TY - JOUR A1 - Tomiak, F. A1 - Schartel, Bernhard A1 - Wolf, M. A1 - Drummer, D. T1 - Particle Size Related Effects of Multi-Component Flame-Retardant Systems in poly(butadiene terephthalate) N2 - Aluminum tris (diethylphosphinate) (AlPi) is known to have an efficient flame-retardant effect when used in poly(butadiene terephthalates) (PBT). Additionally, better flame-retardant effects can be achieved through the partial substitution of AlPi by boehmite in multi-component systems, which have been shown to be an effective synergist due to cooling effects and residue formation. Although the potential of beneficial effects is generally well known, the influence of particle sizes and behavior in synergistic compositions are still unknown. Within this paper, it is shown that the synergistic effects in flammability measured by limiting oxygen index (LOI) can vary depending on the particle size distribution used in PBT. In conducting thermogravimetric analysis (TGA) measurements, it was observed that smaller boehmite particles result in slightly increased char yields, most probably due to increased reactivity of the metal oxides formed, and they react slightly earlier than larger boehmite particles. This leads to an earlier release of water into the system enhancing the hydrolysis of PBT. Supported by Fourier transformation infrared spectroscopy (FTIR), we propose that the later reactions of the larger boehmite particles decrease the portion of highly flammable tetrahydrofuran in the gas phase within early burning stages. Therefore, the LOI index increased by 4 vol.% when lager boehmite particles were used for the synergistic mixture. KW - Flame retardants KW - Aluminum diethylphosphinate KW - Boehmite KW - Poly(butadiene terephthalates) (PBT) KW - Mechanical properties PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-509286 DO - https://doi.org/10.3390/polym12061315 SN - 2073-4360 VL - 12 IS - 6 SP - 1315 PB - MDPI AN - OPUS4-50928 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Morys, Michael A1 - Häßler, Dustin A1 - Krüger, Simone A1 - Schartel, Bernhard A1 - Hothan, Sascha T1 - Beyond the standard time-temperature curve: Assessment of intumescent coatings under standard and deviant temperature curves N2 - Nowadays there are intumescent coatings available for diverse applications. There is no established assessment of their protection performance besides the standard time-temperature curve, but natural fire scenarios often play an important role. A reliable straightforward performance-based assessment is presented. The effective thermal conductivity per thickness is calculated based on intermediate-scale fire tests. The optimum thermal insulation, the time to reach it, and the time until contingent failure of the coating are used for an assessment independent of the heating curve. The procedure was conducted on four different commercially intumescent coatings for steel construction, one solvent-based, one waterborne, one epoxy-based, and a bandage impregnated with a waterborne coating. The performance was studied under four different but similar shaped heating curves with different maximum temperatures (standard time-temperature curve, hydrocarbon curve and two self-designed curves with reduced temperature). The thermal protection performance is crucially affected by the residue morphology. Therefore, a comprehensive morphology analysis, including micro-computed tomography and scanning electron microscopy, was conducted on small-scale residues (7.5 x 7.5 cm2). Two different types of inner structures and the residue surface after different heat exposures were discussed in terms of their influence on thermal protection performance. KW - Intumescence KW - Coating KW - Computed tomography KW - Small scale KW - Heating curves KW - Residue morphology PY - 2020 DO - https://doi.org/10.1016/j.firesaf.2020.102951 SN - 0379-7112 VL - 112 SP - 102951 PB - Elsevier Ltd. AN - OPUS4-50334 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schartel, Bernhard T1 - Flammschutz für technische Kunststoffte für elektronische Anwendungen N2 - Das Brandverhalten stellt wie das ausgezeichnete elektrische Isolationsverhalten, die geringen elektrischen Verluste, die Verarbeitbarkeit und Formbarkeit eine der wesentlichen Schlüsseleigenschaften im Eigenschaftsprofil von Polymerwerkstoffen in der Elektronik und der Elektrotechnik dar. Dabei bedarf es einer Ausrüstung der Polymerwerkstoffe mit Flammschutzmittel. Die Entwicklung von immer effizienteren, synergistischen und multifunktionalen Multikomponentensystemen ist dabei eine herausragende Quelle für Innovation. Die Entwicklung und Verbesserung der werkstoff- und anwendungsspezifischen Flammschutzlösungen bestimmen die aktuellen und zukünftigen Polymermaterialien in der Elektronik und Elektrotechnik mit. Der Vortrag stellt anhand von Beispielen einige der erfolgreichen Konzepte dar. Es wird versucht, über das wissenschaftlich-systematische Verständnis Grundprinzipien und vielversprechende Lösungsstrategien zu verdeutlichen. T2 - Kunststoff trifft Elektronik, KUZ Kunststoffzentrum in Leipzig CY - Leipzig, Germany DA - 29.01.2020 KW - Flame retardant KW - Ssynergy KW - Flame retardant mode of action KW - UL 94 KW - Cone calorimeter PY - 2020 AN - OPUS4-50495 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Schartel, Bernhard A1 - Kebelmann, Katharina ED - Hu, Y. ED - Wang, X. T1 - Fire testing for the development of flame retardant polymeric materials N2 - Flame retarded polymeric materials are used in various applications in which a certain fire behavior is demanded. Protection goals are defined, such as limited flammability in terms of hindered sustained ignition or limited contribution to a fire, and these protection levels are tested with defined specimens or components in defined fire scenarios, that is to say, different fire tests. Passing a specific fire test by meeting whatever its demands is often the most important development goal, so the parameters of the different fire tests vary widely to emphasize different fire properties. Some fire tests are used to screen or provide a general assessment of flame retardant polymers during development, while other fire tests and tailored experiments are performed to address special phenomena or understand the flame retardancy modes of action. For all fire testing, the devil is in the details – demanding know-how and crucial efforts to manage the quality of investigations and advanced interpretation. This chapter aims to offer a structured overview of all these aspects. KW - Fire testing KW - Flame retardant KW - Fire retardant KW - Flammability KW - Ignition KW - Oxygen index KW - Cone calorimeter KW - UL 94 KW - Developing fire KW - Uncertainty KW - Fire resistance PY - 2020 SN - 978-1-138-29578-7 SP - 35 EP - 55 PB - CRC Press AN - OPUS4-50236 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Battig, Alexander A1 - Markwart, J. C. A1 - Wurm, F. R. A1 - Schartel, Bernhard T1 - Sulfur's role in the flame retardancy of thio-ether–linked hyperbranched polyphosphoesters in epoxy resins N2 - Hyperbranched polyphosphoesters are promising multifunctional flame retardants for epoxy resins. These polymers were prepared via thiol-ene polyaddition reactions. While key chemical transformations and modes of actions were elucidated, the role of sulfur in the chemical composition remains an open question. In this study, the FR-performance of a series of phosphorus-based flame retardant additives with and without sulfur (thioethers or sulfones) in their structure are compared. The successful synthesis of thio-ether or sulfone-containing variants is described and verified by 1H and 31P NMR, also FTIR and MALDI-TOF. A decomposition process is proposed from pyrolytic evolved gas analysis (TG-FTIR, Py-GC/MS), and flame retardancy effect on epoxy resins is investigated under pyrolytic conditions and via fire testing in the cone calorimeter. The presence of sulfur increased thermal stability of the flame retardants and introduced added condensed phase action. Likely, Sulfur radical generation plays a key role in the flame-retardant mode of action, and sulfones released incombustible SO2. The results highlight the multifunctionality of the hyperbranched polymer, which displays better fire performance than its low molar mass thio-ether analogue due to the presence of vinyl groups and higher stability than its monomer due to the presence of thio-ether groups. KW - Phosphoester KW - Hyperbranched KW - Sulfur KW - Thio-ether KW - Flame retardant KW - Epoxy resin PY - 2020 DO - https://doi.org/10.1016/j.eurpolymj.2019.109390 SN - 0014-3057 VL - 122 SP - 109390 PB - Elsevier Ltd. AN - OPUS4-50238 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Turski Silva Diniz, Analice A1 - Huth, Christian A1 - Schartel, Bernhard T1 - Dripping and decomposition under fire: Melamine cyanurate vs. glass fibres in polyamide 6 N2 - Manipulating the melt dripping of thermoplastics makes a fire scenario more or less dangerous. Yet, a detailed understanding of this phenomenon has remained a question mark in studies of the flammability of plastics. In this work, the individual and collective impacts of additives on the dripping behaviour of polyamide 6 (PA6) were studied. A set of materials compounded with melamine cyanurate (MCA) and glass fibre (GF) was investigated. Under UL 94 vertical test conditions, the dripping during first and second ignition was quantified and investigated in detail. The number, size and temperature of the drops were addressed, and the materials and their drops evaluated with respect to such aspects as their averaged molecular weight, thermal decomposition and rheological properties. PA6 with V-2 classification improved to V-0 with the addition of MCA, and achieved HB in the presence of GF. PA6/GF/MCA achieved V-2. Non-flaming drops of PA6/MCA consisted of oligomeric fragments. Flaming drops of PA6/GF showed a more pronounced decomposition of PA6 and an increased GF content. The dripping behaviour of PA6/GF/MCA can be understood as a combination of the influence of both additives. The results showed nicely that dripping under fire is neither a straightforward material property nor a simple additive influence, but the complex response of the material influenced by the interaction and competition of different phenomena. KW - Dripping KW - UL 94 KW - Polyamide 6 KW - Melamine cyanurate KW - Glass fibre KW - Flame retardant PY - 2020 DO - https://doi.org/10.1016/j.polymdegradstab.2019.109048 SN - 0141-3910 VL - 171 SP - 109048 PB - Elsevier Ltd. AN - OPUS4-50239 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zirnstein, Benjamin A1 - Schulze, Dietmar A1 - Schartel, Bernhard T1 - Combination of phosphorous flame retardants and aluminum trihydrate in multicomponent EPDM composites N2 - Ethylene propylene diene monomer (EPDM) Rubbers with the flame retardants tris(2-ethylhexyl)phosphate, ammonium polyphosphate, polyaniline, and aluminum trihydroxide were prepared and analyzed in this study. The homogenous dispersion of the fillers in the rubber matrix was confirmed by scanning electron microscope. To investigate the interplay of the different flame retardants, the flame retardants were varied systematically. The comprehensive study sought combinations of flame retardants that allow high loadings of flame retardants without deterioration of the physical and mechanical properties of the EPDM rubber. The eight EPDM rubbers were investigated via thermogravimetric analysis and pyrolysis gas chromatography coupled with a mass spectrometer (Py GC/MS) to investigate the potential synergistic effects. In the Py-GC/MS experiments, 27 pyrolysis products were identified. Furthermore, UL 94, limiting oxygen index, FMVSS 302, glow wire tests, and cone calorimeter tests were carried out. In the cone calorimeter test the EPDM rubbers R-1AP and R-1/2P achieved an increase in residue at flameout of 76% and a reduction in total heat evolved of about 35%. Furthermore, the compounds R-1AP and R-1/2P achieved a reduction in MARHE to about 150 kW m−1, a reduction of over 50% compared to the unprotected rubber R. KW - EPDM KW - Rubber KW - Aluminum hydroxide (ATH) KW - Phosphorous flame retardant PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-502859 DO - https://doi.org/10.1002/pen.25280 SN - 1548-2634 VL - 60 IS - 2 SP - 267 EP - 280 PB - Wiley AN - OPUS4-50285 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schartel, Bernhard A1 - Günther, Martin T1 - Flame retardancy of polyurethanes N2 - Polyurethanes (PU) represent one of the most versatile classes of plastics. They are processed and used as thermoplastic, elastomer, and thermoset. The requirements regarding flammability are correspondingly versatile. Depending on the material and the field of application, specific fire tests have to be fulfilled. This paper describes the different concepts used to fulfil these requirements by choosing the right raw materials and flame retardants. KW - Polyurethane KW - Flame retardant KW - Foam KW - Flammability KW - Pyrolysis KW - Cone calorimeter PY - 2020 VL - 17 IS - 1 SP - 44 EP - 48 PB - Dr. Gupta AN - OPUS4-50737 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Rabe, Sebastian A1 - Sanchez-Olivares, G. A1 - Pérez-Chávez, R. A1 - Schartel, Bernhard ED - Laoutid, F. T1 - Natural Keratin and Coconut Fibres from Industrial Wastes in Flame Retarded Thermoplastic Starch Biocomposites N2 - Natural keratin fibres derived from Mexican tannery waste and coconut fibres from coconut processing waste were used as fillers in commercially available, biodegradable thermoplastic starch-polyester blend to obtain sustainable biocomposites. The morphology, rheological and mechanical properties as well as pyrolysis, flammability and forced flaming combustion behaviour of those biocomposites were investigated. In order to open up new application areas for these Kinds of biocomposites, ammonium polyphosphate (APP) was added as a flame retardant. Extensive flammability and cone calorimeter studies revealed a good flame retardance effect with natural fibres alone and improved effectiveness with the addition of APP. In fact, it was shown that replacing 20 of 30 wt. % of APP with keratin fibres achieved the same effectiveness. In the case of coconut fibres, a synergistic effect led to an even lower heat release rate and total heat evolved due to reinforced char residue. This was confirmed via scanning electron microscopy of the char structure. All in all, these results constitute a good approach towards sustainable and biodegradable fibre reinforced biocomposites with improved flame retardant properties. KW - Biomaterials KW - Biodegradation KW - Calorimetry KW - Composites KW - Flame retardance PY - 2020 SN - 978-3-03928-350-7 SN - 978-3-03928-351-4 SP - 45 EP - 66 PB - MDPI AN - OPUS4-50738 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rabe, Sebastian A1 - Klack, Patrick A1 - Bahr, Horst A1 - Schartel, Bernhard T1 - Assessing the fire behavior of woods modified by N-methylol crosslinking, thermal treatment, and acetylation N2 - Wood products are often treated by different techniques to improve their longevity when used as building materials. Most of the time, the goal is to increase their resistance to weathering effects, deformations in material dimensions or biotic decomposition. These wood treatment techniques have a significant impact on pyrolysis and burning behavior. The general effects of three different common wood treatments on flame retardancy were investigated by comparing treated woods with their untreated counterparts and with other kinds of wood. While the acetylation of beech leads to a slightly increased fire hazard, the thermal treatment of wood and crosslinking of cellulose microfibrils dimethyloldihydroxy-ethyleneurea show a limited flame retarding effect. Switching to woods with a higher lignin content, and thus higher char yield, however, results in a more pronounced improvement in flame retardancy performance. This article delivers a comprehensive and balanced assessment of the general impact of different wood modifications on the fire behavior. Further, it is a valuable benchmark for assessing the flame retardancy effect of other wood modifications. KW - Acetylation KW - Cone claorimeter KW - DMDHEU KW - Heat of combustion KW - Thermal treatment KW - Wood modification PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-507397 DO - https://doi.org/10.1002/fam.2809 SN - 1099-1018 SN - 0308-0501 VL - 44 IS - 4 SP - 530 EP - 539 PB - Wiley Online Libary AN - OPUS4-50739 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ma, S. A1 - Xiao, Y. A1 - Zhou, F. A1 - Schartel, Bernhard A1 - Chan, Yin Yam A1 - Korobeinichev, O. P. A1 - Trubachev, S. A. A1 - Hu, W. A1 - Ma, C. A1 - Hu, Y. T1 - Effects of novel phosphorus-nitrogen-containing DOPO derivative salts on mechanical properties, thermal stability and flame retardancy of flexible polyurethane foam N2 - In this work, a series of 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide (DOPO) derivative salts containing phosphorus and nitrogen were synthesized, and their effects on mechanical properties, thermal stability and flame retardancy of flexible polyurethane foam (FPUF) were investigated. Studies have shown that the addition of DOPO derivatives will increase the tensile strength, compression set, and compression hardness of FPUF, but it will lead to a decrease in elongation at break. Thermogravimetric analysis showed that the initial decomposition temperature of FPUF containing DOPO derivatives was reduecd, but the char reside was significantly improved. A series of combustion tests indicated that the addition of DOPO derivative salts can improve the flame retardancy of FPUF, of which 10-hydroxy-9,10-dihydro-9-oxa-10 phosphaphenanthrene-10-oxide dicyandiamide salt (D-DICY) exhibited the best flame retardancy. When the load of D-DICY was 20 phr, the limiting oxygen index (LOI) of foam reached 24.5%, and the peak heat release rate and total heat release were decreased by 55.7% and 52.9%, respectively. Furthermore, based on the analysis of the gas phase combustion products and the char residue of the condensed phase, the possible flame retardant mechanism was proposed. KW - Flexible polyurethane foam KW - DOPO derivative salts KW - Mechanical properties KW - Thermal stability KW - Flame retardancy PY - 2020 DO - https://doi.org/10.1016/j.polymdegradstab.2020.109160 SN - 0141-3910 VL - 177 SP - 109160 PB - Elsevier Ltd. AN - OPUS4-50740 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schartel, Bernhard A1 - Günther, Martin T1 - Flammschutz von Polyurethanen N2 - Polyurethane (PU) bilden eine der vielseitigsten Klassen der Polymerwerkstoffe. Kein anderer Kunststoff wird sowohl als Thermoplast, als Elastomer wie auch als Duroplast verarbeitet und eingesetzt. Entsprechend vielfältig sind auch die Anforderungen an den Flammschutz. Je nach Material und Anwendung müssen spezifische Brandnormen erfüllt werden. Der vorliegende Aufsatz gibt einen Überblick über die verfügbaren Ansätze, um durch geeignete Auswahl der Rohstoffe und der Flammschutzmittel diese verschiedensten Anforderungen an das Brandverhalten zu erfüllen. KW - Polyurethan KW - Flammschutz KW - Pyrolyse KW - Schaum KW - Cone calorimeter PY - 2020 VL - 20 IS - 1 SP - 48 EP - 53 PB - Dr. Gupta AN - OPUS4-50736 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schartel, Bernhard T1 - Fire Retardants T2 - AircraftFire Colloquium CY - Brussels, Belgium DA - 2014-07-08 PY - 2014 AN - OPUS4-31056 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pappalardo, Salvatore A1 - Russo, Pietro A1 - Acierno, Domenico A1 - Rabe, Sebastian A1 - Schartel, Bernhard T1 - The synergistic effect of organically modified sepiolite in intumescent flame retardant polypropylene N2 - The pyrolysis, flammability and fire behavior of polypropylene (PP) containing an intumescent flame retardant and sepiolite nanoparticles were investigated by performing thermogravimetry, oxygen index (LOI), UL-94, and cone calorimeter tests. The combination of 0.5 wt% of premodified sepiolite (OSEP) with 12 wt% of a commercial intumescent flame retardant showed a clear synergy in LOI, UL-94 ranking and peak heat release rate. The ternary formulation achieved a V-0 classification and, consequently, allowed a reduction in the amount of flame retardant necessary to achieve this result. Whereas OSEP and pristine sepiolite nanoparticles (SEP) affect the performance in PP nanocomposites quite similarly, OSEP outperformed SEP in the combination with intumescent flame retardant. The cone calorimeter results and dynamic rheological measurements confirmed the synergistic effect between the nanofiller and the flame retardant resulting from the improved properties of the residual protective layer. KW - Polypropylene KW - Intumescent flame retardant KW - Sepiolite KW - Cone calorimetry KW - Low oxygen index PY - 2016 DO - https://doi.org/10.1016/j.eurpolymj.2016.01.041 SN - 0014-3057 VL - 76 SP - 196 EP - 207 PB - Elsevier AN - OPUS4-35854 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schartel, Bernhard A1 - Perret, Birgit A1 - Dittrich, Bettina A1 - Ciesielski, M. A1 - Krämer, J. A1 - Müller, P. A1 - Altstädt, V. A1 - Zang, L. A1 - Döring, M. T1 - Flame retardancy of polymers: the role of specific reactions in the condensed phase N2 - Condensed-phase mechanisms play a major role in fire-retardant polymers. Generations of development have followed the concept of charring to improve fire properties. Whereas the principal reactions are believed to be known, the specific description for multicomponent systems is lacking, as is the picture across different systems. A two-step approach is proposed in general, and also presented in greater detail. The second step covers the specific reactions controlling charring, whereas the actual reactants are provided in the preceding step. This model consistently incorporates the variety of structure–property relationships reported. A comprehensive case study is presented on seven phosphorus flame retardants in two epoxy resins to breathe life into the two-step approach. KW - Charring KW - Epoxy KW - Flame retardancy KW - Pyrolysis KW - Thermogravimetric analysis (TGA) PY - 2016 DO - https://doi.org/10.1002/mame.201500250 SN - 1438-7492 SN - 1439-2054 VL - 301 IS - 1 SP - 9 EP - 35 PB - Wiley-VCH Verl. CY - Weinheim AN - OPUS4-35273 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Frasca, Daniele A1 - Schulze, Dietmar A1 - Wachtendorf, Volker A1 - Huth, Christian A1 - Schartel, Bernhard T1 - Multifunctional multilayer graphene/elastomer nanocomposites N2 - Elastomers are usually reinforced and employed in different applications. Various different nanoparticles, including layered silicates, carbon nanotubes, and expanded graphite, are currently being used as nanofiller. Multilayer Graphene (MLG) is proposed as promising nanofiller to improve the functional properties of Chlorine-Isobutylene-Isoprene Rubber (CIIR), Nitrile-Butadiene Rubber (NBR), Natural Rubber (NR) and Styrene–Butadiene Rubber (SBR) at low concentrations. MLG is constituted by only approximately 10 graphene sheets. Nanocomposites with extremely low MLG content (3 phr) showed evident improvement in rheological, mechanical and curing properties. The Young's modulus of the nanocomposites increased more than twice in comparison with the unfilled rubbers. MLG also improved the weathering resistance of the different rubbers. The nanocomposites conserved their initial mechanical properties against weathering exposure. KW - Elastomer KW - Nanocomposite KW - Multilayer graphene PY - 2015 DO - https://doi.org/10.1016/j.eurpolymj.2015.07.050 SN - 0014-3057 SN - 1873-1945 VL - 71 SP - 99 EP - 113 PB - Elsevier Ltd. CY - Oxford AN - OPUS4-33843 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schartel, Bernhard T1 - From Know-how to Challenges in Bench-scale Fire Testing: A Polymer Researcher's Viewpoint T2 - Workshop Small Scale Fire Testing, (FRPM 2015) CY - Berlin, Germany DA - 2015-06-21 PY - 2015 AN - OPUS4-33630 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hörold, Andreas A1 - Schartel, Bernhard A1 - Trappe, Volker A1 - Gettwert, V. A1 - Korzen, Manfred T1 - Protecting the structural integrity of composites in fire: Intumescent coatings in the intermediate scale N2 - The fire behaviour of light-weight material used in structural applications is regarded as the main challenge to be solved for mass transportation. The task is to perform realistic experiments, including a mechanical test scenario under fully developed fires, to improve the material's reliability in structural applications. Our approach utilises an intermediate-scale test set-up (specimen size 500 × 500 mm) to apply realistic compressive loads and fully developed fires directly to one side of a carbon-fibre-reinforced sandwich composite. Three different intumescent coatings were applied to sandwich structures and compared to a bench-scale study. The results emphasise intumescent coatings as a promising method to sustain fire resistance, multiplying the time to failure. Nevertheless, the realistic intermediate-scale test using severe direct flame application underlines the extremely short failure times when the actual composite components are tested without any additional insulation. KW - Carbon-fibre-reinforced KW - Fire stability KW - High-temperature properties KW - Mechanical testing KW - Fully developed fire KW - Post-crash scenario PY - 2015 DO - https://doi.org/10.1177/0731684415609791 SN - 0731-6844 SN - 1530-7964 VL - 34 IS - 24 SP - 2029 EP - 2044 PB - Technomic Publ. Co. CY - Westport, Conn. AN - OPUS4-35120 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Günther, Martin A1 - Lorenzetti, A. A1 - Schartel, Bernhard T1 - From Cells to Residues: Flame-Retarded Rigid Polyurethane Foams N2 - Rigid polyurethane foams (RPUFs) exhibit short times to ignition as well as rapid flame spread and are therefore considered to be hazardous materials. This paper focuses on the fire phenomena of RPUFs, which were investigated through a multimethodological approach. Water-blown polyurethane (PUR) foams without flame retardants (FRs) as well as waterblown PUR foams containing triethyl phosphate as a gas phase-active FR were examined. The aim of this study is to clarify the influence of the FR on the fire phenomena during combustion of the foams. Additionally, materials’ densitieswere varied to range from 30 to 100 kg/m3. Thermophysical properties were studied bymeans of thermogravimetry; fire behavior and flammability were investigated via cone calorimeter and limiting Oxygen index, respectively. During the cone calorimeter test, the temperature development inside the burning specimens was monitored with thermocouples, and cross sections of quenched specimens were examined visually, giving insight into the morphological changes during combustion. The present paper delivers a comprehensive study, illuminating phenomena occurring during foam combustion and the influence of a FR active in the gas phase. The superior fire performance of flameretarded PUR foams was found to be based on flame inhibition, and on increased char yield leading to a more effective protective layer. It was proven that in-depth absorption of radiation is a significant factor for estimation of time to ignition. Cross sections investigated with the electron scanning microscope exhibited a pyrolysis front with an intact foam structure underneath. The measurement of temperature development inside burning specimens implied a shift of burning behavior towards that of non-cellular materials with rising foam density. KW - Polyurethane KW - Rigid foams KW - Fire behavior PY - 2020 DO - https://doi.org/10.1080/00102202.2019.1634060 SN - 0010-2202 SN - 1563-521X VL - 192 IS - 12 SP - 2209 EP - 2237 PB - Taylor & Francis AN - OPUS4-51483 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schartel, Bernhard T1 - Flammschutz für Polymere in der Elektrotechnik N2 - Das Brandverhalten stellt wie das elektrische Isolationsverhalten, die geringen elektrischen Verluste, die Verarbeitbarkeit und Formbarkeit eine der wesentlichen Schlüsseleigenschaften im Eigenschaftsprofil von Polymerwerkstoffen in der Elektrotechnik dar. Dabei bedarf es einer Ausrüstung der Polymere mit Flammschutzmittel. Die Entwicklung von immer effizienteren, synergistischen und multifunktionalen Multikomponentensystemen ist dabei eine herausragende Quelle für Innovation. Die Verbesserung der werkstoff- und anwendungsspezifischen Flammschutzlösungen bestimmen die aktuellen und zukünftigen Polymermaterialien in der Elektrotechnik mit. Der Vortrag stellt anhand von Beispielen einige der erfolgreichen Konzepte dar. Es wird versucht, über das wissenschaftlich systematische Verständnis Grundprinzipien und Lösungsstrategien zu verdeutlichen. T2 - Vortrag des Monats Oktober 2020, Neue Materialien Bayreuth GmbH CY - Bayreuth, Germany DA - 06.10.2020 KW - Flammschutzmittel KW - Elektrotechnik KW - Brandtests KW - Synergie KW - Multikomponentensysteme PY - 2020 AN - OPUS4-51410 LA - mul AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Günther, Martin A1 - Levchik, S. V. A1 - Schartel, Bernhard T1 - Bubbles and collapses: Fire phenomena of flame-retarded flexible polyurethane foams N2 - Flexible polyurethane foams (FPUF) are easy to ignite and exhibit rapid flame spread. In this paper, the fire phenomena of two standard foam formulations containing tris (1,3-dichloro-2-propyl) phosphate (FR-2) and a halogen-freepoly (ethyl ethylene phosphate) (PNX), respectively, as flame retardants are compared. A multimethodological approach is proposed which combines standard fire tests as well as new investigatory approaches. The thermophysical properties of the foams were determined by thermogravimetric analysis (TG), reaction to small flames was studied by means of the limiting oxygen index (LOI) and UL 94 HBF test, and the burning behavior was investigated with the cone calorimeter. Further, temperature development in burning cone calorimeter samples was monitored using thermocouples, and rheological measurements were performed on pyrolyzed material, delivering insight into the dripping behavior of the foams. This paper gives comprehensive insight into the fire phenomena of flame-retarded FPUFs that are driven by the two-step decomposition behavior of the foams. LOI and UL 94 HBF tests showed a reduced flammability and reduced tendency to drip for the flame-retarded foams. TG and cone calorimeter measurements revealed that the two-step decomposition behavior causes two stages during combustion, namely structural collapse and pool fire. The flame-retardant mode of action was identified to take place primarily during the foam collapse and be based mainly on flame inhibition. However, some condensed-phase action was been measured, leading to significantly increased melt viscosity and improved dripping behavior for foams containing PNX. KW - Burning behavior KW - Flame retardant KW - Flexible PU foam PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-512145 DO - https://doi.org/10.1002/pat.4939 SN - 1042-7147 SN - 1099-1581 VL - 31 IS - 10 SP - 2185 EP - 2198 PB - Wiley Online Libary AN - OPUS4-51214 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Goedecke, Caroline A1 - Dittmann, Daniel A1 - Eisentraut, Paul A1 - Wiesner, Yosri A1 - Schartel, Bernhard A1 - Klack, Patrick A1 - Braun, Ulrike T1 - Evaluation of thermoanalytical methods equipped with evolved gas analysis for the detection of microplastic in environmental samples N2 - Microplastic particles are currently detected in almost all environmental compartments. The results of detection vary widely, as a multitude of very different methods are used with very different requirements for analytical validity. In this work four thermoanalytical methods are compared and their advantages and limitations are discussed. One of them is thermal extraction-desorption gas chromatography mass spectrometry (TED-GC/MS), an analysis method for microplastic detection that has become established in recent years. In addition, thermogravimetric analysis coupled with Fourier-transform infrared spectroscopy (TGA-FTIR) and mass spectrometry (TGA-MS) were applied, two methods that are less common in this field but are still used in other research areas. Finally, microscale combustion calorimeter (MCC) was applied, a method not yet used for microplastic detection. The presented results are taken from a recently published interlaboratory comparison test by Becker et al. (2020). Here a reference material consisting of suspended matter and specified added polymer masses was examined, and only the results of the recoveries were presented. In the present paper, however, the results for the individual polymers are discussed in detail and individual perspectives for all instruments are shown. It was found that TED-GC/MS is the most suitable method for samples with unknown matrix and unknown, variable kinds and contents of microplastic. TGA-FTIR is a robust method for samples with known matrix and with defined kinds of microplastic. TGA-MS may offer a solution for the detection of PVC particles in the future. MCC can be used as a very fast and simple screening method for the identification of a potential microplastic load of standard polymers in unknown samples. KW - Microplastic KW - TED-GC/MS KW - TGA-MS KW - TGA-FTIR KW - MCC KW - Thermal analysis PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-516687 DO - https://doi.org/10.1016/j.jaap.2020.104961 VL - 152 SP - 104961 PB - Elsevier B.V. AN - OPUS4-51668 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Battig, Alexander A1 - Sanchez-Olivares, G. A1 - Rockel, Daniel A1 - Maldonado-Santoyo, M. A1 - Schartel, Bernhard T1 - Waste not, want not: The use of leather waste in flame retarded EVA N2 - Leather is among the most ancient, widely used materials worldwide. Industrial-scale leather production produces large quantities of organic waste attained during shaving and buffing steps during processing. In this study, leather wastes (LW) are used as fillers in flame retarded polymer composites. LW is investigated as a multifunctional bio-filler that enhances the fire performance of flame retarded poly(ethylene–vinyl acetate) (EVA) containing phosphorus flame retardants (P-FRs) ammonium polyphosphate (APP) or a melamine-encapsulated APP (eAPP). Using LW from tanneries as adjuvants to enhance P-FRs in EVA reduces industrial wastes that otherwise require costly waste management solutions. Materials are characterized multi-methodically via mechanical tests, electron microscopy, rheology, thermogravimetric analysis, evolved gas analysis, and condensed phase FTIR, also reaction-to-small-flames and cone calorimeter tests. EVA containing 10 wt-% LW and 20 wt-% P-FRs achieve 20% reductions in fire loads versus EVA, and up to 10% reduction in effective heats of combustion versus EVA with equal (30 wt-%) P-FR loadings. Enhanced char stabilization of EVA composites with LW and P-FRs lowered peaks of heat release rates up to 53% compared to EVA, and up to 40% compared to equal P-FRs loadings. Synergisms between LW and P-FRs in EVA are quantified. A chemical decomposition mechanism is proposed. KW - Leather waste KW - Tannery industry KW - EVA KW - Fire protection KW - Flame retardancy KW - Charring PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-532977 DO - https://doi.org/10.1016/j.matdes.2021.110100 SN - 0264-1275 VL - 210 SP - 1 EP - 16 PB - Elsevier CY - Amsterdam AN - OPUS4-53297 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Tan, Yi A1 - Wachtendorf, Volker A1 - Kukofka, Tobias A1 - Klack, Patrick A1 - Ruder, J. A1 - Lin, Xuebao A1 - Schartel, Bernhard T1 - Degradation of flame retardance: A comparison of ethylene‐vinyl acetate and low‐density polyethylene cables with two different metal hydroxides N2 - The durability of flame retardancy is a challenge for cables over long lifetimes. The degradation of flame retardance is investigated in two kinds of exposures, artificial weathering and humidity. In this basic study, typical mineral flame retardants in two polymers frequently used in cable jackets are investigated to get the fundamental picture. Aluminum hydroxide (ATH) and magnesium hydroxide (MDH) are compared in ethylene‐vinyl acetate (EVA), and further in EVA and linear low‐density polyethylene (LLDPE) cables containing the same ATH. The changes in chemical structure at the surface are studied through attenuated total reflectance Fourier transform infrared spectroscopy (ATR‐FTIR), the formation of cracks, and changes in color are investigated. The cone calorimeter and a bench scale fire testing cable module are utilized to evaluate the fire behavior of the cables. Although the flame retardancy deteriorated slightly, it survived harsh exposure conditions for 2000 h. Compared to EVA/MDH and LLDPE/ATH, the fire behavior of EVA/ATH is the least sensitive. Taken together, all of the results converge to estimate that there will be no problem with flame retardancy performance, for materials subjected to natural exposure for several years; the durability of fire retardancy is questionable for longer periods, and thus requires further investigation. KW - Durability KW - Flame retardant KW - Aluminum hydroxide (ATH) KW - Magnesium hydroxide KW - Ethylene-vinyl acetate KW - Cables KW - Weathering PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-519573 DO - https://doi.org/10.1002/app.50149 VL - 138 IS - 14 SP - 50149 PB - Wiley AN - OPUS4-51957 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Daus, Lars-Hendrik A1 - Schartel, Bernhard A1 - Wachtendorf, Volker A1 - Mangelsdorf, R. A1 - Korzen, Manfred T1 - A chain is no stronger than its weakest link: Weathering resistance of water-based intumescent coatings for steel applications N2 - A systematic approach was used to investigate the weathering-induced degradation of a common water–based intumescent coating. In this study, the coatings are intended for humid indoor applications on steel substrates. The coating contains ammonium polyphosphate, pentaerythritol, melamine, and polyvinyl acetate. By replacing each ingredient with a less water-soluble substance, the most vulnerable substances, polyvinyl acetate and pentaerythritol, were identified. Furthermore, the weathering resistance of the system was improved by exchanging the ingredients. The coatings were stressed by artificial weathering tests and evaluated by fire tests. Thermogravimetry and Fourier-transform infrared spectroscopy were used to study the thermal decomposition. This study lays the foundation for the development of a new generation of water-based intumescent coatings. KW - Intumescence KW - Fire resistance KW - Fire protective coatings KW - Weathering KW - Thermogravimetric analyses PY - 2021 DO - https://doi.org/10.1177/0734904120961064 SN - 0734-9041 SN - 1530-8049 VL - 39 IS - 1 SP - 72 EP - 102 PB - SAGE AN - OPUS4-52015 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Schartel, Bernhard ED - Troitzsch, J. ED - Antonatus, E. T1 - The Burning of Plastics N2 - The burning of a polymer is a physico–chemical process strongly influenced by the coupling of a chemical reaction – oxidation of fuel – in the gas phase with a chemical decomposition reaction – pyrolysis – in the condensed phase via heat and mass transfer. The heat and mass flux control the intensity of fire and the ablation of fuel. Indeed, the temperature profile as a function of time may be one of the most important responses of a specimen to understand its burning behavior. Further, several physical phenomena, such as the heat absorption of the materials, thermal conductivity, and also melt flow and dripping, play a major role in determining ignition, flammability, and fire behavior. The burning of a polymer is very complex. The various phenomena interact with each other, e. g., pyrolysis also influences the viscosity of the melt, and, thus, whether dripping or charring results in a protective layer, increasing the shielding effect of the residual protective layer. Only a detailed and comprehensive description opens the door to a well-founded understanding of the burning behavior of polymeric materials. KW - Fire behaviour KW - Plastics KW - Pyrolysis KW - Decomposition KW - Ignition KW - Smoldering KW - Flame spread KW - Steady burning KW - Fire load KW - Fire resistance PY - 2021 SN - 978-1-56990-762-7 SP - 23 EP - 52 PB - Hanser CY - Munich ET - 4th Edition AN - OPUS4-52684 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schartel, Bernhard T1 - Flammschutzmittel in PUR: Eine alte, aktuelle und zukünftige Herausforderung N2 - Überblick über die Herausforderungen, Anforderungen und Lösungswege für den Flammschutz von Polyurethanwerkstoffen (thermoplastisches und elastomeres Polyurethan (TPU, PUR), PUR Hard- und Weichschäume, PIR, PUR Coatings). Die Werkstoffcharakteristika wie Pyrolyse, effektive Verbrennungswärme, Rückstandsausbeute, Verarbeitungsparameter und kg-Preis definieren die Anforderungen an Flammschutzlösungen. Der Flammschutz ist spezifisch für das Material ausgelegt, aber auch für die verschiedenen Anwendungen (Automobilbau, Schienenfahrzeuge, Bauwesen, Elektrotechnik, usw.), d.h. um spezielle Brandtests zu bestehen. Die Pyrolyse und das Brandverhalten von PUR und PUR-Schäumen sowie der flammgeschützten Varianten wird diskutiert. Die gängigen Flammschutzmittel(-kombinationen) werden zusammengefasst und mit Beispielen belegt. T2 - PUR Forum, Flammenschutz in der Polyurethanverarbeitung CY - Online meeting DA - 05.05.2021 KW - Polyurethan KW - Pyrolyse KW - Flammschutz KW - Expandierbarer Graphit KW - Schaum KW - TPU PY - 2021 AN - OPUS4-52590 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Battig, Alexander A1 - Müller, Patrick A1 - Bertin, Annabelle A1 - Schartel, Bernhard T1 - Hyperbranched Rigid Aromatic Phosphorus-Containing Flame Retardants for Epoxy Resins N2 - A rigid aromatic phosphorus-containing hyperbranched flame retardant structure is synthesized from 10-(2,5 dihydroxyphenyl)-10H-9-oxa- 10-phosphaphenanthrene-10-oxide (DOPO-HQ), tris(4-hydroxyphenyl)phosphine oxide (THPPO), and 1,4-terephthaloyl chloride (TPC). The resulting poly-(DOPO-HQ/THPPO-terephthalate) (PDTT) is implemented as a flame retardant into an epoxy resin (EP) at a 10 wt% loading. The effects on EP are compared with those of the monomer DOPO-HQ and triphenylphosphine oxide (OPPh3) as low molar mass flame retardants. The glass transition temperature, thermal decomposition, flammability (reaction to small flame), and burning behavior of the thermosets are investigated using differential scanning calorimetry, thermogravimetric analysis, pyrolysis combustion flow calorimetry, UL 94-burning chamber testing, and cone calorimeter measurements. Although P-contents are low at only 0.6 wt%, the study aims not at attaining V-0, but at presenting a proof of principle: Epoxy resinswith PDTT show promising fire performance, exhibiting a 25% reduction in total heat evolved (THE), a 30% reduction in peak heat release rate (PHRR) due to flame inhibition (21% reduction in effective heat of combustion (EHC)), and an increase in Tg at the same time. This study indicates that rigid aromatic hyperbranched polymeric structures offer a promising route toward multifunctional flame retardancy. KW - Hyperbranched KW - Aromatic KW - Phosphorus KW - Phosphine oxide KW - DOPO KW - Flame retardant KW - Xpoxy resin KW - Rigid PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-525910 DO - https://doi.org/10.1002/mame.202000731 SN - 1439-2054 VL - 306 IS - 4 SP - 731 PB - Wiley AN - OPUS4-52591 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Chan, Yin Yam A1 - Ma, C. A1 - Zhou, F. A1 - Hu, Y. A1 - Schartel, Bernhard T1 - Flame retardant flexible polyurethane foams based on phosphorous soybean-oil polyol and expandable graphite N2 - A phosphorous soybean-oil–based polyol was derived via epoxidation and ring opening reaction as an alternative to petrochemical-based polyol for the synthesis of flexible polyurethane foams (FPUFs). 5-wt.% and 10-wt.% of expandable graphite (EG) were added to further improve flame retardancy. The mechanical properties (tensile strength and compression stress) of the foams were investigated. Thermogravimetric analysis (TGA) coupled with Fourier-transform infrared (FTIR) were conducted to evaluate the pyrolysis; limiting oxygen index (LOI), UL 94 and cone calorimeter were performed to analyze the fire performance of the foams; smoke density chamber was used to investigate the smoke released during burning. When 10-wt.% of EG was used, the flame retardancy of the foams was much enhanced due to the synergistic effect between phosphorus and EG. The char yield was three times higher (54wt.%). The fire load MARHE approached 100 kWm−2, half of the value expected for a superposition. The combination of phosphorous polyols and EG is proposed as strategy for future flame retarded FPUFs. KW - Phosphorous soybean-oil–based polyol KW - Flexible polyurethane foam KW - Expandable graphite KW - Flame retardancy KW - Smoke measurement PY - 2021 DO - https://doi.org/10.1016/j.polymdegradstab.2021.109656 SN - 0141-3910 VL - 191 SP - 9656 PB - Elsevier Ltd. AN - OPUS4-52907 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zhou, F. A1 - Ma, C. A1 - Zhang, K. A1 - Chan, Yin Yam A1 - Xiao, Y. A1 - Schartel, Bernhard A1 - Döring, M. A1 - Wang, B. A1 - Hu, W. A1 - Hu, Y. T1 - Synthesis of Ethyl (Diethoxymethyl)phosphinate Derivatives and Their Flame Retardancy in Flexible Polyurethane Foam: Structure-flame Retardancy Relationships N2 - Three novel liquid ethyl (diethoxymethyl)phosphinate derivatives (EDPs) were synthesized and incorporated into flexible polyurethane foams (FPUFs). The flame retardancy of FPUFs were evaluated by limiting oxygen index (LOI), vertical burning and cone calorimetry tests, and the results indicated the structure-flame retardancy relationship of EDPs. Among these EDPs, P-(diethoxymethyl)-N-phenylphosphonamidate (EDPPA) exhibited the best flame retardant effect, methyl 3-((diethoxymethyl)(ethoxy)phosphoryl)propanoate (EDPMA) the second, and ethyl phenyl (di-ethoxymethyl)phosphonate (EDPPO) the worst. When the incorporation of EDPPA was 10 wt%, the FPUFs could self-extinguish and pass the vertical burning test. Meanwhile, the LOI value of FPUF-PA increased to 23.6% with 20 wt% loading of flame retardant. According to the investigation of volatiles during the thermal degradation of FPUFs and the morphologies of char residues after cone test, we inferred the pos- sible flame retardant mechanism. The results indicated that EDPs could release phosphorus-containing compounds in the gas phase, which would generate phosphorus-containing radicals and play the role of radical scavenger. In the condensed phase, EDPs can promote the formation of dense, intact and thermal stably char layer on the surface of FPUFs. Moreover, we found that the structure influence on flame retardancy was attributed to the atoms linked to the central phosphorus. Our results indicate that these EDPs are promising flame retardants in FPUFs that can be applied to improve the flame retardancy of FPUFs in various practical applications. KW - Ethyl (diethoxymethyl)phosphinate derivatives KW - Flame retardant KW - Flexible polyurethane foam KW - Structure-flame retardancy relationship PY - 2021 DO - https://doi.org/10.1016/j.polymdegradstab.2021.109557 SN - 0141-3910 VL - 188 SP - 109557 PB - Elsevier Ltd. AN - OPUS4-53085 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wahab, M. A. A1 - Kebelmann, Katharina A1 - Schartel, Bernhard A1 - Griffiths, G. T1 - Improving bio-oil chemical profile of seaweeds through anaerobic fermentation pre-treatment N2 - Biomass pre-treatments for bio-oil quality improvement are mainly based on thermal and chemical methods which are costly and hence reduce the sustainability of pyrolysis-based refineries. In this paper, anaerobic digestion (AD) and dark fermentation (DF) are proposed as alternative ‘green’ pre-treatments to improve this situation. For this purpose, three seaweeds namely Sargassum polycystum, (Phaephyta), Gracilaria tenuistipitata, (Rhodophyta) and Ulva reticulata, (Chlorophyta) with high ash and oxygen contents were pre-treated to improve their composition and structure prior to pyrolysis. The results reveal that both biological pre-treatments affected, positively, the composition and structure of the seaweed biomass with AD pre-treatment reducing N and S contents by 86% and 63%, respectively. DF was more efficient in terms of ash and moisture reduction with 25% and 70%, respectively. In addition, oxygen (O) reduction by 27% was observed after DF which was evidenced by FTIR spectroscopy indicating the reduction of most oxygen-containing functional groups in the biomass. On the other hand, the carbon (C) content increased in DF pre-treated seaweeds up to 42%, almost two times higher relative content than C in the raw seaweed. The changes in the composition of pre-treated seaweeds resulted in changes in their thermal degradation and the volatile profiles produced during pyrolysis. Interestingly, anhydrosugars and furans which account for some 70% (by area) in raw seaweeds markedly declined or become undetectable after DF pre-treatment and correspondingly more acetic acid and hydrocarbons were produced while after AD more aromatics with high toluene content (ca.17%) were generated. The results indicate that biooil with profiles more similar to petroleum-based composition i.e. rich in hydrocarbons and low in anhydrosugars, N and S can be generated by AD and DF pre-treatments and opens up the possibility of these approaches to effect cost reduction in the overall generation of bio-based fuels. KW - Anaerobic digestion KW - Dark fermentation KW - Pyrolysis KW - Seaweeds KW - Thermogravimetric analysis KW - Pyrolysis volatiles PY - 2021 DO - https://doi.org/10.1016/j.enconman.2021.114632 SN - 0196-8904 VL - 245 SP - 1 EP - 12 PB - Elsevier CY - Amsterdam AN - OPUS4-53136 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schartel, Bernhard T1 - More Than the Sum of Its Parts: Multicomponent Flame Retardants N2 - Efficient flame retardancy is often achieved only when applying multicomponent systems. Flame retardants are combined or used together with adjuvants or synergists; fibres and fillers contribute to fire properties crucially. Multicomponent systems are discussed in their capacity as general and powerful strategy for achieving and optimizing flame retardant polymeric materials. T2 - 18th European Meeting on Fire Retardant Polymeric Materials, FRPM21 CY - Budapest, Hungary DA - 29.08.2021 KW - Fire Retardant KW - Synergy KW - Pseudo-synergy KW - Filler KW - Fibre reinforced polymers KW - Dripping Agent KW - Adjuvant KW - Synergist KW - Charring Agent KW - Mode of Action PY - 2021 AN - OPUS4-53198 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Chan, Yin Yam A1 - Ma, C. A1 - Zhou, F. A1 - Hu, Y. A1 - Schartel, Bernhard T1 - A liquid phosphorous flame retardant combined with expandable graphite or melamine in flexible polyurethane foam N2 - A systematic series of flexible polyurethane foams (FPUF) with different concentrations of flame retardants, bis([dimethoxyphosphoryl]methyl) phenyl phosphate (BDMPP), and melamine (MA) or expandable graphite (EG) was prepared. The mechanical properties of the FPUFs were evaluated by a universal testing machine. The pyrolysis behaviors and the evolved gas analysis were done by thermogravimetric analysis (TGA) and TGA coupled with Fourier-transform infrared (TG-FTIR), respectively. The fire behaviors were studied by limiting oxygen index (LOI), UL 94 test for horizontal burning of cellular materials (UL 94 HBF), and cone calorimeter measurement. Scanning electronic microscopy (SEM) was used to examine the cellular structure's morphology and the postfire char residue of the FPUFs. LOI and UL 94 HBF tests of all the flame retarded samples show improved flame retardancy. BDMPP plays an essential role in the gas phase because it significantly reduces the effective heat of combustion (EHC). This study highlights the synergistic effect caused by the combination of BDMPP and EG. The measured char yield from TGA is greater than the sum of individual effects. No dripping phenomenon occurs during burning for FPUF-BDMPP-EGs, as demonstrated by the result of the UL 94 HBF test. EG performs excellently on smoke suppression during burning, as evident in the result of the cone calorimeter test. MA reduces the peak heat release rate (pHRR) significantly. The synergistic effect of the combination of BDMPP and EG as well as MA offers an approach to enhance flame retardancy and smoke suppression. KW - Bis([dimethoxyphosphoryl]methyl) phenyl phosphate KW - Expandable graphite KW - Flexible polyurethane foam KW - melamine KW - phosphorous flame retardant PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-541840 DO - https://doi.org/10.1002/pat.5519 SN - 1099-1581 VL - 33 IS - 1 SP - 326 EP - 339 PB - Wiley AN - OPUS4-54184 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Marti, J. A1 - Schartel, Bernhard A1 - Oñate, E. T1 - Simulation of the burning and dripping cables in fire using the particle finite element method N2 - The behavior of the cable jacket in fire characterized by the tendency to melt and drip constitutes a major source of fire hazard. The reason is that the melted material may convey the flame from one point to another, expanding fire and contributing to the fire load. In this article, the capability of a new computational strategy based on the particle finite element method for simulating a bench-scale cables burning test is analyzed. The use bench-scale test has been previously used to simulate the full-scale test described in EN 50399. As the air effect is neglected, a simple combustion model is included. The samples selected are two cables consisting of a copper core and differently flame retarded thermoplastic polyurethane sheets. The key modeling parameters were determined from different literature sources as well as experimentally. During the experiment, the specimen was burned under the test set-up condition recording the process and measuring the temperature evolution by means of three thermocouples. Next, the test was reproduced numerically and compared with a real fire test. The numerical results show that the particle finite element method can accurately predict the evolution of the temperature and the melting of the jacket. KW - Dripping behavior KW - Particle finite element method KW - Cables in fire KW - Fire behavior KW - Fire simulation KW - Cable bundle PY - 2022 DO - https://doi.org/10.1177/07349041211039752 SN - 0734-9041 VL - 40 IS - 1 SP - 3 EP - 25 PB - Sage AN - OPUS4-54185 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wachtendorf, Volker A1 - Schartel, Bernhard A1 - Lin, Xuebao A1 - Tan, Yi A1 - Schoch, R. A1 - Lang, M. A1 - Tröppner, O. A1 - Bosse, M. ED - Ziegahn, K.-F. T1 - Untersuchung der Witterungsbeständigkeit komplexer Funktionalitäten von Polymerwerkstoffen durch künstliche Bewitterung: Flammschutz N2 - In den letzten Jahrzehnten wurde die Degradation der polymeren Matrix von flammgeschützten Polymeren eingehend untersucht. Erst in den letzten Jahren jedoch hat sich die Frage der Lebensdauer der Funktionalität des Flammschutzes selbst als wichtige Fragestellung herauskristallisiert, z.B. bei Kabeln. Deshalb sollte diese Fragestellung durch systematisch-variierte künstliche Klima- und Bewitterungstests an flammgeschützten Polymerwerkstoffen untersucht werden. T2 - 50. Jahrestagung der Gesellschaft für Umweltsimulation (GUS) CY - Online meeting DA - 23.03.2022 KW - Flammschutz, Witterungsbeständigkeit, Langzeitbeständigkeit, UV, E&E PY - 2022 SN - 978-3-9818507-7-2 VL - 50 SP - 143 EP - 148 CY - Pfinztal (Berghausen) AN - OPUS4-54543 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wahab, M. A. A1 - Kebelmann, Katharina A1 - Schartel, Bernhard A1 - Griffiths, G. T1 - Valorization of macroalgae digestate into aromatic rich bio-oil and lipid rich microalgal biomass for enhanced algal biorefinery performance N2 - The valorization of macroalgae digestate as a secondary resource for high value chemicals and nutrients will promote the sustainability and circularity of anaerobic digestion based biorefinery. In this study, three digestates from A. nodosum C.linum and L. digitata were separated into liquid and solid fractions to investigate the production of high value added chemicals through pyrolysis using Pyrolysis Gas Chromatography Mass Spectroscopy (Py-GC/MS) while the filtered liquid fractions were tested as an alternative culture media to grow C. sorokiniana under mixotrophic conditions. The digestates showed different thermal degradation and an improvement of bio-oil profiles compared to the starter material. Pyrolyzates from raw macroalgae were characterized by a high anhydrosugar content in contrast to high aromatics observed in the case of their digestates. Toluene, benzofuran and vinylphenol, base chemicals for many industries, represented together 30–37% of the total chemicals produced during pyrolysis of the three macroalgae digestate. On the other hand, C. sorokiniana cultured on digestate-based media showed a higher lipid content with an increase in monounsaturated fatty acids and a lower poly-unsaturated fatty acid content in comparison to microalgae grown in standard tris-acetate-phosphate media. Thus, the acyl composition was shifted in a direction more suitable for biodiesel production by this process. In addition, the increase of Chemical Oxygen Demand and Volatile Fatty Acids concentration in the digestate was found to reduce ammonium toxicity. Finally, 94% of Chemical Oxygen Demand and 83% of ammonium were removed by microalgae from the digestate-based media which will reduce the pollution risk of the biorefinery. Overall, the results indicate that using macroalgae solid digestates can generate improvements in the quality of products obtained by pyrolysis and the liquid digestate can positively influence microalgae growth and its products. KW - Macroalgae KW - Anaerobic digestion KW - Aromatics KW - Microalgae culture KW - Biorefinery PY - 2022 DO - https://doi.org/10.1016/j.jclepro.2022.130925 SN - 0959-6526 VL - 341 SP - 1 EP - 10 PB - Elsevier Ltd. AN - OPUS4-54365 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schartel, Bernhard T1 - Non-vegan flame-retardant (adjuvants in) biocomposites N2 - Emanating from developing flame retarded biocomposites, we have proposed renewable natural fibers (including keratin) taken from industrial waste as an authentic sustainable approach. More recently, we have investigated non-vegan flame retardant approaches. This paper loves to give you an insight into our ongoing projects on biogenic industrial wastes like leather, bone meal, and insects. Materials were characterized multi-methodically, flame retardant modes of action quantified, decomposition mechanism proposed, and synergisms explained. Considering the large quantities of leather waste (LW) in industrial-scale production, we underline LW as multifunctional bio-adjuvants. LW enhances the flame retardancy of poly(ethylene-vinyl acetate) (EVA) containing phosphorus flame retardants (P-FR). Products/by-products of the invertebrate and vertebrate farming, respectively, are promising bio-based adjuvants in flame retarded bio-epoxy thermosets. While the addition of bone meal yields the formation of an inorganic shield, protein-based powders from insects provide an intumescent behavior. In combination with a P-FR superior charring and self-extinguishing are obtained. Acknowledgement: In part of this work was supported by the Volkswagen Foundation grant “Experiment!” No. 97437. T2 - Fire and Polymers, workshop, ACS Division of Polymer Chemistry CY - Napa, California, US DA - 05.06.2022 KW - Fire behaviour KW - Renewable KW - Circular economy KW - Biocomposite PY - 2022 AN - OPUS4-55025 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gleuwitz, F. Robert A1 - Battig, Alexander A1 - Schartel, Bernhard T1 - Tenebrio molitor Beetle as a “Nonvegan” Adjuvant to Flame Retardants in Tannic Acid-Based Epoxy Thermosets N2 - Material solutions that meet both circular bioeconomy policies and high technical requirements have become a matter of particular interest. In this work, a prospectively abundant proteinrich waste resource for the manufacturing of flame-retardant epoxy biocomposites, as well as for the synthesis of biobased flame retardants or adjuvants, is introduced. Different biomass fillers sourced from the cultivation of the mealworm beetle Tenebrio molitor are embedded in a bioepoxy resin cured with tannic acid and investigated regarding the fire performance of the thermosets. By means of spectroscopic and thermal analysis (attenuated total reflectance FTIR spectroscopy, thermogravimetric analysis-coupled FTIR spectroscopy, and differential scanning calorimetry), the influence of the biomass microparticles on the curing and thermal degradation behavior is evaluated. The final performance of the biocomposites is assessed based on fire testing methodology (limited oxygen index, UL-94, and cone calorimetry). Providing a high charring efficiency in the specific tannic acid-based epoxy matrix, the protein-rich adult beetle is further investigated in combination with commercial environmentally benign flame retardants in view of its potential as an adjuvant. The results highlight a char forming effect of nonvegan fillers in the presence of tannic acid, particularly during thermal decomposition, and point toward the potential of protein-based flame retardants from industrial insect rearing for future formulations. KW - Tannic acid KW - Flame retardancy KW - Sustainable KW - Epoxy resin KW - Insects PY - 2022 DO - https://doi.org/10.1021/acssuschemeng.2c00746 SN - 2168-0485 VL - 10 IS - 19 SP - 6313 EP - 6324 PB - ACS AN - OPUS4-54845 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Chan, Yin Yam A1 - Schartel, Bernhard T1 - It Takes Two to Tango: Synergistic Expandable Graphite–Phosphorus Flame Retardant Combinations in Polyurethane Foams N2 - Due to the high flammability and smoke toxicity of polyurethane foams (PUFs) during burning, distinct efficient combinations of flame retardants are demanded to improve the fire safety of PUFs in practical applications. This feature article focuses on one of the most impressive halogen-free combinations in PUFs: expandable graphite (EG) and phosphorus-based flame retardants (P-FRs). The synergistic effect of EG and P-FRs mainly superimposes the two modes of action, charring and maintaining a thermally insulating residue morphology, to bring effective flame retardancy to PUFs. Specific interactions between EG and P-FRs, including the agglutination of the fire residue consisting of expanded-graphite worms, yields an outstanding synergistic effect, making this approach the latest champion to fulfill the demanding requirements for flame-retarded PUFs. Current and future topics such as the increasing use of renewable feedstock are also discussed in this article. KW - Synergy KW - Phosphorus-containing flame retardant KW - Expandable graphite KW - Polyurethane foams PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-551958 DO - https://doi.org/10.3390/polym14132562 SN - 2073-4360 VL - 14 IS - 13 SP - 2562 PB - MDPI AN - OPUS4-55195 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Schartel, Bernhard ED - Morgan, A.B. T1 - Multicomponent Flame Retardants N2 - The important take home message of this chapter: When multicomponent flame retardant systems are applied to polymeric materials, it becomes possible to address multiple fire properties, increase efficiency, and minimize flame retardant use to maximize polymer property balance. Flame retardants are combined or used together with adjuvants or synergists; fibers and fillers make a crucial contribution to their fire properties. Multicomponent systems are discussed in their capacity as an overall powerful strategy for achieving and optimizing non-halogenated flame-retardant polymeric materials. KW - Flame retardants KW - Synergy KW - Adjuvants KW - Fillers KW - Fibres PY - 2022 SN - 978-1-119-75056-7 SP - 413 EP - 474 PB - Scrivener Publishing LLC CY - Bevery ET - 2nd Edition AN - OPUS4-54426 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schartel, Bernhard T1 - Flame retardancy features sustainability: Fake fiction, food for thought, or future N2 - • Renewable sources find their way into flame retardancy • Innovative solutions meet sustainability • Facing recycling and circular economy T2 - AMI Fire Retardants in Plastics CY - Philadelphia, PA, US DA - 26.04.2023 KW - Flame retardants KW - Sustainability KW - Resources from waste streams KW - Biocomposite KW - Vitrimers PY - 2023 AN - OPUS4-57415 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Lenz, J. U. A1 - Pospiech, D. A1 - Komber, H. A1 - Korwitz, A. A1 - Kobsch, O. A1 - Paven, M. A1 - Albach, R. W. A1 - Günther, Martin A1 - Schartel, Bernhard T1 - Effective halogen-free flame-retardant additives for crosslinked rigid polyisocyanurate foams: Comparison of chemical structures N2 - The impact of phosphorus-containing flame retardants (FR) on rigid polyisocyanurate (PIR) foams is studied by systematic variation of the chemical structure of the FR, including non-NCO-reactive and NCO-reactive dibenzo[d,f][1,3,2]dioxaphosphepine 6-oxide (BPPO)- and 9,10 dihydro-9-oxa-10 phosphaphenanthrene-10-oxide (DOPO)-containing compounds, among them a number of compounds not reported so far. These PIR foams are compared with PIR foams without FR and with standard FRs with respect to foam properties, thermal decomposition, and fire behavior. Although BPPO and DOPO differ by just one oxygen atom, the impact on the FR properties is very significant: when the FR is a filler or a dangling (dead) end in the PIR polymer network, DOPO is more effective than BPPO. When the FR is a subunit of a diol and it is fully incorporated in the PIR network, BPPO delivers superior results. KW - Flame retardant; KW - Dibenzo[d,f][1,3,2]dioxaphosphepine 6-oxide; BPPO KW - 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide; DOPO KW - Polyisocyanurate; PIR KW - Rigid foam KW - Cone calorimeter KW - Pudovik reaction PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-567712 DO - https://doi.org/10.3390/ma16010172 SN - 1996-1944 VL - 16 IS - 1 SP - 1 EP - 22 PB - MDPI CY - Basel AN - OPUS4-56771 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Turski Silva Diniz, Analice A1 - Schartel, Bernhard T1 - The effects of property variation on the dripping behaviour of polymers during UL94 test simulated by particle finite element method N2 - The dripping behaviour of polymers is often observed experimentally through the UL94 flammability standard test. In this work, polymeric dripping under fire is investigated numerically using particle finite element method. A parametric analysis was carried out to observe the influence of a single property on overall dripping behaviour via a UL94 vertical test model. Surrogates and property ranges were defined for variation of the following parameters: glass transition temperature (Tg), melting temperature (Tm), decomposition temperature (Td), density (ρ), specific heat capacity (Cp), apparent effective heat of combustion of the volatiles, char yield (μ), thermal conductivity (k), and viscosity (η). Polyamide, poly(ether ether ketone), poly(methyl methacrylate), and polysulfone were used as benchmarks. Simulated results showed that specific heat capacity, thermal conductivity, and char yield allied with viscosity were the properties that most influenced dripping behaviour (starting time and occurrence). KW - Dripping KW - PFEM KW - UL 94 KW - Simulation KW - Fire behaviour PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-597449 DO - https://doi.org/10.1515/epoly-2023-0194 SN - 1618-7229 VL - 24 IS - 1 PB - De Gruyter AN - OPUS4-59744 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Sunder, S. A1 - Jauregui Rozo, Maria A1 - Schartel, Bernhard A1 - Ruckdäschel, H. T1 - Adapting intumescent/low-melting glass flame-retardant formulations for transfer to glass-fiber-reinforced composites and post-fire mechanical analysis N2 - The residual post-fire mechanical properties of fiber-reinforced epoxy composites are influenced by their fire residues after burning. This study uses intumescent/low-melting glass flame retardants to tailor fire residues in epoxy resin. Processibility of prepregs and their quality are analysed for transfer of the flame-retardant epoxy resins to layered glass-fiber reinforced composites. Minimal effects were found on the pre-fire flexural strengths of the composites due to low loading of the flame retardants. However, when transferred to glass-fiber reinforced composites, the fire residues diminish significantly. Further studies are required to improve theoretical and experimental estimations of the post-fire mechanics of the composites. T2 - SAMPE Europe Conference 2023 CY - Madrid, Spain DA - 03.10.2023 KW - Fire residue KW - Prepregs KW - Mechanics KW - Lightweight materials KW - Composites KW - Flame retardancy PY - 2023 SP - 1 EP - 7 AN - OPUS4-59138 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sanchez Olivares, G. A1 - Rockel, Daniel A1 - Calderas, F. A1 - Schartel, Bernhard T1 - Utilizing leather fibers from industrial wastes as bio-filler to improve flame retardancy in polypropylene N2 - Combining buffing leather fibers from industrial waste streams with ammonium polyphosphate and bentonite clay is proposed as a flame-retardant additive for polypropylene. The paper addresses how they can be processed into attractive composites with the desired mechanical properties. Buffing leather fibers function as a multifunctional bio-filler and as a synergist for the flame retardant, resulting in fire retardancy successful enough to increase the oxygen index (LOI) by up to 7 vol.-% and to achieve a V0 UL 94 classification. Impressively reduced heat release rates are obtained in the cone calorimeter at 50 kW/m2 irradiation; for instance, the maximum average rate heat evolved (MARHE) drops from 765 to below 200 kW m􀀀 2. The synergistic effects are quantified and shown to be very strong for LOI and MARHE. This work opens the door to use waste buffing leather fibers as a promising multifunctional and synergistic bio-filler. KW - Polypropylene KW - Flame retardancy KW - Industrial waste KW - Leather fibers KW - Bio-filler PY - 2024 DO - https://doi.org/10.1016/j.jiec.2023.11.008 SN - 1226-086X SN - 1876-794X VL - 132 SP - 148 EP - 160 PB - Elsevier B.V. AN - OPUS4-59556 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Goller, Sebastian M. A1 - Schartel, Bernhard A1 - Krüger, Simone T1 - Block it and rock it: Smoke suppressants that form a protective layer in PA 6.6 N2 - To ensure fire safety, polymers are filled with flame retardants and smoke suppressants. To meet the highest requirements, it is essential to understand the decomposition of those polymeric materials. This study reveals interactions between polymer, smoke suppressants, and flame retardants, and discusses their impact on the materials’ flame retardancy, smoke emission, smoke toxicity, and particle emission in conventional loadings to provide deeper general understanding. Low melting oxide glass, melem, spherical silica, sepiolite, melamine polyphosphate, and boehmite in an aluminum diethylphosphinate flame-retarded polyamide 6.6 were investigated. All smoke suppressants improve the protective layer and act as an adjuvant. Silica and melem performed best under forced flaming conditions. Spherical silica reduces the peak of heat release rate by 39% and the total heat evolved by 14%, whereas 10 wt% melem lowers the total smoke production by 41%. Melem alters the mode of action of aluminum diethylphosphinate from gas to more condensed phase activity. This change reduces flame inhibition and hence smoke toxicity, but further improves the protective layer due to charring reactions in the decomposition mechanism. In addition, the sizes of the smoke particles decrease because of the prolonged time in the pyrolytic zone. This study highlights that interactions between polymer, flame retardants, and smoke suppressants can significantly determine the smoking and burning behavior. KW - Smoke suppressant KW - Flame retardancy KW - Aluminum diethylphosphinate KW - Smoke KW - Polyamide 6.6 PY - 2024 DO - https://doi.org/10.1177/07349041231220250 SN - 0734-9041 VL - 42 IS - 2 SP - 117 EP - 141 PB - SAGE Publications AN - OPUS4-59533 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hupp, Vitus A1 - Schartel, Bernhard A1 - Flothmeier, K. A1 - Hartwig, A. T1 - Fire Behavior of Pressure-sensitive Adhesive Tapes and Bonded Materials N2 - Pressure-sensitive adhesive tapes are used in several industrial applications such as con-struction, railway vehicles and the automotive sector,where the burning behavior is ofcrucial importance. Flame retarded adhesivetapes are developed and provided, however,often without considering the interaction of adhesive tapes and the bonded materialsduring burning nor the contribution of the tapes to fire protection goal of the bondedcomponents in distinct fire tests. This publication delivers an empirical comprehensiveknowledge how adhesive tapes and their flame retardancy effect the burning behaviorof bonded materials. With a special focus on the interaction between the single compo-nents, one flame retarded tape and one tapewithout flame retardant are examined inscenarios of emerging and developing fires, along with their bonds with the commonmaterials wood, zinc-plated steel, mineral wool, polycarbonate, and polymethylmethacry-late. The flame retardant significantly improved the flame retardancy of the tape as afree-standing object and yielded a V-2 rating in UL 94 vertical test and raised the OxygenIndex by 5 vol.%. In bonds, or rather laminates, the investigations prove that the choiceof carrier and substrates are the factors with the greatest impact on the fire propertiesand can change the peak of heat release rate and the maximum average rate of heatemission up to 25%. This research yielded a good empirical overall understanding of thefire behavior of adhesive tapes and bonded materials. Thus, it serves as a guide for tapemanufacturers and applicants to develop tapes and bonds more substrate specific. KW - Adhesives KW - Cone calorimeter KW - Flame retardancy KW - Laminates KW - Phosphorus flame retardants KW - Pressure-sensitive adhesive KW - Tapes PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-593207 DO - https://doi.org/10.1002/fam.3171 SN - 0308-0501 SN - 1099-1018 VL - 48 IS - 1 SP - 114 EP - 127 PB - Wiley CY - New York, NY AN - OPUS4-59320 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schartel, Bernhard T1 - Flame Retardancy of Polymers - A Bunch of Thoughts N2 - Short overview is given of BAM's research within the topic "Flame Retardancy of Polymeric Materials". Fire science is identified as a crucial compentenc of BAM following our mission "Safety in Technology and Chemistry". In the area of polymers we work interdisciplinary, in the dimensions from nm to 2m, and we love to combine experiment and simulation. Multimethodical examples are given to describe the burning phenomena and flame-retardant modes of action. Further some examples are presented for tailored bench-scale fire testing and assessing concepts. Our goal is to provide the fundaments for a evidenced-based development of future materials. T2 - Klausurtagung Transregio 150 CY - Weinheim, Germany DA - 21.11.2023 KW - Flame retardants KW - Mode of action KW - Flame retardancy concepts KW - Flame inhibition KW - Protective layer KW - Charring KW - Dripping KW - Synergy PY - 2023 AN - OPUS4-58899 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Turski Silva Diniz, Analice A1 - Marti, J. M. A1 - Schartel, Bernhard T1 - High Heat Resistance Can Be Deceiving: Dripping Behavior of Polyamide 4.6 in Fire N2 - Polyamide 4.6 (PA46) is a high-heat-resistant polymer, but it has no dripping resistance under fire. Three commercial grades of PA46 are investigated under UL 94 vertical fire test conditions. Their performances are discussed based on the materials’ structural, thermal, and rheological properties. PA46 presents flaming drops, whereas dripping is prevented in the flame-retarded PA46. Friction-modified PA46 has increased flaming dripping. Temperature profiles of the specimens under fire and the temperature of the drops are measured by thermocouples. A UL 94 vertical test configuration consisting of two flame applications is designed to assess the quantitative dripping behavior of the set of materials by the particle finite element method (PFEM). Polymer properties (activation energy and Arrhenius coefficient of decomposition, char yield, density, effective heat of combustion, heat of decomposition, specific heat capacity, and thermal conductivity) in addition to rheological responses in high temperatures are estimated and measured as input parameters for the simulations. The dripping behavior obtained by simulated materials corresponds with the experimental results in terms of time and drop size. A consistent picture of the interplay of the different phenomena controlling dripping under fire appears to deliver a better understanding of the role of different materials’ properties KW - Dripping KW - UL 94 KW - PFEM KW - High heat resistance KW - Polyamide 4.6 KW - Flammability PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-586015 DO - https://doi.org/10.1002/mame.202300091 SN - 1439-2054 SN - 1438-7492 VL - 308 IS - 10 SP - 1 EP - 11 PB - Wiley-VCH AN - OPUS4-58601 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Schaumann, P. A1 - Hothan, Sascha A1 - Mund, M. A1 - Häßler, Dustin A1 - Schartel, Bernhard A1 - Daus, Lars-Hendrik T1 - Bewertung des Feuerwiderstandes von Stahlkonstruktionen mit reaktiven Brandschutzsystemen unter Berücksichtigung des Alterungsverhaltens N2 - Im Rahmen des Forschungsprojektes IGF 20470N wurden Untersuchungen zum Alterungsverhalten von reaktiven Brandschutzsystemen (RBS) auf Stahlbauteilen durchgeführt. Mithilfe der Ergebnisse einer umfangreichen Literaturrecherche sowie experimentellen und numerischen Untersuchungen sollte ein Vorschlag für ein Prüfkonzept zum Nachweis einer Nutzungsdauer von RBS von mehr als 10 Jahren auf Basis von Kurzzeitversuchen abgeleitet werden. Dabei setzt die Bewertung des Alterungsverhaltens von RBS voraus, dass die Mechanismen der Alterung hinreichend bekannt sind. Dafür wurden zunächst systematisch Daten von Kurz- und Langzeitversuchen von nationalen Zulassungsprüfungen der letzten Jahrzehnte ausgewertet. Anschließend wurden umfangreiche experimentelle Untersuchungen an einer wasserbasierten sowie einer epoxidharzbasierten Richtrezeptur durchgeführt. Da aus der Literatur bekannt ist, dass die Einflüsse der Bewitterung zu einer Veränderung der Konzentration der Bestandteile innerhalb der Beschichtung führen können, wurden Untersuchungen mit Mangelrezepturen durchgeführt, wobei systematisch einzelne Bestandteile reduziert wurden. Neben optischen Untersuchungen wurden thermoanalytische Verfahren (DSC-TG-, ATR-FTIR-, Elementar-, Farbanalyse) angewandt sowie Brandversuche an beschichteten Stahlplatten durchgeführt. Des Weiteren wurden die Richtrezepturen den beschleunigten Kurzzeitversuchen gemäß EAD 350402-00-1106 (2017) unterzogen, welche die Zulassung von Produkten auf europäischer Ebene regelt. Für die wasserbasierte Richtrezeptur wurden die Bewitterung für den feuchten Innenraum (Typ Z1) mehrfach wiederholt (1x, 3x, 6x). Für die epoxidharzbasierte Richtrezeptur entsprach die Bewitterung dem Zyklus für die Außenanwendung (Typ X). In Brandversuchen sowie thermoanalytischen und optischen Untersuchungen wurde das Alterungsverhalten sowie die thermische Schutzwirkung analysiert. Anschließend wurden numerische Simulationen von Stahlbauteilen mit gealterten RBS durchgeführt und anhand der experimentellen Untersuchungen validiert. Mithilfe der numerischen Modelle kann eine Bewertung der thermischen Schutzwirkung von Stahlbauteilen mit gealterten RBS vorgenommen werden. Mithilfe der gesammelten Erkenntnisse wurde ein Vorschlag für ein Prüfkonzept für den Nachweis einer Nutzungsdauer von mehr als 10 Jahren abgeleitet. Das Prüfkonzept besteht dabei aus einem Katalog von Möglichkeiten, die aktuellen Zulassungsprüfungen auf europäischer Ebene für eine Nutzungsdauer von 10 Jahren auf einen längeren Zeitraum zu erweitern. N2 - Within the scope of the research project IGF 20470N, investigations were carried out on the assessment of the aging behavior of intumescent coatings (ICs) for the fire protection of steel members. With the help of the results of an extensive literature research as well as experimental and numerical investigations, a proposal for a test concept for the proof of a service life of ICs of more than 10 years was to be derived on the basis of short-term tests. The evaluation of the aging behavior of ICs presupposes that the aging mechanisms are sufficiently known. For this purpose, data from short- and long-term tests of national approval tests of the last decades were first systematically evaluated. Subsequently, extensive experimental investigations were carried out on a water-based and epoxy resin-based model formulation. Since it is known from the literature that the effects of weathering may lead to a change in the concentrations of the constituents within the coating, investigations were carried out with formulations of the ICs in which individual constituents were systematically reduced. In addition to optical investigations, thermoanalytical methods (DSC-TG-, ATR-FTIR-, elemental-, color analysis) were used and fire tests were carried out on coated steel plates. Furthermore, the model formulations were subjected to the accelerated short-term tests of EAD 350402-00-1106 (2017), which regulates the approval of products at the European level. For the water-based model formulation, the weathering for the interior application with a high moisture content (type Z1) was repeated several times (1x, 3x, 6x). For the epoxy resin-based model formulation, the weathering corresponded to the cycle for exterior application (type X). Fire tests as well as thermoanalytical and optical investigations were carried out to analyze the aging behavior and the thermal protection performance. Subsequently, numerical simulations of steel members with aged ICs were carried out and validated on the basis of the experimental investigations. With the help of the numerical models, an evaluation of the thermal protection performance of steel members with aged ICs can be carried out. Bases on the findings, a proposal for a test concept for the verification of a service life of more than 10 years was derived. The test concept consists of a catalogue of possibilities for extending the current approval tests at European level for a service life of 10 years to a longer period. KW - Brandschutz KW - Dauerhaftigkeit KW - Alterung KW - Reaktive Brandschutzsysteme KW - Brandversuche PY - 2022 UR - https://dast.deutscherstahlbau.de/veroeffentlichungen/forschungsberichte SP - 1 EP - 367 PB - Stahlbau Verlags- und Service GmbH CY - Düsseldorf AN - OPUS4-57257 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -