TY - JOUR A1 - Heinze, Christoph A1 - Pittner, Andreas A1 - Rethmeier, Michael A1 - Babu, S. S. T1 - Dependency of martensite start temperature on prior austenite grain size and its influence on welding-induced residual stresses N2 - Austenite grain growth during welding is a critical factor for controlling weld microstructure in addition to nominal composition and thermal cycles. Recently, experimental data suggesting a decrease in martensite start temperature with a decrease in prior austenite grain size has been published. However, the actual sensitivity of this phenomenon on residual stresses evolution in the heat-affected zone has not been investigated, yet. Therefore, a numerical model was modified to consider this phenomenon. Numerical simulations were performed for welding of a low-alloy structural steel with minimum yield strength of 355 MPa (S355J2+N) and a heat-resistant steel P91 or 9Cr–1Mo, respectively. The results clarify the influence of prior austenite grain size on the residual stress development and show the importance martensite transformation temperatures and final martensite fraction. Consequently, the residual stress evolution of P91, which completely transforms to martensite while cooling, based on the enhanced model leads to maximum stress differences of 200 MPa in the heat-affected zone. KW - Prior austenite grain size KW - Martensite start temperature KW - Welding-induced residual stress KW - Numerical simulation KW - Gas metal arc welding PY - 2013 U6 - https://doi.org/10.1016/j.commatsci.2012.11.058 SN - 0927-0256 VL - 69 SP - 251 EP - 260 PB - Elsevier CY - Amsterdam AN - OPUS4-27633 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Heinze, Christoph A1 - Michael, Thomas A1 - Pittner, Andreas A1 - Rethmeier, Michael T1 - Microcrack formation during gas metal arc welding of high-strength fine-grained structural steel N2 - The recent development of high-performance-modified spray arc processes in gas metal arc welding due to modern digital control technology and inverter power sources enables a focused spray arc, which results in higher penetration depths and welding speed. However, microcracks occurred in the weld metal while approaching the process limits of the modified spray arc, represented by a 20-mm double layer DV-groove butt-weld. These cracks were detected in structural steel exhibiting a yield strength level of up to 960 MPa and are neither dependent on the used weld power source nor a consequence of the modified spray arc process itself. The metallographic and fractographic investigations of the rather exceptional fracture surface lead to the classification of the microcracks as hot cracks. The effects of certain welding parameters on the crack probability are clarified using a statistical design of experiment. However, these microcracks do not impact the design specification for toughness in the Charpy V-notch test (absorbed energy at -40 °C for the present material is 30 J). KW - High-strength low-alloy steel KW - Welding KW - Fracture KW - Design of experiments KW - Microcracking PY - 2014 U6 - https://doi.org/10.1007/s40195-013-0011-5 SN - 1006-7191 SN - 1000-9442 VL - 27 IS - 1 SP - 140 EP - 148 PB - Springer CY - Shenyang AN - OPUS4-30123 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Heinze, Christoph A1 - Michael, Thomas A1 - Pittner, Andreas A1 - Rethmeier, Michael T1 - Schwierigkeiten bei der Anwendung der aktuellen Normung in Bezug auf Mikrorisse in Schweißverbindungen hochfester vergüteter Feinkornbaustähle N2 - Die aktuelle Normung bezüglich mikroskopischer Untersuchungen von Schweißverbindungen und die Zulässigkeit von Mikrorissen sowie deren Definition ist nicht eindeutig. Nach der Darstellung derzeit gültiger Normen im Bereich der Bewertung von Schweißnähten, Qualifizierung von Schweißverfahren und Ausführung von Schweißverbindungen, wird auf Grundlage aktueller Schweißversuche an hochfesten vergüteten Feinkornbaustählen die Problematik von Mikrorissen diskutiert. Offene Punkte und Fragen bzw. Verbesserungsmöglichkeiten werden aufgezeigt und zur Diskussion gestellt. Schließlich wird auf die Klärung des Einflusses von Mikrorissen auf die mechanisch- technologischen Werkstoffkennwerte der Schweißverbindung unter statischer sowie zyklischer Beanspruchung hingewiesen. --------------------------------------------------------------------------------------------------------------------------------------------------------------- Neither the latest standardisation with regard to microscopic investigations on welded joints nor the permissibility of microcracks and their definition are unambiguous. According to the representation of currently applicable standards in the fields of the assessment of welds, the qualification of welding processes and the execution of welded joints, the problems associated with microcracks are discussed on the basis of the latest welding tests on high-strength quenched-and-tempered fine-grained structural steels. Not only outstanding points and questions but also improvement possibilities are indicated and opened for discussion. Finally, attention is drawn to the clarification of the influence of microcracks on the mechanical- technological material parameters of the welded joint subjected to both static and cyclic stresses. KW - Festigkeit KW - Hochfester Stahl KW - Normen KW - Rissbildung KW - Schweißnahtfehler KW - Werkstofffragen KW - Strength KW - High-strength steel KW - Standards KW - Crack formation KW - Weld defects KW - Material questions PY - 2012 SN - 0036-7184 VL - 64 IS - 7 SP - 412 EP - 416 PB - Verl. für Schweißen u. Verwandte Verfahren, DVS-Verl. CY - Düsseldorf AN - OPUS4-26338 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -