TY - JOUR A1 - Frasca, Daniele A1 - Schulze, Dietmar A1 - Wachtendorf, Volker A1 - Huth, Christian A1 - Schartel, Bernhard T1 - Multifunctional multilayer graphene/elastomer nanocomposites N2 - Elastomers are usually reinforced and employed in different applications. Various different nanoparticles, including layered silicates, carbon nanotubes, and expanded graphite, are currently being used as nanofiller. Multilayer Graphene (MLG) is proposed as promising nanofiller to improve the functional properties of Chlorine-Isobutylene-Isoprene Rubber (CIIR), Nitrile-Butadiene Rubber (NBR), Natural Rubber (NR) and Styrene–Butadiene Rubber (SBR) at low concentrations. MLG is constituted by only approximately 10 graphene sheets. Nanocomposites with extremely low MLG content (3 phr) showed evident improvement in rheological, mechanical and curing properties. The Young's modulus of the nanocomposites increased more than twice in comparison with the unfilled rubbers. MLG also improved the weathering resistance of the different rubbers. The nanocomposites conserved their initial mechanical properties against weathering exposure. KW - Elastomer KW - Nanocomposite KW - Multilayer graphene PY - 2015 DO - https://doi.org/10.1016/j.eurpolymj.2015.07.050 SN - 0014-3057 SN - 1873-1945 VL - 71 SP - 99 EP - 113 PB - Elsevier Ltd. CY - Oxford AN - OPUS4-33843 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Tan, Yi A1 - Wachtendorf, Volker A1 - Kukofka, Tobias A1 - Klack, Patrick A1 - Ruder, J. A1 - Lin, Xuebao A1 - Schartel, Bernhard T1 - Degradation of flame retardance: A comparison of ethylene‐vinyl acetate and low‐density polyethylene cables with two different metal hydroxides N2 - The durability of flame retardancy is a challenge for cables over long lifetimes. The degradation of flame retardance is investigated in two kinds of exposures, artificial weathering and humidity. In this basic study, typical mineral flame retardants in two polymers frequently used in cable jackets are investigated to get the fundamental picture. Aluminum hydroxide (ATH) and magnesium hydroxide (MDH) are compared in ethylene‐vinyl acetate (EVA), and further in EVA and linear low‐density polyethylene (LLDPE) cables containing the same ATH. The changes in chemical structure at the surface are studied through attenuated total reflectance Fourier transform infrared spectroscopy (ATR‐FTIR), the formation of cracks, and changes in color are investigated. The cone calorimeter and a bench scale fire testing cable module are utilized to evaluate the fire behavior of the cables. Although the flame retardancy deteriorated slightly, it survived harsh exposure conditions for 2000 h. Compared to EVA/MDH and LLDPE/ATH, the fire behavior of EVA/ATH is the least sensitive. Taken together, all of the results converge to estimate that there will be no problem with flame retardancy performance, for materials subjected to natural exposure for several years; the durability of fire retardancy is questionable for longer periods, and thus requires further investigation. KW - Durability KW - Flame retardant KW - Aluminum hydroxide (ATH) KW - Magnesium hydroxide KW - Ethylene-vinyl acetate KW - Cables KW - Weathering PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-519573 DO - https://doi.org/10.1002/app.50149 VL - 138 IS - 14 SP - 50149 PB - Wiley AN - OPUS4-51957 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Daus, Lars-Hendrik A1 - Schartel, Bernhard A1 - Wachtendorf, Volker A1 - Mangelsdorf, R. A1 - Korzen, Manfred T1 - A chain is no stronger than its weakest link: Weathering resistance of water-based intumescent coatings for steel applications N2 - A systematic approach was used to investigate the weathering-induced degradation of a common water–based intumescent coating. In this study, the coatings are intended for humid indoor applications on steel substrates. The coating contains ammonium polyphosphate, pentaerythritol, melamine, and polyvinyl acetate. By replacing each ingredient with a less water-soluble substance, the most vulnerable substances, polyvinyl acetate and pentaerythritol, were identified. Furthermore, the weathering resistance of the system was improved by exchanging the ingredients. The coatings were stressed by artificial weathering tests and evaluated by fire tests. Thermogravimetry and Fourier-transform infrared spectroscopy were used to study the thermal decomposition. This study lays the foundation for the development of a new generation of water-based intumescent coatings. KW - Intumescence KW - Fire resistance KW - Fire protective coatings KW - Weathering KW - Thermogravimetric analyses PY - 2021 DO - https://doi.org/10.1177/0734904120961064 SN - 0734-9041 SN - 1530-8049 VL - 39 IS - 1 SP - 72 EP - 102 PB - SAGE AN - OPUS4-52015 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Qiu, Y. A1 - Wachtendorf, Volker A1 - Klack, Patrick A1 - Qian, L. A1 - Liu, Z. A1 - Schartel, Bernhard T1 - Improved flame retardancy by synergy between cyclotetrasiloxane and phosphaphenanthrene/triazine compounds in epoxy thermoset N2 - A siloxane compound (MVC) and a bi-group phosphaphenanthrene/triazine compound (TGD) were employed in epoxy thermosets to explore high-efficiency flame retardant systems. With only 1wt% MVC and 3wt% TGD, an epoxy thermoset passed UL 94 V-0 rating test and achieved a limiting oxygen index value of 34.0%, exhibiting an excellent flame retardant effect. The MVC/TGD system not only decreased the peak value of heat release rate and effective heat of combustion but also imparted an improved charring ability to thermosets, thereby outstandingly reducing the flammability of 1%MVC/3%TGD/EP. Compared with the fire performance of 4%TGD/EP and 4%MVC/EP, the MVC/TGD system showed an obvious flame retardant synergistic effect, mainly depending on the general improvement of flame inhibition, charring and barrier effects of the thermoset during combustion. Evolved gas analysis combinedwith condensed-phase pyrolysis product Analysis jointly revealed the details of the changed pyrolysis mode. KW - Flame retardant KW - Epoxy resin KW - Synergy KW - Siloxane KW - DOPO KW - Triazine PY - 2017 DO - https://doi.org/10.1002/pi.5466 SN - 0959-8103 SN - 1097-0126 VL - 66 IS - 12 SP - 1883 EP - 1890 PB - Wiley AN - OPUS4-42950 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bandow, Nicole A1 - Will, Verena A1 - Wachtendorf, Volker A1 - Simon, Franz-Georg T1 - Contaminant release from aged microplastic N2 - Recycled plastic granules of high-density polyethylene, polyvinyl chloride and polystyrene the size of microplastics were exposed to artificial aging conditions (2000 h; photooxidative and thermo-oxidative) to simulate their fate outdoors. Their potential to leach into water during the aging process was investigated using column percolation tests. Aging-related changes on the surface of the material were characterised by IR measurements indicating oxidation reactions with the formation of new adsorption bands (C=O, C–O and OH), especially in the case of photooxidative aging. These findings were confirmed by the identification of leachable organic compounds. Leaching of total organic carbon, Cl, Ca, Cu and Zn is clearly affected by changes due to aging, and their release is increased after photooxidative aging. In general, exposure to photooxidative conditions shows a greater influence on aging and thus on leaching and seems to be the more important mechanism for the aging of microplastic in the environment. Comparison with the total content of inorganic species revealed that, for most elements, less than 3% of the total content is released after 2000 h of photooxidative aging. KW - Column percolation tests KW - Heavy metals KW - Photo-oxidation KW - Thermo-oxidation PY - 2017 DO - https://doi.org/10.1071/EN17064 SN - 1448-2517 SN - 1449-8979 VL - 14 IS - 6 SP - 394 EP - 405 AN - OPUS4-43222 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Fornacon-Wood, C. A1 - Stühler, M. R. A1 - Gallizioli, C. A1 - Manjunatha, B. R. A1 - Wachtendorf, Volker A1 - Schartel, Bernhard A1 - Plajer, A. J. T1 - Precise construction of weather-sensitive poly(ester-alt-thioesters) from phthalic thioanhydride and oxetane N2 - We report the selective ring opening copolymerisation (ROCOP) of oxetane and phthalic thioanhydride by a heterobimetallic Cr(III)K catalyst precisely yielding semi-crystalline alternating poly(esteralt- thioesters) which show improved degradability due to the thioester links in the polymer backbone. KW - Sulfur containing polymers KW - Durability KW - Weathering KW - Synthesis PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-590762 DO - https://doi.org/10.1039/d3cc03315e SN - 1364-548X VL - 59 IS - 76 SP - 11353 EP - 11356 PB - RSC AN - OPUS4-59076 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Milks, A. A1 - Lehmann, J. A1 - Leder, D. A1 - Sietz, M. A1 - Koddenberg, T. A1 - Böhner, U. A1 - Wachtendorf, Volker A1 - Terberger, T. T1 - A double-pointed wooden throwing stick from Schöningen, Germany: Results and new insights from a multianalytical study N2 - The site of Schöningen (Germany), dated to ca. 300,000 years ago, yielded the earliest large-scale record of humanly-made wooden tools. These include wooden spears and shorter double-pointed sticks, discovered in association with herbivores that were hunted and butchered along a lakeshore. Wooden tools have not been systematically analysed to the same standard as other Palaeolithic technologies, such as lithic or bone tools. Our multianalytical study includes micro-CT scanning, 3-dimensional microscopy, and Fourier transform infrared spectroscopy, supporting a systematic technological and taphonomic analysis, thus setting a new standard for wooden tool analysis. In illustrating the biography of one of Schöningen’s double-pointed sticks, we demonstrate new human behaviours for this time period, including sophisticated woodworking techniques. The hominins selected a spruce branch which they then debarked and shaped into an aerodynamic and ergonomic tool. They likely seasoned the wood to avoid cracking and warping. After a long period of use, it was probably lost while hunting, and was then rapidly buried in mud. Taphonomic alterations include damage from trampling, fungal attack, root damage and compression. Through our detailed analysis we show that Middle Pleistocene humans had a rich awareness of raw material properties, and possessed sophisticated woodworking skills. Alongside new detailed morphometrics of the object, an ethnographic review supports a primary function as a throwing stick for hunting, indicating potential hunting strategies and social contexts including for communal hunts involving children. The Schöningen throwing sticks may have been used to strategically disadvantage larger ungulates, potentially from distances of up to 30 metres. They also demonstrate that the hominins were technologically capable of capturing smaller fast prey and avian fauna, a behaviour evidenced at contemporaneous Middle Pleistocene archaeological sites. KW - FTIR KW - Stone Age KW - Middle Pleistocene KW - Throwing-stick KW - Wood KW - Micro-CT scanning KW - 3-dimensional microscopy PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-580012 DO - https://doi.org/10.1371/journal.pone.0287719 SN - 1932-6203 VL - 18 IS - 7 SP - 1 EP - 32 PB - PLOS CY - San Francisco, California, US AN - OPUS4-58001 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Meyer, S. A1 - Timmel, S. A1 - Gläser, M. A1 - Braun, Ulrike A1 - Wachtendorf, Volker A1 - Hagendorf, C. T1 - Polymer foil additives trigger the formation of snail trails in photovoltaic modules N2 - After several months of operation, many photovoltaic (PV) modules develop a discolouration defect called snail trails which appear as irregular dark traces across the cells. These traces are caused by silver nanoparticles accumulating within the encapsulation foil directly above the grid finger. In this work we systematically investigate combinations of encapsulation and back-sheet foils with respect to their susceptibility for snail trails. We can show that certain additive compositions within the encapsulation and back sheet foils are critical for the formation of the discolouring silver nanoparticles. We suggest a reaction model explaining the formation of snail trails from a chemical point of view. This fundamental understanding allows the rapid testing of foils for their snail trail sensitivity as well as the special design of resistant foils. KW - Snail trails KW - Encapsulation foil KW - Back-sheet foil KW - Additives KW - Silver nanoparticles PY - 2014 DO - https://doi.org/10.1016/j.solmat.2014.06.028 SN - 0927-0248 VL - 130 SP - 64 EP - 70 PB - Elsevier B.V. CY - Amsterdam [u.a.] AN - OPUS4-31249 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Frasca, Daniele A1 - Schulze, Dietmar A1 - Wachtendorf, Volker A1 - Morys, Michael A1 - Schartel, Bernhard T1 - Multilayer graphene/chlorine-isobutene-isoprene rubber nanocomposites: the effect of dispersion N2 - Multilayer graphene (MLG) is composed of approximately 10 sheets of graphene. It is a promising nanofiller just starting to become commercially available. The Dispersion of the nanofiller is essential to exploit the properties of the nanocomposites and is dependent on the preparation method. In this study, direct incorporation of 3 parts per hundred of rubber (phr) MLG into chlorine-isobutene- isoprene rubber (CIIR) on a two-roll mill did not result in substantial enhancement of the material properties. In contrast, by pre-mixing the MLG (3 phr) with CIIR using an ultrasonically assisted solution mixing procedure followed by two-roll milling, the properties (rheological, curing, and mechanical) were improved substantially compared with the MLG/CIIR nanocomposites mixed only on the mill. The Young’s moduli of the nanocomposites mixed in solution increased by 38%. The CIIR/MLG nanocomposites produced via solution showed superior durability against weathering exposure. KW - Multilayer graphene KW - Nanocomposite KW - Dispersion KW - Rubber PY - 2016 DO - https://doi.org/10.1002/pat.3740 SN - 1042-7147 SN - 1099-1581 VL - 27 IS - 7 SP - 872 EP - 881 PB - Wiley AN - OPUS4-36866 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schulz, Ulrich A1 - Wachtendorf, Volker A1 - Geburtig, Anja T1 - Pinholes - the negative impact of mildew growth PY - 2004 SN - 0930-3847 VL - 5 SP - 26 EP - 30 PB - Vincentz CY - Hannover AN - OPUS4-21350 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wachtendorf, Volker A1 - Geburtig, Anja T1 - Chemiluminescence for the early detection of weathering effects of coatings - Part I: Fundamentals KW - Chemiluminescence KW - Weathering KW - Polymer KW - Oxidation PY - 2010 SN - 1547-0083 VL - 7 IS - 4 SP - 66 EP - 71 PB - Federation of Societies for Coatings Technology CY - Blue Bell, Pa. AN - OPUS4-21493 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wachtendorf, Volker A1 - Geburtig, Anja T1 - Chemiluminescence for the early detection of weathering effects of coatings - Part II: Experimental set-up and examination KW - Chemiluminescence KW - Weathering KW - Polymer KW - Oxidation PY - 2010 SN - 1547-0083 VL - 7 IS - 5 SP - 38 EP - 44 PB - Federation of Societies for Coatings Technology CY - Blue Bell, Pa. AN - OPUS4-21494 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Appajaiah, Anilkumar A1 - Wachtendorf, Volker A1 - Daum, Werner T1 - Climatic exposure of polymer optical fibers: Thermooxidative stability characterization by chemiluminescence N2 - The optical transmission stability was investigated for commercially available polymer optical fibers (POFs) which were exposed to a climate of 92°C and 95% relative humidity for about 3300 h. The optical transmission stability of POFs was correlated to their thermooxidative stability. POFs possessed identical core material, poly(methyl methacrylate), but they differed in the materials used for the claddings. The optical transmission was measured online using a prototype device called multiplexer. The chemiluminescence (CL) technique was applied to characterize the thermooxidative stability and degradation of POFs. CL analysis reveals the thermooxidative degradation of bare POFs (core and cladding), predominantly of the claddings, as a result of climatic exposure. Ultraviolet-visible transmittance measurements demonstrated more changes in the claddings as compared to the cores due to degradation. The CL and optical measurements data indicated that the optical transmission stability of POFs was dependent mainly on the thermooxidative stability of the claddings and their chemical compositions. KW - Ageing KW - Polymer optical fiber KW - Degradation KW - Chemiluminescence KW - Transparency PY - 2007 DO - https://doi.org/10.1002/app.23955 SN - 0021-8995 SN - 1097-4628 VL - 103 IS - 3 SP - 1593 EP - 1601 PB - Wiley InterScience CY - Hoboken, NJ AN - OPUS4-19072 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Braun, Ulrike A1 - Wachtendorf, Volker A1 - Geburtig, Anja A1 - Bahr, Horst A1 - Schartel, Bernhard T1 - Weathering resistance of halogen-free flame retardance in thermoplastics N2 - The influence of weathering on the fire retardancy of polymers is investigated by means of a cone calorimeter test, before and after artificial weathering. The surface degradation was monitored using different techniques (ATR–FTIR, microscopy, colour measurement). Different kinds of polymeric materials were chosen, all as they are used in practice: polycarbonate (PC) blends, polyamide (PA) and polypropylene (PP) flame-retarded with arylphosphate, melamine cyanurate (MC) and intumescent formulation based on ammonium polyphosphate (APP), respectively. All samples show material degradation at the surface due to weathering. No significant weathering influence occurs on the flame retardancy when it is a bulk property, as was observed for aryl phosphates in PC blends and MC in PA. When the fire retardancy is dominated by a surface mechanism, dependence on the duration of weathering is detected: for intumescent formulations based on ammonium APP in PP, a worsening in the formation of the intumescent network was observed. KW - Fire retardancy KW - Weathering resistance KW - Degradation KW - Intumescence KW - Cone calorimeter PY - 2010 DO - https://doi.org/10.1016/j.polymdegradstab.2010.08.020 SN - 0141-3910 SN - 1873-2321 VL - 95 IS - 12 SP - 2421 EP - 2429 PB - Applied Science Publ. CY - London AN - OPUS4-22612 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Damerau, Thomas A1 - Sabelus, Silke A1 - Wachtendorf, Volker A1 - Hennecke, Manfred A1 - Greiner, A. T1 - Photochemische und thermische Stabilität eines Phenylen-Vinylen-Polymeren KW - Photostability KW - Fluorescence KW - Chemiluminescence PY - 1996 SN - 0016-3538 VL - 40 IS - 7 SP - 710 EP - 712 PB - GIT-Verlag CY - Darmstadt AN - OPUS4-23205 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Geburtig, Anja A1 - Wachtendorf, Volker A1 - Trubiroha, Peter T1 - Accelerated weathering test for plastics and coatings that are exposed to acidic precipitation N2 - Due to the occurrence of acidic precipitation, and due to the fact that polymers and stabilizers may be sensititve to acids, it is important to have a laboratory test that combines weathering exposure with acidic exposure. The loss of stabilization caused by an acid damage of stabilizing system gets evident only over the weathering progress. For solid samples, for wich mostly the surface properties are relevant, the "Acid Dew and Fog Test" (ADF test) was established. For woven or tufted materials, the "Acid Rain Test" (AR test) was developed. The proposed weathering tests aim at plastics as well as at coatings. T2 - 7th International Symposium on Weatherability (7th ISW) CY - Kanagawa, Japan DA - 2008-10-23 KW - Acid rain KW - ADF KW - Acid Dew and Fog test KW - Artificial Weathering test PY - 2009 SN - 1346-0633 VL - 21 IS - 2 SP - 69 EP - 73 PB - Materiaru-Raifu-Gakkai CY - Tokyo AN - OPUS4-18270 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Geburtig, Anja A1 - Wachtendorf, Volker T1 - Determination of the spectral sensitivity and temperature dependence of polypropylene crack formation caused by UV-irradiation N2 - For polypropylene of varied stabilization, spectral sensitivity as well as temperature dependence of irradiation caused crack formation was determined in artificial irradiation tests. UV radiant exposure HUV necessary to generate crack formation was measured both in spectrally dispersed irradiation and artificial irradiation in a Fluorescent UV lamp device. Dependencies were fitted to a plateau function and an Arrhenius function, respectively, to describe the action of irradiation by response functions. Applied to weather data from Phoenix, the results were compared with respective outdoor exposure results. KW - Weathering KW - UV KW - Temperature KW - Numerical simulation PY - 2010 DO - https://doi.org/10.1016/j.polymdegradstab.2010.06.014 SN - 0141-3910 SN - 1873-2321 VL - 95 IS - 10 SP - 2118 EP - 2123 PB - Applied Science Publ. CY - London AN - OPUS4-21913 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Trubiroha, Peter A1 - Geburtig, Anja A1 - Wachtendorf, Volker T1 - Referenzmaterialien für Bewitterungsprüfungen von polymeren Werkstoffen KW - Referenzmaterial KW - Bestrahlen KW - Bewitterern KW - Polymer PY - 2003 SN - 0341-230X SN - 1431-827X VL - 36 IS - 3 SP - 35 EP - 39 PB - Baltz CY - München AN - OPUS4-2864 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Appajaiah, Anilkumar A1 - Wachtendorf, Volker A1 - Daum, Werner T1 - Characterization of thermo-oxidative stability of polymer optical fibers using chemiluminescence technique N2 - The thermo-oxidative stability of commercially available polymer optical fibers (POFs) and their components (cores and claddings) was investigated. All the bare POFs (core and cladding only) studied here were based on poly(methyl methacrylate) (PMMA) core. The fibers were exposed to 100 °C/low humidity for about 4200 h. Chemiluminescence (CL) technique was applied to investigate the thermo-oxidative stability and for measuring the transmission loss during exposure a prototype device called multiplexer was used. POFs exhibited variation in thermo-oxidative stability although they possessed identical core material PMMA. This was due to difference in the chemical compositions of claddings. Claddings were more susceptible to the thermo-oxidative degradation compared to cores. The thermo-oxidative degradation of both the cladding and the core was found in POFs as a result of climatic exposure. POFs showed an early drop-off followed by a slow decline of transmission. The early drop-off of transmission was attributed to physical changes like thermal expansion and the slow decline of transmission to chemical changes like oxidative degradation of POFs. A good linear relationship between optical transmission stability and thermo-oxidative stability of POFs was established from these studies. KW - Polymer optical fibers (POFs) KW - Chemiluminescence (CL) KW - Thermo-oxidative stability KW - Aging KW - Optical transmission stability PY - 2006 DO - https://doi.org/10.1016/j.polymdegradstab.2006.05.006 SN - 0141-3910 SN - 1873-2321 VL - 91 IS - 11 SP - 2605 EP - 2613 PB - Applied Science Publ. CY - London AN - OPUS4-13984 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Simone A1 - Brademann-Jock, Kerstin A1 - Wachtendorf, Volker A1 - Rauth, W. A1 - Klimmasch, T. A1 - Krüger, P. T1 - Analysis of weathering effects in automotive coatings by thermoluminescence KW - Automotive coatings KW - Weathering KW - Thermoluminescence PY - 2006 SN - 0048-4225 N1 - Sprachen: Englisch/Italienisch - Languages: English/Italian VL - 82 IS - 17 SP - 5 EP - 11 AN - OPUS4-14296 LA - mul AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -