TY - JOUR A1 - Richter, Anja A1 - Buchberger, G. A1 - Stifter, D. A1 - Duchoslav, J. A1 - Hertwig, Andreas A1 - Bonse, Jörn A1 - Heitz, J. A1 - Schwibbert, Karin T1 - Spatial Period of Laser-Induced Surface Nanoripples on PET Determines Escherichia coli Repellence N2 - Bacterial adhesion and biofilm formation on surfaces are associated with persistent microbial contamination, biofouling, and the emergence of resistance, thus, calling for new strategies to impede bacterial surface colonization. Using ns-UV laser treatment (wavelength 248 nm and a pulse duration of 20 ns), laser-induced periodic surface structures (LIPSS) featuring different submicrometric periods ranging from ~210 to ~610 nm were processed on commercial poly(ethylene terephthalate) (PET) foils. Bacterial adhesion tests revealed that these nanorippled surfaces exhibit a repellence for E. coli that decisively depends on the spatial periods of the LIPSS with the strongest reduction (~91%) in cell adhesion observed for LIPSS periods of 214 nm. Although chemical and structural analyses indicated a moderate laser-induced surface oxidation, a significant influence on the bacterial adhesion was ruled out. Scanning electron microscopy and additional biofilm studies using a pili-deficient E. coli TG1 strain revealed the role of extracellular appendages in the bacterial repellence observed here. KW - Laser-induced periodic surface structures (LIPSS) KW - Laser processing KW - Polyethylene terephthalate KW - Biofilm formation KW - Cell appendages KW - Biomimetic KW - F pili PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-537431 DO - https://doi.org/10.3390/nano11113000 VL - 11 IS - 11 SP - 3000 PB - MDPI AN - OPUS4-53743 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Grabmayer, K. A1 - Wallner, G.M. A1 - Beißmann, S. A1 - Braun, Ulrike A1 - Steffen, R. A1 - Nitsche, D. A1 - Röder, B. A1 - Buchberger, W. A1 - Lang, R.W. T1 - Accelerated aging of polyethylene materials at high oxygen pressure characterized by photoluminescence spectroscopy and established aging characterization methods N2 - Two commercial polyethylene grades were exposed to water at elevated temperatures and enhanced oxygen pressure. To characterize their aging behavior laser-induced photoluminescence spectroscopy was applied. Additionally, aging characterization was performed by established methods such as tensile testing, infrared (IR) spectroscopy, high performance liquid chromatography (HPLC), differential scanning calorimetry (DSC) and UV–VIS spectroscopy. During the initial stages of aging, the overall concentration of phenolic antioxidants as well as oxidation onset temperatures decreased exponentially. Simultaneously, significant discoloration due to the formation of conjugated degradation products from phenolic antioxidants (e.g., quinone methides) was detected. After the consumption of antioxidants, photoluminescence started to grow continuously presumably due to the formation of photoluminescent unsaturated carbonyls. In the final stages of aging, embrittlement of the materials as characterized by the degradation of mechanical properties (i.e., loss in ductility) coincided with rising carbonyl index values as well as an increase in crystallinity due to chemicrystallization. Between integrated photoluminescence intensity and carbonyl index, a linear correlation was established. In the induction period, the photoluminescence method exhibited a significantly higher sensitivity to reflect aging induced material changes. KW - Polyethylene KW - PE-RT KW - High oxygen pressure KW - Photoluminescence spectroscopy KW - Aging PY - 2014 DO - https://doi.org/10.1016/j.polymdegradstab.2014.06.021 SN - 0141-3910 SN - 1873-2321 VL - 109 SP - 40 EP - 49 PB - Applied Science Publ. CY - London AN - OPUS4-31349 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -