TY - JOUR A1 - Lorenzetti, A. A1 - Besco, S. A1 - Hrelja, D. A1 - Roso, M. A1 - Gallo, Emanuela A1 - Schartel, Bernhard A1 - Modesti, M. T1 - Phosphinates and layered silicates in charring polymers: The flame retardancy action in polyurethane foams N2 - Nanocomposites of a charring polymer (like polyurethane foam) filled with aluminum phosphinate (AlPi) with or without melamine cyanurate (MelCy) have been prepared by microwave processing and their thermal stability and fire behavior have been studied. Results on the interaction between flame retardants and layered silicates were provided as well as detailed investigation of the char strength, which has been carried out using a suitably developed method based on dynamic-mechanic analysis. Generally, the thermo-oxidative stability in presence of layered silicates was higher than the counterparts even if an additive rather than synergic effect took place; however, in some cases the interaction between clays and phosphinate led to a significant decrease of weight residue. In nitrogen the residue amounts were about the same but a higher amount of phosphorus was retained in the solid phase in presence of clays. Cone calorimeter results showed that the use of phosphinates led to a decrease of the PHRR; further addition of clays did not reduce the PHRR owing to the worse quality of char layer as demonstrated by the char strength test. However, it has been shown that the partial substitution of aluminum phosphinate with melamine cyanurate gave improved results: the AlPi–MelCy filled foams showed similar pHRR and THE but lower TSR and higher char strength than AlPi filled foams. It was also confirmed that phosphinate acted by flame inhibition but its action was depressed by the use of nanoclays owing to their interaction. KW - Phosphinate KW - Nanocomposite KW - Polyurethane KW - Interaction KW - Flame retardant PY - 2013 DO - https://doi.org/10.1016/j.polymdegradstab.2013.08.002 SN - 0141-3910 SN - 1873-2321 VL - 98 IS - 11 SP - 2366 EP - 2374 PB - Applied Science Publ. CY - London AN - OPUS4-29281 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Dittrich, Bettina A1 - Wartig, K.-A. A1 - Hofmann, D. A1 - Mülhaupt, R. A1 - Schartel, Bernhard T1 - Carbon black, multiwall carbon nanotubes, expanded graphite and functionalized graphene flame retarded polypropylene nanocomposites N2 - Herein, we examine the influence of adding functionalized graphene (FG), distinct expanded graphites and carbon nanofillers such as carbon black and multiwall carbon nanotubes on mechanical properties, morphology, pyrolysis, response to small flame and burning behavior of a V-2 classified flame-retarded polypropylene (PP). Among carbon fillers, FG and multilayer graphene (MLG) containing fewer than 10 layers are very effectively dispersed during twin-screw extrusion and account for enhanced matrix reinforcement. In contrast to the other fillers, no large agglomerates are detected for PP-FR/FG and PP-FR/MLG, as verified by electron microscopy. Adding FG to flame-retardant PP prevents dripping due to reduced flow at low shear rates and shifts the onset of thermal decomposition to temperatures 40°C higher. The increase in the onset temperature correlates with the increasing specific surface areas (BET) of the layered carbon fillers. The reduction of the peak heat release rate by 76% is attributed to the formation of effective protection layers during combustion. The addition of layered carbon nanoparticles lowers the time to ignition. The presence of carbon does not change the composition of the evolved pyrolysis gases, as determined by thermogravimetric analysis combined with online Fourier-transformed infrared measurements. FG and well-exfoliated MLG are superior additives with respect to spherical and tubular carbon nanomaterials. KW - Graphene KW - Flame retardancy KW - Nanocomposites KW - Polypropylene KW - Carbon nanoparticles PY - 2013 DO - https://doi.org/10.1002/pat.3165 SN - 1042-7147 SN - 1099-1581 VL - 24 IS - 10 SP - 916 EP - 926 PB - John Wiley & Sons, Ltd. CY - Chichester AN - OPUS4-29337 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schartel, Bernhard A1 - Perret, Birgit A1 - Dittrich, Bettina A1 - Ciesielski, M. A1 - Krämer, J. A1 - Müller, P. A1 - Altstädt, V. A1 - Zang, L. A1 - Döring, M. T1 - Flame retardancy of polymers: the role of specific reactions in the condensed phase N2 - Condensed-phase mechanisms play a major role in fire-retardant polymers. Generations of development have followed the concept of charring to improve fire properties. Whereas the principal reactions are believed to be known, the specific description for multicomponent systems is lacking, as is the picture across different systems. A two-step approach is proposed in general, and also presented in greater detail. The second step covers the specific reactions controlling charring, whereas the actual reactants are provided in the preceding step. This model consistently incorporates the variety of structure–property relationships reported. A comprehensive case study is presented on seven phosphorus flame retardants in two epoxy resins to breathe life into the two-step approach. KW - Charring KW - Epoxy KW - Flame retardancy KW - Pyrolysis KW - Thermogravimetric analysis (TGA) PY - 2016 DO - https://doi.org/10.1002/mame.201500250 SN - 1438-7492 SN - 1439-2054 VL - 301 IS - 1 SP - 9 EP - 35 PB - Wiley-VCH Verl. CY - Weinheim AN - OPUS4-35273 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pappalardo, Salvatore A1 - Russo, Pietro A1 - Acierno, Domenico A1 - Rabe, Sebastian A1 - Schartel, Bernhard T1 - The synergistic effect of organically modified sepiolite in intumescent flame retardant polypropylene N2 - The pyrolysis, flammability and fire behavior of polypropylene (PP) containing an intumescent flame retardant and sepiolite nanoparticles were investigated by performing thermogravimetry, oxygen index (LOI), UL-94, and cone calorimeter tests. The combination of 0.5 wt% of premodified sepiolite (OSEP) with 12 wt% of a commercial intumescent flame retardant showed a clear synergy in LOI, UL-94 ranking and peak heat release rate. The ternary formulation achieved a V-0 classification and, consequently, allowed a reduction in the amount of flame retardant necessary to achieve this result. Whereas OSEP and pristine sepiolite nanoparticles (SEP) affect the performance in PP nanocomposites quite similarly, OSEP outperformed SEP in the combination with intumescent flame retardant. The cone calorimeter results and dynamic rheological measurements confirmed the synergistic effect between the nanofiller and the flame retardant resulting from the improved properties of the residual protective layer. KW - Polypropylene KW - Intumescent flame retardant KW - Sepiolite KW - Cone calorimetry KW - Low oxygen index PY - 2016 DO - https://doi.org/10.1016/j.eurpolymj.2016.01.041 SN - 0014-3057 VL - 76 SP - 196 EP - 207 PB - Elsevier AN - OPUS4-35854 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Patrick A1 - Schartel, Bernhard T1 - Melamine poly(metal phosphates) as flame retardant in epoxy resin: Performance, modes of action, and synergy N2 - Melamine poly(metal phosphates) (MPMeP) are halogen-free flame retardants commercialized under the brand Name Safire. Melamine poly(aluminum phosphate) (MPAlP), melamine poly(zinc phosphate) (MPZnP), and melamine poly(Magnesium phosphate) (MPMgP) were compared in an epoxy resin (EP). The thermal decomposition, flammability, burning behavior, and glass transition temperature were investigated using thermogravimetric analysis, pyrolysis combustion flow calorimeter, UL 94 testing, cone calorimeter, and differential scanning calorimetry. While the materials exhibited similarities in their pyrolysis, EP+MPZnP and EP+MPMgP showed better fire behavior than EP+MPAlP due to superior protective properties of the fire residues. Maintaining the 20 wt % loading, MPZnP was combined with various other flame retardants. A synergistic effect was evident for melamine polyphosphate (MPP), boehmite, and a derivative of 6H-Dibenzo[c,e][1,2]oxaphosphinine-6-oxide. The best overall performance was observed for EP+(MPZnP+MPP) because of the best protection effectiveness of the fire residue. EP +(MPZnP+MPP) achieved V1/V0 in UL 94, and an 80% reduction in the peak heat release rate. This study evaluates the efficiency of MPMeP in EP, alone and in combination with other flame retardants. MPMeP is a suitable flame retardant for epoxy resin, depending on its kind and synergists. KW - flame retardance KW - thermogravimetric analysis KW - thermosets PY - 2016 DO - https://doi.org/10.1002/APP.43549 SN - 0021-8995 SN - 1097-4628 VL - 133 IS - 24 SP - 43549 PB - Wiley AN - OPUS4-35855 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hörold, Andreas A1 - Schartel, Bernhard A1 - Trappe, Volker A1 - Gettwert, V. A1 - Korzen, Manfred T1 - Protecting the structural integrity of composites in fire: Intumescent coatings in the intermediate scale N2 - The fire behaviour of light-weight material used in structural applications is regarded as the main challenge to be solved for mass transportation. The task is to perform realistic experiments, including a mechanical test scenario under fully developed fires, to improve the material's reliability in structural applications. Our approach utilises an intermediate-scale test set-up (specimen size 500 × 500 mm) to apply realistic compressive loads and fully developed fires directly to one side of a carbon-fibre-reinforced sandwich composite. Three different intumescent coatings were applied to sandwich structures and compared to a bench-scale study. The results emphasise intumescent coatings as a promising method to sustain fire resistance, multiplying the time to failure. Nevertheless, the realistic intermediate-scale test using severe direct flame application underlines the extremely short failure times when the actual composite components are tested without any additional insulation. KW - Carbon-fibre-reinforced KW - Fire stability KW - High-temperature properties KW - Mechanical testing KW - Fully developed fire KW - Post-crash scenario PY - 2015 DO - https://doi.org/10.1177/0731684415609791 SN - 0731-6844 SN - 1530-7964 VL - 34 IS - 24 SP - 2029 EP - 2044 PB - Technomic Publ. Co. CY - Westport, Conn. AN - OPUS4-35120 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wilke, Antje A1 - Langfeld, Kirsten A1 - Ulmer, B. A1 - Andrievici, V. A1 - Hörold, Andreas A1 - Limbach, P. A1 - Bastian, Martin A1 - Schartel, Bernhard T1 - Halogen-free Multicomponent Flame Retardant Thermoplastic Styrene-Ethylene-Butylene-Styrene Elastomers Based on Ammonium Polyphosphate – Expandable Graphite Synergy N2 - Developing flame retarded thermoplastic elastomers (TPES) based on styrene−ethylene−butylene−styrene, polypropylene, and mineral oil is a challenging task because of their very high fire loads and flammability. A promising approach is the synergistic combination of expandable graphite (EG) and ammonium polyphosphate (APP). Cone calorimetry, oxygen index, and UL 94 classification were applied. The optimal EG:APP ratio is 3:1, due to the most effective fire residue morphology. Exchanging APP with melamine-coated APPm yielded crucial improvement in fire properties, whereas replacing EG/APP with melamine polyphosphate did not. Adjuvants, such as aluminum diethyl phosphinate (AlPi), zinc borate, melamine cyanurate, titanium dioxide, dipentaerylthritol, diphenyl-2-ethyl phosphate, boehmite, SiO2, chalk, and talcum, were tested. All flame retardants reinforced the TPE-S. The combination with AlPi is proposed, because with 30 wt % flame retardants a maximum averaged rate of heat emission below 200 kW m−2 and a V-0 rating was achieved. Multicomponent EG/APP/adjuvants systems are proposed as a suitable route to achieve efficient halogen-free flame retarded TPE-S. KW - Thermoplastic elastomers KW - Amonium polyphosphate KW - Expandable graphite KW - Synergy PY - 2017 DO - https://doi.org/10.1021/acs.iecr.7b01177 SN - 0888-5885 VL - 56 IS - 29 SP - 8251 EP - 8263 PB - ACS Publications AN - OPUS4-41509 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Watolla, Marie-Bernadette A1 - Gluth, Gregor A1 - Sturm, Patrick A1 - Rickard, W.D.A. A1 - Krüger, Simone A1 - Schartel, Bernhard T1 - Intumescent geopolymer-bound coatings for fire protection of steel N2 - The passive fire protection of steel structures and other load-bearing components will continue to gain importance in future years. In the present contribution, novel intumescent aluminosilicate (geopolymer-bound) composites are proposed as fire-protective coatings on steel. Steel plates coated with these materials were exposed to the standard temperature-time curve as defined in ISO 834 – 1:1999. The coatings partially foamed during curing and expanded further during thermal exposure, demonstrating their intumescent characteristic.Thermogravimetryandoscillatory rheometry determined that the intumescent behavior is attributed to a transition to a viscous state (loss factor > 1) in the temperature range of major water release, differing from conventional geopolymers. XRD and SEM images showed that the coatings had characteristics of ceramic or glass-ceramic foams after fire resistance testing, suggesting superior performance under challenging conditions. The thickness of the coatings influenced their foaming and intumescent behavior and thus the time for the coated steel plates to reach 500 °C. A number of additives were also studied with the best performance obtained from samples containing sodium tetraborate.Acoating of just 6mmwas able to delay the time it takes for a steel substrate to reach 500 °C to more than 30 minutes. KW - Geopolymers KW - Fire protection KW - Intumescence KW - Coatings KW - Fire resistance PY - 2017 UR - https://www.ceramic-science.com/articles/all-articles.html?article_id=100558 DO - https://doi.org/10.4416/JCST2017-00035 VL - 8 IS - 3 (Topical issue: Geopolymers) SP - 351 EP - 364 PB - Göller Verlag CY - Baden-Baden AN - OPUS4-42139 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Deng, C. A1 - Yin, Huajie A1 - Li, R.-M. A1 - Huang, S.-C. A1 - Schartel, Bernhard A1 - Wang, Y.-Z. T1 - Modes of action of a mono-component intumescent flame retardant MAPP in polyethylene-octene elastomer N2 - A mono-component intumescent flame retardant named ethylenediamine-modified ammonium polyphosphate (MAPP) is used in polyethylene-octene elastomer (POE). Insight into the flame-retardant mechanisms of the MAPP is provided from a new perspective. The fire performance of POE/MAPP composites is investigated by oxygen index (OI) and vertical burning (UL-94) tests. POE Composite containing 35 wt% MAPP achieves a V-0 rating, and its OI is 29.3 vol%. The thermogravimetric Analysis (TGA) and Fourier transform infrared spectra (FTIR) confirm that the incorporation of ethylenediamine changes the thermal decomposition of APP, mainly resulting in the formation of char layer with a thermally stable structure. Cone calorimeter analysis revealed the flame-retardant modes of action of MAPP in POE under forced-flaming conditions. Quantitative analysis illustrates that both the residue due to charring and the fuel dilution/flame Inhibition resulting from the release of incombustible products/ phosphorus species decrease the total heat release (fire load) by 20e28%. The residue increases linearly with increasing MAPP content, whereas the reduction in effective heat of combustion levels off. Moreover, the flame-retardant effect resulting from the protective properties of the char is discovered to be the dominant mode of action (up to 85% reduction) with respect to the peak heat release rate, leading to the excellent flame retardancy of POE/MAPP. KW - Ammonium polyphosphate KW - Flame retardant KW - Carbonization KW - Elastomer PY - 2017 DO - https://doi.org/10.1016/j.polymdegradstab.2017.03.006 SN - 0141-3910 SN - 1873-2321 VL - 138 SP - 142 EP - 150 PB - Elsevier AN - OPUS4-39901 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schartel, Bernhard A1 - Wilkie, Charles A. A1 - Camino, G. T1 - Recommendations on the scientific approach to polymer flame retardancy: Part 2 - concepts N2 - The usage of concepts in scientific communication is critical to our ability to inform the reader about work that has been performed. The significance and thus the quality of scientific discussion rely on the precise use of concepts. In this second part of a two-part paper, concerning the scientific basis of polymer fire retardancy, the proper use of concepts is addressed. Distinct concepts in flame retardancy are discussed, such as fire residue, the correlation of fire performance with char yield according to van Krevelen, catalysis, and wicking. Synergy is discussed in detail, as well as approaches to quantify it, due to its importance for flame retardant polymers. The preceding first paper (part 1) discussed the proper use of scientific terms, thermal analysis, and fire testing. Thus, together these two papers support the community by offering recommendations and addressing some of the most relevant points. They encourage to review scientific practice in the field of flame retardancy of polymers. KW - Char KW - Synergism KW - Flame retardancy KW - Flammability KW - Fire growth indices KW - Synergy index PY - 2017 DO - https://doi.org/10.1177/0734904116675370 SN - 0734-9041 SN - 1530-8049 VL - 35 IS - 1 SP - 3 EP - 20 PB - Sage AN - OPUS4-39084 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gallo, Emanuela A1 - Stöcklein, Waldemar A1 - Klack, Patrick A1 - Schartel, Bernhard T1 - Assessing the reaction to fire of cables by a new bench-scale method N2 - The recently approved EU Construction Products Regulation (CPR) applies to cables as construction products. The difficulty of predicting the fire performance of cables with respect to propagation of flame and contribution to fire hazards is well known. The new standard EN 50399 describes a full-scale test method for the classification of vertically mounted bunched cables according to CPR. Consideration of the material, time, and thus cost requires an alternative bench-scale fire test, which finds strong demand for Screening and development purposes. The development of such a bench-scale fire test to assess the fire Performance of multiple vertically mounted cables is described. A practical module for the cone calorimeter is proposed, simulating the fire scenario of the EN 50399 on the bench scale. The efficacy of this module in predicting full-scale CPR test results is shown for a set of 20 different optical cables. Key properties such as peak heat release rate (PHRR), fire growth rate (FIGRA), and flame spread are linked to each other by factors of around 5. In a case study, the bench-scale test designed was used to investigate the influence of the main components on the fire behaviour of a complex optical cable. KW - Optical cables KW - Construction products regulation KW - Bench-scale fire testing KW - Reaction to fire KW - Cone calorimeter PY - 2017 DO - https://doi.org/10.1002/fam.2417 SN - 0308-0501 SN - 1099-1018 VL - 41 IS - 6 SP - 768 EP - 778 PB - Wiley AN - OPUS4-42092 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rabe, Sebastian A1 - Schartel, Bernhard T1 - The rapid mass calorimeter: Understanding reduced-scale fire test results N2 - The effects of reducing specimen size on the fire behavior of polymeric materials were investigated by means of the rapid mass calorimeter, a high-throughput Screening instrument. Results from the rapid mass calorimeter were compared with those from the cone calorimeter. Correlation coefficients between the different measures of each method and between the two methods are discussed to elucidate the differences and similarities in the two methods. Materials with characteristic heat release rate (HRR) curves in the cone calorimeter were evaluated in detail. The rapid mass calorimeter produces valuable and interpretable results with HRR curve characteristics similar to cone calorimeter results. Compared to cone calorimeter measurements, material savings of 96% are achieved, while maintaining the Advantages of a macroscopic fire test. KW - Rapid mass calorimeter KW - High throughput KW - Cone calorimeter KW - Flame retardancy PY - 2017 DO - https://doi.org/10.1016/j.polymertesting.2016.11.027 SN - 0142-9418 VL - 57 SP - 165 EP - 174 PB - Elsevier AN - OPUS4-38739 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gómez-Fernández, S. A1 - Günther, Martin A1 - Schartel, Bernhard A1 - Corcuera, M. A. A1 - Eceiza, A. T1 - Impact of the combined use of layered double hydroxides, lignin and phosphorous polyol on the fire behavior of flexible polyurethane foams N2 - Flexible polyurethane foams with densities of 40 ± 2 kg m−3 were prepared by combining different ecofriendly fillers such as layered double hydroxides (LDH) and kraft lignin (a byproduct of the pulp and paper industry) with a phosphorous polyol (E560) in order to study their effect on the mechanical performance and fire behavior of the foams. Two series of foams were prepared, some containing lignin or LDH separately, and some with a combination of both: one of the series was prepared without E560 (0E foam series) and the other with 5 parts per hundred of E560 polyol (5E series). The use of fillers resulted in increased viscosity of the reactive mixture, requiring higher blowing agent content in order to hold the density of the foams constant. It was observed that urea phase segregation was favored in the series of 0E foams due to their lower viscosity than the 5E series. This had consequent effects on the resilience, compression force deflection and compression set of these foams. In terms of fire behavior it was observed that while the limiting oxygen index decreased, cone calorimeter results showed that the combination of lignin, LDH and E560 decreased the heat release of the foams. In addition, the combination of fillers and E560 contributed to increase the viscosity of the pyrolysis products, preventing the dripping of the molten polymer, which is a key factor in flame propagation towards adjacent objects in fire scenarios. KW - Ligning KW - Foam KW - Flexible polyurethane foam KW - Flame retardant PY - 2018 SN - 0926-6690 VL - 125 SP - 346 EP - 359 PB - Elsevier B.V. AN - OPUS4-45971 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schartel, Bernhard A1 - Günther, Martin T1 - Flame retardancy of polyurethanes N2 - Polyurethanes (PU) represent one of the most versatile classes of plastics. They are processed and used as thermoplastic, elastomer, and thermoset. The requirements regarding flammability are correspondingly versatile. Depending on the material and the field of application, specific fire tests have to be fulfilled. This paper describes the different concepts used to fulfil these requirements by choosing the right raw materials and flame retardants. KW - Polyurethane KW - Flame retardant KW - Foam KW - Flammability KW - Pyrolysis KW - Cone calorimeter PY - 2020 VL - 17 IS - 1 SP - 44 EP - 48 PB - Dr. Gupta AN - OPUS4-50737 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Goller, Sebastian M. A1 - Krüger, Simone A1 - Schartel, Bernhard T1 - No business as usual: The effect of smoke suppressants commonly used in the flame retardant PA6.6 on smoke and fire properties N2 - As most of polymeric materials are inherently flammable, flame retardants (FR) are commonly used to reduce their fire risks. Nevertheless, these flame retardant materials are often detrimental to smoke parameters like specific optical density or smoke toxicity. The influence of several smoke suppressants (SP)-zinc stannate, zinc phosphate, titanium oxide and hydrotalcite-were investigated with respect to flame retardancy, smoke emission, particle emission and smoke toxicity in a diethyl aluminum phosphinate (AlPi) flame retardant polyamide 6.6 (PA6.6). It was shown that the interaction between SP, FR and polymer is crucial for smoke and fire properties and can change the mode of action of the FR as well the decomposition mechanism of the polymer. Small amounts of SP show less effect on forced flaming behavior and the optical density, but they can influence flammability and the particle size distribution of the soot particles. The flame retardancy was significantly enhanced by 5 wt.-% zinc stannate in PA6.6 under forced flaming conditions. The charring mechanism was improved, and the mode of action of AlPi switched from the gas to the condensed phase. This resulted of in a reduced PHRR and TSP and an increase in residue yield. The smoke toxicity and optical density were reduced in the smoke density chamber as well. The smoke particles shifted to smaller sizes as the time in the pyrolytic zone increased. The formation of a dense char is assumed to be the key factor to enhance smoke suppression and flame retardancy properties. KW - Polyamide 6.6 KW - Smoke suppression KW - Flame retardancy KW - Zinc stannate KW - Smoke density PY - 2023 DO - https://doi.org/10.1016/j.polymdegradstab.2023.110276 SN - 0141-3910 VL - 209 PB - Elsevier Ltd. AN - OPUS4-56981 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schartel, Bernhard A1 - Beck, Uwe A1 - Bahr, Horst A1 - Hertwig, Andreas A1 - Knoll, Uta A1 - Weise, Matthias T1 - Sub-micrometre coatings as an infrared mirror: a new route to flame retardancy N2 - Most of the polymeric materials used are easy to ignite and show extensive flame spread along their surfaces. Apart from extensive heat release rates, their short time to ignition (tig), in particular, is a key fire hazard. Preventing ignition eliminates fire hazards completely. Protection layers that shift tig by more than an order of magnitude are powerful flame retardancy approaches presenting an alternative to the usual flame retardancy concepts. Coatings are proposed that consist of a three-layer system to ensure adhesion to the substrate, acting as an infrared (IR) mirror and protecting against oxidation. The IR-mirror layer stack is realised by physical vapour deposition in the sub-micrometre (<1 µm) range, reducing heat absorption by up to an order of magnitude. Not only is the ease of ignition diminished (tig is increased by several minutes), the flame spread and fire growth indices are also remarkably reduced to as little as 1/10 of the values of the uncoated polymers open for further optimization. Sub-micrometre thin IR-mirror coatings yielding surface absorptivity <0.1 are proposed as a novel and innovative flame retardancy approach. KW - Coating KW - Fire protection KW - Physical vapour deposition (PVD) KW - IR mirror KW - Ignition PY - 2012 DO - https://doi.org/10.1002/fam.1122 SN - 0308-0501 SN - 1099-1018 VL - 36 IS - 8 SP - 671 EP - 677 PB - Heyden CY - London AN - OPUS4-27210 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kempel, Florian A1 - Schartel, Bernhard A1 - Marti, J.M. A1 - Butler, K.M. A1 - Rossi, R. A1 - Idelsohn, S.R. A1 - Onate, E. A1 - Hofmann-Böllinghaus, Anja T1 - Modelling the vertical UL 94 test: competition and collaboration between melt dripping, gasification and combustion N2 - An experimental and numerical investigation of the effect of bisphenol A bis(diphenyl phosphate) (BDP) and polytetrafluoroethylene (PTFE) on the fire behaviour of bisphenol A polycarbonate/acrylonitrile butadiene styrene (PC/ABS) in the vertical UL 94 scenario is presented. Four PC/ABS blends were discussed, which satisfy different UL 94 classifications due to the competing effects of gasification, charring, flame inhibition and melt flow/dripping. For numerical investigation, the particle finite element method (PFEM) is used. Its capability to model the complex fire behaviour of polymers in the UL 94 is analysed. The materials' properties are characterised, in particular the additives impact on the dripping behaviour during thermal exposure. BDP is an efficient plasticiser; adding PTFE prevents dripping by causing a flow limit. PFEM simulations reproduce the dripping and burning behaviour, in particular the competition between gasification and dripping. The thermal impact of both the burner and the flame is approximated taking into account flame inhibition, charring and effective heat of combustion. PFEM is a promising numerical tool for the investigation of the fire behaviour of polymers, particularly when large deformations are involved. Not only the principal phenomena but also the different UL 94 classifications and the extinction times are well predicted. KW - Melt dripping KW - UL 94 KW - Particle finite element method (PFEM) KW - Simulation KW - Bisphenol A polycarbonate/acrylonitrile butadiene styrene (PC/ABS) KW - Polytetrafluoroethylene (PTFE) KW - Bisphenol A bis(diphenyl phosphate) (BDP) PY - 2015 DO - https://doi.org/10.1002/fam.2257 SN - 0308-0501 SN - 1099-1018 VL - 39 IS - 6 SP - 570 EP - 584 PB - Heyden CY - London AN - OPUS4-34285 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kempel, Florian A1 - Schartel, Bernhard A1 - Linteris, G.T. A1 - Stoliarov, S.I. A1 - Lyon, R.E. A1 - Walters, R.N. A1 - Hofmann-Böllinghaus, Anja T1 - Prediction of the mass loss rate of polymer materials: Impact of residue formation N2 - Two different numerical simulation tools, Fire Dynamic Simulator (FDS) and ThermaKin, are investigated with respect to their capability to predict the mass loss rate of polymer materials exposed to different fires. For validation, gasification apparatus and cone calorimeter tests are conducted. The main focus is on the influence of residue formation. Therefore, poly (butylene terephthalate) (PBT) and PBT reinforced with glass fibres (PBT-GF) are investigated and compared. PBT decomposes almost completely, while PBT-GF forms residue. The materials are characterised in order to provide suitable input parameters. Additionally the total incident heat flux to the sample is measured. With accurate input parameters, FDS and ThermaKin predicted the pyrolysis behaviour of PBT very well. Only some limitations are identified regarding the residue-forming PBT-GF. Both numerical simulation tools demonstrate a high value regarding the assessment of parameters' relative impacts and thus the evaluation of optimisation routes in polymer and composite development. KW - Polymer KW - Pyrolysis simulation KW - Residue formation KW - Fire dynamics simulator (FDS) KW - ThermKin PY - 2012 DO - https://doi.org/10.1016/j.combustflame.2012.03.012 SN - 0010-2180 SN - 1556-2921 VL - 159 IS - 9 SP - 2974 EP - 2984 PB - Elsevier CY - New York, NY AN - OPUS4-26382 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Braun, Ulrike A1 - Bahr, Horst A1 - Sturm, Heinz A1 - Schartel, Bernhard T1 - Flame retardancy mechanisms of metal phosphinates and metal phosphinates in combination with melamine cyanurate in glass-fiber reinforced poly(1,4-butylene terephthalate): the influence of metal cation N2 - The pyrolysis and fire behavior of glass-fiber reinforced poly(butylene terephthalate) (PBT/GF) with two different metal phosphinates as flame retardants in combination with and without melamine cyanurate (MC) were analyzed by means of thermogravimetry, thermogravimetry coupled with infrared spectroscopy, flammability, and cone calorimeter tests as well as scanning electron microscopy/energy dispersive X-ray spectroscopy and X-ray fluorescence spectroscopy. In PBT/GF, dosages of 13-20% of the halogen-free flame retardant aluminum phosphinate or aluminum phosphinate in combination with MC fulfill the requirements for electrical engineering and electronics applications (UL 94 = V-0; LOI > 42%), whereas the use of the same amount of zinc phosphinate or zinc phosphinate in combination with MC does not improve the fire behavior satisfactorily (UL 94 = HB; LOI = 27-28%). The performance under forced flaming conditions (cone calorimeter) is quite similar for both of the metal phosphinates. The use of aluminum and zinc salts results in similar flame inhibition predominantly due to the release of the phosphinate compounds in the gas phase. Both metal phosphinates and MC interact with the polymer changing the decomposition characteristics. However, part of the zinc phosphinate vaporizes as a complete molecule. Because of the different decomposition behavior of the metal salts, only the aluminum phosphinate results in a small amount of thermally stable carbonaceous char. In particular, the aluminum phosphinate-terephthalate formed is more stable than the zinc phosphinate-terephthalate. The small amount of char has a crucial effect on the thermal properties and mechanical stability of the residue and thus the flammability. KW - Flame retardance KW - Polyester KW - Phosphinates KW - Pyrolysis KW - Cone calorimeter PY - 2008 DO - https://doi.org/10.1002/pat.1147 SN - 1042-7147 SN - 1099-1581 VL - 19 IS - 6 SP - 680 EP - 692 PB - John Wiley & Sons, Ltd. CY - Chichester AN - OPUS4-17620 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hörold, Andreas A1 - Schartel, Bernhard A1 - Trappe, Volker A1 - Korzen, Manfred A1 - Bünker, J. T1 - Fire stability of glass-fibre sandwich panels: The influence of core materials and flame retardants N2 - Fire resistance has become a key property for structural lightweight sandwich components in aviation, shipping, railway vehicles, and construction. The development of future composite materials and components demands adequate test procedures for simultaneous application of compression and fully developed fire. Therefore an intermediate-scale approach (specimen size = 500 mm x 500 mm) is applied with compressive loads (up to 1 MN) and direct application of a burner to one side of the specimens, as established in aviation for severe burn-through tests. The influence of different core structures (polyvinylchloride foam, polyisocyanorate foam reinforced by stitched glass bridges, and balsa wood) was investigated for glass-fibre-reinforced sandwich specimens with and without flame retardants applied on the fabrics, in the matrix, and on surface for each specimen at the same time. Times to failure were increased up to a factor of 4. The intumescent coating prolongs the time to failure significantly. What is more, using the intrinsic potential of the front skin together with the core to protect a load bearing back skin in sandwich panels, the design of the core – here using the wood core – is the most promising approach. KW - Fire resistance KW - Fire stability KW - Glass-fibre-reinforced plastics KW - Composite KW - Core materials PY - 2017 DO - https://doi.org/10.1016/j.compstruct.2016.11.027 SN - 0263-8223 SN - 1879-1085 VL - 160 SP - 1310 EP - 1318 PB - Elsevier AN - OPUS4-38622 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -