TY - JOUR A1 - Straße, Anne A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Study on Duplex Stainless Steel Powder Compositions for the Coating of thick Plates of Laser Beam Welding N2 - Duplex stainless steels combine the positive properties of its two phases, austenite and ferrite. Due to its good corrosion resistance, high tensile strength, and good ductility, it has multiple applications. But laser beam welding of duplex steels changes the balanced phase distribution in favor of ferrite. This results in a higher vulnerability to corrosion and a lower ductility. Herein, different powder combinations consisting of duplex and nickel for coating layers by laser metal deposition (LMD) are investigated. Afterward, laser tracks are welded, and the temperature cycles are measured. The ferrite content of the tracks is analyzed by feritscope, metallographic analysis, and electron backscatter diffraction. The goal is the development of a powder mixture allowing for a duplex microstructure in a two-step process, where first the edges of the weld partners are coated with the powder mixture by LMD and second those edges are laser beam welded. The powder mixture identified by the pretests is tested in the two-step process and analyzed by metallographic analysis, energy-dispersive X-ray spectroscopy, and Vickers hardness tests. The resulting weld seams show a balanced duplex microstructure with a homogenous nickel distribution and a hardness of the weld seam similar to the base material. KW - Duplex AISI 2205 KW - Laser metal deposition KW - Laser beam welding KW - Nickel KW - Stainless steels PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-547024 DO - https://doi.org/10.1002/adem.202101327 SN - 1438-1656 SP - 1 EP - 11 PB - Wiley-VCH CY - Weinheim AN - OPUS4-54702 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Giuseppe, Pignatelli A1 - Anne, Strasse A1 - Gumenyuk, Andrey A1 - Gornushkin, Igor B. T1 - Online monitoring of 3D printing of steel via optical emission spectroscopy N2 - Additive manufacturing by laser metal deposition (LMD) requires continuous online monitoring to ensure quality of printed parts. Optical emission spectroscopy (OES) is proposed for the online detection of printing defects by monitoring minute variations in the temperature of a printed spot during laser scan. A two-lens optical system is attached to a moving laser head and focused on a molten pool created on a substrate during LMD. The light emitted by the pool is collected by an ultraviolet–visible (UV–vis) spectrometer and processed. Two metrics are used to monitor variations in the surface temperature: the spectrally integrated emission intensity and correlation coefficient. The variations in the temperature are introduced by artificial defects, shallow grooves, and holes of various widths and diameters carved on a substrate surface. The metrics show sufficient sensitivity for revealing the surface defects, except for the smallest holes with an under-millimeter diameter. Additionally, numeric simulations are carried out for the detection of emission in the UV–vis and near-infrared (NIR) spectral ranges at various surface temperatures. It is concluded that both the metrics perform better in the NIR range. In general, this work demonstrates that spectrally resolved OES suits well for monitoring surface defects during 3D metal printing. KW - Process control KW - Additive manufacturing KW - Laser metal deposition KW - Optical emission spectroscopy KW - Optical sensor PY - 2022 DO - https://doi.org/10.1515/mt-2021-2082 VL - 64 IS - 1 SP - 24 EP - 32 PB - De Gruyter AN - OPUS4-54413 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gornushkin, Igor B. A1 - Pignatelli, Giuseppe A1 - Strasse, Anne T1 - Optical detection of defects during laser metal deposition: Simulations and experiment N2 - Laser metal deposition is a rapidly evolving method for additive manufacturing that combines high performance and simplified production routine. Quality of production depends on instrumental design and operational parameters that require constant control during the process. In this work, feasibility of using optical spectroscopy as a control method is studied via modeling and experimentally. A simplified thermal model is developed based on the time-dependent diffusion-conduction heat equation and geometrical light collection into detection optics. Intense light emitted by a laser-heated spot moving across a sample surface is collected and processed to yield the temperature and other temperature-related parameters. In a presence of surface defects the temperature field is distorted in a specific manner that depends on a shape and size of the defect. Optical signals produced by such the distorted temperature fields are simulated and verified experimentally using a 3D metal printer and a sample with artificially carved defects. Three quantities are tested as possible metrics for process monitoring: temperature, integral intensity, and correlation coefficient. The shapes of the simulated signals qualitatively agree with the experimental signals; this allows a cautious inference that optical spectroscopy is capable of detecting a defect and, possibly, predicting its character, e.g. inner or protruding. KW - Additive manufacturing KW - Laser metal deposition (LMD) KW - Thermal model KW - Optical sensor KW - Process control PY - 2021 DO - https://doi.org/10.1016/j.apsusc.2021.151214 SN - 0169-4332 VL - 570 SP - 1 EP - 13 PB - Elsevier CY - Amsterdam AN - OPUS4-53292 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Straße, Anne A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Preliminary study to investigate the applicability of optical strain measurement technique for the detection of hot cracks in laser metal deposited layers N2 - Laser metal deposition (LMD) as an additive manufacturing technique became increasingly important in recent years and thus the demand for component safety. This is the reason, for the need for reliable in-situ defect detection techniques. For laser beam weld seams an optical measurement technique based on an optical flow algorithm was successfully used to define the critical straining conditions that lead to hot cracking. This algorithm was adapted for bead-on-plate weld seams on LMD deposited layers of IN718 alloy while performing external strain on the specimen in an externally loaded hot cacking test facility. The resulting transversal hot cracks along the weld seam were localized via X-Ray inspection and the type of cracking confirmed by Scanning Electron Microscopy (SEM). The strain distribution was measured in the vicinity of the solidification front and correlated to the detected hot cracks. Based on the results this technique could be adopted for LMD experiments. T2 - 12th CIRP Conference on Photonic Technologies [LANE 2022] CY - Fürth, Germany DA - 04.09.2022 KW - Strain measurement KW - Optical flow KW - Laser Metal Deposition (LMD) KW - Critical strain PY - 2022 AN - OPUS4-55642 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Straße, Anne A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael ED - Schmidt, M. ED - Vollertsen, F. ED - Schmidt, B. M. T1 - Preliminary study to investigate the applicability of optical strain measurement technique for the detection of hot cracks in laser metal deposited layers N2 - Laser metal deposition (LMD) as an additive manufacturing technique became increasingly important in recent years and thus the demand for component safety. This is the reason, for the need for reliable in-situ defect detection techniques. For laser beam weld seams an optical measurement technique based on an optical flow algorithm was successfully used to define the critical straining conditions that lead to hot cracking. This algorithm was adapted for bead-on-plate weld seams on LMD deposited layers of IN718 alloy while performing external strain on the specimen in an externally loaded hot cacking test facility. The resulting transversal hot cracks along the weld seam were localized via X-Ray inspection and the type of cracking confirmed by Scanning Electron Microscopy (SEM). The strain distribution was measured in the vicinity of the solidification front and correlated to the detected hot cracks. Based on the results this technique could be adopted for LMD experiments. T2 - 12th CIRP Conference on Photonic Technologies [LANE 2022] CY - Fürth, Germany DA - 04.09.2022 KW - Laser Metal Deposition (LMD) KW - Strain measurement KW - Optical flow KW - Critical strain PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-556445 DO - https://doi.org/10.1016/j.procir.2022.08.034 VL - 111 SP - 335 EP - 339 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-55644 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Straße, Anne A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Study on Duplex Stainless Steel Powder Compositions forthe Coating of Thick Plates for Laser Beam Welding N2 - Duplex stainless steels combine the positive properties of its two phases, austenite and ferrite. Due to its good corrosion resistance, high tensile strength and good ductility it has multiple applications. But laser beam welding of duplex steels changes the balanced phase distribution in favor of ferrite. This results in a higher vulnerability to corrosion and a lower ductility. In this study different powder combinations consisting of duplex and nickel for coating layers by laser metal deposition are investigated. Afterwards laser tracks are welded, and the temperature cycles measured. The ferrite content of the tracks are analyzed by feritscope, metallographic analysis and Electron Backscatter Diffraction. The goal is the development of a powder mixture allowing for a duplex microstructure in a two-step process, where firstly the edges of the weld partners are coated with the powder mixture by LMD and secondly those edges are laser beam welded. The powder mixture identified by the pretests is tested in the two-step process and analyzed by metallographic analysis, energy dispersive X-ray spectroscopy and Vickers hardness tests. The resulting weld seams show a balanced duplex microstructure with a homogenous nickel distribution and a hardness of the weld seam similar to the base material. KW - Duplex AISI 2205 KW - Stainless Steel KW - Laser Beam Welding KW - Nickel KW - Laser Metal Deposition PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-554663 DO - https://doi.org/10.1002/adem.202101327 SN - 1438-1656 VL - 24 IS - 6 SP - 1 EP - 11 PB - Wiley-VCH CY - Weinheim AN - OPUS4-55466 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Straße, Anne A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael ED - Schmidt, M. ED - Vollertsen, F. ED - Govekar, E. T1 - LMD coatings as filler material for laser beam welded 30 mm thick plates N2 - The development of high energy laser sources enables single-pass welds of thick plates up to 30 mm, but often additional materials are needed to influence the properties of the weld seams. However, the homogenous distribution of filler materials in form of e.g. electrodes is only possible up to 7 mm while the elements are only traceable up to a depth of 14 mm. To overcome this problem a two-step process is used where first the edges of the weld partners are coated with the filler material by laser metal deposition (LMD) and afterwards are welded by laser beam. Single-pass welds with electromagnetic weld pool support of 30 mm thick S355 J2+N-plates with austenitic AISI 316L-coatings were investigated as well as the influence of the coatings to the penetration depth of the laser beam without electromagnetic weld pool support in double-sided joints. The weld seams were tested by X-ray inspection and cross sections. T2 - 11th CIRP Conference on Photonic Technologies [LANE 2020] CY - Online meeting DA - 07.09.2020 KW - Penetration depth KW - Laser metal deposition (LMD) KW - Laser beam welding KW - Filler material distribution PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-512790 DO - https://doi.org/10.1016/j.procir.2020.09.055 SN - 2212-8271 VL - 94 SP - 293 EP - 297 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-51279 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Straße, Anne A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - LMD coatings as filler material for laser beam welded 30 mm thick plates N2 - The development of high energy laser sources enables single-pass welds of thick plates up to 30 mm, but often additional materials are needed to influence the properties of the weld seams. However, the homogenous distribution of filler materials in form of e.g. electrodes is only possible up to 7 mm while the elements are only traceable up to a depth of 14 mm. To overcome this problem a two-step process is used where first the edges of the weld partners are coated with the filler material by laser metal deposition (LMD) and afterwards are welded by laser beam. Single-pass welds with electromagnetic weld pool support of 30 mm thick S355 J2+N-plates with austenitic AISI 316L-coatings were investigated as well as the influence of the coatings to the penetration depth of the laser beam without electromagnetic weld pool support in double-sided joints. The weld seams were tested by X-ray inspection and cross sections. T2 - 11th CIRP Conference on Photonic Technologies [LANE 2020] CY - Online meeting DA - 07.09.2020 KW - Penetration depth KW - Laser metal deposition (LMD) KW - Laser beam welding KW - Filler material distribution PY - 2020 AN - OPUS4-51276 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Straße, Anne A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Nahteigenschaftsverbesserung von dickwandigen laserstrahlgeschweißten Duplexblechen mittels pulveraufgetragenen Pufferschichten N2 - Duplexstähle finden aufgrund ihrer Eigenschaften, wie der guten Korrosionsbeständigkeit, einer hohen Festigkeit bei gleichzeitig guter Duktilität häufig industrielle Anwendung. Durch die hohen Abkühlraten beim Laserstrahlschweißen weisen Schweißnähte jedoch anstelle eines ausgeglichenen Duplexgefüges einen deutlich erhöhten Ferritanteil, im Vergleich zum Basiswerkstoff, auf. Dies führt zu einer verringerten Duktilität sowie Korrosionsbeständigkeit. Um dieses Problem zu lösen, wurde ein Prozess entwickelt, der auf einer Kantenbeschichtung mit nickelhaltigem Zusatzmaterial der zu fügenden Bleche mittels Laser-Pulver-Auftragschweißen (LPA) basiert. Die resultierenden Schweißnähte wurden zerstörend anhand von Schliffbildern, EDX-Aufnahmen, Härtemessungen und Kerbschlagbiegeversuchen geprüft. T2 - 40. Assistentenseminar der Füge- und Schweißtechnik CY - Braunlage, Germany DA - 25.09.2019 KW - Laser-Pulver-Auftragschweißen; Laserstrahlschweißen, Duplex, Pufferschichten PY - 2020 VL - 357 SP - 131 EP - 140 PB - DVS Media CY - Düsseldorf AN - OPUS4-50144 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Straße, Anne A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Kantenbeschichtung für das Laserstrahlschweißen dickwandiger Duplexstahl-Bleche N2 - Duplexstähle finden in vielen industriellen Bereichen Anwendung, dies ist nicht zuletzt ihren hervorragenden Eigenschaften, wie einer guten Korrosionsbeständigkeit, einer guten Duktilität bei trotzdem hoher Festigkeit, zuzuschreiben. Diese Eigenschaften werden jedoch durch das Schweißen, vor allem das Laserstrahlschweißen, beeinträchtigt, da die hohen Abkühlraten zu erhöhten Ferritanteilen im Schweißgut führen. Mit Hilfe eines zweistufigen Prozesses, bei dem die Kanten der Fügepartner vor dem Schweißen mit nickelhaltigem Pulver beschichtet werden, soll dieses Problem für dickwandige Bleche gelöst werden. In diesem Zusammenhang wurden verschiedene Prozessparameter für den Laser-Pulver-Auftragschweiß-Prozess untersucht sowie die defektfreie Schweißung dieser beschichteten Kanten mit unterschiedlichen Prozessgasen. KW - Pufferschichten KW - Laser-Pulver-Auftragschweißen KW - Laserstrahlschweißen KW - Duplex PY - 2020 VL - 72 IS - 7 SP - 382 EP - 387 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-50145 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -