TY - JOUR A1 - Trubiroha, Peter A1 - Geburtig, Anja A1 - Wachtendorf, Volker T1 - Referenzmaterialien für Bewitterungsprüfungen von polymeren Werkstoffen KW - Referenzmaterial KW - Bestrahlen KW - Bewitterern KW - Polymer PY - 2003 SN - 0341-230X SN - 1431-827X VL - 36 IS - 3 SP - 35 EP - 39 PB - Baltz CY - München AN - OPUS4-2864 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ramanujam, Maalolan A1 - Wachtendorf, Volker A1 - Purohit, Purv A1 - Mix, Renate A1 - Schönhals, Andreas A1 - Friedrich, Jörg Florian T1 - A detailed dielectric relaxation spectroscopy study of artificial UV weathered low density polyethylene N2 - Artificial weathering of LDPE under dry conditions (<10% of relative humidity) by UV radiation was monitored by dielectric spectroscopy. For an apolar polymer like LDPE, dielectric study yields information about the change in structure and dynamics of the system. The fluctuations of the polar groups which are generated as a result of photooxidation such as carbonyl groups can be monitored as characteristic relaxation processes like the αc or β mode. The dielectric loss characterized by typical dielectric parameters like the activation energy and dielectric strength are strongly dependent upon changes induced by photooxidation in the amorphous and crystalline domains. This paper discusses in detail how the foil reached its mechanical disintegration. It was found that initial stages of weathering induce chain scission and/or crosslinking in the amorphous domains of the polymer and the motional processes in the crystalline regions are not affected. After this induction period, an increase in the degree of crystallization was observed by employing differential calorimetry. The increasing crystallinity is considered as one of the reasons for embrittlement which finally leads to the complete loss of the structural integrity. KW - Artificial weathering KW - UV radiation KW - Dielectric relaxation KW - LDPE PY - 2012 DO - https://doi.org/10.1016/j.tca.2011.12.003 SN - 0040-6031 SN - 1872-762X VL - 530 SP - 73 EP - 78 PB - Elsevier CY - Amsterdam AN - OPUS4-25547 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Simone A1 - Wachtendorf, Volker A1 - Rauth, W. A1 - Klimmasch, T. A1 - Krüger, P. T1 - Screening the weathering stability of automotive coatings by chemiluminescence N2 - Chemiluminescence (CL) is a sensitive method of investigating the thermo-oxidative stability of polymers in the early stages of degradation. Therefore, CL measurements were applied to different automotive coatings to evaluate their degradation behavior during artificial weathering. In this work, CL measurements were carried out for different automotive coatings to follow their degradation behavior during artificial weathering. The CL emission depends on sample-specific parameters like stabilizer, matrix, or hardener; experimental parameters like the oxygen partial pressure; and exposure parameters like the duration of weathering. The potential of CL could be demonstrated by classifying materials into categories of good, medium, and low degradation performance at a much earlier stage of weathering exposure than in combination with the usual visual detection of weathering effects. KW - Accelerated weathering KW - Coating KW - Chemiluminescence KW - Sensitive detection KW - Weathering PY - 2008 DO - https://doi.org/10.1007/s11998-007-9071-7 SN - 1547-0091 SN - 1935-3804 VL - 5 IS - 1 SP - 17 EP - 24 PB - Springer CY - Blue Bell, Pa. AN - OPUS4-16723 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Geburtig, Anja A1 - Wachtendorf, Volker A1 - Trubiroha, Peter T1 - Accelerated weathering test for plastics and coatings that are exposed to acidic precipitation N2 - Due to the occurrence of acidic precipitation, and due to the fact that polymers and stabilizers may be sensititve to acids, it is important to have a laboratory test that combines weathering exposure with acidic exposure. The loss of stabilization caused by an acid damage of stabilizing system gets evident only over the weathering progress. For solid samples, for wich mostly the surface properties are relevant, the "Acid Dew and Fog Test" (ADF test) was established. For woven or tufted materials, the "Acid Rain Test" (AR test) was developed. The proposed weathering tests aim at plastics as well as at coatings. T2 - 7th International Symposium on Weatherability (7th ISW) CY - Kanagawa, Japan DA - 2008-10-23 KW - Acid rain KW - ADF KW - Acid Dew and Fog test KW - Artificial Weathering test PY - 2009 SN - 1346-0633 VL - 21 IS - 2 SP - 69 EP - 73 PB - Materiaru-Raifu-Gakkai CY - Tokyo AN - OPUS4-18270 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Simone A1 - Brademann-Jock, Kerstin A1 - Wachtendorf, Volker A1 - Rauth, W. A1 - Klimmasch, T. A1 - Krüger, P. T1 - Analysis of weathering effects in automotive coatings by thermoluminescence KW - Automotive coatings KW - Weathering KW - Thermoluminescence PY - 2006 SN - 0048-4225 N1 - Sprachen: Englisch/Italienisch - Languages: English/Italian VL - 82 IS - 17 SP - 5 EP - 11 AN - OPUS4-14296 LA - mul AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Simone A1 - Wachtendorf, Volker A1 - Rauth, W. T1 - Kürzer in der Klimakammer - Rasche Beurteilung der Bewitterungsstabilität von 2K-PUR-Autolacken mittels Chemilumineszenz KW - Weathering KW - Chemiluminescence KW - Degradation KW - Coatings PY - 2007 SN - 0014-7699 VL - 113 IS - 9 SP - 46 EP - 49 PB - Vincentz CY - Hannover AN - OPUS4-15786 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Appajaiah, Anilkumar A1 - Wachtendorf, Volker A1 - Daum, Werner T1 - Characterization of thermo-oxidative stability of polymer optical fibers using chemiluminescence technique N2 - The thermo-oxidative stability of commercially available polymer optical fibers (POFs) and their components (cores and claddings) was investigated. All the bare POFs (core and cladding only) studied here were based on poly(methyl methacrylate) (PMMA) core. The fibers were exposed to 100 °C/low humidity for about 4200 h. Chemiluminescence (CL) technique was applied to investigate the thermo-oxidative stability and for measuring the transmission loss during exposure a prototype device called multiplexer was used. POFs exhibited variation in thermo-oxidative stability although they possessed identical core material PMMA. This was due to difference in the chemical compositions of claddings. Claddings were more susceptible to the thermo-oxidative degradation compared to cores. The thermo-oxidative degradation of both the cladding and the core was found in POFs as a result of climatic exposure. POFs showed an early drop-off followed by a slow decline of transmission. The early drop-off of transmission was attributed to physical changes like thermal expansion and the slow decline of transmission to chemical changes like oxidative degradation of POFs. A good linear relationship between optical transmission stability and thermo-oxidative stability of POFs was established from these studies. KW - Polymer optical fibers (POFs) KW - Chemiluminescence (CL) KW - Thermo-oxidative stability KW - Aging KW - Optical transmission stability PY - 2006 DO - https://doi.org/10.1016/j.polymdegradstab.2006.05.006 SN - 0141-3910 SN - 1873-2321 VL - 91 IS - 11 SP - 2605 EP - 2613 PB - Applied Science Publ. CY - London AN - OPUS4-13984 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Damerau, Thomas A1 - Sabelus, Silke A1 - Wachtendorf, Volker A1 - Hennecke, Manfred A1 - Greiner, A. T1 - Photochemische und thermische Stabilität eines Phenylen-Vinylen-Polymeren KW - Photostability KW - Fluorescence KW - Chemiluminescence PY - 1996 SN - 0016-3538 VL - 40 IS - 7 SP - 710 EP - 712 PB - GIT-Verlag CY - Darmstadt AN - OPUS4-23205 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wachtendorf, Volker A1 - Geburtig, Anja T1 - Alterungseffekte bei Polymerwerkstoffen messen N2 - Bei der Auswahl von Werkstoffen spielt deren Alterung oft eine untergeordnete Rolle, stattdessen wird häufig der ungealterte Ausgangszustand optimiert. Materialien altern aber unterschiedlich. Der Effekt der molekularen Alterung spiegelt sich in den Eigenschaften mehr oder weniger stark und in unterschiedlichem zeitlichen Verlauf wider. Da es kein physikalisch-chemisches Modell dafür gibt, sind Alterungseffekte empirisch zu bestimmen. KW - Alterung KW - Polymerwerkstoff KW - Eigenschaftsänderung PY - 2012 DO - https://doi.org/10.1002/nadc.201290356 SN - 1439-9598 SN - 1521-3854 VL - 60 IS - 10 SP - 1018 EP - 1022 PB - Wiley-VCH Verl. CY - Weinheim AN - OPUS4-26666 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Geburtig, Anja A1 - Goedecke, Thomas A1 - Wachtendorf, Volker T1 - Combined impact of ultraviolet and chemical fluids on high-density polyethylene packaging material N2 - To investigate the ageing behaviour of filled plastic containers outdoors, square cuts of the wall of two high-density polyethylene (HDPE) types were exposed to ultraviolet (UV) radiation at their front side and to specific liquid chemicals (de-ionized water, surfactant or White Spirit) at their back. The UV radiant exposure at the front side was 80 MJ/m². To compare the actions of the different exposures, separate dark backside fluid exposures were performed, in parallel. Besides, UV weathering was carried out until a UV radiant exposure of 325 MJ/m², being roughly comparable to outdoor exposure of one year in Northern Australia. An unpigmented HDPE included in the investigation gave no sufficient protection for the White Spirit. In addition, it showed clear degradation after several of these exposures. In combination with the White Spirit, an increase of carbonyl bonds was measured, presumably assignable to degradation products of the White Spirit. For a pigmented HDPE material, with the implemented combined exposures, no relevant damage was observed, within applied the exposure period. KW - Weathering KW - UV KW - HDPE KW - Packaging PY - 2012 DO - https://doi.org/10.1002/pts.959 SN - 0894-3214 VL - 25 IS - 1 SP - 53 EP - 61 PB - Wiley CY - Chichester, UK AN - OPUS4-25417 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kalbe, Ute A1 - Krüger, Oliver A1 - Wachtendorf, Volker A1 - Berger, Wolfgang A1 - Hally, S. T1 - Development of leaching procedures for synthetic turf systems containing scrap tyre granules N2 - Scrap tyres are widely reused in the form of granules as infill materials or component of sub-base layers in construction of sporting grounds such as synthetic turf areas and athletic track surfaces. The recycled rubber may contain organic and inorganic pollutants due to the presence of vulcanisation catalysts, stabilisers and other additives which can be released into soil and groundwater in the case of outdoor sports facilities. In order to evaluate the amount of potentially mobile pollutants, leaching tests can be employed. This study aimed particularly at the investigation of the feasibility of column tests using complete synthetic surface flooring or turf system assemblies. The release of zinc and polycyclic aromatic hydrocarbons (PAH) leached from components of sports surfaces containing recycled rubber granules was considered. Additionally, batch tests on coated and uncoated styrene butadiene rubber (SBR) granules aged by artificial weathering were performed to indicate its possible influence on the leaching behaviour of zinc and PAH. The chosen approach of column tests simulating typical complete synthetic sports surface installations has been proven to be feasible and robust. The time-dependent leaching behaviour and interactions between single components can be evaluated by column tests. Zinc was the most relevant contaminant in the eluates and its leachability was enhanced after accelerated ageing by artificial weathering. Leachable PAH were found in relatively low but well detectable amounts which increase by ageing as well. KW - Waste rubber KW - SBR KW - Artificial turf KW - Leaching KW - behaviour KW - Column test KW - Batch test KW - Weathering PY - 2013 DO - https://doi.org/10.1007/s12649-013-9248-5 SN - 1877-2641 SN - 1877-265X VL - 4 IS - 4 SP - 745 EP - 757 PB - Springer Science + Business Media CY - Dordrecht AN - OPUS4-29454 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Geburtig, Anja A1 - Wachtendorf, Volker A1 - Falkenhagen, Jana T1 - Combined impact of UV radiation and nitric acid on high‐density polyethylene containers as a laboratory test N2 - In a laboratory test, transparent high‐density polyethylene (HDPE) jerrycans have been exposed to both UV radiation and 55 wt‐% nitric acid solution at (41 ± 2)°C, for up to 20 days. For comparison, UV radiant exposure (21 days) and nitric acid exposure (up to 6 weeks) were performed separately, at nearly equal temperatures. The damages are compared with FTIR spectroscopy in ATR and HT‐gel permeation chromatography(GPC) on a molecular level and with hydraulic internal pressure testing as a component test. For the used jerrycans, relevant oxidation can only be found after the combined exposure. This is caused by the decomposition of nitric acid into nitrous gases by UV radiation, which is also observed at lower concentrations (28 wt‐%). After 6 days of laboratory exposure, this is rated as critical, which corresponds to about 1/10 year in Central Europe, according to the UV radiant exposure. The gradual increase in oxidative damage shows the reproducibility of the test. KW - Molecular mass distribution KW - High-density polyethylene KW - Nitric acid KW - UV radiation PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-550141 DO - https://doi.org/10.1002/pts.2673 SN - 0894-3214 SP - 1 EP - 7 PB - John Wiley & Sons Ltd AN - OPUS4-55014 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Meyer, S. A1 - Timmel, S. A1 - Gläser, M. A1 - Braun, Ulrike A1 - Wachtendorf, Volker A1 - Hagendorf, C. T1 - Polymer foil additives trigger the formation of snail trails in photovoltaic modules N2 - After several months of operation, many photovoltaic (PV) modules develop a discolouration defect called snail trails which appear as irregular dark traces across the cells. These traces are caused by silver nanoparticles accumulating within the encapsulation foil directly above the grid finger. In this work we systematically investigate combinations of encapsulation and back-sheet foils with respect to their susceptibility for snail trails. We can show that certain additive compositions within the encapsulation and back sheet foils are critical for the formation of the discolouring silver nanoparticles. We suggest a reaction model explaining the formation of snail trails from a chemical point of view. This fundamental understanding allows the rapid testing of foils for their snail trail sensitivity as well as the special design of resistant foils. KW - Snail trails KW - Encapsulation foil KW - Back-sheet foil KW - Additives KW - Silver nanoparticles PY - 2014 DO - https://doi.org/10.1016/j.solmat.2014.06.028 SN - 0927-0248 VL - 130 SP - 64 EP - 70 PB - Elsevier B.V. CY - Amsterdam [u.a.] AN - OPUS4-31249 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Appajaiah, Anilkumar A1 - Wachtendorf, Volker A1 - Daum, Werner T1 - Climatic exposure of polymer optical fibers: Thermooxidative stability characterization by chemiluminescence N2 - The optical transmission stability was investigated for commercially available polymer optical fibers (POFs) which were exposed to a climate of 92°C and 95% relative humidity for about 3300 h. The optical transmission stability of POFs was correlated to their thermooxidative stability. POFs possessed identical core material, poly(methyl methacrylate), but they differed in the materials used for the claddings. The optical transmission was measured online using a prototype device called multiplexer. The chemiluminescence (CL) technique was applied to characterize the thermooxidative stability and degradation of POFs. CL analysis reveals the thermooxidative degradation of bare POFs (core and cladding), predominantly of the claddings, as a result of climatic exposure. Ultraviolet-visible transmittance measurements demonstrated more changes in the claddings as compared to the cores due to degradation. The CL and optical measurements data indicated that the optical transmission stability of POFs was dependent mainly on the thermooxidative stability of the claddings and their chemical compositions. KW - Ageing KW - Polymer optical fiber KW - Degradation KW - Chemiluminescence KW - Transparency PY - 2007 DO - https://doi.org/10.1002/app.23955 SN - 0021-8995 SN - 1097-4628 VL - 103 IS - 3 SP - 1593 EP - 1601 PB - Wiley InterScience CY - Hoboken, NJ AN - OPUS4-19072 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wachtendorf, Volker A1 - Geburtig, Anja T1 - Chemiluminescence for the early detection of weathering effects of coatings - Part I: Fundamentals KW - Chemiluminescence KW - Weathering KW - Polymer KW - Oxidation PY - 2010 SN - 1547-0083 VL - 7 IS - 4 SP - 66 EP - 71 PB - Federation of Societies for Coatings Technology CY - Blue Bell, Pa. AN - OPUS4-21493 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wachtendorf, Volker A1 - Geburtig, Anja T1 - Chemiluminescence for the early detection of weathering effects of coatings - Part II: Experimental set-up and examination KW - Chemiluminescence KW - Weathering KW - Polymer KW - Oxidation PY - 2010 SN - 1547-0083 VL - 7 IS - 5 SP - 38 EP - 44 PB - Federation of Societies for Coatings Technology CY - Blue Bell, Pa. AN - OPUS4-21494 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Geburtig, Anja A1 - Wachtendorf, Volker T1 - Determination of the spectral sensitivity and temperature dependence of polypropylene crack formation caused by UV-irradiation N2 - For polypropylene of varied stabilization, spectral sensitivity as well as temperature dependence of irradiation caused crack formation was determined in artificial irradiation tests. UV radiant exposure HUV necessary to generate crack formation was measured both in spectrally dispersed irradiation and artificial irradiation in a Fluorescent UV lamp device. Dependencies were fitted to a plateau function and an Arrhenius function, respectively, to describe the action of irradiation by response functions. Applied to weather data from Phoenix, the results were compared with respective outdoor exposure results. KW - Weathering KW - UV KW - Temperature KW - Numerical simulation PY - 2010 DO - https://doi.org/10.1016/j.polymdegradstab.2010.06.014 SN - 0141-3910 SN - 1873-2321 VL - 95 IS - 10 SP - 2118 EP - 2123 PB - Applied Science Publ. CY - London AN - OPUS4-21913 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schulz, Ulrich A1 - Wachtendorf, Volker A1 - Geburtig, Anja T1 - Pinholes - the negative impact of mildew growth PY - 2004 SN - 0930-3847 VL - 5 SP - 26 EP - 30 PB - Vincentz CY - Hannover AN - OPUS4-21350 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Theiler, Geraldine A1 - Wachtendorf, Volker A1 - Elert, Anna Maria A1 - Weidner, Steffen T1 - Effects of UV radiation on the friction behavior of thermoplastic polyurethanes N2 - The effects of weathering exposure on unfilled and filled thermoplastic polyurethanes (TPU) materials are described as performed under different humidity conditions. For this purpose, a weathering device was used with UV-A 340 nm lamps at a constant temperature of 40 °C. The effects of environmental (UV and humidity condition) degradation on the frictional properties of TPU materials are presented along with surface analyses to characterize the chemistry of the degradative process. Photooxidative degradation of unfilled polymer leads to deterioration of physical and mechanical properties, which affects its tribological behavior significantly. Due to crosslinking, the stiffness of the material increases, reducing drastically the friction coefficient of unfilled TPUs. The frictional behavior of glass fiber reinforced TPU is less affected by radiation. KW - Photooxidation KW - UV radiation KW - Friction KW - TPU KW - Humidity PY - 2018 DO - https://doi.org/10.1016/j.polymertesting.2018.08.006 SN - 0142-9418 SN - 1873-2348 VL - 70 SP - 467 EP - 473 PB - Elsevier Ltd. CY - Amsterdam AN - OPUS4-45709 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Geburtig, Anja A1 - Wachtendorf, Volker A1 - Trubiroha, P. T1 - Exposure response function for a quantitative prediction of weathering caused aging of polyethylene N2 - The exposure response function of the carbonyl formation over the bulk has been determined for a high-density polyethylene of a thickness of 200 μm, which was used as a weathering reference material according to ISO TR 19032. To this end, spectral sensitivity was studied by local measurement of the effect of spectrally dispersed irradiation. Both the exposure device and the methodology of determination are described. The temperature dependency of photooxidation was determined by UV exposure at various temperatures between 23 and 80 °C. Deviations from linearity and thus reciprocity below 40 °C are discussed and assumed to be related to diffusion limitations. An Arrhenius approach –based on data of linear carbonyl formation – has been incorporated into the exposure response function. Using this exposure response function, aging in terms of the distribution of a quantitative property change over a plastic component can be predicted for a specific outdoor location with real chronologic weather data as input for the exposure. Thus, artificial and natural weathering can be linked and compared. The established exposure response function has been validated by outdoor exposure results from the literature. If an estimated diffusion limitation is taken into consideration, calculations and published data are in good agreement. KW - Irradiation KW - Weathering KW - Spectral sensitivity KW - Temperature dependency KW - Spectral irradiation PY - 2019 DO - https://doi.org/10.3139/120.111348 SN - 0025-5300 VL - 61 IS - 6 SP - 517 EP - 526 PB - Carl Hanser Verlag GmbH & Co. KG AN - OPUS4-48295 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -