILEM TC 281-CCC N2 - The current understanding of the carbonation and the prediction of the carbonation rate of alkali-activated concretes is complicated inter alia by the wide range of binder chemistries used and testing conditions adopted. To overcome some of the limitations of individual studies and to identify general correlations between mix design parameters and carbonation resistance, the RILEM TC 281-CCC ‘Carbonation of Concrete with Supplementary Cementitious Materials’ Working Group 6 compiled and analysed carbonation data for alkali-activated concretes and mortars from the literature. For comparison purposes, data for blended Portland cement-based concretes with a high percentage of SCMs (≥ 66% of the binder) were also included in the database. The analysis indicates that water/CaO ratio and water/binder ratio exert an influence on the carbonation resistance of alkali-activated concretes; however, these parameters are not good indicators of the carbonation resistance when considered individually. A better indicator of the carbonation resistance of alkali-activated concretes under conditions approximating natural carbonation appears to be their water/(CaO + MgOeq + Na2Oeq + K2Oeq) ratio, where the subscript ‘eq’ indicates an equivalent amount based on molar masses. Nevertheless, this ratio can serve as approximate indicator at best, as other parameters also affect the carbonation resistance of alkali-activated concretes. In addition, the analysis of the database points to peculiarities of accelerated tests using elevated CO2 concentrations for low-Ca alkali-activated concretes, indicating that even at the relatively modest concentration of 1% CO2, accelerated testing may lead to inaccurate predictions of the carbonation resistance under natural exposure conditions. KW - Alkali-activated materials KW - Durability KW - Carbonation KW - Accelerated testing PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-560037 DO - https://doi.org/10.1617/s11527-022-02041-4 VL - 55 IS - 8 SP - 1 EP - 15 PB - Springer Nature AN - OPUS4-56003 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hein, Sebastian A1 - Philipp, Rosemarie A1 - Duewer, D.L. A1 - Gasca-Aragon, H. A1 - Lippa, K. A1 - Toman, B. A1 - Bremser, Wolfram A1 - Calderón, M. A. A. A1 - Castorena, A.P. A1 - Caixeiro, J.M.R. A1 - Do Rego, E.C.P. A1 - Rosso, A. A1 - De Arechavaleta, R. A1 - O'Connor, G. A1 - Holcombe, G. A1 - Ellison, S.L.R. A1 - Splett, J.D. A1 - Schantz, M.M. A1 - Sharpless, K.E. A1 - Croft, M. A1 - Archer, M. A1 - De Vos, J. A1 - Konopelko, L.A. A1 - Kustikov, Y. T1 - Final report on CCQM-K79: Comparison of value-assigned CRMs and PT materials: Ethanol in aqueous matrix N2 - The 2010 CCQM-K79 'Comparison of value-assigned CRMs and PT materials: Ethanol in aqueous media' is the second key comparison directly testing the chemical measurement services provided to customers by National Metrology Institutes (NMIs) and Designated Institutes (DIs). CCQM-K79 compared the assigned ethanol values of proficiency test (PT) and certified reference materials (CRMs) using measurements made on these materials under repeatability conditions. Nine NMIs submitted 27 CRM or value-assigned PT materials for evaluation. These materials represent many of the higher-order reference materials then available for this commercially and forensically important measurand. The assigned ethanol mass fraction in the materials ranged from 0.1 mg/kg to 334 mg/kg. All materials were stored and prepared according the specifications provided by each NMI. Samples were processed and analyzed under repeatability conditions by one analytical team using a gas chromatography with flame ionization detection (GC-FID) method of demonstrated trueness and precision. Given the number of materials and the time required for each analysis, the majority of the measurements were made in two measurement campaigns ('runs'). Due to a shipping delay from one NMI, an unanticipated third campaign was required. In all three campaigns, replicate analyses (three injections of one preparation separated in time) were made for one randomly selected unit of each of the 27 materials. Nine of the 27 materials were gravimetrically diluted before measurement to provide solutions with ethanol mass fraction in the established linear range of the GC-FID method. The repeatability measurement value for each analyzed solution was estimated as the mean of all replicate values. The within- and between-campaign variance components were estimated using one-way ANOVA. Markov Chain Monte Carlo Bayesian analysis was used to estimate 95% level-of-confidence coverage intervals for the mean values. Uncertainty-weighted generalized distance regression was used to establish the key comparison reference function (KCRF) relating the assigned values to the repeatability measurements. On the basis of leave-one-out cross-validation, all of the assigned values for all 27 materials were deemed equivalent at the 95% level of confidence. These materials were used to define the KCRF. Parametric bootstrap Monte Carlo was used to estimate 95% level-of-confidence coverage intervals for the degrees of equivalence of materials, d ± U95(d), and of the participating NMIs, D ± U95(D). Because of the very wide range of ethanol mass fraction in the materials, these degrees of equivalence are expressed in percent relative form: %d ± U95(%d) and %D ± U95(%D). The median of the absolute values of the %D for the participating NMIs is less than 0.05% with a median U95(%D) of less than 1%. These results demonstrate that the participating NMIs have the ability to correctly value-assign CRMs and proficiency test materials for ethanol in aqueous media and similar measurands. PY - 2013 DO - https://doi.org/10.1088/0026-1394/50/1A/08005 SN - 0026-1394 SN - 1681-7575 VL - 50 IS - 1A / Technical Suppl. 2013 / 08005 SP - 1 EP - 49 PB - Inst. of Physics Publ. CY - Bristol AN - OPUS4-27730 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -