TY - THES A1 - Aristia, Gabriela T1 - Polyaniline/Silicon Dioxide Composite-Based Coating for Corrosion Protection in Geothermal Systems N2 - Geothermal energy is one of the cleanest renewable alternatives to reduce the dependency on fossil fuel [1, 2]. Despite its promising future, its implementation faces various challenges, one of them being corrosion processes. To implement this energy, hot fluids are pumped from a geothermal well. These hot fluids originate from deep within the earth, so consist of different ionic species and gases in a wide range of temperatures, which lead to their corrosive nature. In terms of geothermal energy resources, Indonesia is at the forefront, with the highest preserved geothermal energy in the world of about 29 GWe and 312 potential geothermal locations [3]. Geothermal wells in Sibayak (North Sumatera), Indonesia, belong to young stratovolcanoes and have operating temperatures varying from 36 °C at the near ground surface to 310 °C at the bottom of the well, which is liquid-dominated with acidic and saline properties [4, 5]. Therefore, this geothermal fluid creates an aggressive environment that is conducive to corrosion of the powerplant infrastructure. Parts of the geothermal powerplant infrastructure, such as pipelines and heat exchangers, are commonly made of metals, e.g. carbon steel and stainless steel. Consequently, they may undergo corrosion and scaling when exposed to the geothermal fluid, especially for carbon steel. To ensure the safety and longevity of a geothermal powerplant, the infrastructure is constructed of expensive corrosion resistant alloys [6–10], e.g., titanium and Ni-Cr based alloys, or carbon steel which needs to be protected by coatings or inhibitors. To address the corrosion of carbon steel in the geothermal environment, artificial geothermal water was used to simulate a geothermal well in Sibayak, Indonesia, with pH 4 and a saline composition of 1,500 mg/l Cl-, 20 mg/l SO42-, 15 mg/l HCO3-, 200 mg/l Ca2+, 250 mg/l K+, and 600 mg/l Na+. Carbon steel underwent the most severe corrosion at 150°C in an oxygen-containing solution with a corrosion rate of 0.34 mm/year, which is approximately ten times higher than that in the absence of dissolved oxygen. In all conditions, pitting corrosion was observed, which necessitate a protection strategy on carbon steel. In order to promote a cost effective and locally available option, this work focused on an easily applicable coating which utilized local resources. Toward developing such protective coating based on the locally available resources in Indonesia which can yield good corrosion resistance and thermal stability in geothermal environment, two additional components, i.e. polyaniline (PANI) and silicon dioxide, were used to modify an alkyd-based commercial coating. The selection of the alkyd-based coating as a matrix focused on the industrial convenience basis, where the coating application procedure should be simple and easy to apply within reasonable costs. The alkyd-based coating underwent severe blistering when exposed to the artificial geothermal water at 70 and 150°C due to the reaction between CaCO3 (as one of its components) and the artificial geothermal water, as well as a possible alkyd hydrolysis in the initial stage of exposure. In the oxygen-free solution, the degradation was controlled by chemical and thermal reactions, whereas in the aerated condition, oxidization at the coating surface further accelerated polymer degradation. PANI was chosen as one of the anticorrosion pigments which was widely developed over the past decades. To investigate the interaction between PANI and the artificial geothermal water, PANI film was electrochemically deposited on the carbon steel surface and exposed to the artificial geothermal water. Electrochemically synthesized oxalate-doped PANI was protective against corrosion of carbon steel in artificial geothermal water at room temperature. The mechanism involved an exchange of electroactive species within the coating layer, as confirmed by electrochemical impedance spectra. Interaction of ionic species, such as Cl-, Na+, Ca2+ from the artificial geothermal water, with the outer layer of PANI is suggested both at 25°C and 150°C, based on the EDX spectra of the coating surface after exposure to the artificial geothermal water. Thus, the protection mechanism of PANI is not solely based on the physical barrier layer properties, but rather associated with the redox mediated properties of PANI, which selectively allow ionic species intrusion from the electrolyte into the PANI layer. Although PANI is a promising candidate as an anticorrosion coating, its morphological characterization reveals that electrochemically deposited PANI is not stable for an application at 150°C. Therefore, another approach was used to promote better protective behavior of PANI by dispersing chemically synthesized PANI in the alkyd-based coating. To enhance the thermal stability of the coating, silicon dioxide (SiO2) was added, which was able to prolong the sustainability of coated metals until 28 days compared to the unmodified alkyd-based coating, which underwent a change in color to brown/orange only within 7 days of exposure. This improvement might be associated with the role of SiO2 to proportionate the thermal expansion coefficient of the coating system to be compatible with that of carbon steel. Although the coating is thermally enhanced, the electrolyte might still intrude through the coating resulting in the change of coating color after 28 days of exposure in the artificial geothermal water. When PANI was added, the coating system provided an active corrosion protection on the carbon steel surface. The chemical and morphological characterization of the PANI-alkyd and SiO2-alkyd coating system showed that coatings were improved, and no blisters were observed, albeit the degradation continued. Based on the results of exposure tests, the combined coating system was further investigated. The combinational coating of PANI/SiO2-alkyd was used with 2 wt% of PANI and 15 wt% of SiO2. Electrochemical tests indicated cathodic protection at 150°C, as the Ecorr of PANI/SiO2 remained approximately 400 mV lower than the carbon steel potential. The impedance spectra of the combinational coating of PANI/SiO2 showed a continuous decrease in the absolute impedance value over time. A significant decrease was observed within one day of exposure, followed by a slow gradual decrease, which might be associated with water absorption in the coating. FTIR spectra revealed that several peaks associated with the organic portion of the coatings were reduced after the specimens were exposed for 6 months. However, the absorption peaks related to the inorganic portion of the coatings remained stable until 6 months. Morphological characterization of the combinational coating of PANI/SiO2 showed that there were no blisters or significant discoloration of coatings after long-term exposure for 6 months in artificial geothermal water at 150°C, indicating that the chemical degradation does not significantly affect the functionality of the coating. This clearly shows the durability of PANI/SiO2 coating in the geothermal condition, suggesting that this coating can be used for such geothermal application. However, further testing of this coating should be conducted in a real geothermal environment on-site to ensure safety and viability. KW - Geothermal KW - Corrosion KW - Coating KW - Polyaniline KW - Electrochemical impedance spectroscopy PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:188-refubium-26704-6 UR - https://refubium.fu-berlin.de/handle/fub188/26704 DO - https://doi.org/10.17169/refubium-26461 SP - 1 EP - 175 CY - Berlin AN - OPUS4-51281 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Aristia, Gabriela A1 - Le, Quynh Hoa A1 - Bäßler, Ralph T1 - Integrated Coating System for Corrosion Protection of Carbon Steel in Artificial Geothermal Brine T2 - Proceedings AMPP International Corrosion Conference 2022 N2 - Corrosive geothermal brines are a major challenge to geothermal power-plants. For cost reasons, plant designers prefer to use carbon and low alloyed steels, which are susceptible to uniform and localized corrosion when exposed to geothermal brines having acidic and saline properties. To solve such problem, coatings or inhibitors would be a protective solution as an alternative to the use of high alloyed materials. This study investigated a coating system consisting of polyaniline/silicon dioxide based on resources locally available in Indonesia. Protection against corrosion of carbon steel was shown by long-term (28 day) exposure and electrochemical tests of coated carbon steels, performed in an artificial acidic and saline geothermal brine, comparable to the conditions encountered at a site in Indonesia. Therefore, an integrated coating system is proposed for corrosion protection, combining the electrochemical functionality of polyaniline and the physical advantages of silica. T2 - AMPP International Corrosion Conference CY - Online meeting DA - 06.03.2022 KW - Geothermal KW - Corrosion KW - Coating KW - Polyaniline KW - Silicon dioxide PY - 2022 SP - 1 EP - 11 CY - Houston TX (USA) AN - OPUS4-54451 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bäßler, Ralph A1 - Aristia, Gabriela T1 - Geothermie aus dem Vulkan – sicher und wirtschaftlich JF - Materials and Corrosion N2 - Indonesien gilt aufgrund seiner vielen Vulkane als einer der Hotspots für Geothermie. Doch Salz und Hitze setzen den Geothermie‐Anlagen zu und gefährden ihre Sicherheit und Wirtschaftlichkeit. Ein Team an der BAM hat günstigen, lokal verfügbaren Baustahl jetzt so beschichtet, dass ein nachhaltiger und sicherer Betrieb der Geothermie‐Kraftwerke möglich ist ‐ auch unter Extrembedingungen. Das BAM‐Team will das Beschichtungssystem nun den Anwendern in Indonesien zur Verfügung stellen, damit es unter Realbedingungen in einem Geothermie‐Kraftwerk getestet werden kann. Der Schutz vor Korrosion ist mitentscheidend, weil sie die Lebensdauer dieser Kraftwerke bestimmt. Unsere Arbeit könnte die Effizienz der Energieproduktion mit Geothermie wesentlich verbessern. KW - Geothermie KW - Korrosion PY - 2020 DO - https://doi.org/10.1002/maco.202070086 SN - 1521-4176 SN - 0947-5117 VL - 71 IS - 8 SP - 1 EP - 2 PB - WILEY‐VCH Verlag GmbH & Co. KGaA CY - Weinheim AN - OPUS4-51074 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Aristia, Gabriela T1 - Fireside Chat - Sharing PhD N2 - Erfahrung einer indonesischen Stipendiatin beim Aufenthalt in Deutschland als Doktorandin; Hinweise und Empfehlungen für indonesische Jungwissenschaftler und Studenten T2 - Fireside Chat der Indonesischen Botschaft CY - Berlin, Germany DA - 21.11.2019 KW - Indonesien PY - 2019 AN - OPUS4-49737 LA - mul AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Aristia, Gabriela T1 - Fenomena Korosi pada aplikasi panas bumi N2 - To accelerate the development of Indonesian geothermal energy, progress should be done in all aspects. Corrosion is an important part on the technological development to ensure the safety and longevity of a power plant. T2 - Fireside Chat der Indonesischen Botschaft CY - Berlin, Germany DA - 21.11.2019 KW - Corrosion KW - Korosi KW - Korrosion PY - 2019 AN - OPUS4-49735 LA - mul AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Aristia, Gabriela A1 - Bäßler, Ralph A1 - Roth, C. T1 - Electrochemical study of polyaniline/silicon dioxide containing coatings in geothermal solution N2 - Polyaniline/Silicon Dioxide containing coatings were electrochemically investigated in a saline geothermal solution. With the increase of exposure time, impedance values of coated specimens decreased at low frequency, which could be caused by the decrease of pore resistance due to electrolyte or water uptake. Coating system needs further optimization work. T2 - NACE International Annual Corrosion Conference CY - Phoenix, AZ, USA DA - 15.04.2018 KW - Geothermal KW - Coating KW - SiO2 KW - Polyaniline KW - Corrosion PY - 2018 AN - OPUS4-44918 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Aristia, Gabriela A1 - Bäßler, Ralph A1 - Roth, C. T1 - Electrochemical measurement of polyaniline containing coating at high temperature: PROBLEMS AND CHALLENGES N2 - This presentation describes special aspects when performing measurements at high temperatures. Especially electrochemical issues are addressed for impedance spectroscopy, like overlapping time constants, handling of noise etc. T2 - Electrochemical Doctoral School “Corrosion: from analysis to modelling” CY - Brussels Belgium DA - 04.02.2019 KW - Polyaniline KW - Geothermal KW - Electrochemical impedance spectroscopy PY - 2019 AN - OPUS4-47917 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Aristia, Gabriela A1 - Le, Quynh Hoa A1 - Bäßler, Ralph T1 - Electrochemical deposition of polyaniline on carbon steel for corrosion study in geothermal solution N2 - Polyaniline has been widely developed for many applications, e.g., sensor, supercapacitor component, electrochromic devices, and anticorrosion pigments [1]. Although the addition of polyaniline pigment in organic coatings has been an alternative for corrosion protection in industrial application, the protection mechanism is still not fully understood [2]. Herein in this study, as a part of the development of polyaniline/silicon dioxide coating for geothermal application, polyaniline has been deposited electrochemically on carbon steel surface and tested in geothermal solution to study the contribution of polyaniline in the corrosion protection of a polyaniline-based composite in the geothermal system. The electrochemical deposition was carried out by immersing carbon steel in 0.1 M oxalic acid and 0.05 M aniline, with the polarization potential of -0.6 – 1.5 V vs. Ag/AgCl, and a scan rate of 10 mV/s. To observe the surface/interface reaction between the electrolyte and electrode surface during the electrochemical polymerization, electrochemical impedance spectroscopy (EIS) measurement was applied after each cycle. For corrosion study in the geothermal application, this experiment used an artificial geothermal solution with the composition of 1,500 mg/l Cl-, 20 mg/l SO42-, 15 mg/l HCO3-, 200 mg/l Ca2+, 250 mg/l K+, and 600 mg/l Na+, and pH 4 to simulate a geothermal brine found in Sibayak, Indonesia. Electrochemical measurements were performed by monitoring the open circuit potential over seven days, with the interruption of EIS every 22 hours. The experiments were performed at room temperature and 150 °C (1 MPa) in a free oxygen environment. Polyaniline coated carbon steel is more durable in a room temperature environment compared to 150 °C, which could be caused by the iron oxalate dissolution at elevated temperature. This degradation was further proven by the impedance spectra, which showed a reduction of approximately ten times for specimens measured at 150 °C as compared to the specimens measured at room temperature. T2 - 4th International Conference on Functional Materials Science 2018 (ICFMS 2018) CY - Bali, Indonesia DA - 13.11.2018 KW - Polyaniline KW - Electrochemical deposition KW - Corrosion PY - 2018 AN - OPUS4-46742 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Aristia, Gabriela A1 - Le, Quynh Hoa A1 - Bäßler, Ralph T1 - Electrochemical deposition of polyaniline on carbon steel for corrosion study in geothermal solution JF - Materials Science Forum N2 - Polyaniline has been widely developed for many applications, e.g. sensor, supercapacitor components, electrochromic devices, and anticorrosion pigments. Although the addition of polyaniline pigment in organic coatings has been an alternative for corrosion protection in industrial applications, the protection mechanism is still not fully understood. Herein in this study, as a part of the development of polyaniline/silicon dioxide coating for geothermal application, polyaniline has been deposited electrochemically on carbon steel surface in oxalic acid medium and tested in geothermal solution to understand the contribution of polyaniline to the corrosion protection of a polyaniline-based composite in the geothermal system. To observe the surface/interface reaction between the electrolyte and electrode surface during the electrochemical polymerization, electrochemical impedance spectroscopy (EIS) was applied after each cycle. For corrosion study in the geothermal application, an artificial geothermal solution was used with the composition of 1,500 mg/l Cl⁻, 20 mg/l SO₄²⁻, 15 mg/l HCO₃⁻, 200 mg/l Ca²⁺, 250 mg/l K⁺, and 600 mg/l Na⁺, and pH 4 to simulate a geothermal brine found in Sibayak, Indonesia. An electrochemical measurement was performed by monitoring the open circuit potential over seven days, with the interruption by EIS every 22 hours. The experiments were performed at room temperature and 150 °C (1 MPa) in an oxygen-free environment. Impedance spectra showed a reduction of the total impedance value of approximately 10 times for specimens measured at 150 °C compared to the specimens measured at room temperature, suggesting a less stable layer at high temperature. KW - Corrosion KW - Electrochemical deposition KW - Polyaniline PY - 2019 DO - https://doi.org/10.4028/www.scientific.net/MSF.966.107 SN - 1662-9752 VL - 966 SP - 107 EP - 115 PB - Trans Tech Publications Ltd CY - Zürich AN - OPUS4-48776 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Aristia, Gabriela A1 - Le, Quynh Hoa A1 - Bäßler, Ralph T1 - Effect of CO2 gas on carbon steel corrosion in an acidic-saline based geothermal fluid T2 - Electronic Proceedings Eurocorr 2019 N2 - Geothermal energy is one of the most promising energy resources to replace fossil fuel. To extract this energy, hot fluids of various salts and gases are pumped up from a geothermal well having a certain depth and location. Geothermal wells in volcanic regions often contain highly corrosive CO2 and H2S gases that can be corrosive to the geothermal power-plants, which are commonly constructed of different steels, such as carbon steel. This research focuses on the corrosion behaviour of carbon steel exposed to an artificial geothermal fluid containing CO2 gas, using an artificial acidic-saline geothermal brine as found in Sibayak, Indonesia. This medium has a pH of 4 and a chloride content of 1,500 mg/L. Exposure tests were conducted for seven days at 70 °C and 150 °C to simulate the operating temperatures for low and medium enthalpy geothermal sources. Surface morphology and cross-section of the specimens from the above experiments were analysed using scanning electron microscope (SEM) and energy dispersive X-ray (EDX). Electrochemical tests via open circuit potential (OCP) and electrochemical impedance spectroscopy (EIS) were performed to understand the corrosion processes of carbon steel in CO2-containing solution both at 70 °C and 150 °C. Localized corrosion was observed to a greater extent at 70 °C due to the less protectiveness of corrosion product layer compared to that at 150 °C, where FeCO3 has a high corrosion resistance. However, a longer exposure test for 28 days revealed the occurrence of localized corrosion with deeper pits compared to the seven-day exposed carbon steel. In addition, corrosion product transformation was observed after 28 days, indicating that more Ca2+ cations incorporate into the FeCO3 structure. T2 - EUROCORR 2019 CY - Sevilla, Spain DA - 09.09.2019 KW - Carbon steel KW - CO2 KW - EIS KW - Geothermal KW - Corrosion PY - 2019 SP - Paper 200245, 1 EP - 5 CY - Madrid, Spain AN - OPUS4-49099 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -