TY - JOUR A1 - Ruffini, A. A1 - Le Bouar, Y. A1 - Finel, A. A1 - Epishin, A. I. A1 - Fedelich, Bernard A1 - Feldmann, Titus A1 - Viguier, B. A1 - Poquillon, D. T1 - Dislocations interacting with a pore in an elastically anisotropic single crystal nickel-base superalloy during hot isostatic pressing N2 - The formation of pores in CMSX-4 nickel based superalloys is detrimental to the service life of the material. A way to avoid the problem is to treat the superalloys under Hot Isostatic Pressing (HIP), which enables a large volume fraction of pores to be annihilated. This paper aims to understand the contribution of plastic activity related to the gliding of dislocations on the pore annihilation. Simulations based on a phase-field model of dislocation are performed and make it possible to consider the strong anisotropy of the CMSX-4 under HIP conditions in conjunction to the strong elastic heterogeneity introduced by the pore. For pores with a radius of few micrometers, it is shown that edge parts of dislocation lines that present an extra half atomic plane oriented towards the pore are stacked above and under it in the direction which is perpendicular to their slip-planes, causing an increase of the number of dislocation along the four octahedral directions of the FCC single crystal which intersect the pore center. Results are streamlined within the isotropic elastic theory of dislocations. Effects of elastic anisotropy and dislocation reactions are also investigated in order to specify what would be the dislocation configuration around a pore in CMSX-4 under HIP conditions. Notably, the elastic anisotropy is shown to significantly modify the arrangement of dislocations close to the pore equator. Simulations also allow for the characterization of pore/dislocation interactions when dislocations are involved in Low Angle Boundaries as experimentally observed. KW - HIP KW - Superalloys KW - Dislocation KW - Pore KW - Phase-field PY - 2022 DO - https://doi.org/10.1016/j.commatsci.2021.111118 SN - 0927-0256 VL - 204 SP - 1 EP - 14 PB - Elsevier CY - Amsterdam AN - OPUS4-54220 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Epishin, A. I. A1 - Fedelich, Bernard A1 - Viguier, B. A1 - Schriever, Sina A1 - Svetlov, I. L. A1 - Petrushin, N. V. A1 - Saillard, R. A1 - Proietti, A. A1 - Poquillon, D. A1 - Chyrkin, A. T1 - Creep of single-crystals of nickel-base γ-alloy at temperatures between 1150 °C and 1288 °C N2 - A γ-analogue of the superalloy CMSX-4 that does not contain the strengthening γ′ -phase and only consists of the γ-solid solution of nickel has been designed, solidified as single-crystals of different orientations, and tested under creep conditions in the temperature range between 1150 and 1288 °C. The tests have revealed a very high creep anisotropy of this alloy, as was previously found for CMSX-4 at supersolvus temperature of 1288 °C. This creep anisotropy could be explained by the dominance of 〈011〉{111} octahedral slip. Furthermore, the analysis of the creep data has yielded a high value of the creep activation energy, Qc≈442 kJ/mol, which correlates with the high activation energy of Re diffusion in Ni. This supports the hypothesis that dislocation motion in the γ-matrix of Re-containing superalloys is controlled by the diffusion of the Re atoms segregating at the dislocation core. The Norton stress exponent n is close to 5, which is a typical value for pure metals and their alloys. The absence of γ′ -reprecipitation after high-temperature creep tests facilitates microstructural investigations. It has been shown by EBSD that creep deformation results in an increasing misorientation of the existing low angle boundaries. In addition, according to TEM, new low angle boundaries appear due to reactions of the a/2 〈011〉 mobile dislocations and knitting of new networks. KW - Nickel alloys KW - Single-crystals KW - Creep KW - Electron microscopy KW - Deformation mechanisms PY - 2021 DO - https://doi.org/10.1016/j.msea.2021.141880 SN - 0921-5093 VL - 825 SP - 1 EP - 13 PB - Elsevier CY - Amsterdam AN - OPUS4-53132 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Epishin, A. A1 - Bokstein, B. A1 - Svetlov, I. A1 - Fedelich, Bernard A1 - Feldmann, Titus A1 - Le Bouar, Y. A1 - Ruffini, A. A1 - Finel, A. A1 - Viguier, B. A1 - Poquillon, D. T1 - A vacancy model for pore annihilation during hot isostatic pressing of single-crystal nickel-base superalloys N2 - An improved diffusion model is proposed for pore annihilation during HIP of single-crystal nickel-base superalloys. The model assumes the pore dissolution by emission of vacancies and their sink to the low angle boundaries. Calculation, considering distribution of the pore sizes, predicts the kinetics of pore annihilation similar to the experimental one. KW - Single crystal superalloys KW - Hot isostatic pressing (HIP) KW - Porosity KW - Diffusion KW - Vacancies PY - 2018 DO - https://doi.org/10.1134/S2075113318010100 SN - 2075-1133 VL - 9 IS - 1 SP - 57 EP - 65 PB - Pleiades Publishing, Ltd. AN - OPUS4-43990 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Epishin, A. A1 - Fedelich, Bernard A1 - Nolze, Gert A1 - Schriever, Sina A1 - Feldmann, Titus A1 - Farzik Ijaz, M. A1 - Viguier, B. A1 - Poquillon, D. A1 - Le Bouar, Y. A1 - Ruffini, A. A1 - Finel, A. T1 - Creep of single crystals of nickel-based superalloys at ultra-high homologous temperature N2 - The creep behavior of single crystals of the nickel-based superalloy CMSX-4 was investigated at 1288 °C, which is the temperature of the hot isostatic pressing treatment applied to this superalloy in the industry. It was found that at this super-solvus temperature, where no gammaPrime-strengthening occurs, the superalloy is very soft and rapidly deforms under stresses between 4 and 16 MPa. The creep resistance was found to be very anisotropic, e.g., the creep rate of [001] crystals was about 11 times higher than that of a [111] crystal. The specimens of different orientations also showed a very different necking behavior. The reduction of the cross-sectional area psi of [001] crystals reached nearly 100 pct, while for a [111] crystal psi = 62 pct. The EBSD analysis of deformed specimens showed that despite such a large local strain the [001] crystals did not recrystallize, while a less deformed [111] crystal totally recrystallized within the necking zone. The recrystallization degree was found to be correlated with deformation behavior as well as with dwell time at high temperature. From the analysis of the obtained results (creep anisotropy, stress dependence of the creep rate, traces of shear deformation, and TEM observations), it was concluded that the main strain contribution resulted from <01-1>{111} octahedral slip. T2 - 3rd European Conference on Superalloys (‘Eurosuperalloys 2018’) CY - Oxford, UK DA - 9.9.2018 KW - Single-crystal KW - Superalloy KW - Creep KW - Isostatic hot pressing (HIP) PY - 2018 DO - https://doi.org/10.1007/s11661-018-4729-6 SN - 1073-5623 SN - 1543-1940 VL - 49A IS - 9 SP - 3973 EP - 3987 PB - Springer Sciences & Business Media CY - New York, NY AN - OPUS4-45660 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Vattré, A. A1 - Fedelich, Bernard T1 - On the relationship between anisotropic yield strength and internal stresses in single crystal superalloys N2 - The present work focuses on the cubic slip phenomenon in single crystal superalloys with a high fraction of γ' precipitates at high temperature. The macroscopically apparent cubic slip mechanism is known to significantly reduce the tensile and creep strength of <1 1 1> oriented specimens. However, recent results obtained by 3D dislocation dynamics (Vattré et al., 2009) suggest a new interpretation of the so-called pseudo-cubic slip related to the nature of the dislocation network formation at the interfaces. These results are taken into account in a micromechanical model to improve the estimation of the strain hardening anisotropy. In accordance with the discrete simulations, it is shown that a key role is played by the combination of the activated octahedral slip systems as a function of the crystal orientation. In the <1 1 1> case, the contribution of the activated systems to kinematical hardening compensate, whereas strain hardening remains high for the <0 0 1> case. The experimental dependence of plastic flow on the orientation is also explained at the dislocation-scale mechanisms. Results are presented for the alloy CMSX-4 in several orientations. KW - Nickel-base superalloys KW - High-temperature deformation KW - Micromechanical modeling KW - Strengthening mechanisms PY - 2011 DO - https://doi.org/10.1016/j.mechmat.2011.07.007 SN - 0167-6636 SN - 1872-7743 VL - 43 IS - 12 SP - 930 EP - 951 PB - Elsevier CY - Amsterdam AN - OPUS4-24927 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Apel, E. A1 - Deubener, J. A1 - Bernard, A. A1 - Müller, Ralf A1 - Kappert, H. A1 - Rheinberger, V. A1 - Höland, W. T1 - Phenomena and mechanisms of crack propagation in glass-ceramics N2 - Lithium disilicate, leucite and apatite glass-ceramics have become state-of-the-art framework materials in the fabrication of all-ceramic dental restorative materials. The goal of this study was to examine the crack propagation behaviour of these three known glass-ceramic materials after they have been subjected to Vickers indentation and to characterize their crack opening profiles (δmeas vs. (a-r)). For this purpose, various methods of optical examination were employed. Optical microscopy investigations were performed to examine the crack phenomena at a macroscopic level, while high-resolution techniques, such as scanning electron microscopy (SEM) and atomic force microscopy (AFM), were employed to investigate the crack phenomena at a microscopic level. The crack patterns of the three glass-ceramics vary from fairly straightforward to more complex, depending on the amount of residual glass matrix present in the material. The high-strength lithium disilicate crystals feature a high degree of crosslinking, thereby preventing crack propagation. In this material, the crack propagates only through the residual glass phase, which constitutes 30%–40% by volume. Having a high glass content of more than 65% by volume, the leucite and apatite glass-ceramics show far more complex crack patterns. Cracks in the leucite glass-ceramic propagate through both the glass and crystal phase. The apatite glass-ceramic shows a similar crack behaviour as an inorganic–organic composite material containing nanoscale fillers, which are pulled out in the surroundings of the crack tip. The observed crack behaviour and the calculated View the MathML source values of the three types of glass-ceramics were compared to the Kkic values determined according to the SEVNB method. KW - Glass KW - Viscosity KW - Water content PY - 2008 DO - https://doi.org/10.1016/j.jmbbm.2007.11.005 SN - 1751-6161 VL - 1 IS - 4 SP - 313 EP - 325 PB - Elsevier CY - Amsterdam AN - OPUS4-18308 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scholz, A. A1 - Nazmy, M. A1 - Fedelich, Bernard A1 - Tinga, T. A1 - Huls, R. T1 - Modelling of microstructure and mechanical property changes in gas turbine alloys T2 - 9th Liège conference: Materials for advanced power engineering 2010 CY - Liège, Belgium DA - 2010-09-27 KW - Nickel base superalloys KW - Degradation KW - Modelling KW - Microstructure KW - Mechanical properties PY - 2010 SP - 567 EP - 587 AN - OPUS4-22261 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Epishin, A. A1 - Fedelich, Bernard A1 - Link, T. A1 - Feldmann, Titus A1 - Svetlov, I.L. T1 - Pore annihilation in a single-crystal nickel-base superalloy during hot isostatic pressing: Experiment and modelling N2 - Pore annihilation during hot isostatic pressing (HIP) was investigated in the single-crystal nickel-base superalloy CMSX-4 experimentally by interrupted HIP tests at 1288 °C/103 MPa. The kinetics of pore annihilation was determined by density measurement and quantitative metallography. Transmission electron microscopy of a HIPed specimen showed that the pores shrink via dislocation movement on octahedral glide planes. Theoretically pore closure under HIP condition was modelled by the finite element method using crystal plasticity and large strain theories. The modelling gives a similar kinetics of pore annihilation as observed experimentally, however somewhat higher annihilation rate. KW - Nickel based superalloys KW - Electron microscopy KW - Crystal plasticity KW - Bulk deformation KW - Finite element method PY - 2013 DO - https://doi.org/10.1016/j.msea.2013.08.034 SN - 0921-5093 SN - 1873-4936 VL - 586 SP - 342 EP - 349 PB - Elsevier CY - Amsterdam AN - OPUS4-29418 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Feldmann, Titus A1 - Fedelich, Bernard A1 - Epishin, A. T1 - Simulation of Hot Isostatic Pressing in a Single-Crystal Ni Base Superalloy with the Theory of Continuously Distributed Dislocations Combined with Vacancy Diffusion N2 - Single-crystal components made of nickel base superalloys contain pores after casting and homogenization heat treatment. Hot isostatic pressing (HIP), which is carried above the γ' -solvus temperature of the alloy, is industrially applied to reduce porosity. A modeling of HIP based on continuously distributed dislocations is developed in a 2D setting. Glide and climb of straight-edge dislocations, as well as vacancy diffusion, are the deformation mechanisms taken into account. Thereby, dislocation glide is controlled by dragging a cloud of large atoms, and climb is controlled by vacancy diffusion. Relying on previous investigations of the creep behavior at HIP temperatures, it is assumed that new dislocations are nucleated at low-angle boundaries (LAB) and move through subgrains until they either reach the opposite LABs or react with other dislocations and annihilate. Vacancies are created at the pore surface and diffuse through the alloy until they are either consumed by climbing dislocations or disappear at the LABs. The field equations are solved by finite elements. It is shown that pore shrinking is mostly controlled by vacancy diffusion as the shear stresses at the LABs are too low to nucleate a sufficient amount of dislocations. KW - Nickel-base superalloys KW - HIP KW - Dislocation KW - Creep KW - Model PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-542309 DO - https://doi.org/10.1002/adem.202101341 VL - 2022 PB - Wiley AN - OPUS4-54230 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Epishin, A. A1 - Camin, B. A1 - Hansen, L. A1 - Heuser, M. A1 - Lopez-Galilea, I. A1 - Ruttert, B. A1 - Theisen, W. A1 - Fedelich, Bernard T1 - Refinement and Experimental Validation of a Vacancy Model of Pore Annihilation in Single-Crystal Nickel-Base Superalloys during Hot Isostatic Pressing N2 - Initially, as-cast and homogenized single crystals of nickel-base superalloy CMSX-4 are subjected to hot isostatic pressing at 1288 °C. Two series of experiments are conducted: under the same pressure of 103 MPa but with different durations, between 0.5 and 6 h, and under different pressures, between 15 and 150 MPa, but for the same time of 0.5 h. The porosity annihilation is investigated metallographically and by high-resolution synchrotron X-ray tomography. The obtained experimental results are compared with the predictions of the vacancy model proposed recently in the group. Herein, the model is further refined by coupling with X-ray tomography. The model describes the evolution of the pore arrays enclosed in the 3D synchrotron tomograms during hot isostatic pressing and properly predicts the time and stress dependences of the pore annihilation kinetics. The validated model and the obtained experimental results are used for selecting the optimal technological parameters such as applied pressure and processing time KW - Superalloys KW - HIP KW - Single-Crystal KW - Diffusion PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-526859 DO - https://doi.org/10.1002/adem.202100211 VL - 23 IS - 7 SP - 211 AN - OPUS4-52685 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -