TY - JOUR A1 - Weidner, Steffen A1 - Falkenhagen, Jana A1 - Krüger, Ralph-Peter A1 - Just, Ulrich T1 - Principle of Two-Dimensional Characterization of Copolymers N2 - Two-dimensional polymer characterization is used for a simultaneous analysis of molar masses and chemical heterogeneities (e.g., end groups, copolymer composition, etc.). This principle is based on coupling of two different chromatographic modes. Liquid adsorption chromatography at critical conditions (LACCC) is applied for a separation according to the chemical heterogeneity, whereas in the second-dimension fractions are analyzed with regard to their molar mass distribution by means of size exclusion chromatography (SEC). Because appropriate standards for a calibration of the SEC are seldom available, matrix-assisted laser desorption/ionization-time-of-flight mass spectrometry (MALDI-TOF MS) was used to substitute the SEC. The LACCC-MALDI MS coupling enables acquiring additional structural information on copolymer composition, which can considerably enhance the performance of this coupled method. KW - MALDI-TOF MS KW - Chromatographie KW - Kopplung PY - 2007 U6 - https://doi.org/10.1021/ac062145f SN - 0003-2700 SN - 1520-6882 VL - 79 IS - 13 SP - 4814 EP - 4819 PB - American Chemical Society CY - Washington, DC AN - OPUS4-17722 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Meyer, A. A1 - Kricheldorf, H. R. T1 - Sn(II)2-ethylhexanoate-catalyzed polymerizations of L-lactide in solution – Solution grown crystals of cyclic Poly(L-Lactide)s N2 - L-lactide (LA) was polymerized in toluene by means of neat tin(II) 2-ethylhexanoate (SnOct2). Concentration, time and temperature were varied. The isothermally crystallized polyLAs (PLA) were characterized in the virgin state with regard to topology, molar mass, melting temperature (Tm), crystal modification, high or low Tm morphology, crystallinity and crystal thickness. Even a small amount of solvent favored cyclization relative to polymerization in bulk, so that cyclic polylactides were obtained at 115 ◦C and even at 95 ◦C. At all temperatures the α-modification of PLA was obtained along with crystallinities up to 90%. With 6 M solution the high Tm morphology with Tm’s > 190 ◦C was obtained at 115 ◦C. The crystal thickness of crystallites grown from solution at 115 ◦C was on the average 10–20% higher than that of PLA polymerized in bulk. At a polymerization temperature of 75 ◦C cyclization was incomplete and fewer perfect crystallites were formed. A new hypothesis for the crystal growth of cyclic polyLAs is proposed. KW - Polylactide KW - MALDI-TOF MS KW - Crystalinity KW - Polymerization PY - 2022 U6 - https://doi.org/10.1016/j.polymer.2022.125142 SN - 0032-3861 VL - 255 SP - 1 EP - 9 PB - Elsevier CY - Oxford AN - OPUS4-55283 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. A1 - Weidner, Steffen A1 - Meyer, A. T1 - Ring-expansion polymerization (REP) of L-lactide with cyclic tin catalysts – About formation of extended ring crystals and optimization of Tm and ΔHm N2 - L-Lactide was polymerized in bulk at 140 °C with three different cyclic tin catalysts and the time was varied from 1 d up to 14 d. The MALDI TOF spectra confirmed the formation of cyclic polylactides (PLAs) and displayed a characteristic change of peak intensity distribution with formation of a “saw tooth pattern”. This pattern confirms a previous hypothesis that cyclic PLAs tend to form crystallites with extended ring conformation and relatively smooth surface. This type of crystallites is formed under thermodynamic control by transesterification on the surface of the crystallites. In this way PLAs with extraordinarily high melting temperatures (Tm's up to 200.6 °C) and extraordinarily high melting enthalpy were obtained (ΔHm's up to 105 J g−1). These ΔHm values require a revision of the maximum ΔHm value calculated in the literature for ideal PLA crystals. KW - Polylactide KW - MALDI-TOF MS KW - ring-expansion polymerization PY - 2022 U6 - https://doi.org/10.1016/j.polymer.2022.125516 SN - 0032-3861 VL - 263 SP - 125516 PB - Elsevier Ltd. AN - OPUS4-56338 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen A1 - Meyer, A. T1 - About the Influence of (Non-)Solvents on the Ring Expansion Polymerization of l-Lactide and the Formation of Extended Ring Crystals N2 - Ring-expansion polymerizations (REPs) catalyzed by two cyclic tin catalysts(2-stanna-1.3-dioxa-4,5,6,7-dibenzazepine [SnBiph] and 2,2-dibutyl-2-stanna-1,3-dithiolane [DSTL) are performed at 140 °C in bulk. Small amounts (4 vol%) of chlorobenzene or other solvents are added to facilitate transesterification reactions (ring–ring equilibration) in the solid poly(l-lactide)s. In the mass range up to m/z 13 000 crystalline PLAs displaying a so-called saw-tooth pattern in the MALDI-TOF mass spectra are obtained indicating the formation of extended-ring crystals. The characteristics of extended-ring crystallites and folded-ring crystallites are discussed. Furthermore, extremely high melting temperatures (Tm’s up to 201.2 °C) and melting enthalpies (𝚫Hm’s up to 106 J g−1)) are found confirming that 𝚫Hmmax, the 𝚫Hm of a perfect crystal, is around or above 115 J g−1 in contrast to literature data. KW - Polylactide KW - MALDI-TOF MS KW - Ring-expansion polymerization KW - Crystals PY - 2022 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-565038 SN - 1022-1352 SP - 1 EP - 8 PB - Wiley VHC-Verlag AN - OPUS4-56503 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen T1 - Synthesis of polylactides by means of tin catalysts N2 - This article reviews the usefulness of tin(II) and tin(IV) salts and compounds as catalysts for the polymerization of lactides. The text is subdivided into nine parts mainly reflecting different polymerization strategies, such as ring-opening polymerization (ROP), ring-expansion polymerization (REP), ROP combined with simultaneous polycondensation (ROPPOC), various catalysts with unknown polymerization mechanisms, and polycondensation of lactic acid. Since the toxicity of tin salts and compounds is a matter of concern and frequently mentioned in numerous publications, the first section deals with facts instead of myths about the toxicity of tin salts and compounds. KW - Polylactide KW - MALDI-TOF MS KW - Tin catalysts PY - 2022 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-545050 SP - 1 EP - 30 PB - Royal Society for Chemistry AN - OPUS4-54505 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen A1 - Scheliga, F. T1 - Ring-Expansion Polymerization of 𝝐-Caprolactone, Glycolide, and l-lactide with a Spirocyclic Tin(IV) Catalyst Derived from or 2,2′-Dihydroxy-1,1′-Binaphthyl – New Results and a Revision N2 - In contrast to other cyclic tin bisphenoxides, polymerizations of glycolide and l-lactide with the spirocyclic tin(IV) bis-1,1′-bisnapthoxide yield linear chains having a 1,1′-bisnapthol end group and no cycles. In the case of l-lactide, LA/Cat ratio and temperature are varied and at 160 °C or below, all polylactides mainly consist of even-numbered chains. A total predominance of even-numbered chains is also found for homopolymerization of glycolide, or the copolymerization of glycolide and l-lactide, when conducted <120 °C. Linear chains having a bisnaphthol end group are again the main reaction products of ring-expansion polymerizations (REP) of 𝝐-caprolactone, but above 150 °C cycles are also formed. KW - Polylactide KW - MALDI-TOF MS KW - Polymerization PY - 2021 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-541931 VL - 222 IS - 24 SP - 1 EP - 10 PB - Wiley VCH GmbH AN - OPUS4-54193 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen A1 - Falkenhagen, Jana T1 - The role of transesterifications in reversible polycondensations and a reinvestigation of the Jacobson-Beckmann-Stockmayer experiments N2 - The polycondensations of adipic acid and 1,10-decanediol catalyzed by toluene sulfonic acid (TSA) were reinvestigated using MALDI TOF mass spectrometry and NMR spectroscopy. Unexpected reactions of TSA were detected along with incomplete conversion of the monomers. Furthermore, transesterification reactions of end-capped poly(1,10-decanediol adipate) and end-capped poly(ε-caprolactone) catalyzed by TSA were studied. Despite the quite different (ionic) reaction mechanisms, it was found that for polycondensations performed in bulk intermolecular transesterification is more efficient than the intramolecular “back-biting”; this scenario was not considered in the Jacobson–Stockmayer theory of reversible polycondensations. These results also confirm that the Jacobson–Stockmayer explanation of reversible polycondensations solely on the basis of ring chain equilibration is not only devoid of any experimental evidence, but also in contradiction to the results elaborated in this work. KW - Polylactide KW - MALDI-TOF MS KW - Polycondensation PY - 2022 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-543402 SN - 1759-9962 SP - 1 EP - 9 PB - RSC Publ. CY - Cambridge AN - OPUS4-54340 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen A1 - Scheliga, F. T1 - SnOct2-catalyzed and alcohol-initiated ROPS of L-lactide - Control of the molecular weight and the role of cyclization N2 - Ring-opening polymerizations (ROP) of l-lactide (LA) are conducted in bulk at 130, 160, or 180 °C and are initiated with two different alcohols at 160 °C. The lactide/initiator ratio (LA/In) is varied from 50/1 (20/1 at 180 °C) to 900/1 and the lactide/catalyst ratio (LA/Cat) between 2000/1 and 8000/1. At all temperatures a nearly perfect control of number average molecular weight (Mn) via the LA/In ratio is feasible up to LA/In = 200/1, but at higher ratios the Mn value lags behind the theoretical values and the discrepancy increases with higher LA/Cat ratios. Variation of the LA/Cat ratio influences the formation of cycles but does not significantly influence Mn, when the LA/In ratio is kept constant. The formation of cycles is favored by lower In/Cat ratios and is the main reason for the unsatisfactory control of Mn at high LA/In ratios. The results also suggest that the cycles are mainly or exclusively formed by end-to-end cyclization and not, as believed previously, by back-biting. KW - Polylactide KW - MALDI-TOF MS KW - Cyclization KW - Ring-opening polymerization PY - 2022 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-543066 SN - 1521-3935 SP - 1 EP - 10 PB - Wiley-VCH CY - Weinheim AN - OPUS4-54306 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen A1 - Meyer, A. T1 - Poly(L-lactide): Optimization of Melting Temperature and Melting Enthalpy N2 - Twice recrystallized L-lactide was polymerized with a dozen of different tin or bismuth catalysts in bulk at 160°C for 24 h and was annealed at 150°C afterwards. In two cases Tm values above 197.0°C were obtained. The parameters causing a scattering of the DSC data were studied and discussed. The samples prepared with SnCl2, 2,2-dibutyl-2-stanna-1,3-ditholane (DSTL) or cyclic tin(II) bisphenyldioxide (SnBiph) were subject to annealing programs with variation of time and temperatures, revealing that the Tm´s did not increase. However, an increase of Hm was achieved with maximum values in the range of 93-96 J g-1 corresponding to crystallinities off around 90%. Further studies were performed with once recrystallized L-lactide. Again, those samples directly crystallized from the polymerization process showed the highest Tm values. These data were compared with the equilibrium Tm0 and Hm0 data calculated by several research groups for perfect crystallites. A Tm0 of 213+/-2°C and a Hm0 of 106 J g-1 show the best agreement with the experimental data. The consequences of annealing for the thickness growth of crystallites are discussed on the basis of SAXS measurements. Finally, a comparison of cyclic and linear poly L-lactide)s is discussed. KW - Polylactide KW - MALDI-TOF MS KW - Transesterification PY - 2021 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-538656 SP - 1 EP - 10 PB - Royal Society for Chemistry AN - OPUS4-53865 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Kricheldorf, H. R. T1 - SnOct2-catalyzed ROPs of L-lactide initiated by acidic OH- compounds: Switching from ROP to polycondensation and cyclization N2 - Ring-opening polymerizations (ROPs) of L-lactide are performed in bulk at 130°C with tin(II) 2-ethylhexanoate as catalyst and various phenols of differentacidity as initiators. Crystalline polylactides having phenyl ester end groups are isolated, which are almost free of cyclics. The dispersities and molecular weights are higher than those obtained from alcohol-initiated ROPs under identical conditions. Polymerizations at 160°C yield higher molecular weights than expected from the monomer/initiator ratio and a considerable fraction of cycles. The fraction of cycles increases with higher reactivity of the ester end group indicating that the cycles are formed by end-to-end cyclization. KW - Polylactide KW - MALDI-TOF MS KW - Polymerization PY - 2021 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-540250 SN - 2642-4150 VL - 60 IS - 5 SP - 785 EP - 793 PB - Wiley AN - OPUS4-54025 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen A1 - Falkenhagen, Jana T1 - Reversible Polycondensations outside the Jacobson-Stockmayer Theory and a New Concept of Reversible Polycondensations N2 - L-Lactide was polymerized with tin(II)acetate, tin(II)2-ethyl hexanoate, diphenyltin dichloride and dibutyltin bis(pentafluorophenoxide) at 130 °C in bulk. When an alcohol was added as initiator, linear chains free of cycles were formed having a degree of polymerization (DP) according to the lactide/initiator (LA/In) ratio. Analogous polymerizations in the absence of an initiator yielded high molar mass cyclic polylactides. Quite similar results were obtained when ε-caprolactone was polymerized with or without initiator. Several transesterification experiments were conducted at 130 °C, either with polylactide or poly(ε-caprolactone) indicating that several transesterification mechanisms are operating under conditions that do not include formation of cycles by back-biting. Furthermore, reversible polycondensations (revPOCs) with low or moderate conversions were found that did not involve any kind of cyclization. Therefore, These results demonstrate the existence of revPOCs, which do neither obey the theory of irreversible polycondensation as defined by Flory nor the hypothesis of revPOCs as defined by Jacobson and Stockmayer. A new concept encompassing any kind of revPOCs is formulated in the form of a “polycondensation triangle”. KW - Polylactide KW - MALDI-TOF MS KW - Polycondensation PY - 2021 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-530831 VL - 12 IS - 35 SP - 5003 EP - 5016 PB - Royal Society for Chemistry AN - OPUS4-53083 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Meyer, A. A1 - Weidner, Steffen T1 - High Tm Poly(l-lactide)s by Means of Bismuth Catalysts? N2 - One series of BiSub-catalyzed ring-opening polymerizations (ROPs) is per-formed at 160 °C for 3 days with addition of difunctional cocatalysts to find out, if poly(l-lactide) crystallizes directly from the reaction mixture. An analogous series is performed with monofunctional cocatalysts. High Tm crystal-lites (Tm > 190 °C) are obtained from all bifunctional cocatalysts, but not from all monofunctional ones. It is shown by means of SAXS measurements that the high Tm values are mainly a consequence of a transesterification–homogenization process across the lamellar surfaces resulting in thickness and smoothing of the surfaces. An unusual enthalpy-driven modification of the molecular weight distribution is found for samples that have crystallized during the polymerization. A third series of ROPs is performed at 170 °C for 2 h followed by annealing at 120 °C (2 h) to induce crystallization. Complete transformation of the resulting low Tm crystallites (Tm < 180 °C) into the high Tm crystallites by annealing at 170 °C for 1 d is not achieved, despite variation of the cocatalyst. KW - Polylactide KW - MALDI-TOF MS KW - Crystallization PY - 2021 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-522777 SN - 1022-1352 VL - 222 IS - 8 SP - 19 PB - Wiley AN - OPUS4-52277 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen T1 - Polymerization of L-lactide with SnCl2: A Low Toxic and Eco-friendly Catalyst N2 - Polymerizations of L-lactide catalyzed either by neat SnCl2 or by SnCl2 + difunctional cocatalysts were conducted in bulk at 180, 160 and 140 °C with variation of the Lac/Cat ratio and time. With neat SnCl2 poly(L-lactide) having weight average molecular weights (uncorrected Mw’s) up to 190 000 g mol−1 were obtained mainly consisting of linear chains. Addition of salicylic acid or 1,1-bisphenol yielded a higher fraction of cyclic polylactides but lower molecular weights. Furthermore, SnCl2 was compared with Bu2SnCl2 and various other metal chlorides and the best results were obtained with SnCl2. With ethyl L-lactate as initiator SnCl2-catalyzed ROPs were performed at 120 °C and the lac/initiator ratio was varied. All these experiments were conducted under conditions allowing for comparison with ROPs catalyzed with neat Sn(II)-2-ethyhexanoate. Such a comparison was also performed with ε-caprolactone as monomer. KW - Catalyst KW - Polylactide KW - MALDI-TOF MS KW - Polycondensation PY - 2021 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-520517 SN - 1566-2543 SP - 1 EP - 13 PB - Springer Nature AN - OPUS4-52051 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Meyer, A. A1 - Kricheldorf, H. R. A1 - Weidner, Steffen T1 - ROPs of L-lactide catalyzed by neat Tin(II)2-ethylhexanoate - Influence of the reaction conditions on Tm and ΔHm N2 - L-Lactide was polymerized by means of neat SnOct2 with variation of LA/Cat ratio, temperature and time. The resulting cyclic polylactides crystallized spontaneously at 160 °C or below, but needed nucleation via mechanical stress at 165 or 170 °C. All the crystalline polylactides obtained directly from ROP above 120 °C had melting temperatures (Tm) above 189 °C (up to 194.5 °C). SnOct2 also enabled transformation of low Tm poly(L-lactide)s (Tm <180 °C) into the high Tm m1odification by annealing, due to the impact of transesterification reactions in the interphase between the crystallites. The influence of crystallization temperature and annealing time on the crystal thickness was studied via SAXS measurements. A comparison with the crystallization and annealing experiments reported by Pennings and coworkers and Tsuji and Ikada is discussed, and a satisfactory agreement has been found, because those authors also studied polyLA samples containing SnOct2 in its active form. It is also demonstrated in this work that the high Tm modification cannot be obtained when the catalyst is removed or poisoned as it is true for commercial polylactides. KW - Polylactide KW - MALDI-TOF MS KW - Crystallization PY - 2021 U6 - https://doi.org/10.1016/j.polymer.2021.124122 SN - 0032-3861 VL - 231 SP - 1 EP - 10 PB - Elsevier CY - Oxford AN - OPUS4-53194 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Meyer, A. A1 - Falkenhagen, Jana A1 - Kricheldorf, H. R. T1 - SnOct2-catalyzed and alcohol-initiated ROPs of L-lactide – About the influence of initiators on chemical reactions in the melt and the solid state N2 - SnOct2 (Sn(II) 2-ethylhexanoate) catalyzed ROPs of L-lactide were performed in bulk with eight different alcohols as initiators. The time was varied between 1 h and 24 h for all initiators. For two initiators the temperature was also lowered to 115 ◦C. Even-numbered chains were predominantly formed in all polymerizations at short times, but the rate of transesterification (e.g. even/odd equilibration) and the molecular weight distribution were found to depend significantly on the nature of the initiator. Observed transesterification reactions also continued in solid poly (L-lactide), and with the most active initiator, almost total equilibration was achieved even at 130 ◦C. This means that all chains including those of the crystallites were involved in transesterification reactions proceeding across the flat surfaces of the crystallites. The more or less equilibrated crystalline polylactides were characterized by DSC and SAXS measurements with regard to their melting temperature (Tm), crystallinity and crystal thickness. KW - Polylactide KW - MALDI-TOF MS KW - Crystallization KW - Catalysts KW - SAXS PY - 2021 U6 - https://doi.org/10.1016/j.eurpolymj.2021.110508 VL - 153 SP - 110508 PB - Elsevier Ltd. AN - OPUS4-52633 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen T1 - Alcohol-Initiated and SnOct2-Catalyzed Ring-Opening Polymerization (ROP) of L-Lactide in Solution: A Re-investigation N2 - Alcohol-initiated ring-opening polymerizations (ROP) of L-lactide (LA) were studied in solution at 70 °C, whereupon the nature of the alcohol, the LA/initiator ratio, the LA/SnOct2 ratio and the time were varied. In contrast to literature, neat SnOct2 is catalytically active in THF and several aromatic but donor solvents, such as 1,3-dioxolane, dimethylformamide (DMF) or N-methyl pyrrolidone (NMP), strongly reduce the activity of SnOct2. In agreement with literature, no cycles were formed by neat SnOct2 at 70 °C in toluene, whereas almost complete cyclization occurs at 115 °C. This finding is attributed to strongly reduced mobility of the initially formed linear chains having one Sn-O-CH and one anhydride end group. Due to better solvation and enhanced mobility cyclization occurs in THF at 70 °C. KW - Polylactide KW - Ring-opening polymerization KW - MALDI-TOF MS KW - Transesterification PY - 2023 U6 - https://doi.org/10.1016/j.eurpolymj.2023.111822 SN - 0014-3057 SP - 1 EP - 18 PB - Elsevier CY - New York, NY [u.a.] AN - OPUS4-56818 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Lahcini, M. A1 - Weidner, Steffen A1 - Oumayama, J. A1 - Scheliga, F. A1 - Kricheldorf, H. R. T1 - Unsaturated Copolyesters of Lactide N2 - Four classes of unsaturated copolyesters of L-lactide were prepared either from isosorbide or bis(hydroxymethyl)tricyclodecane in combination with fumaric acid or from 1,4-butenediol or 1,4- butynediol with terephthalic acid. All syntheses were performed in such a way that lactide was oligomerized with a diol as the initiator and the resulting oligomers were polycondensed with a dicarboxylic acid dichloride either in a one-pot synthesis or in a two-step procedure. For most copolyesters the SEC measurements gave weight average molecular weights in the range of 30–60 kg mol⁻1 and dispersities in the range of 4.2–6.2. The MALDI-TOF mass spectra displayed a high content of cycles and indicated an irreversible kinetic course of all polycondensations. Glass-transition temperatures (Tg) above 90 °C were only found for two copolyesters of isosorbide. Addition of bromine to copolyesters of 1,4-butenediol yielded flame retarding biodegradable polymers. KW - Copolyester KW - MALDI-TOF MS KW - SEC KW - Lactide PY - 2016 U6 - https://doi.org/10.1039/c6ra16008e VL - 2016/6 IS - 96 SP - 93496 EP - 93504 PB - Royal Society of Chemistry AN - OPUS4-37913 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Hoskins, Jessica A1 - Falkenhagen, Jana A1 - Weidner, Steffen ED - Udomkichdecha, W. ED - Böllinghaus, T. ED - Manonukul, A. ED - Lexow, J. T1 - Characterization of randomly branched polymers utilizing liquid chromatography and mass spectrometry N2 - Branching in polymers is an important way to modify the materials properties, however the characterization of random branching in polymeric materials is a challenge in polymer analysis. In this work, liquid adsorption chromatography methods are developed for a commercially available hyperbranched polyester (Boltorn™). This Chromatographie techniques was then coupled to offline MALDI-TOF MS analysis, a first in the analysis of randomly branched polymers. The coupling of these two techniques provides superior MALDI-TOF spectra, enabling the easy identification of structural subdistributons based on theoretical molecular weight. Detailed analysis of the MALDI-TOF spectra shows that these Chromatographie conditions separate cyclic Boltorn polymers (with no core molecule) from non-cyclic polymers (with core molecule), and these are the only two architectures observed. MALDI MS also confirms that the Chromatographie Separation mode is adsorption, but further analysis is needed to determine if there is a Separation by degree of branching. KW - Hyperbranched polyesters KW - Polymer mass spectrometry KW - Polymer chromatography KW - Liquid adsorption chromatography KW - MALDI-TOF MS KW - Carbon capture KW - Climate change KW - Lubricant KW - Micro manufacturing KW - Multiphysics simulations KW - WMRIF PY - 2014 SN - 978-3-319-11339-5 SN - 978-3-319-11340-1 SP - 1 EP - 10 PB - Springer AN - OPUS4-32519 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, Hans R. A1 - Weidner, Steffen T1 - Ring-expansion polymerization of meso-lactide catalyzed by dibutyltin derivatives N2 - Meso-Lactide was polymerized in bulk at 60, 80, and 100 °C by means of three different types of catalysts: dibutyltinsulfides (2,2-dibutyl-2-stanna-1,3-dithiolane and 2,20-dibutyl-2-stanna-1,3-dithiane), dibutyltin derivatives of substituted cate-chols (BuCa, CyCa, and BzCa), and dibutyltin derivatives of2,2 dihydroxybiphenyl (SnBi) and 2,2-dihydroxy-1,10-binaphthyl(SnNa. Only the latter two catalysts were active at 60 °C. The architecture of the resulting polylactides depends very much on the structure of the catalyst and on the temperature. At the lowest temperature (60 °C), SnBi and SnNa mainly yielded even-numbered linear chains, but SnNa also yielded even-numbered cycles at 100 °C and short reaction times. In contrast,BuCa, CyCa, and BzCa mainly yielded odd-numbered cycles, although the same catalysts yielded even-numbered linear chains when benzylalcohol was added. KW - MALDI-TOF MS KW - Cyclisation KW - Catalysts KW - Polyester KW - Polymerization PY - 2018 U6 - https://doi.org/10.1002/pola.28948 SN - 1099-0518 SN - 0022-3832 VL - 56 IS - 7 SP - 749 EP - 759 PB - Wiley Periodicals Inc. AN - OPUS4-44278 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weidner, Steffen A1 - Kricheldorf, H. A1 - Scheliga, F. T1 - Cyclic polylactides via ring-expansion polymerization N2 - We will report on a new kind of ring-expansion polymerization (REP) of cyclic esters based of three classes of catalysts. In contrast to REP described previously these new polymerizations are characterized by a self-extrusion of the catalysts resulting in cyclic homopolyesters as the only reaction product. These REP of L-lactide were performed in bulk at temperatures between 100 and 180°C without racemization. A simplified scheme of a REP catalyzed by BuCa or SnBi is presented below. With meso-lactide temperatures down to 60°C were realized. Depending on catalyst, time and temperature with equal quantities of even and odd-numbered cycles a strong predominance of either even or odd-numbered cycles was found. T2 - 255th ACS National Meeting CY - New Orleans, LA, USA DA - 18.03.2018 KW - MALDI-TOF MS KW - Poly(lactide) KW - Polymerisation KW - Catalysts PY - 2018 AN - OPUS4-44833 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -