TY - JOUR A1 - Kricheldorf, H.R. A1 - Mix, Renate A1 - Weidner, Steffen T1 - Poly(ester urethane)s derived from lactide, isosorbide, terephthalic acidm abd various diisocyanates N2 - Isosorbide-initiated oligomerizations of ʟ-lactide were preformed in bulk using SnCl2 as catalyst. The resulting telechelic OH-terminated oligoesters were in situ subjected to simultaneous polycondensation and polyaddition with mixtures of terephthaloyl chloride and diisocyanates. Most polymerizations were conducted with 4,4'-diisocyanatodiphenyl methane and 2,4-diisocyanato toluene. The consequences of excess diisocyanate and four different catalysts were studied. The isosorbide/lactide ratio and the terephthalic acid/diisocyanate ratio were varied. Number average molecular weights up to 15 kDa with polydispersities around 3–5 were obtained. Depending on the chemical structure of the copolyester and on the feed ratio, incorporation of urethane groups may reduce or enhance the glass-transition temperature, but the thermal stability decreases dramatically regardless of composition. KW - Cyclization KW - Isosorbide KW - Lactide KW - Polyaddition KW - Polycondensation KW - Polyesters KW - Polyurethanes PY - 2014 U6 - https://doi.org/10.1002/pola.27069 SN - 0360-6376 SN - 0887-624X VL - 52 IS - 6 SP - 867 EP - 875 PB - Wiley CY - Hoboken, NJ AN - OPUS4-30299 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Becker, Roland A1 - Scholz, Philipp A1 - Jung, Christian A1 - Weidner, Steffen T1 - Thermo-Desorption Gas Chromatography-Mass Spectrometry for investigating the thermal degradation of polyurethanes N2 - Thermo-Desorption Gas Chromatography-Mass Spectrometry (TD-GC-MS) was used to investigate the thermal degradation of two different polyurethanes (PU). PU samples were heated at different heating rates and the desorbed products were collected in a cold injection system and thereafter submitted to GC-MS. Prospects and limitations of the detection and quantification of semi-volatile degradation products were investigated. A temperature dependent PU depolymerization was found at temperatures above 200 °C proved by an increasing release of 1,4-butanediol and methylene diphenyl diisocyanate (MDI) representing the main building blocks of both polymers. Their release was monitored quantitatively based on external calibration with authentic compounds. Size Exclusion Chromatography (SEC) of the residues obtained after thermodesorption confirmed the initial competitive degradation mechanism indicating an equilibrium of crosslinking and depolymerization as previously suggested. Matrix-Assisted Laser Desorption Ionization (MALDI) mass spectrometry of SEC fractions of thermally degraded PUs provided additional hints on degradation mechanism. KW - Thermo-desorption KW - Mass spectrometry KW - Polyurethanes KW - Thermal degradation PY - 2023 U6 - https://doi.org/10.1039/D3AY00173C SN - 1759-9660 SP - 1 EP - 6 PB - Royal Society for Chemistry AN - OPUS4-57307 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -