TY - JOUR A1 - Stark, Wolfgang A1 - Hoster, B. A1 - Kürten, Ch. T1 - Nachtemperung von duroplastischen Bauteilen - Spagat zwischen Eigenschaftsverbesserung und Eigenschaftsverschlechterung JF - GAK: Gummi, Fasern, Kunststoffe PY - 2005 SN - 0176-1625 VL - 58 IS - 11 SP - 718 EP - 722 PB - Gupta CY - Ratingen AN - OPUS4-11592 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Stark, Wolfgang A1 - Hoster, B. A1 - Kürten, C. T1 - Längenänderung bei erhöhten Temperaturen und Aushärtegrad von duroplastischen Formteilen JF - GAK: Gummi, Fasern, Kunststoffe KW - Harnstoffharze KW - Verzug KW - Spritzgießen KW - Aushärtegrad KW - Schrumpf PY - 2006 SN - 0176-1625 VL - 59 IS - 10 SP - 627 EP - 631 PB - Gupta CY - Ratingen AN - OPUS4-14444 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hoster, B. A1 - Jaunich, Matthias A1 - Stark, Wolfgang T1 - Monitoring of the vulcanisation process by ultrasound during injection moulding JF - The e-journal of nondestructive testing & ultrasonics N2 - Today rubber is due to its unique property profile one of the most important materials for the production of bearings, dampers or also tires and tubes. In the production of rubber goods a chemical cross-linking reaction (vulcanisation) generates the final material properties. This process takes place during the shape giving of the rubber compound in the mould and can proceed for several minutes. The cross-linking process is influenced by the mixture of the basic polymer, the cross-linking agent, the influence of catalysts and inhibitors and especially the processing conditions. The quality of every ingredient, the reproducibility of the mixing ratio, the homogeneity of the mixture and the accurateness in temperature control can have a direct influence on the cross linking reaction. To control the quality of a rubber compound and verify the processing conditions in industry moving die rheometers, named curemeter, are involved in the production process. Starting from our experience in cure monitoring of thermosetting materials by measuring ultrasound velocity in the mould we extended the measuring principle to rubber vulcanisation monitoring. After first investigations using a compression mould we dealt here with on-line monitoring of vulcanisation in an injection moulding process which is one of the most used techniques in rubber industry. KW - Ultrasonic KW - Sound velocity KW - Vulcanisation KW - On-line monitoring KW - Injection moulding PY - 2009 UR - https://www.ndt.net/search/docs.php3?id=8042 SN - 1435-4934 VL - 14 IS - 9 SP - 1 EP - 9 PB - NDT.net CY - Kirchwald AN - OPUS4-19858 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -