TY - JOUR A1 - Ta, N. A1 - Bilal, M. U. A1 - Häusler, I. A1 - Saxena, A. A1 - Lin, Y.-Y. A1 - Schleifer, F. A1 - Fleck, M. A1 - Glatzel, U. A1 - Skrotzki, Birgit A1 - Darvishi Kamachali, Reza T1 - Simulation of the θ′ Precipitation Process with Interfacial Anisotropy Effects in Al-Cu Alloys N2 - The effects of anisotropic interfacial properties and heterogeneous elasticity on the growth and ripening of plate-like θ′-phase (Al2Cu) in Al-1.69 at.% Cu alloy are studied. Multi-phase-field simulations are conducted and discussed in comparison with aging experiments. The precipitate/matrix interface is considered to be anisotropic in terms of its energy and mobility. We find that the additional incorporation of an anisotropic interfacial mobility in conjunction with the elastic anisotropy result in substantially larger aspect ratios of the precipitates closer to the experimental observations. The anisotropy of the interfacial energy shows comparably small effect on the precipitate’s aspect ratio but changes the interface’s shape at the rim. The effect of the chemo-mechanical coupling, i.e., the composition dependence of the elastic constants, is studied as well. We show that the inverse ripening phenomenon, recently evidenced for δ’ precipitates in Al-Li alloys (Park et al. Sci. Rep. 2019, 9, 3981), does not establish for the θ′ precipitates. This is because of the anisotropic stress fields built around the θ′ precipitates, stemming from the precipitate’s shape and the interaction among different variants of the θ′ precipitate, that disturb the chemo-mechanical effects. These results show that the chemo-mechanical effects on the precipitation ripening strongly depend on the degree of sphericity and elastic isotropy of the precipitate and matrix phases. KW - Aging KW - Phase-field simulation KW - Interfacial anisotropy KW - Chemo-mechanical coupling KW - Precipitation KW - Elasticity KW - θ′-(Al2Cu) precipitate phase PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-522672 DO - https://doi.org/10.3390/ma14051280 VL - 14 IS - 5 SP - 1280 PB - MDPI AN - OPUS4-52267 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jürgens, Maria A1 - Olbricht, Jürgen A1 - Fedelich, Bernard A1 - Skrotzki, Birgit T1 - Low Cycle Fatigue and Relaxation Performance of Ferritic–Martensitic Grade P92 Steel N2 - Due to their excellent creep resistance and good oxidation resistance, 9–12% Cr ferritic–martensitic stainless steels are widely used as high temperature construction materials in power plants. However, the mutual combination of different loadings (e.g., creep and fatigue), due to a “flexible” operation of power plants, may seriously reduce the lifetimes of the respective components. In the present study, low cycle fatigue (LCF) and relaxation fatigue (RF) tests performed on grade P92 helped to understand the behavior of ferritic–martensitic steels under a combined loading. The softening and lifetime behavior strongly depend on the temperature and total strain range. Especially at small strain amplitudes, the lifetime is seriously reduced when adding a hold time which indicates the importance of considering technically relevant small strains. KW - Ferritic–martensitic steel KW - P92 KW - Low cycle fatigue KW - Relaxation fatigue KW - Cyclic softening PY - 2019 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-473905 DO - https://doi.org/10.3390/met9010099 VL - 9 IS - 1 SP - 99, 1 EP - 25 PB - MDPI AN - OPUS4-47390 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sonntag, Nadja A1 - Jürgens, Maria A1 - Skrotzki, Birgit A1 - Olbricht, Jürgen T1 - Creep-fatigue of P92 in service-like tests with combined stress- and strain-controlled dwell times N2 - Complex service-like relaxation- and creep-fatigue tests with strain- and stress-controlled dwells and fatigue cycle durations of approx. 2200 s were performed exemplarily on a grade P92 steel at 620 ◦C in this study. The results indicate deviations in the prevailing creep mechanisms of long-term relaxation and creep dwells, affecting subsequent dwells, load shifts, and the macroscopic softening behavior quite differently. In addition, fracture surfaces and longitudinal metallographic sections reveal intergranular crack growth for complex loading with stress-controlled dwells, whereas complex strain-controlled tests enhance oxidation and transgranular crack propagation. These findings substantiate the limited transferability of relaxation-fatigue to creep-fatigue conditions. KW - Tempered martensite-ferritic steel KW - P92 KW - Dwell periods KW - Creep-fatigue interaction KW - Stress relaxation PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-564239 DO - https://doi.org/10.1016/j.ijfatigue.2022.107381 SN - 0142-1123 VL - 168 SP - 1 EP - 12 PB - Elsevier Ltd. AN - OPUS4-56423 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sonntag, Nadja A1 - Skrotzki, Birgit A1 - Stegemann, Robert A1 - Löwe, Peter A1 - Kreutzbruck, M. T1 - The role of surface topography on deformation-induced magnetization under inhomogeneous elastic-plastic deformation N2 - It is widely accepted that the magnetic state of a ferromagnetic material may be irreversibly altered by mechanical loading due to magnetoelastic effects. A novel standardized nondestructive testing (NDT) technique uses weak magnetic stray fields, which are assumed to arise from inhomogeneous deformation, for structural health monitoring (i.e., for detection and assessment of damage). However, the mechanical and microstructural complexity of damage has hitherto only been insufficiently considered. The aim of this study is to discuss the phenomenon of inhomogeneous “self-magnetization” of a polycrystalline ferromagnetic material under inhomogeneous deformation experimentally and with stronger material-mechanical focus. To this end, notched specimens were elastically and plastically deformed. Surface magnetic states were measured by a three-axis giant magnetoresistant (GMR) sensor and were compared with strain field (digital image correlation) and optical topography measurements. It is demonstrated that the stray fields do not solely form due to magnetoelastic effects. Instead, inhomogeneous plastic deformation causes topography, which is one of the main origins for the magnetic stray field formation. Additionally, if not considered, topography may falsify the magnetic signals due to variable lift-off values. The correlation of magnetic vector components with mechanical tensors, particularly for multiaxial stress/strain states and inhomogeneous elastic-plastic deformations remains an issue. KW - Magnetic stray fields KW - Magnetomechanical effect KW - Damage KW - Topography KW - Multiaxial deformation KW - Notch KW - Plastic deformation KW - Metal magnetic memory KW - Digital image correlation KW - Structural steel PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-457878 DO - https://doi.org/10.3390/ma11091518 SN - 1996-1944 VL - 11 IS - 9 SP - 1518, 1 EP - 26 PB - MDPI CY - Basel, Switzerland AN - OPUS4-45787 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Häusler, Ines A1 - Darvishi Kamachali, Reza A1 - Hetaba, W. A1 - Skrotzki, Birgit T1 - Thickening of T-1 Precipitates during Aging of a High Purity Al–4Cu–1Li–0.25Mn Alloy N2 - The age hardening response of a high-purity Al–4Cu–1Li–0.25Mn alloy (wt. %) during isothermal aging without and with an applied external load was investigated. Plate shaped nanometer size T1 (Al2CuLi) and θ′ (Al2Cu) hardening phases were formed. The precipitates were analyzed with respect to the development of their structure, size, number density, volume fraction and associated transformation strains by conducting transmission electron microscopy (TEM) and scanning transmission electron microscopy (STEM) studies in combination with geometrical Phase analysis (GPA). Special attention was paid to the thickening of T1 phase. Two elementary types of single-layer T1 precipitate, one with a Li-rich (Type 1) and another with an Al-rich (Defect Type 1) central layer, were identified. The results show that the Defect Type 1 structure can act as a precursor for the Type 1 structure. The thickening of T1 precipitates occurs by alternative stacking of These two elementary structures. The thickening mechanism was analyzed based on the magnitude of strain associated with the precipitation transformation normal to its habit plane. Long-term aging and aging under load resulted in thicker and structurally defected T1 precipitates. Several types of defected precipitates were characterized and discussed. For θ′ precipitates, a ledge mechanism of thickening was observed. Compared to the normal aging, an external load applied to the peak aged state leads to small variations in the average sizes and volume fractions of the precipitates. KW - Al-Cu-Li-alloy KW - Precipitation KW - T1 precipitate KW - Microstructure evolution KW - Thickening KW - Creep KW - Volume fraction KW - Number density KW - Strain difference PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-471207 DO - https://doi.org/10.3390/ma12010030 SN - 1996-1944 VL - 12 IS - 1 SP - 30, 1 EP - 23 PB - MDPI AN - OPUS4-47120 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Beygi Nasrabadi, Hossein A1 - Hanke, T. A1 - Weber, M. A1 - Eisenbart, M. A1 - Bauer, F. A1 - Meissner, R. A1 - Dziwis, G. A1 - Tikana, L. A1 - Chen, Yue A1 - Skrotzki, Birgit T1 - Toward a digital materials mechanical testing lab N2 - To accelerate the growth of Industry 4.0 technologies, the digitalization of mechanical testing laboratories as one of the main data-driven units of materials processing industries is introduced in this paper. The digital lab infrastructure consists of highly detailed and standard-compliant materials testing knowledge graphs for a wide range of mechanical testing processes, as well as some tools that enable the efficient ontology development and conversion of heterogeneous materials’ mechanical testing data to the machine-readable data of uniform and standardized structures. As a basis for designing such a digital lab, the mechanical testing ontology (MTO) was developed based on the ISO 23718 and ISO/IEC 21838-2 standards for the semantic representation of the mechanical testing experiments, quantities, artifacts, and report data. The trial digitalization of materials mechanical testing lab was successfully performed by utilizing the developed tools and knowledge graph of processes for converting the various experimental test data of heterogeneous structures, languages, and formats to standardized Resource Description Framework (RDF) data formats. The concepts of data storage and data sharing in data spaces were also introduced and SPARQL queries were utilized to evaluate how the introduced approach can result in the data retrieval and response to the competency questions. The proposed digital materials mechanical testing lab approach allows the industries to access lots of trustworthy and traceable mechanical testing data of other academic and industrial organizations, and subsequently organize various data-driven research for their faster and cheaper product development leading to a higher performance of products in engineering and ecological aspects. KW - General Engineering KW - General Computer Science PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-582698 DO - https://doi.org/10.1016/j.compind.2023.104016 SN - 0166-3615 VL - 153 SP - 1 EP - 15 PB - Elsevier B.V. AN - OPUS4-58269 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Jakob A1 - Han, Ying A1 - Fritsch, Tobias A1 - Hejazi, Bardia A1 - Ulbricht, Alexander A1 - Skrotzki, Birgit A1 - Bruno, Giovanni T1 - X-ray computed tomography quantifies primary phases and reveals crack morphology in high-cycle fatigue of aluminum alloy EN AW-2618A N2 - Since the introduction of high-strength aluminum alloys understanding their fatigue behavior is of high interest for the structural integrity of engineering components, in this context, the alloy EN AW-2618A gains its high strength from both nanometer size precipitates and micrometer size primary phases. The latter phases are often identified as crack initiation sites. In this study, it uses a combination of synchrotron and laboratory-based X-ray computed tomography to image and quantify such primary phases and the fatigue cracks appearing in interrupted tests. Based on the gray-level differences in the synchrotron X-ray computed tomography scans, this study is able to distinguish low- and high-absorbing particles. The dominant (volume fraction >99%) high absorbing primary phase can be quantified in good agreement with results of Thermo-Calc calculations. To image the fatigue crack, laboratory X-ray computed tomography scans are performed at different tensile loads to open the crack. The results show that with an appropriate crack opening tensile load, the fatigue crack morphology can be reliably revealed. Based on these results, the influence of the primary phases on the fatigue crack initiation and propagation are discussed. KW - X-ray computed tomography KW - Fatigue KW - Aluminum KW - Primary phases PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-632724 DO - https://doi.org/10.1002/adem.202500235 SN - 1527-2648 SP - 1 EP - 9 PB - Wiley-VCH CY - Weinheim AN - OPUS4-63272 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Stegemann, Robert A1 - Cabeza, Sandra A1 - Pelkner, Matthias A1 - Lyamkin, Viktor A1 - Sonntag, Nadja A1 - Bruno, Giovanni A1 - Skrotzki, Birgit A1 - Kreutzbruck, Marc T1 - Evaluation of high spatial resolution imaging of magnetic stray fields for early damage detection N2 - The paper discusses the evaluation of elastic and plastic strain states in two low-carbon steels of the same steel group with high spatial resolution GMR (giant magneto resistance) sensors. The residual stress distributions of tungsten inert gas welded plates were determined by means of neutron diffraction as a reference. The normal component of local residual magnetic stray fields arise in the vicinity of the positions of maximum stress. The experiments performed on flat tensile specimen indicate that the boundaries of plastic deformations are a source of stray fields. The spatial variations of magnetic stray fields for both the weld and the tensile samples are in the order of the earths magnetic field. T2 - 43rd Annual Review of Progress in Quantitative Nondestructive Evaluation, Volume 36 CY - Atlanta, Georgia, USA DA - 17.07.2016 KW - Plastic deformation KW - GMR KW - Neutron diffraction KW - Residual stress KW - Microstructure KW - Low carbon steel KW - TIG weld PY - 2017 SN - 978-0-7354-1474-7 DO - https://doi.org/10.1063/1.4974688 SN - 0094-243X VL - 1806 IS - 1 SP - Article UNSP 110010-1 EP - 10 PB - AIP Publishing CY - Melville, NY 11747 AN - OPUS4-39279 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Beygi Narsabadi, Hossein A1 - Vafaeenezhad, H. A1 - Klotz, U.E. A1 - Tiberto, D. A1 - Hosseinabadi, F. A1 - Mishurova, Tatiana A1 - Bruno, Giovanni A1 - Skrotzki, Birgit T1 - XCT-assisted micromechanical modeling of the effect of pores on the plastic deformation and mechanical characteristics of PBF-LB/M-produced copper alloys N2 - Due to the low absorption of fiber laser by copper particles, the laser-based powder bed fusion (PBF-LB/M) processing of copper components is accompanied by the development of different types of porosities within the printed samples. This research aims to assess the consequences of various process-induced pores on the me chanical characteristics and deformation of PBF-LB/M-produced copper alloys. Several copper alloys were processed using metal-coated particles and varied laser intensities, yielding samples with different types and amounts of porosities. For instance, CuCrZr alloys processed at 325 J/mm³ and 257 J/mm³ had 0.009 % and 1.117 % porosities, dominated by keyhole and lack-of-fusion pores, respectively. Moreover, PBF-LB/M pro cessing of Cr- and Nb-coated CuNi3SiCr particles accompanied by the generation of 0.004 % and 1.861 % porosities within the samples, predominantly featuring metallurgical and oxidation pores, respectively. Compression and nanoindentation tests revealed that the CuNi3SiCr alloy exhibited superior mechanical properties compared to the CuCrZr sample (nanoindentation hardness values 2.2 GPa and 1.4 GPa, respectively), while the presence of lack-of-fusion pores notably diminished their mechanical performance. X-ray computed tomography (XCT) reconstruction slices and scanning electron microscopy (SEM) images were then used for developing the representative volume elements (RVEs) based micromechanical models. The micromechanical simulations established a structure-property correlation that can simulate the compressive deformation and mechanical characteristics of PBF-LB/M-produced copper alloys as a function of their incorporated pore characteristics. Due to the closure of the pores at the first stages of deformation, samples with minimal keyhole and metallurgical porosities exhibited homogeneous plastic deformation. On the other side, based on the JohnsonCook model, strain concentration and crack propagation around the lack-of-fusion pores lead to damage initi ation in the printed samples at a strain level of 5 % KW - X-ray Computed tomography KW - Defects KW - Copper alloys KW - PBF-LB/M KW - Micromechanics PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-624004 DO - https://doi.org/10.1016/j.msea.2025.147836 SN - 0921-5093 VL - 924 PB - Elsevier B.V. AN - OPUS4-62400 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zia, Ghezal Ahmad Jan A1 - Hanke, Thomas A1 - Skrotzki, Birgit A1 - Völker, Christoph A1 - Bayerlein, Bernd T1 - Enhancing Reproducibility in Precipitate Analysis: A FAIR Approach with Automated Dark-Field Transmission Electron Microscope Image Processing N2 - AbstractHigh-strength aluminum alloys used in aerospace and automotive applications obtain their strength through precipitation hardening. Achieving the desired mechanical properties requires precise control over the nanometer-sized precipitates. However, the microstructure of these alloys changes over time due to aging, leading to a deterioration in strength. Typically, the size, number, and distribution of precipitates for a quantitative assessment of microstructural changes are determined by manual analysis, which is subjective and time-consuming. In our work, we introduce a progressive and automatable approach that enables a more efficient, objective, and reproducible analysis of precipitates. The method involves several sequential steps using an image repository containing dark-field transmission electron microscopy (DF-TEM) images depicting various aging states of an aluminum alloy. During the process, precipitation contours are generated and quantitatively evaluated, and the results are comprehensibly transferred into semantic data structures. The use and deployment of Jupyter Notebooks, along with the beneficial implementation of Semantic Web technologies, significantly enhances the reproducibility and comparability of the findings. This work serves as an exemplar of FAIR image and research data management. KW - Industrial and Manufacturing Engineering KW - General Materials Science KW - Automated image analysis KW - FAIR research data management KW - Reproducibility KW - microstructural changes PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-593905 DO - https://doi.org/10.1007/s40192-023-00331-5 SN - 2193-9772 SP - 1 EP - 15 PB - Springer Science and Business Media LLC CY - Heidelberg AN - OPUS4-59390 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -