TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen A1 - Scheliga, F. T1 - Ring-opening polymerizations of L-Lactide catalyzed by zinc caprylate: Syntheses of cyclic and linear poly(L-lactide)s N2 - Alcohol-initiated ring-opening polymerizations (ROPs) of L-Lactide (LA) were conducted in bulk at 130 °C catalyzed by Zn acetate (ZnAc2), lactate (ZnLac2), or caprylate (ZnCap2). 11-undecenol (UND), 1-hydroxymethylnaphtalene (HMN), and 4-nitrobenzylalcohol (4NB) were used as alcohols. Whereas variation of the alcohols had little effect, the usefulness of the catalysts increased in the order: acetate < lactate < caprylate. Hence, further alcohol-initiated polymerizations were performed with ZnCap2 alone and with variation of the lactide/catalyst (LA/Cat) ratio. With increasing LA/Cat ratio higher fractions of cyclic poly(L-lactide) (PLA) were found, so that the measured degree of polymerization (DP) is considerably lower than the theoretical value (i.e., 2 x LA/alcohol). With neat ZnCap2 cyclic PLAs were the largely prevailing reaction products. For these cyclic PLAs weight average molar masses (Mw) up to 134,000 were obtained and an optical purity around 99% was indicated by 13C NMR spectroscopy and DSC measurements even after 48 h at 150 or 160 °C. KW - Cyclization KW - Lactide KW - Ring opening polymerization KW - Transesterification KW - Zinc catalyst KW - MALDI PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-557565 DO - https://doi.org/10.1002/pol.20220328 SN - 2642-4150 SP - 1 EP - 10 PB - Wiley AN - OPUS4-55756 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, Hans R. A1 - Weidner, Steffen T1 - Ring-ring equilibration (RRE) of cyclic poly(L-lactide)s by means of cyclic tin catalysts N2 - With 2,2-dibutyl-2-stanna-1,3-dithiolane (DSTL) and 2-stanna-1,3-dioxa-4,5,6,7-dibenzoxepane (SnBiPh) as catalysts ring-expansion polymerizations (REP) were performed either in 2 M solution using three different solvents and two different temperatures or in bulk at 140 and 120 ◦C. A kinetically controlled rapid REP up to weight average molecular masses (Mẃs) above 300 000 was followed by a slower degradation of the molecular masses at 140 ◦C, but not at 120 ◦C Furthermore, a low molecular mass cyclic poly(L-lactide) (cPLA) with a Mn around 16 000 was prepared by polymerization in dilute solution and used as starting material for ring-ring equilibration at 140 ◦C in 2 M solutions. Again, a decrease of the molecular mass was detectable, suggesting that the equilibrium Mn is below 5 000. The degradation of the molecular masses via RRE was surprisingly more effective in solid cyclic PLA than in solution, and a specific transesterification mechanism involving loops on the surface of crystallites is proposed. This degradation favored the formation of extended-ring crystallites, which were detectable by a “saw-tooth pattern” in their MALDI mass spectra. KW - Organic Chemistry KW - Polymers and Plastics KW - MALDI-TOF MS KW - Materials Chemistry PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-593819 DO - https://doi.org/10.1016/j.eurpolymj.2024.112765 SN - 0014-3057 VL - 206 SP - 1 EP - 8 PB - Elsevier B.V. AN - OPUS4-59381 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Meyer, A. A1 - Kricheldorf, H. R. T1 - Ring–Ring Equilibration in Solid, Even-Numbered Cyclic Poly(l-lactide)s and their Stereocomplexes N2 - Even-numbered cyclic poly(d-lactide) and poly(l-lactide) are prepared by ringexpansion polymerization. The cyclic pol(l-lactide) is annealed either at 120 or at 160 °C for several days. The progress of transesterification in the solid state is monitored by the formation of odd-numbered cycles via matrix-assisted laser desorption/ionization-time of flight mass spectrometry. The changes of the crystallinity are monitored by differential scanning calorimetry, wideand small-angle x-ray scattering (WAXS and SAXS) measurements. Despite total even-odd equilibration at 160 °C, the crystallinity of poly(l-lactide) is not reduced. Furthermore, the crystallinity of the stereocomplexes of both cyclic polylactides do not decrease or vanish, as expected, when a blocky or random stereosequence is formed by transesterification. This conclusion is confirmed by 13C NMR spectroscopy. These measurements demonstrate that transesterification is a ring–ring equilibration involving the loops on the surfaces of the lamellar crystallites thereby improving crystallinity and 3D packing of crystallites without significant broadening of the molecular weight distribution. KW - Polylactide KW - MALDI-TOF MS KW - Cyclization PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-506458 DO - https://doi.org/10.1002/macp.202000012 VL - 221 IS - 9 SP - 2000012 PB - Wiley-VCH Verlag AN - OPUS4-50645 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen T1 - ROP of L-lactide and ε-caprolactone catalyzed by tin(ii) and tin(iv) acetates–switching from COOH terminated linear chains to cycles N2 - The catalytic potential of tin(II)acetate, tin(IV)acetate, dibutyltin-bis-acetate and dioctyl tin-bis-acetate was compared based on polymerizations of L-lactide conducted in bulk at 160 or 130C. With SnAc2 low-Lac/Cat ratios (15/1–50/1) were studied and linear chains having one acetate and one carboxyl end group almost free of cyclics were obtained. Higher monomer/catalyst ratios and lower temperatures favored formation of cycles that reached weight average molecular weights (Mw's) between 100,000 and 2,500,000. SnAc4 yielded mixtures of cycles and linear species under all reaction conditions. Dibutyltin- and dioctyl tin bis-acetate yielded cyclic polylactides under most reaction conditions with Mw's in the range of 20,000–80,000. Ring-opening polymerizations performed with ε-caprolactone showed similar trends, but the formation of COOH-terminated linear chains was significantly more favored compared to analogous experiments with lactide. The reactivity of the acetate catalysts decreased in the following order: SnAc2> SnAc4>Bu2SnAc2 Oct2SnAc2. KW - Catalyst KW - MALDI-TOF MS KW - Ring-opening polymerization KW - Tin acetates KW - Polylactide PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-520831 DO - https://doi.org/10.1002/pol.20200866 SP - 1 EP - 12 PB - Wiley Online Library AN - OPUS4-52083 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen T1 - ROP of L-lactide and ε-caprolactone catalyzed by tin(ii) andtin(iv) acetates–switching from COOH terminated linear chains to cycles N2 - The catalytic potential of tin(II)acetate, tin(IV)acetate, dibutyltin-bis-acetate and dioctyl tin-bis-acetate was compared based on polymerizations of L-lactide conducted in bulk at 160 or 130°C. With SnAc2 low-Lac/Cat ratios (15/1–50/1) were studied and linear chains having one acetate and one carboxyl end group almost free of cyclics were obtained. Higher monomer/catalyst ratios and lower temperatures favored formation of cycles that reached weight average molecular weights (Mw's) between 100,000 and 2,500,000. SnAc4 yielded mixtures of cycles and linear species under all reaction conditions. Dibutyltin- and dioctyl tin bis-acetate yielded cyclic polylactides under most reaction conditions with Mw's in the range of 20,000–80,000. Ring-opening polymerizations performed with ε-caprolactone showed similar trends, but the formation of COOH-terminated linear chains was significantly more favored compared to analogous experiments with lactide. The reactivity of the acetate catalysts decreased in the following order: SnAc2> SnAc4>Bu2SnAc2~Oct2SnAc2 KW - Polylactide KW - MALDI-TOF MS KW - Catalyst KW - Ring-opening polymerization KW - Tin acetates PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-521923 DO - https://doi.org/10.1002/pol.20200866 VL - 59 IS - 5 SP - 439 EP - 450 PB - Wiley Online Library AN - OPUS4-52192 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Meyer, A. A1 - Kricheldorf, H. R. A1 - Weidner, Steffen T1 - ROPs of L-lactide catalyzed by neat Tin(II)2-ethylhexanoate - Influence of the reaction conditions on Tm and ΔHm N2 - L-Lactide was polymerized by means of neat SnOct2 with variation of LA/Cat ratio, temperature and time. The resulting cyclic polylactides crystallized spontaneously at 160 °C or below, but needed nucleation via mechanical stress at 165 or 170 °C. All the crystalline polylactides obtained directly from ROP above 120 °C had melting temperatures (Tm) above 189 °C (up to 194.5 °C). SnOct2 also enabled transformation of low Tm poly(L-lactide)s (Tm <180 °C) into the high Tm m1odification by annealing, due to the impact of transesterification reactions in the interphase between the crystallites. The influence of crystallization temperature and annealing time on the crystal thickness was studied via SAXS measurements. A comparison with the crystallization and annealing experiments reported by Pennings and coworkers and Tsuji and Ikada is discussed, and a satisfactory agreement has been found, because those authors also studied polyLA samples containing SnOct2 in its active form. It is also demonstrated in this work that the high Tm modification cannot be obtained when the catalyst is removed or poisoned as it is true for commercial polylactides. KW - Polylactide KW - MALDI-TOF MS KW - Crystallization PY - 2021 DO - https://doi.org/10.1016/j.polymer.2021.124122 SN - 0032-3861 VL - 231 SP - 1 EP - 10 PB - Elsevier CY - Oxford AN - OPUS4-53194 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sötebier, Carina A1 - Bierkandt, Frank A1 - Rades, Steffi A1 - Jakubowski, Norbert A1 - Panne, Ulrich A1 - Weidner, Steffen T1 - Sample loss in asymmetric flow field-flow fractionation coupled to inductively coupled plasma-mass spectrometry of silver nanoparticles N2 - In this work, sample losses of silver nanoparticles (Ag NPs) in asymmetrical flow field-flow fractionation (AF4) have been systematically investigated with the main focus on instrumental conditions like focusing and cross-flow parameters as well as sample concentration and buffer composition. Special attention was drawn to the AF4 membrane. For monitoring possible silver depositions on the membrane, imaging laser ablation coupled to inductively coupled plasma mass spectrometry (LA-ICP-MS) was used. Our results show that the sample residue on the membrane was below 0.6% of the total injected amount and therefore could be almost completely avoided at low sample concentrations and optimized conditions. By investigation of the AF4 flows using inductively coupled plasma mass spectrometry (ICP-MS), we found the recovery rate in the detector flow under optimized conditions to be nearly 90%, while the cross-flow, slot-outlet flow and purge flow showed negligible amounts of under 0.5%. The analysis of an aqueous ionic Ag standard solution resulted in recovery rates of over 6% and the ionic Ag content in the sample was found to be nearly 8%. Therefore, we were able to indicate the ionic Ag content as the most important source of sample loss in this study. KW - Asymmetric flow filed-flow fractionation KW - ICP-MS KW - Nanoparticles KW - Sample loss KW - Quantification PY - 2015 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-336171 DO - https://doi.org/10.1039/c5ja00297d SN - 0267-9477 SN - 1364-5544 VL - 30 IS - 10 SP - 2214 EP - 2222 PB - Royal Society of Chemistry CY - London AN - OPUS4-33617 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kühn, Gerhard A1 - Weidner, Steffen A1 - Decker, Renate A1 - Ghode, Archana A1 - Friedrich, Jörg Florian T1 - Selective surface functionalization of polyolefins by plasma treatment followed by chemical reduction N2 - Polymer surfaces can be finished with functional groups upon exposure to a plasma. Species of the plasma gas are attached at surface carbon atoms, forming functional groups of different composition. To produce a modified polymer surface with a high density and homogeneity of hydroxyl groups only, the oxygen-plasma-formed oxygen functional groups were chemically reduced by diborane and LiAlH4 with yields of 10 to 11 OH groups per 100 carbon atoms in the 3 to 5 nm near-surface layer as detected by X-ray photoelectron spectroscopy (XPS). The identification of hydroxyl groups was performed by means of attenuated total reflectance–Fourier transform infrared spectroscopy and XPS. KW - Attenuated total reflectance-Fourier transorm infrared spectroscopy KW - Chemical reduction of functional groups KW - Plasma modification KW - X-ray photoelectron spectroscopy PY - 1999 DO - https://doi.org/10.1016/S0257-8972(99)00232-7 SN - 0257-8972 VL - 116-119 SP - 796 EP - 801 PB - Elsevier Science CY - Lausanne AN - OPUS4-6983 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mechichi, R. A1 - Chabbah, T. A1 - Chatti, S. A1 - Jlalia, I. A1 - Sanglar, Corinne A1 - Casablanca, H. A1 - Vulliet, E. A1 - Marestin, C. A1 - Mercier, R. A1 - Weidner, Steffen A1 - Errachid, A. A1 - Hammani, M. A1 - Jaffrezic-Renault, N. A1 - Abderrazak, H. T1 - Semi‑interpenetrating Network‑Coated Silica Gel Based on Green Resources for the Efcient Adsorption of Aromatic Pollutants from Waters N2 - In the framework of the development of green analytical chemistry, a silica gel (SG) coated with a semi-penetrating network based on the partially biosourced poly(ethersulfone) is studied for a greener extraction process of aromatic organic pollutants. An optimized composition of the semi-penetrating network (80% of the linear polymer (LP): isosorbide-based poly(ethersulfone) and 20% cross-linking agent (XP) type bismaleimide) leads to a total adsorption of the selected aromatic pollutants, whatever their hydrophilicity. Adsorption characteristic, kinetics and isotherms of the SG-semi-INP LP80/XP20 for p-hydroxybenzoic acid and for toluic acid were studied. Langmuir model led to a better ftting of the adsorption isotherms; the adsorption of toluic acid is easier than that of p-hydroxybenzoic acid. 1/n values of benzoic acid was lower for SGsemi-INP LP80/XP20 compared to biochar and to cross-linked methacrylate resin, showing a higher adsorption efciency. KW - Isosorbide KW - Semi-interpenetrating networks KW - Silica gel modification KW - Aromatic pollutants KW - Adsorption PY - 2022 DO - https://doi.org/10.1007/s42250-022-00463 SN - 2522-5758 SP - 1 EP - 18 PB - Springer AN - OPUS4-55720 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sötebier, Carina A1 - Weidner, Steffen A1 - Jakubowski, Norbert A1 - Panne, Ulrich A1 - Bettmer, J. T1 - Separation and quantification of silver nanoparticles and silver ions using reversed phase high performance liquid chromatography coupled to inductively coupled plasma mass spectrometry in combination with isotope dilution analysis N2 - A reversed phase high performance liquid chromatography coupled to an inductively coupled plasma mass spectrometer (HPLC-ICP-MS) approach in combination with isotope dilution analysis (IDA) for the separation and parallel quantification of nanostructured and ionic silver (Ag) is presented. The main focus of this work was the determination of the ionic Ag concentration. For a sufficient stabilization of the ions without dissolving the nanoparticles (NPs), the eluent had to be initially optimized. The determined Ag ion concentration was in a good agreement with results obtained using ultrafiltration. Further, the mechanism of the NP separation in the HPLC column was investigated. Typical size exclusion effects were found by comparing results from columns with different pore sizes. Since the recovery rates decreased with increasing Ag NP size and large Ag NPs did not elute from the column, additional interactions of the particles with the stationary phase were assumed. Our results reveal that the presented method is not only applicable to Ag NPs, but also to gold and polystyrene NPs. Finally, IDA-HPLC-ICP-MS experiments in single particle mode were performed to determine the particle cut-off size. The comparison with conventional spICP-MS experiments resulted in a similar diameter and particle size distribution. KW - ICP-MS KW - Silver nanoparticles KW - HPLC KW - Isotope dilution analysis KW - Field flow fractionation KW - Toxicology PY - 2016 DO - https://doi.org/10.1016/j.chroma.2016.09.028 SN - 0021-9673 VL - 1468 SP - 102 EP - 108 PB - Elsevier B.V. AN - OPUS4-38642 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -