TY - JOUR A1 - Purohit, Purv A1 - Wang, D.-Y. A1 - Wurm, Andreas A1 - Schick, C. A1 - Schönhals, Andreas T1 - Comparison of thermal and dielectric spectroscopy for nanocomposites based on polypropylene and layered double hydroxide - proof of interfaces N2 - Polymer based nanocomposites by melt blending of synthesized ZnAl-Layered Double Hydroxide (ZnAl-LDH) and polypropylene (PP) were investigated by temperature modulated differential scanning calorimetry (TMDSC). The LDH was organically modified by using a surfactant, sodium dodecylbenzene sulfonate (SDBS) to increase the interlayer spacing of the LDH, so that polymer segments can intercalate the inter layer galleries. The glass transition temperature (Tg) and the thermal relaxation strength (Δcp) were determined. The Tg remains constant for concentration till 12 wt% of LDH and a slight reduction of 3 K might be observed for 16 wt% LDH but within the experimental error. The thermal relaxation strength decreases indicating reduction in the amount of mobile polymer segments from amorphous fraction. This finding is supported by the increase in the rigid amorphous fraction (RAF) which is attributed to the polymer molecules which are in close proximity to the crystals and the LDH sheets, as they hinder their mobility. This is analyzed in detail and related to the dielectric relaxation spectroscopy (BDS) results. KW - Polypropylene KW - Layered double hydroxide KW - Nanocomposites KW - Temperature modulated differential scanning calorimetery KW - Dielectric spectroscopy KW - Rigid amorphous fraction PY - 2014 DO - https://doi.org/10.1016/j.eurpolymj.2014.03.005 SN - 0014-3057 SN - 1873-1945 VL - 55 SP - 48 EP - 56 PB - Elsevier CY - Oxford AN - OPUS4-30626 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schönhals, Andreas T1 - Nano-sized Relaxation Spectroscopy of Miscible PVME/PS Blend Thin Films N2 - The moleculat dynamics of ultra thin films of polystyrene/poly(vinyl methyl ether) blends as revealed by nanosized specific heat and dielectric spectroscopy is discussed. T2 - Viscous liquids and the glass transition XV CY - Søminestationen, Holbæk, Denmark DA - 21.06.2018 KW - Thin polymeric films KW - Dielectric spectroscopy KW - Specific heat spectroscopx PY - 2018 AN - OPUS4-45280 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schönhals, Andreas T1 - Glass transition of thin polymeric films as revealed by calorimetric and dielectric techniques N2 - The structure and dynamics of thin polymeric films is reviewed and discussed in the frame work of novel theoretical approaches T2 - Lähnwitzseminar on Calorimetry CY - Rostock-Warnemünde, Germany DA - 03.06.2018 KW - Thin polymeric films KW - Dielectric spectroscopy KW - Thermal süectroscopy PY - 2018 AN - OPUS4-45164 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yin, Huajie A1 - Dittrich, Bettina A1 - Farooq, Muhammad A1 - Kerling, S. A1 - Wartig, K.-A. A1 - Hofmann, D. A1 - Huth, Christian A1 - Okolieocha, C. A1 - Altstädt, V. A1 - Schönhals, Andreas A1 - Schartel, Bernhard T1 - Carbon-based nanofillers/poly(butylene terephthalate): thermal, dielectric, electrical and rheological properties N2 - The influence of distinct carbon based nanofillers: expanded graphite (EG), conducting carbon black (CB), thermally reduced graphene oxide (TRGO) and multi-walled carbon nanotubes (CNT) on the thermal, dielectric, electrical and rheological properties of polybutylene terephthalate (PBT) was examined. The glass transition temperature (Tg) of PBT nanocomposites is independent of the filler type and content. The carbon particles act as nucleation agents and significantly affect the melting temperature (Tm), the crystallization temperature (Tc) and the degree of crystallinity of PBT composites. PBT composites with EG show insulating behaviour over the tested concentration range of 0.5 to 2 wt.-% and hardly changed rheological behaviour. CB, CNT and TRGO induce electrical conductivity to their particular PBT composites by forming a conducting particle network within the polymer matrix. CNT reached the percolation threshold at the lowest concentration (<0.5 wt.-%), followed by TRGO (<1 wt.-%) and CB (<2 wt.-%). With the formation of a particle network, the flow behaviour of composites with CB, CNT and TRGO is affected, i.e., a flow limit occurs and the melt viscosity increases. The degree of influence of the carbon nanofillers on the rheological properties of PBT composites follows the same order as for electrical conductivity. Electrical and rheological results suggest an influence attributed to the particle dispersion, which is proposed to follow the order of EG<< CB