TY - CONF A1 - Weltschev, Margit T1 - Innovative korrosionsbeständige höherlegierte Tankwerkstoffe T2 - Gefahrgut-Technik-Tage Berlin 2004 CY - Berlin, Germany DA - 2004-11-25 PY - 2004 AN - OPUS4-5138 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit T1 - Innovative korrosionsbeständige höherlegierte Tankwerkstoffe T2 - 7. Gefahrgut-Technik-Tage (GTT) CY - Berlin, Deutschland DA - 2004-11-25 PY - 2004 VL - 7 SP - 52 EP - 60 PB - Storck CY - Hamburg AN - OPUS4-4844 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit A1 - Werner, Jan A1 - Heming, Frank A1 - Jochems, Frank T1 - Impact of biocomponents in the fuel and heating oil on the compatibility of sealing materials N2 - The objective of this research was to determine the resistance of frequently used sealing materials such as FKM, FVMQ, VMQ, EPDM, CR, CSM, IIR, PA, NBR and PUR in fuels and heating oil with and without admixtures of biogenic sources such as E10, diesel fuel with 5 % biodiesel, non-aged and 2 year aged B10 (heating oil with 10 % biodiesel), pure diesel, standard heating oil and premium grade fuel Super plus at 20 °C, 40 °C and 70 °C. Mass, tensile strength and breaking elongation of the test specimens were determined before and after the exposure for 84 days in the fuels. The visual examination of some elastomer test specimens clearly showed the great volume increase until break or partial dissolution. Shore hardness A and D (for PA) were determined before and after exposure of the test specimens in the biofuels for 42 days. There is not determined a threshold for the reduction in tensile properties and Shore hardness in the international standards. Therefore a threshold of 15 % was determined for the evaluation of the compatibility. In summary, it can be therefore stated that the chemical resistance of the fluoropolymers FKM and FVMQ in fuels and biofuels is the best one. T2 - CORROSION 2016 CY - Vancouver, Kanada DA - 06.03.2016 KW - sealing materials KW - compatibility KW - biofuels PY - 2016 SP - Paper No. 7307, 1 EP - 12 PB - NACE INTERNATIONAL, Publications Division CY - Houston, Texas 77084 (USA) AN - OPUS4-35622 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit A1 - Werner, Jan A1 - Heming, Frank A1 - Jochems, Frank T1 - Impact of biocomponents in the fuel and heating oil on the compatibility of sealing materials N2 - The objective of this research was to determine the resistance of frequently used sealing materials such as FKM, FVMQ, VMQ, EPDM, CR, CSM, IIR, PA, NBR and PUR in fuels and heating oil with and without admixtures of biogenic sources such as E10, diesel fuel with 5 % biodiesel, non-aged and 2 year aged B10 (heating oil with 10 % biodiesel), pure diesel, standard heating oil and premium grade fuel Super plus at 20 °C, 40 °C and 70 °C. Mass, tensile strength and breaking elongation of the test specimens were determined before and after the exposure for 84 days in the fuels. The visual examination of some elastomer test specimens clearly showed the great volume increase until break or partial dissolution. Shore hardness A and D (for PA) were determined before and after exposure of the test specimens in the biofuels for 42 days. There is not determined a threshold for the reduction in tensile properties and Shore hardness in the international standards. Therefore a threshold of 15 % was determined for the evaluation of the compatibility. In summary, it can be therefore stated that the chemical resistance of the fluoropolymers FKM and FVMQ in fuels and biofuels is the best one. T2 - CORROSION 2016 CY - Vancouver, Kanada DA - 06.03.2016 KW - compatibility KW - sealing materials KW - biofuels PY - 2016 AN - OPUS4-35623 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit A1 - Otremba, Frank A1 - Sklorz, Christian A1 - Rehfeldt, Rainer T1 - Impact of biocomponents in the fuel and heating oil on the compatibility of fluorocarbon rubber under compressed conditions N2 - Materials compatibility is a major concern whenever the fuel composition is changed. The question arises of whether sealing materials are resistant to fuels with bioethanol and biodiesel (rapeseed oil fatty acid methyl ester). Previous research considered the resistance of frequently used sealing materials such as FKM (fluorocarbon rubber), FVMQ (methyl-fluoro-silicone rubber), VMQ (methyl-vinyl-silicone rubber), EPDM (ethylene-propylene-diene rubber), CR (chloroprene rubber), CSM (chlorosulfonated polyethylene), IIR (butyl rubber), PA (polyamides), NBR (acrylonitrile-butadiene rubber) and PUR (polyester urethane rubber) in fuels and heating oil with admixtures of biogenic substances such as biodiesel and B10 (heating oil with 10 % biodiesel) under purely static conditions. The aim of this study was to evaluate the fluorocarbon rubber performance under compressed conditions. For the investigations, the mass and the compression set of the FKM test specimens were determined before and after exposure for 3, 7, 14, 28, 56 and 90 days in E10 (fuel with 10 % ethanol), E85 (fuel with 85 % ethanol), biodiesel (fatty acid methyl ester, FAME), Super (fuel with max. 5 % ethanol), diesel fuel with max. 5 % biodiesel, pure diesel fuel, Super Plus (fuel without ethanol) and heating oil with 10 % biodiesel (B10) at 40 °C according to ISO 815-1 “Rubber, vulcanized or thermoplastic - determination of compression set – Part 1: At ambient or elevated temperatures”. The compression set test belongs beside the determination of the Shore hardness, the density and the tensile properties to the basic test methods for elastomers. It was measured in regular time intervals up to a re-drying of more than 90 days after relaxation of test specimens. For comparison, FKM test specimens were exposed without fuel under compressed conditions at 40 °C. The highest mass increase of FKM test specimens was measured after 90 days exposure in E10 by 9 %, followed by 8 % in Super fuel, by 4 % in E85 and by 0.6 % in biodiesel. Mass increase and swelling of the test specimens in E10 and Super fuel with max. 5 % ethanol had an influence on the compression set values which were subject to high fluctuations in comparison to the values obtained after exposure to other fuels such as biodiesel, diesel fuel and B10. The results of the present work confirmed the higher swelling of the elastomers such as FKM in E10 obtained under static condition. It can be concluded on the basis of the mass increase and compression set values that FKM is resistant in all fuels under compressed conditions at 40 °C. T2 - EUROCORR 2018 CY - Krakow, Poland DA - 09.09.2018 KW - Sealing materials KW - Compression set KW - Compatibility KW - Fuels KW - Heating oil KW - Biodiesel KW - Bioethanol PY - 2018 AN - OPUS4-45935 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weltschev, Margit A1 - Bäßler, Ralph T1 - Höherlegieren gegen Korrodieren - Besondere Stähle und Legierungen für Tanks PY - 2002 SN - 0016-5808 VL - 47 IS - 11 SP - 18 EP - 20 PB - Storck CY - Hamburg AN - OPUS4-1635 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weltschev, Margit T1 - Hochlegierte Sonderedelstähle und Nickelbasislegierungen für den Behälterbau PY - 2001 SN - 1434-9728 SN - 1436-4948 SN - 0372-2457 SN - 0376-1185 VL - 42 IS - 7-8 SP - 55 EP - 57 PB - Springer-VDI-Verl. CY - Düsseldorf AN - OPUS4-1209 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baensch, Franziska A1 - Baer, Wolfram A1 - Chruscicki, Sebastian A1 - Habib, Abdel Karim A1 - Homann, Tobias A1 - Hussels, Maria-Teresa A1 - Prager, Jens A1 - Schmidt, Dirk A1 - Stajanca, Pavol A1 - Weltschev, Margit A1 - Wossidlo, Peter T1 - Feasibility study - Continuous monitoring of pipes using distributed acoustic and fibre optic sensors N2 - The feasibility study „AGIFAMOR. Ageing infrastructures – distributed acoustic monitoring of pipes” is an interdisciplinary research project at BAM internally financed from 2015 to 2018. Therefore, the quite young fibre optic sensing technology of distributed acoustic sensing (DAS) was investigated to possibly be extended towards a global condition monitoring system for pipelines operating in real time. DAS is a highly dynamic fibre optic sensing technology based on the method of coherent optical time domain reflectometry (C-OTDR). DAS allows capturing strain changes in the range of kHz. For the experimental work, the most suitable application yielding an optimum sensitivity was proven by wrapping a standard single-mode silica fibre around the pipe. The DAS sensitivity was investigated regarding the detection of 1) incidents that initiate propagation of acoustic waves in the pipe wall, 2) changes inside the pipeline causing altered flow and 3) damage development in the pipe wall. Therefore, several testing setups in laboratory as well as in real scale were realized. For comparison purposes, experiments were accompanied by acoustic emission analyses and by measurements with accelerometers. DAS was found to be very sensitive to gas ignition and its propagation across the pipe. Furthermore, the ability of DAS to detect and localize acoustic signals associated with pipeline leakage was demonstrated. The detection of crack formation and propagation within the pipe wall by means of DAS was studied during bending tests on several pipe segments, but was not proven so far with certainty. As expected, these studies turned out as the most difficult challenge due to the random occurrence and transient nature of microscopic damage phenomena. T2 - Proceedings of the International Symposium on Structural Health Monitoring and Nondestructive Testing CY - Saarbrücken, Germany DA - 04.10.2018 KW - Accelerometers KW - Acoustic emission KW - Fibre optic acoustic sensing KW - Continous monitoring KW - Bending tests on pipe segments KW - Leak detection PY - 2018 SP - Paper 21 AN - OPUS4-46375 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit A1 - Bäßler, Ralph T1 - Evaluation of the Resistance of Metallic Materials under the Influence of Biofuels N2 - Changes in fuel composition and the introduction of alternative fuels often create problems of corrosion and degradation in materials. The objective of this research was to determine the corrosion behaviour of commercial metallic tank materials (unalloyed steels, austenitic CrNi- and CrNiMo-steels, aluminium and its alloys) in fuels and heating oil with admixtures of biogenic sources, such as gasoline with addition of ethanol (E10, E85), pure biodiesel and heating oil with 10 % biodiesel (B10). Metallic tank materials were evaluated as resistant in a liquid if the annual corrosion rate due to uniform corrosion did not exceed 0.1 mm/year, and localized corrosion effects in the form of pitting corrosion, stress corrosion cracking and crevice corrosion did not occur. The corrosion rates of the tank materials after exposure to E10, E85, non-aged and two-year aged pure biodiesel, and non-aged and one-year aged heating oil B10 for four weeks at 50 °C, according to DIN 50905/4, were well below the limit of 0.1 mm/year. For the unalloyed steels, the formation of rust was observed independently of the biofuels amount of ageing. U-bend specimens made of unalloyed steel were not damaged in form of stress corrosion cracking in all test fuels at this test temperature. T2 - CORROSION 2017 CY - New Orleans, LA, USA DA - 26.03.2017 KW - Biodiesel KW - Bioethanol KW - Tank materials KW - Corrosion resistance KW - Stress corrosion cracking PY - 2017 SP - Paper No 8854, 1 EP - 12 PB - NACE International Publications Division CY - Houston, Texas, USA AN - OPUS4-39638 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit A1 - Bäßler, Ralph T1 - Evaluation of the resistance of metallic materials under the influence of biofuels N2 - Changes in fuel composition and the introduction of alternative fuels often create problems of corrosion and degradation in materials. The objective of this research was to determine the corrosion behaviour of commercial metallic tank materials (unalloyed steels, austenitic CrNi- and CrNiMo-steels, aluminium and its alloys) in fuels and heating oil with admixtures of biogenic sources, such as gasoline with addition of ethanol (E10, E85), pure biodiesel and heating oil with 10 % biodiesel (B10). Metallic tank materials were evaluated as resistant in a liquid if the annual corrosion rate due to uniform corrosion did not exceed 0.1 mm/year, and localized corrosion effects in the form of pitting corrosion, stress corrosion cracking and crevice corrosion did not occur. The corrosion rates of the tank materials after exposure to E10, E85, non-aged and two-year aged pure biodiesel, and non-aged and one-year aged heating oil B10 for four weeks at 50 °C, according to DIN 50905/4, were well below the limit of 0.1 mm/year. For the unalloyed steels, the formation of rust was observed independently of the biofuels amount of ageing. U-bend specimens made of unalloyed steel were not damaged in form of stress corrosion cracking in all test fuels at this test temperature. T2 - CORROSION 2017 CY - New Orleans, LA, USA DA - 26.03.2017 KW - Biodiesel KW - Bioethanol KW - Tank materials KW - Corrosion resistance KW - Stress corrosion cracking PY - 2017 AN - OPUS4-39642 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit A1 - Bäßler, Ralph T1 - Evaluation of the resistance of metallic and polymeric materials used for tanks for the transport of dangerous goods T2 - ACHEMA CY - Frankfurt am Main, Germany DA - 2012-06-20 PY - 2012 AN - OPUS4-26089 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit A1 - Bäßler, Ralph T1 - Evaluation of the resistance of highly alloyed stainless steels and nickel alloys for the transport of dangerous goods T2 - 9th International Conference and Exhibition "Problem of Corrosion and Corrosion Protection of Materials" CY - Lviv, Ukraine DA - 2008-06-10 KW - Corrosion resistance KW - High alloyed stainless steel KW - Nickel-based alloy KW - Transport KW - Dangerous goods PY - 2008 SN - 0430-6252 N1 - Serientitel: Physico Chemical Mechanics of Materials – Series title: Physico Chemical Mechanics of Materials IS - Special Issue No. 7 SP - 17 EP - 28 CY - Lviv, Ukraine AN - OPUS4-17623 LA - rus AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit A1 - Bäßler, Ralph A1 - Werner, H. A1 - Alves, H. T1 - Evaluation of the resistance of alloy 31 and alloy 59 for the transport of mixed acids in tanks T2 - EUROCORR 2007 CY - Freiburg im Breisgau, Germany DA - 2007-09-09 KW - Korrosionsbeständigkeit KW - Höherlegierte Werkstoffe KW - Mischsäuren KW - BAM-Liste KW - BAM-List KW - Acid corrosion KW - High-alloyed stainless steel KW - Nickel-base alloy KW - Corrosion test PY - 2007 N1 - Serientitel: EFC-Event – Series title: EFC-Event IS - 289 SP - 1 EP - 10 PB - DECHEMA CY - Frankfurt am Main AN - OPUS4-15853 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit A1 - Pötzsch, Sina A1 - Bäßler, Ralph T1 - Entwicklung einer Prüfmethode zur Bewertung der Materialbeständigkeit von Bauteilen in Mitteldestillatanwendungen N2 - Für Bauteile (Komponenten) von Versorgungsanlagen für flüssige Brenn- und Kraftstoffe muss die Beständigkeit der metallenen Werkstoffe und Polymere nachgewiesen werden. Im Anwendungsfall von Heizöl mit 20 % biogenen Anteilen in Form von Rapsölfettsäuremethylester (FAME, Biodiesel) ist es für eine konservative Beurteilung des Korrosionssystems Werkstoff/Medium/Umgebung wichtig, die Alterungs­effekte des Mediums einzubeziehen. Entwicklung eines Prüfverfahrens für die Untersuchung der Beständigkeit von metallenen Werkstoffen und Polymeren in Heizöl und Heizöl-FAME-Blends, das für eine Vorauswahl der Werkstoffe und zum Nachweis der Beständigkeit im Hinblick auf die bauaufsichtlichen Zulassungsverfahren geeignet ist. Ein Schwerpunkt wird bei den metallenen Werkstoffen auf der Erprobung von Messmethoden liegen, mit denen sich in kurzer Versuchszeit ein Korrosionsangriff detektieren lässt. Metallene Werkstoffe: Weder örtliche Korrosion noch erhöhte Flächenkorrosion (Korrosionsrate:< 0,1 m/Jahr) sind bei den bisher geprüften Werkstoffen: Aluminium, C-Stahl 1.0037, austenitischer CrNi-Stahl 1.4301, Kupfer und Messing in Heizöl und B20 (Heizöl mit 20% Biodiesel) aufgetreten. Diese Werkstoffe sind in den Prüfmedien Heizöl und B20 als beständig zu bewerten. Es wurde keine signifikante Veränderung des pH-Wertes der Prüfmedien gemessen. Polymere: Massebestimmung: Die Prüfkörper der Elastomere ACM, HNBR und PUR sowie in geringerem Maße PE neigten zur Quellung in Heizöl und B20 nach 42 d und 84 d Auslagerung; für PA 6, POM und PVC wurde keine Masseänderung gemessen. Die Masseänderung der Prüfkörper in Heizöl und B20 ist mit Ausnahme von PUR vergleichbar. Bei PE traten Verfärbungen durch die Brennstoffe auf. Zugeigenschaften: ACM, HNBR, PE und PVC sind in Heizöl und B20 beständig, da die Änderung der Zugfestigkeit und der Reißdehnung < 15 % beträgt. PA und POM sind bedingt beständig, da die Änderung der Zugfestigkeit und der Reißdehnung < 30% beträgt. T2 - DGMK-Projekttreffen CY - Rostock, Germany DA - 28.03.2019 KW - Beständigkeitsbewertung KW - Metallene Werkstoffe KW - Polymere KW - Heizöl KW - Heizöl-FAME-Blends PY - 2019 AN - OPUS4-47841 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Ackermann, H. A1 - Pötzsch, Sina A1 - Weltschev, Margit A1 - Bäßler, Ralph A1 - Plum, W. T1 - Entwicklung einer Prüfmethode zur Bewertung der Materialbeständigkeit von Bauteilen in Mitteldestillatanwendungen N2 - Im Vorhaben wurde eine forcierte Prüfmethode zur Bestimmung der Beständigkeit von metallenen Werkstoffen gegenüber Brennstoffen aus Mitteldestillaten und Gemischen aus Mitteldestillat und paraffinischen Kohlenwasserstoffen, die jeweils Fettsäuremethylester (FAME) als biogene Komponente enthalten, entwickelt. Bei der Prüfmethode werden Prüfkörper des jeweiligen Werkstoffes in speziellen Prüfmedien ausgelagert. Die Zusammensetzung von zwei Prüfmedien wurde im Vorhaben erarbeitet. Diese Prüfmedien erfassen die Effekte der Alterung des FAME, die zu erwarten sind, wenn der Brennstoff länger als 2 Jahre im Feld lagert. Sie decken den Bereich bis 20 % (V/V) FAME-Anteil ab. Die Auslagerung kann bei geringem Aufwand unter Atmosphärendruck durchgeführt werden. Die Eignung einer Auswahl von metallenen Werkstoffen und Polymerwerkstoffen, die für Versorgungsanlagen für Mitteldestillat relevant sind, wurde durch Auslagerung in folgenden nicht gealterten Brennstoffen bestimmt: Heizöl EL schwefelarm (B0), Heizöl EL schwefelarm mit 20 % (V/V) FAME (B20), FAME (B100) und hydriertes Pflanzenöl (HVO). Die Werkstoffe wurden auch in einem 1 Jahr gealterten B20 und einem 8 Jahre gealtertem B10 ausgelagert. Die Temperatur bei der Auslagerung betrug 50 °C für die metallenen Werkstoffe und 40 °C und 70 °C für die Polymerwerkstoffe. Die Ergebnisse der Beständigkeitsbewertung wurden in Beständigkeitslisten zusammengefasst. Die mit B20 erhaltenen Bewertungen gelten generell für Gemische aus Heizöl EL schwefelarm und FAME mit einem FAME-Gehalt bis 20 % (V/V). Sie sind auch auf Gemische aus Dieselkraftstoff und FAME mit einem FAME-Gehalt bis 20 %(V/V) übertragbar. Die forcierte Prüfmethode kann insbesondere KMUs bei der Weiterentwicklung von bestehenden Produkten und der Entwicklung von neuen Produkten als ein kostengünstiger Schnelltest zur Überprüfung der Werkstoff- und Bauteilbeständigkeit gegenüber Mitteldestillaten mit hohem FAME-Anteil dienen. Sie kann für die Hersteller die Sicherheit erhöhen, dass Bauteile die Freigabeprüfungen der Bauaufsicht bestehen, wobei die Freigabe jedoch nur für Deutschland gültig ist. Die Erkenntnisse des Forschungsvorhabens können in eine harmonisierte Europäische Norm für alternative Brenn- und Kraftstoffe einfließen. Diese ist für die Bauteilhersteller die Voraussetzung für die Erschließung des europäischen Marktes.   N2 - Within this project, a forced test method was developed to determine the resistance of metallic materials to middle distillate fuels and mixtures of middle distillate and paraffinic hydrocarbons both with fatty acid methyl ester (FAME) as a biogenic component. In the method, specimens of the material are immersed in special test media. The compositions of two test media were developed within the project. These test media include the influence of aging of the FAME which is to be expected after a storage of the fuel exceeding 2 years in the field. They cover a range of up to 20 % (v/v) FAME content. The exposure test can be carried out at ambient pressure with little effort. Suitability of selected metallic and polymer materials relevant for middle distillate supply systems was determined by exposure to the following non-aged fuels: low-sulfur light fuel oil (B0), low-sulfur light fuel oil with 20 % (v/v) FAME (B20), FAME (B100) and hydrogenated vegetable oil (HVO). The materials were also exposed in the 1-year-aged B20 and 8-year-aged B10. Test temperature was 50 °C for metallic materials and 40 °C and 70 °C for polymers. Resulting materials resistances were summarized in resistance tables. Resistances obtained in B20 are valid for any mixture of low-sulfur light fuel oil and FAME containing up to 20 % (v/v) FAME. They are also transferable to mixtures of diesel and FAME having a FAME content of up to 20 % (v/v). This method with special test media is a cost-effective rapid test for checking resistance of materials to middle distillates having a high FAME content. It can support SMEs manufacturing components for supply systems in further development of existing and new products. It increases the manufacturers' certainty that components will pass approval tests of authorities. Results of this research project can be incorporated into a harmonized European standard for alternative fuels. This is the prerequisite for component manufacturers to access the European market. KW - Heizöl KW - FAME KW - Biobrennstoff PY - 2020 UR - https://dgmk.de/publikationen/ SN - 978-3-947716-14-2 SN - 0937-9762 SP - 1 EP - 153 PB - DGMK CY - Hamburg AN - OPUS4-51110 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weltschev, Margit T1 - Emissionsfrei auch im Leckagefall / Doppelwandige Behälter für die sichere Gefahrstofflagerung KW - Leckage KW - Gefahrstofflagerung KW - Doppelwandbehälter PY - 1999 SN - 0009-2800 IS - 8 SP - 28 EP - 30 PB - Konradin-Verl. CY - Leinfelden AN - OPUS4-744 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit T1 - Einsatz von höherlegierten Sonderedelstählen und Nickelbasislegierungen im Tankbau T2 - Gefahrgut-Technik-Tage Berlin 2002 "Innovative Tanktechnik" CY - Berlin, Deutschland DA - 2002-11-14 PY - 2002 PB - Storck-Akademie CY - Hamburg AN - OPUS4-1787 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit T1 - Einsatz von höherlegierten Sonderedelstählen und Nickelbasislegierungen im Tankbau T2 - Gefahrgut-Technik-Tage Berlin 2002 CY - Berlin, Germany DA - 2002-11-14 PY - 2002 AN - OPUS4-3682 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit A1 - Bäßler, Ralph T1 - Einsatz von höherlegierten metallischen Werkstoffen, ferritischen Chromstählen und Duplexstählen für den Transport von Gefahrgütern T2 - GfKORR: Sitzung des AK - Korrosion undl Korrosionsschutz CY - Duisburg, Germany DA - 2012-06-14 PY - 2012 AN - OPUS4-26088 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit T1 - Einfluss von Biokomponenten in Kraftstoffen und Heizöl auf die Beständigkeit von Fluorkautschuk unter Praxisbedingungen N2 - Die Bewertung der Werkstoffbeständigkeit ist von großer Bedeutung bei Änderung der Zusammensetzung der Kraftstoffe und des Heizöls, insbesondere die Frage nach der Beständigkeit der Dichtungswerkstoffe bei Zusätzen von Bioethanol und Biodiesel (Rapsölfettsäuremethylester). Vorhergehende Untersuchungen (Messungen der Veränderungen der Masse, der Zugeigenschaften und der Härte) bezogen sich auf die Bewertung der Beständigkeit häufig verwendeter Dichtungswerkstoffe wie FKM, FVMQ, VMQ, EPDM, CR, CSM, IIR, PA, NBR und PUR in Kraftstoffen und Heizöl mit 10 % Biodiesel (nicht gealtert und bis zu 5 Jahre gealtert) unter statischen Bedingungen. Ziel der Untersuchungen war die Bewertung der Beständigkeit von Fluorkautschuk unter verpressten Bedingungen in Analogie zu den Einsatzbedingungen in der Praxis. Die Masse und der Druckverformungsrest von Prüfkörpern aus FKM wurden vor und nach der Auslagerung über einen Zeitraum von 3, 7, 14, 28, 56 und 90 Tagen in E10 (Kraftstoff mit max. 10 % Ethanol), E85 (Kraftstoff mit 85 % Ethanol), Biodiesel (Rapsölfettsäuremethylester), Super (Kraftstoff mit max. 5 % Ethanol), Dieselkraftstoff mit max. 5 % Biodiesel, Super Plus (Kraftstoff ohne Ethanolzusatz) und Heizöl mit 10 % Biodiesel (B10) bei 40 °C gemäß ISO 815-1 bestimmt. Die Druckverformungsrestprüfung zählt neben der Messung der Härte, der Dichte und der Zugeigenschaften zu den wichtigsten Grundprüfverfahren der Elastomerindustrie. Nach Ende der Auslagerung in den Kraftstoffen und der Aufhebung der Verpressung wurde der Druckverformungsrest der Prüfkörper in regelmäßigen Zeitabständen bis zu einer Rücktrocknung > 90 Tage bestimmt. Zum Vergleich wurden Prüfkörper aus FKM ohne Kraftstoff oder Heizöl unter Verpressung bei 40 °C ausgelagert. Die Masseänderung der Prüfkörper aus FKM betrug nach 90 Tagen Auslagerung in E10 9 %, in Super 8 %, in E85 4% und 0,6 % in Biodiesel. Die Erhöhung der Masse und die damit verbundene Quellung der Prüfkörper in E10 und Super mit 5 – 10% Ethanolzusatz hatte einen Einfluss auf den Druckverformungsrest, der sprunghaften Veränderungen unterlag im Vergleich zu den Werten nach Auslagerung in Biodiesel, Dieselkraftstoff und Heizöl B10 bei 40 °C. Zum Vergleich, unter statischen Bedingungen verringerte sich die Zugfestigkeit der Prüfkörper aus FKM nach Auslagerung in E10 bei 40 °C um 31 % und die Reißdehnung um 18 %. T2 - BAM-Abteilungskolloquium CY - Berlin, Germany DA - 22.11.2018 KW - Fluorkautschuk (FKM) KW - Kraftstoffe mit biogenen Anteilen KW - Druckverformungsrestprüfung PY - 2018 AN - OPUS4-46887 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -