TY - JOUR A1 - Mezera, Marek A1 - Alamri, S. A1 - Hendriks, W. A. P. M. A1 - Hertwig, Andreas A1 - Elert, Anna Maria A1 - Bonse, Jörn A1 - Kunze, T. A1 - Lasagni, A. F. A1 - Römer, G. R. B. E. T1 - Hierarchical micro-/nano-structures on polycarbonate via UV pulsed laser processing JF - Nanomaterials N2 - Hierarchical micro/-nanostructures were produced on polycarbonate polymer surfaces by employing a two-step UV-laser processing strategy based on the combination of Direct Laser Interference Patterning (DLIP) of gratings and pillars on the microscale (3 ns, 266 nm, 2 kHz) and subsequently superimposing Laser-induced Periodic Surface Structures (LIPSS; 7–10 ps, 350 nm, 100 kHz) which adds nanoscale surface features. Particular emphasis was laid on the influence of the direction of the laser beam polarization on the morphology of resulting hierarchical surfaces. Scanning electron and atomic force microscopy methods were used for the characterization of the hybrid surface structures. Finite-difference time-domain (FDTD) calculations of the laser intensity distribution on the DLIP structures allowed to address the specific polarization dependence of the LIPSS formation observed in the second processing step. Complementary chemical analyzes by micro-Raman spectroscopy and attenuated total reflection Fourier-transform infrared spectroscopy provided in-depth information on the chemical and structural material modifications and material degradation imposed by the laser processing. It was found that when the linear laser polarization was set perpendicular to the DLIP ridges, LIPSS could be formed on top of various DLIP structures. FDTD calculations showed enhanced optical intensity at the topographic maxima, which can explain the dependency of the morphology of LIPSS on the polarization with respect to the orientation of the DLIP structures. It was also found that the degradation of the polymer was enhanced for increasing accumulated fluence levels. KW - Direct laser interference patterning KW - Laser-induced periodic surface structures (LIPSS) KW - Polycarbonate KW - Hierarchical structures KW - Surface functionalization PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-509101 DO - https://doi.org/10.3390/nano10061184 SN - 2079-4991 VL - 10(6) IS - Special issue "Laser-generated periodic nanostructures" SP - 1184-1 EP - 1184-19 PB - MDPI CY - Basel AN - OPUS4-50910 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Mielentz, Frank A1 - Milmann, Boris A1 - Wöstmann, Jens A1 - Krause, Martin A1 - Maierhofer, Christiane A1 - Römer, A. A1 - Völkel, W. T1 - Untersuchungen zur zerstörungsfreien Bestimmung des Hohlraumgehaltes von Asphaltschichten T2 - Fachtagung Bauwerksdiagnose 2006 - Praktische Anwendungen Zerstörungsfreier Prüfungen T2 - DGZfP-Fachtagung Bauwerksdiagnose "Praktische Anwendungen Zerstörungsfreier Prüfungen" CY - Berlin, Deutschland DA - 2006-02-22 KW - Asphalt KW - Hohlraumgehalt KW - Zerstörungsfreie Prüfung KW - Ultraschallverfahren KW - Ultraschall-Rückstreuung KW - Radarverfahren PY - 2006 SN - 3-931381-71-4 SP - 1(?) EP - 9(?) PB - DGZfP CY - Berlin AN - OPUS4-12116 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Peruzzi, N. A1 - Galli, S. A1 - Helmholz, H. A1 - Kardjilov, N. A1 - Krüger, D. A1 - Markötter, Henning A1 - Moosmann, J. A1 - Orlov, D. A1 - Prgomet, Z. A1 - Willumeit-Römer, R. A1 - Wennerberg, A. A1 - Bech, M. T1 - Multimodal ex vivo methods reveal that Gd-rich corrosion byproducts remain at the implant site of biodegradable Mg-Gd screws JF - Acta Biomaterialia N2 - Extensive research is being conducted on magnesium (Mg) alloys for bone implant manufacturing, due to their biocompatibility, biodegradability and mechanical properties. Gadolinium (Gd) is among the most promising alloying elements for property control in Mg alloy implants; however, its toxicity is contro- versial. Investigating Gd behavior during implant corrosion is thus of utmost importance. In this study, we analyzed the degradation byproducts at the implant site of biodegradable Mg-5Gd and Mg-10Gd implants after 12 weeks healing time, using a combination of different imaging techniques: histology, energy-dispersive x-ray spectroscopy (EDX), x-ray microcomputed tomography (μCT) and neutron μCT. The main finding has been that, at the healing time in exam, the corrosion appears to have involved only the Mg component, which has been substituted by calcium and phosphorus, while the Gd remains localized at the implant site. This was observed in 2D by means of EDX maps and extended to 3D with a novel application of neutron tomography. X-ray fluorescence analysis of the main excretory organs also did not reveal any measurable accumulation of Gd, further reinforcing the conclusion that very limited or no removal at all of Gd-alloy happened during degradation. KW - Magnesium-gadolinium alloy KW - Biodegradable implant KW - Multimodal analysis KW - Energy-dispersive x-ray spectroscopy KW - Micro-computed tomography PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-535910 DO - https://doi.org/10.1016/j.actbio.2021.09.047 SN - 1742-7061 SP - 1 EP - 10 PB - Elsevier Ltd. AN - OPUS4-53591 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kaur, I. A1 - Ellis, L.-J. A1 - Romer, I. A1 - Tantra, R. A1 - Carriere, M. A1 - Allard, S. A1 - Mayne-L'Hermite, M. A1 - Minelli, C. A1 - Unger, Wolfgang A1 - Potthoff, A. A1 - Rades, Steffi A1 - Valsami-Jones, E. T1 - Dispersion of nanomaterials in aqueous media: Towards protocol optimization JF - Journal of Visualized Experiments N2 - The sonication process is commonly used for de-agglomerating and dispersing nanomaterials in aqueous based media, necessary to improve homogeneity and stability of the suspension. In this study, a systematic step-wise approach is carried out to identify optimal sonication conditions in order to achieve a stable dispersion. This approach has been adopted and shown to be suitable for several nanomaterials (cerium oxide, zinc oxide, and carbon nanotubes) dispersed in deionized (DI) water. However, with any change in either the nanomaterial type or dispersing medium, there needs to be optimization of the basic protocol by adjusting various factors such as sonication time, power, and sonicator type as well as temperature rise during the process. The approach records the dispersion process in detail. This is necessary to identify the time Points as well as other above-mentioned conditions during the sonication process in which there may be undesirable changes, such as damage to the particle surface thus affecting surface properties. Our goal is to offer a harmonized approach that can control the Quality of the final, produced dispersion. Such a guideline is instrumental in ensuring dispersion quality repeatability in the nanoscience community, particularly in the field of nanotoxicology. KW - Dispersion of nanomaterials KW - Aqueous media KW - Protocol development PY - 2017 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-435886 UR - https://www.jove.com/video/56074 DO - https://doi.org/10.3791/56074 SN - 1940-087X IS - 130 SP - e560741, 1 EP - e560741, 23 PB - MyJove Corp. CY - Cambridge, MA, USA AN - OPUS4-43588 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Goebbels, K. A1 - Römer, Manfred A1 - Crostack, H.-A. T1 - Quantitativer Vergleich verschiedener Ultraschall-Prüfverfahren zur Verbesserung des Signal-Rausch-Abstandes beim Vorliegen kohärenten Untergrundes JF - Materialprüfung = Materials testing PY - 1979 SN - 0025-5300 VL - 21 IS - 8 SP - 261 EP - 267 PB - Carl Hanser Verlag CY - München AN - OPUS4-9177 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -