TY - JOUR A1 - Treninkov, I. A. A1 - Petrushin, N. V. A1 - Epishin, A. I. A1 - Svetlov, I. L. A1 - Nolze, Gert A1 - Elyutin, E. S. T1 - Experimental Determination of Temperature Dependence of Structural–Phase Parameters of Nickel-Based Superalloy N2 - The temperature dependences of the periods of the crystal lattices of the γ and γ' phases, their dimensional mismatch (misfit), and volume fraction of the γ' phase of an experimental single-crystal hightemperature nickel-based alloy have been determined by X-ray diffraction analysis in the temperature range of 18–1150°C. The temperature ranges in which intense changes in the structural and phase characteristics of the alloy under study take place have been determined. KW - X-ray diffraction analysis KW - High temperatures KW - Nickel-based superalloys KW - Single crystal KW - Crystal lattice period PY - 2022 DO - https://doi.org/10.1134/s2075113322010373 SN - 2075-1133 VL - 13 IS - 1 SP - 171 EP - 178 PB - Springer Science + Business Media CY - Dordrecht AN - OPUS4-54466 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Petrushin, N. V. A1 - Epishin, A. I. A1 - Svetlov, I. L. A1 - Nolze, Gert A1 - Elyutin, E. S. A1 - Solov'ev, A. E. T1 - Influence of the Sign of the γ/γ' Misfit on the Structure and Creep Strength of Single Crystals of Nickel-Based Superalloys N2 - Using the method of directional solidification, single crystals of experimental nickel-based superalloys with negative, zero, and positive γ/γ' misfits are obtained. The γ' solvus, solidus, and liquidus temperatures of the alloys are determined, and the microstructures of the alloys after directional solidification, heat treatment, and creep tests are investigated. Creep tests are performed at temperatures of 800 and 1000°C. It is found that single crystals of the alloy with a negative γ/γ' misfit have the highest creep resistance and lifetime (the crystal lattice period of the γ' phase is smaller than that of the γ matrix). KW - Nickel-based superalloys KW - Single crystal KW - Creep KW - Creep strength KW - Microstructure, γ/γ' misfit PY - 2023 DO - https://doi.org/10.1134/s207511332301029x SN - 2075-1133 VL - 14 IS - 1 SP - 13 EP - 22 AN - OPUS4-59505 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -