TY - GEN A1 - Wäsche, Rolf A1 - Steinborn, Gabriele A1 - Klaffke, Dieter ED - Somiya, S. T1 - Gas pressure sintering of SiCp-alumina composites made by gelcasting and their tribological properties N2 - COMPOSITE MATERIALS OF A 99.7 % ALPHA-ALUMINA MATRIX WITH PLATELETS OF SILICON CARBIDE (SICP) HAVE BEEN PREPARED BY GELCASTING. DENSIFICATION WAS CARRIED OUT BY GAS-PRESSURE SINTERING WITHOUT FURTHER SINTERING AIDS. FIVE DIFFERENT COMPOSITIONS WITH 0, 5, 10, 15, AND 20 VOL.% SICP RESP. HAVE BEEN INVESTIGATED AND TRIBOLOGICAL PROPERTIES WERE CHARACTERIZED. INCREASING AMOUNT OF SICP AS RIGID PARTICLES IN THE FINE GRAINED MATRIX COMPLICATE THE DENSIFICATION PROCESS. WITH THE APPLICATION OF 50 BAR AR PRESSURE DURING THE FINAL SINTERING STEP AT A TEMPERATURE OF 1700 DEGREE C THE DENSITY OF THE SAMPLES COULD BE INCREASED BY 3-5%. INVESTIGATION OF THE TRIBOLOGICAL PROPERTIES AGAINST STEEL AS A COUNTERBODY UNDER UNLUBRICATED OSCILLATING SLIDING CONDITIONS SHOWED A HIGH COEFFICIENT OF FRICTION AND AN INCREASING WEAR RATE UP TO A SICP CONTENT OF 10 VOL. % . AT 15 AND 20 VOL. % SICP RESP. BOTH THE COEFFICIENT OF FRICTION AND THE COEFFICIENT OF WEAR DROP DOWN. T2 - 3rd IUMRS International Conference on Advanced Materials (ICAM) CY - Tokyo, Japan DA - 1993-08-31 PY - 1994 SN - 0-444-81993-2 N1 - Serientitel: Transactions of the Materials Research Society of Japan – Series title: Transactions of the Materials Research Society of Japan IS - 16B SP - 791 EP - 794 PB - Elsevier CY - Amsterdam AN - OPUS4-1433 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Dörfel, Ilona A1 - Wäsche, Rolf A1 - Rabe, Torsten A1 - Steinborn, Gabriele T1 - Tribological Induced Microstructural Changes in Subsurface Layers of Si3N4-Based Materials KW - Tribologie PY - 1994 SN - 1013-9826 VL - 89-91 SP - 763 EP - 767 PB - Trans Tech Publ. CY - Aedermannsdorf AN - OPUS4-577 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wäsche, Rolf A1 - Steinborn, Gabriele T1 - Characterisation of the secondary properties of alumina - measuring the isoelectric point by a streaming potential method PY - 1997 SN - 0173-9913 SN - 0196-6219 VL - 74 IS - 5 SP - 235 EP - 239 PB - Göller CY - Baden-Baden AN - OPUS4-1434 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wäsche, Rolf A1 - Steinborn, Gabriele T1 - Influence of Slip Viscosity on the Mechanical Properties of High Purity Alumina made by Gelcasting KW - High purity alumina KW - Gelcasting KW - Solid content KW - Viscosity KW - Deairing KW - Bending strenght KW - Microstructure KW - Computertomography KW - Defect type PY - 1997 SN - 1013-9826 VL - 132 SP - 374 EP - 377 PB - Trans Tech Publ. CY - Aedermannsdorf AN - OPUS4-1435 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wäsche, Rolf A1 - Steinborn, Gabriele T1 - Influence of the Dispersants in Gelcasting of Nanosized TiN PY - 1997 SN - 0955-2219 SN - 1873-619X IS - 17 SP - 421 EP - 426 PB - Elsevier CY - Oxford AN - OPUS4-1429 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Steinborn, Gabriele A1 - Wäsche, Rolf A1 - Reichel, U. T1 - Fabrication of porous ceramics made from nano sized alumina powder by gelcasting N2 - The gelcasting process was used for manufacturing porous ceramic bodies from nano sized powders. 3 different powders with specific surface areas between 12 and 30 m²/g were used. Solid content of the corresponding slurries was dependent on the milling procedure and the use of a suitable dispersant. For bimodal GradeA powder solid content was as high as 58 vol%. For sintering temperatures between 1250 and 1600°C the porosity varied between 45 and 20%, whereas the pore radii varied between 50 and 91nm. The grain size of crystallites in the sintered microstructures was about 1um. The reflection ratio for visible light increased in comparison to a reference sample made from conventional powder from 0.8 to 0.95 in the wavelenght range around 400nm. T2 - 2nd International Conference on Shaping of Advanced Ceramics CY - Gent, Belgium DA - 2002-10-24 PY - 2002 SP - 103 EP - 108 AN - OPUS4-1813 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Klaffke, Dieter A1 - Steinborn, Gabriele A1 - Wäsche, Rolf A1 - Wötting, G. ED - Degischer, H.-P. T1 - Tribologische Untersuchungen an SiC- und Si3N4-basierten Keramiken T2 - 14. Symposium Verbundwerkstoffe und Werkstoffverbunde CY - Wien, Österreich DA - 2003-07-02 PY - 2003 SN - 3-527-30762-1 SP - 545 EP - 550 PB - Wiley-VCH CY - Weinheim AN - OPUS4-2591 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Steinborn, Gabriele A1 - Fritz, Ulrich A1 - Rabe, Torsten A1 - Wäsche, Rolf T1 - Dispergierung von Nanopulvern in Foliengießschlickern KW - Dispergierung KW - Nanopulver KW - Folie PY - 2004 SN - 0173-9913 SN - 0196-6219 VL - 18 IS - 1 SP - 43 EP - 50 PB - Göller CY - Baden-Baden AN - OPUS4-5219 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wäsche, Rolf A1 - Paulick, Carl A1 - Steinborn, Gabriele A1 - Richter, V. A1 - Werner, M. T1 - Joining of ceramic components in the green state via LPIM N2 - It has been successfully demonstrated that ceramic materials can be joined in the green state without a second phase by using low pressure injection molded parts. The investigation of the joining interface revealed that a high quality interface can be achieved by carefully adjusting the different manufacturing steps. The use of monomodal particle size distribution in the used powder CT3000SG is inferior to a broader particle size distribution obtained by replacing 33% of the finer alumina powder by coarser CT1200SG. In this way the dewaxing process is significantly improved when the wall thickness of the part exceeds 3 mm. The investigation of the mechanical properties of the joined and sintered parts revealed, that the bending strength of the joined specimens achieved about 80 % of the unjoined, monolithic specimens. T2 - 4th International Conference on Advanced Materials and Processing CY - Hamilton, New Zealand DA - 2006-12-10 KW - Joining KW - Ceramics KW - Green state KW - Interface KW - Bending strength KW - Low pressure injection molding PY - 2005 UR - http://www.scientific.net/3-908453-89-5/207/ SN - 1022-6680 SN - 1662-8985 VL - 29-30 SP - 207 EP - 210 PB - Trans Tech Publ. CY - Zurich AN - OPUS4-19001 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wäsche, Rolf A1 - Klaffke, Dieter A1 - Steinborn, Gabriele T1 - Tribological testing of Ca-Ba infiltrated zirconia KW - Friction KW - Wear KW - Ca-Ba fluoride KW - Infiltration KW - Porous zirconia PY - 2005 UR - http://www.om.ugal.ro/AnnalsFasc8Tribology/pdf/2005/9-Annals2005-3-Wasche.pdf SN - 1221-4590 SN - 1220-0824 SP - 53 EP - 59 CY - Gala¸ti AN - OPUS4-12365 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -