TY - CONF A1 - Trubiroha, P. A1 - Geburtig, Anja A1 - Wachtendorf, Volker T1 - Natural versus artificial weathering of polymers – main differences in climatic conditions T2 - Proceedings 8th European Weathering Symposium - Natural and Artificial Ageing of Polymers N2 - Different climatic conditions and weather variables during natural and artificial exposure of polymers may be reasons for an unsatisfying correlation between the ageing results. Here the main differences are discussed for: - Global solar radiation In weathering devices there is a constant spectral irradiance which is 5 times higher than the averaged spectral irradiance outdoors, which is strongly varying in its diurnal course. Intensified weathering using Fresnel reflectors concentrates only the direct solar radiation with a relatively low UV proportion. Problems of reciprocity may arise from the different mean of irradiance levels. - Temperatures at specimen surfaces. Because of the high irradiance levels mentioned above, artificial exposures may lead to high surface temperatures and large temperature differences between differently coloured specimen surfaces, if the artificial radiation source emits much VIS- and IR-radiation. Outdoors the surface temperature and temperature differences of exposed specimens are influenced by considerably lower irradiance levels and additionally by an effective radiation loss in the night. - Relative humidity at specimen surfaces In weathering devices the relative humidity at specimen surfaces is very low if it is uncontrolled. If controlled by ultrasonic humidifiers or spray nozzles, the additional exposure to water droplets is quite likely. - Wetness on specimen surfaces All usual spray programs prescribed in weathering standards recommend frequently changing of short spray/dry periods and result in total times of wetness (TOW) of the exposed specimen surfaces which is only about 30 % of the outdoor TOW. - Acidic precipitation and bio films Acidic precipitation and bio films are usual outdoor conditions which are only considered in special weathering tests. T2 - 8th European Weathering Symposium CY - Vienna, Austria DA - 20.09.2017 KW - Artificial weathering KW - Natural weathering KW - Weathering parameters PY - 2017 SN - 978-3-9818507-1-0 VL - 18 SP - 63 EP - 75 CY - Karlsruhe AN - OPUS4-42127 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wachtendorf, Volker A1 - Barthel, Anne-Kathrin A1 - Geburtig, Anja A1 - Trubiroha, P. ED - Reichert, T. T1 - Low-Temperature Irradiation Experiments for PE, PA, and PC Matrices T2 - Proceedings 8th European Weathering Symposium - Natural and Artificial Ageing of Polymers N2 - In this paper, we demonstrate the effects of radiation exposures of polymeric materials with UV-A 340 nm lamps (ISO 4892-3, Type 1A) at -10 °C in comparison to an irradiation at +50 °C using a Global UV Test 200 fluorescent lamp device from Weiss Umwelttechnik GmbH, which incorporates an active cooling appliance. While the effects at -10 °C actually are lower than at + 50°C their extent was clearly beyond expectations. T2 - 8th European Weathering Symposium CY - Vienna, Austria DA - 20.09.2017 KW - Artificial weathering KW - Irradiation KW - Low-temperature KW - Photo-oxidation KW - Polyamide KW - Polycarbonate KW - Polyethylene PY - 2017 SN - 978-3-9818507-1-0 VL - 18 SP - Paper 22, 319 EP - 329 PB - Thomas Würtz Grafik Design CY - Karlsruhe AN - OPUS4-42130 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wachtendorf, Volker A1 - Kalbe, Ute A1 - Krüger, O. A1 - Bandow, Nicole ED - Brown, R. ED - Gedde, U.W. ED - Hedenqvist, M.S. T1 - Influence of weathering on the leaching behaviour of zinc and PAH from synthetic sports surfaces JF - Polymer Testing N2 - Synthetic materials used for outdoor sports grounds consist of a mix of inorganic, organic and polymeric compounds that show ageing due to weathering and a complex leaching behaviour by percolation of rainwater, which can limit its lifetime. Additionally, weathering exposure induces degradation processes in the polymers, which leads to the formation of new surfaces allowing water to access additional reservoirs of leachable compounds. A laboratory test comprising artificial weathering, ozonisation and subsequent leaching was developed to investigate this behaviour in a reproducible and controllable way. The experiments showed a general decline of Zn, polycyclic aromatic hydrocarbons (PAH) and total organic carbon (TOC) concentrations after an initial increase. Within this general trend, the course of concentration over exposure duration is very specific for individual sample materials and the analyte under investigation. The results indicate that weathering and degradation behaviour cannot be predicted from initial material conditions. Thus, weathering experiments are recommended to fill this gap of knowledge. KW - Athletic tracks KW - Artificial turf KW - Ageing KW - Artificial weathering KW - Polymer degradation KW - Rubber granules KW - Leaching KW - Contamination PY - 2017 DO - https://doi.org/10.1016/j.polymertesting.2017.09.021 SN - 0142-9418 SN - 1873-2348 VL - 63 IS - October SP - 621 EP - 631 PB - Elsevier Ltd. CY - Amsterdam, The Netherlands AN - OPUS4-42205 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -