TY - GEN A1 - Pfennig, Anja A1 - Kranzmann, Axel T1 - Influence of CO2 on the corrosion behaviour of 13%Cr martensitic stainless steel AISI 420 and low alloyed steel AISI 4140 exposed to saline aquifer water environment T2 - International Conference on Environment 2008 (ICENV 2008) - Environmental Management and Technologies Towards Sustainable Development CY - Penang, Malaysia DA - 2008-12-15 KW - Steel KW - Pipeline KW - Corrosion KW - Carbonate layer KW - CCS KW - CO2-injection KW - CO2-storage PY - 2008 SN - 978-983-3986-39-2 SP - 1 EP - 9 AN - OPUS4-18669 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pfennig, Anja A1 - Kranzmann, Axel T1 - Borehole integrity of austenitized and annealed pipe steels suitable for carbon capture and storage (CCS) N2 - Properties of pipe steels for CCS (carbon capture and storage) technology require resistance against the corrosive environment of a potential CCS-site (heat, pressure, salinity of the aquifer, CO2-partial pressure). The influence of austenitzing in heat treatment routines of two different injection pipe Steels (1.4034, X46Cr13 and 1.4021, X20Cr13) was evaluated. Steel coupons were austenitized at different temperatures (900- 1050 °C) for different lengths of time (30-90 min) before quenching and annealing prior to long term corrosion experiments (60°C, 100 bar, artificial brine close to a CCS-site in the Northern German Basin, Germany). In general, fewer pits are found on X46Cr13. Comparing steels with 13% chromium each the higher carbon content of X46Cr13 (0.46% C) results in a lower number of pits compared to X20Cr13 (0.20% C). It is found that neither the carbon content of the steels nor austenitizing temperature has much influence, but local corrosion behaviour is most susceptible towards austenitzing time. T2 - 2016 APCBEES Pattaya Conference CY - Pattaya, Thailand DA - 23.01.2016 KW - Heat Treatment KW - CCS KW - CO2 KW - Corrosion KW - Steel PY - 2016 AN - OPUS4-38444 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Pfennig, Anja A1 - Schiz, J. A1 - Kranzmann, Axel ED - Jha, A. ED - Wang, C. ED - Neelameggham, N.R. ED - Guillen, D.P. ED - Li, L. ED - Belt, C.K. ED - Kirchain, R. ED - Spangenberger, J.S. ED - Johnson, F. ED - Gomes, A.J. ED - Pandey, A. ED - Hosemann, P. T1 - The role of austenitizing routines of pipe steels during CCS N2 - Properties of pipe steels for CCS technology require resistance against the corrosive environment of a potential CCS-site (heat, pressure, salinity of the aquifer, CO2-partial pressure). The influence of austenitizing in heat treatment routines of two different injection pipe steels (1.4034, X46Cr13 and 1.4021, X20Cr13) was evaluated. Steel coupons were austenitized at different temperatures (900 – 1050 °C) for different lengths of time (30–90 min) before quenching and annealing prior to long term corrosion experiments (60°C, 100 bar, artificial brine close to a CCS-site in the Northern German Basin, Germany). In general, fewer pits are found on X46Cr13. Comparing steels with 13% chromium each the higher carbon content of X46Cr13 (0.46% C) results in a lower number of pits compared to X20Cr13 (0.20% C). It is found that neither the carbon content of the steels nor austenitizing temperature has much influence, but local corrosion behaviour is most susceptible towards austenitizing time KW - Corrosion KW - CCS KW - Carbon storage KW - Aquifer KW - Austenitizing PY - 2015 SN - 978-1-119-08240-8 DO - https://doi.org/10.1002/9781119093220.ch15 SP - 131 EP - 137 PB - Wiley AN - OPUS4-34924 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pfennig, Anja A1 - Schiz, Johann A1 - Kranzmann, Axel T1 - The Role of Austenitizing Routines of Pipe Steels During CCS T2 - TMS 2015 144th Annual Meeting & Exhibition CY - Orlando, Florida, USA DA - 2015-03-15 PY - 2015 AN - OPUS4-34745 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pfennig, Anja A1 - Wolf, Marcus T1 - High-Temperatur-High Pressure Stress-Strain Testing of Materials in CO2-Containing Saline Solutions T2 - TMS 2015, 144th Annual Meeting and Exhibition CY - Orlando, Florida, USA DA - 2015-03-15 PY - 2015 AN - OPUS4-34746 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pfennig, Anja A1 - Kranzmann, Axel T1 - Einfluss der Wärmebehandlung auf die Korrosionsbeständigkeit von hochlegierten Chromhaltigen Stählen unter CCS-Bedingungen T2 - Kraftwerksforum 2015 CY - Dresden, Germany DA - 2015-10-13 PY - 2015 AN - OPUS4-34828 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pfennig, Anja A1 - Kranzmann, Axel T1 - Borehole integrity of austenitized and annealed pipe steels suitable for carbon capture and storage (CCS) N2 - Properties of pipe steels for CCS (carbon capture and storage) technology require resistance against the corrosive environment of a potential CCS-site (heat, pressure, salinity of the aquifer, CO2-partial pressure). The influence of austenitzing in heat treatment routines of two different injection pipe steels (1.4034, X46Cr13 and 1.4021, X20Cr13) was evaluated. Steel coupons were austenitized at different temperatures (900-1050 °C) for different lengths of time (30-90 min) before quenching and annealing prior to long term corrosion experiments (60°C, 100 bar, artificial brine close to a CCS-site in the Northern German Basin, Germany). In general, fewer pits are found on X46Cr13. Comparing steels with 13% chromium each the higher carbon content of X46Cr13 (0.46% C) results in a lower number of pits compared to X20Cr13 (0.20% C). It is found that neither the carbon content of the steels nor austenitizing temperature has much influence, but local corrosion behaviour is most susceptible towards austenitzing time. T2 - 6th International Conference on Future Environment and Energy (ICFEE 2016) CY - Pattaya, Thailand DA - 23.01.2016 KW - CCS KW - CO2 KW - Corrosion KW - Steel KW - Heat treatment PY - 2016 SP - 9 EP - 14 AN - OPUS4-38980 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pfennig, Anja A1 - Kranzmann, Axel A1 - Wolthusen, Helmut T1 - Unusual Corrosion Behavior of 1.4542 Exposed a Laboratory Saline Aquifer Water CCS-Environment N2 - Differently heat treated coupons of 1.4542 were kept at T=60 °C and ambient pressure as well as p=100 bar for 700 h - 8000 h in an a) water saturated supercritical CO2 and b) CO2-saturated synthetic aquifer environment similar to on-shore CCS-sites in the Northern German Basin. Surface corrosion layers are homogeneous but unusually discontinuously ellipsoidal. After 8000 h at 100 bar maximum corrosion rate in the liquid phase is approximately 0.014 mm/year, with normalizing providing best corrosion resistance and approximately 0.003 mm/year in the supercritical phase where hardening+tempering at 670 °C leads to lowest corrosion rates. KW - CO2-storage KW - Supercritical CO2 KW - Steel KW - Pipeline KW - Corrosion KW - CCS PY - 2017 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-418472 DO - https://doi.org/10.1016/j.egypro.2017.03.1679 VL - 114 SP - 5229 EP - 5240 PB - Elsevier Ltd. AN - OPUS4-41847 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pfennig, Anja A1 - Wolf, Marcus A1 - Gröber, Andre A1 - Böllinghaus, Thomas A1 - Kranzmann, Axel T1 - Corrosion fatigue of 1.4542 exposed to a laboratory saline aquifer water CCS-environment N2 - X5CrNiCuNb16-4 has been proven to be sufficient resistant in corrosive environments, but shows rather unusual corrosion behaviour in CCS environment. Therefore a series of 30 specimens was tested at stress amplitudes between 150 MPa and 500 MPa (sinusoidal dynamic test loads, R=-1; resonant frequency ∼ 30 Hz). Due to the rather heterogeneous fine machined surfaces (Rz=4) the specimens are comparable with prefabricated parts. X5CrNiCuNb16-4 reached the maximum number of cycles (10 x 106) at a stress amplitude of 150 MPa and lies 60% below the stress amplitude measured in air. The scatter range TN = 1:34 is disproportionately large. Although the fracture surface exhibited the typical striations and corroded surface areas no significant differences were found. The hardness was found to be homogeneous in all specimens tested at 335 HV10. Non-metallic inclusions were found within the microstructure, but no correlation could be found between the inclusions and early rupture. Still specimens that showed inclusions at the fracture surface and its cross section endured lower number of cycles. Additionally Aluminium was analysed in specimens with low number of cycles and may be cause for early rupture during corrosion fatigue tests. These findings reveal a very high sensitivity on a homogeneous microstructure upon the corrosion and corrosion fatigue behaviour of X5CrNiCuNb16-4 and needs to be taken into account when regarding this steel as pipe steel during injection of CO2 into saline aquifers. T2 - 13th International Conference on Greenhouse Gas Control Technologies CY - Lausanne, Switzerland DA - 14.11.2016 KW - Steel KW - Corrosion fatigue KW - Electrochemistry KW - Reliability KW - CCS KW - CO2-storage PY - 2017 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-418525 DO - https://doi.org/10.1016/j.egypro.2017.03.1678 SN - 1876-6102 VL - 114 SP - 5219 EP - 5228 AN - OPUS4-41852 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pfennig, Anja A1 - Kranzmann, Axel T1 - Borehole integrity of austenitized and annealed pipe steels suitable for carbon capture and storage (CCS) N2 - Properties of pipe steels for CCS (carbon capture and storage) technology require resistance against the corrosive environment of a potential CCS-site (heat, pressure, salinity of the aquifer, CO2-partial pressure). The influence of austenitzing in heat treatment routines of two different injection pipe steels (1.4034, X46Cr13 and 1.4021, X20Cr13) was evaluated. Steel coupons were austenitized at different temperatures (900- 1050 °C) for different lengths of time (30-90 min) before quenching and annealing prior to long term corrosion experiments (60°C, 100 bar, artificial brine close to a CCS-site in the Northern German Basin, Germany). In general, fewer pits are found on X46Cr13. Comparing steels with 13% chromium each the higher carbon content of X46Cr13 (0.46% C) results in a lower number of pits compared to X20Cr13 (0.20% C). It is found that neither the carbon content of the steels nor austenitizing temperature has much influence, but local corrosion behaviour is most susceptible towards austenitzing time. T2 - International Conference on Future Environment and Energy CY - Pattaya, Thailand DA - 23.01.2016 KW - Corrosion KW - CCS KW - Carbon storage KW - Aquifer KW - Austenitizing PY - 2017 SP - Article A0005, 213 EP - 219 AN - OPUS4-41854 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pfennig, Anja A1 - Kranzmann, Axel T1 - Potential of martensitic stainless steel X5CrNiCuNb 16-4 as pipe steel in corrosive CCS environment N2 - Pipe steels suitable for carbon capture and storage technology (CCS) require resistance against the corrosive environment of a potential CCS-site (heat, pressure, salinity of the aquifer, CO2-partial pressure). X5CrNiCuNb16-4 has been proven to be sufficient resistant in corrosive environments, but shows rather unusual corrosion behaviour in CCS environment. Therefore differently heat treated coupons of 1.4542 were kept at T=60 °C and ambient pressure as well as p=100 bar for 700 h - 8000 h in an a) water saturated supercritical CO2 and b) CO2-saturated synthetic aquifer environment similar to on-shore CCS-sites in the Northern German Basin. Additionally fatigue tests were performed via push-pull tests with a series of 30 specimens was tested at stress amplitudes between 150 MPa and 500 MPa (sinusoidal dynamic test loads, R=-1; resonant frequency ~ 30 Hz). Best corrosion resistance in the liquid phase is achieved via normalizing prior to exposure and hardening+tempering at 670 °C leads to lowest corrosion rates in the supercritical phase. With no regard to atmosphere discontinuously ellipsoidal surface corrosion regions appear after exposure of 4000 h and more. The endurance limit of X5CrNiCuNb16-4 measured in air is reduced by more than 50% when exposed to CCS environment (maximum number of cycles (10 x 106) at a stress amplitude of 150 MPa) The scatter range TN = 1:34 is disproportionately large contributing to an overall unusual corrosion behaviour. KW - Corrosion KW - CCS KW - Carbon storage KW - Aquifer KW - Heat treatment KW - Fatigue KW - Endurance limit PY - 2017 DO - https://doi.org/10.18178/ijesd.2017.8.7.998 SN - 2010-0264 VL - 8 IS - 7 SP - 466 EP - 473 AN - OPUS4-41863 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pfennig, Anja A1 - Bäßler, Ralph T1 - Effect of CO2 on the stability of steels with 1% and 13% Cr in saline water N2 - In engineering storage sites for Carbon Sequestration the CO2-induced corrosion of injection pipe steels is a relevant safety issue when emission gasses are compressed in deep geological layers. The reliability of the steels suitable for the geological onshore CCS-site (Carbon Capture and Storage) at Ketzin, Germany, is demonstrated in laboratory experiments in equivalent corrosive environment (T = 60 °C, p = 1–60 bar, aquifer water, CO2-flow rate of 3 L/h, 700–8000 h exposure time). Corrosion kinetics and microstructures were characterized using specimens of the heat treated steel 42CrMo4 (1.7225) used for casing, and specimens of the martensitic stainless injection-pipe steel X46Cr13 (1.4034). KW - Corrosion KW - Layer products KW - Kinetics KW - Steel KW - Carbon Capture and Storage KW - Low alloyed steel KW - Stainless steel KW - SEM KW - Pitting corrosion KW - Kinetic parameters PY - 2009 DO - https://doi.org/10.1016/j.corsci.2009.01.025 SN - 0010-938X VL - 51 IS - 4 SP - 931 EP - 940 PB - Elsevier CY - Orlando, Fla. AN - OPUS4-19144 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pfennig, Anja A1 - Wolf, M. A1 - Kranzmann, Axel T1 - Corrosion and Corrosion Fatigue of Steels in Downhole CCS Environment—A Summary N2 - Static immersion tests of potential injection pipe steels 42CrMo4, X20Cr13, X46Cr13, X35CrMo4, and X5CrNiCuNb16-4 at T = 60°C and ambient pressure, as well as p = 100 bar were performed for 700–8000 h in a CO2-saturated synthetic aquifer environment similar to CCS sites in the Northern German Basin (NGB). Corrosion rates at 100 bar are generally lower than at ambient pressure. The main corrosion products are FeCO3 and FeOOH with surface and local corrosion phenomena directly related to the alloy composition and microstructure. The appropriate heat treatment enhances corrosion resistance. The lifetime reduction of X46Cr13, X5CrNiCuNb16-4, and duplex stainless steel X2CrNiMoN22-5-3 in a CCS environment is demonstrated in the in situ corrosion fatigue CF experiments (axial push-pull and rotation bending load, 60°C , brine: Stuttgart Aquifer and NGB, flowing CO2: 30 L/h, +/- applied potential). Insulating the test setup is necessary to gain reliable data. S-N plots, micrographic-, phase-, fractographic-, and surface analysis prove that the life expectancy of X2CrNiMoN22-5-3 in the axial cyclic load to failure is clearly related to the surface finish, applied stress amplitude, and stress mode. The horizontal grain attack within corrosion pit cavities, multiple fatigue cracks, and preferable deterioration of austenitic phase mainly cause fatigue failure. The CF life range increases significantly when a protective potential is applied. KW - Carbon capture and storage KW - Steel KW - High alloyed steel KW - Corrosion KW - Corrosion fatigue KW - CCS PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-523948 DO - https://doi.org/10.3390/pr9040594 VL - 9 IS - 4 SP - 594 PB - MDPI CY - Basel, Switzerland AN - OPUS4-52394 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pfennig, Anja T1 - Vom Blended Learning zum Full Online – so einfach geht es nicht – Praxiserfahrungen zum Einsatz von Lehrfilmen N2 - Mit Beginn der Covid-19 Pandemie und dem damit verbundenen ausschließlichen Lehren im online-Format war die Hoffnung verbunden ein Blended Learning Lehrformat für die Studieeingangsphase ohne viel konzeptionelle Änderungen übertragen zu können. Der Kurs Werkstofftechnik als Grundlagenfach für den Maschinenbau baut sich auf inverted classroom Lehrszenarien auf, deren Lerngrundlage hierfür eigens produzierte und auf das Lernziel abgestimmte Lehrfilme und Lightboard-Vorlesungen darstellen. Im Kontext der Studieneingangsphase bieten audiovisuell stimulierende Lehrfilme umfassende Lernmedien, wenn sie analog der Lerninhalte einem technischen und didaktischen Qualitätsanspruch genügen. In der Praxis des SS2020 und WS2020/21 hat sich gezeigt, dass die Moderation und Durchführung eines online-Kurses sich deutlich von dem eins blended learning-Kurses unterscheidet. Um denselben Lernerfolg bei Studierenden zu erzielen, müs-sen Anforderungen viel genauer und detaillierter verfasst werden, Studierende enger und persönlicher begleitet werden und Lehrfilme und Lernmedien in einen Gesamtzusammenhang gestellt werden. Im Folgenden werden aus persönlicher Erfahrung heraus niederschwellige, zum Teil ungewöhnliche praktische Erfahrungen zur erfolgreichen Umsetzung von Lehrfilm-basierten inverted classroom Lehrszenarien zusammengefasst und im Hinblick auf die online-Lehre bewertet. T2 - 19. Fachtagung Bildungstechnologien (DELFI) CY - Bonn, Germany DA - 13.09.2021 KW - Inverted classroom KW - Lehrfilm KW - Lehrfilmformate KW - Online KW - Covid-19 PY - 2021 SP - 289 EP - 295 AN - OPUS4-54154 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pfennig, Anja T1 - Improving Learning Outcome for GSL (German as a Second Language) Students in a Blended Learning Cumulative Assessment Material Science Course N2 - First year students especially with migration background and language deficiencies rate material science in mechanical engineering as one of the fundamental courses with high work load and necessity of language skills due to the descriptive nature of the course. Therefore a blended learning course structure using based on inverted classroom teaching scenarios was established. Heart of the self-study period are visualizing peer-to-peer lecture films supported by micro-lectures along with various online teaching materials. Although students with migration background generally scored lower in tests due to the lack of language skills improved learning outcomes are demonstrated in high quality class discussions and in overall understanding. This paper introduces the learning structure and graded activities, evaluates the course and compares results of native German-speaking students to those of students with migration background. KW - Portfolio KW - Diversity KW - Blended learning KW - Inverted classroom KW - Lecture films PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-541557 DO - https://doi.org/10.17706/ijeeee.2021.11.3.93-100 SN - 2010-3654 VL - 11 IS - 3 SP - 93 EP - 100 AN - OPUS4-54155 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pfennig, Anja T1 - How flipped classroom teaching methods in first year studying succeed N2 - Flipping the classroom is a method to let students study on their own and then take time to discuss their questions and do extended hands-on lectures or exercises in class – or in the case of the covid-19 pandemic during plenary online sessions. First year mechanical engineering students use different teaching materials (mainly lecture videos, lightboard videos and micromodule lectures) to study from a distance and comprehend the principle underlying science in theory. Then the online plenary lectures offer the opportunity to apply their knowledge and transfer different scientific aspects of the course to get the bigger picture. Exercises, worked solutions, selfassessed tests and peer-instruction during present time help students to check on their learning progress. However, the self-study periods and (online) plenary sessions need to be guided carefully. To meet the course learning outcome and overcome the diversity of a first year class various practical leads have to be fulfilled to turn flipped classroom teaching into success. T2 - 7th International Conference on Higher Education Advances (HEAd’21) CY - Valencia, Spain DA - 20.06.2021 KW - Inverted classroom KW - Flipped classroom KW - Online teaching KW - Lecture videos KW - First year students PY - 2021 DO - https://doi.org/10.4995/HEAd21.2021.12792 SP - 1211 EP - 1219 AN - OPUS4-54156 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pfennig, Anja A1 - Wolf, M. A1 - Kranzmann, Axel T1 - Corrosion and Corrosion Fatigue of Steels in Downhole CCS Environment—A Summary N2 - Static immersion tests of potential injection pipe steels 42CrMo4, X20Cr13, X46Cr13, X35CrMo4, and X5CrNiCuNb16-4 at T = 60 °C and ambient pressure, as well as p = 100 bar were performed for 700–8000 h in a CO2-saturated synthetic aquifer environment similar to CCS sites in the Northern German Basin (NGB). Corrosion rates at 100 bar are generally lower than at ambient pressure. The main corrosion products are FeCO3 and FeOOH with surface and local corrosion phenomena directly related to the alloy composition and microstructure. The appropriate heat treatment enhances corrosion resistance. The lifetime reduction of X46Cr13, X5CrNiCuNb16-4, and duplex stainless steel X2CrNiMoN22-5-3 in a CCS environment is demonstrated in the in situ corrosion fatigue CF experiments (axial push-pull and rotation bending load, 60 °C, brine: Stuttgart Aquifer and NGB, flowing CO2: 30 L/h, +/− applied potential). Insulating the test setup is necessary to gain reliable data. S-N plots, micrographic-, phase-, fractographic-, and surface analysis prove that the life expectancy of X2CrNiMoN22-5-3 in the axial cyclic load to failure is clearly related to the surface finish, applied stress amplitude, and stress mode. The horizontal grain attack within corrosion pit cavities, multiple fatigue cracks, and preferable deterioration of austenitic phase mainly cause fatigue failure. The CF life range increases significantly when a protective potential is applied. KW - Steel KW - High alloyed steel KW - Corrosion fatigue KW - Cabon capture and storage KW - CCS PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-541626 DO - https://doi.org/10.3390/pr9040594 VL - 9 IS - 4 SP - 594 PB - MDPI AN - OPUS4-54162 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pfennig, Anja A1 - Kranzmann, Axel T1 - Local Corrosion of Martensitic Stainless Steels during Exposure to Saline Aquifer Water and CO2 Environment N2 - Carbon Capture and Storage (CCS) is well acknowledged to mitigate climate change. Therefore, pipe Steels suitable for CCS technology require resistance against the corrosive environment of a potential CCS-site, e.g. heat, pressure, salinity of the aquifer, CO2-partial pressure. Samples of different mild and high alloyed stainless injection-pipe Steels partially heat treated: 42CrMo4, X20Cr13, X46Cr13, X35CrMo4 as well as X5CrNiCuNb16-4 were kept at T=60 °C and ambient pressure as well as p=100 bar for 700 h - 8000 h in a CO2-saturated synthetic aquifer environment similar to possible geological on-shore CCS-sites in the northern German Basin. Main corrosion products analysed on pits are FeCO3 and FeOOH. The carbon content does not show significant influence on the pitting behaviour. Generally, higher chromium Content results in better corrosion resistance. Although X35CrMo17-1 and X5CrNiCuNb16-4 show low surface corrosion rates, their resistance against local corrosion in CCS environment is not significantly better compared to the much less costly Steels X20Cr13 and X46Cr13. KW - Corrosion KW - CCS KW - Carbon storage KW - Aquifer KW - Heat treatment PY - 2018 DO - https://doi.org/10.18178/ijcea.2018.9.1.694 SN - 2010-0221 VL - 9 SP - 26 EP - 31 PB - International Association of Computer Science and Information Technology Press CY - Singapore AN - OPUS4-46627 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pfennig, Anja A1 - Kranzmann, Axel T1 - Impact of saline aquifer water on surface and shallow pit corrosion of martensitic stainless steels during exposure to CO2 environment (CCS) N2 - Pipe steels suitable for carbon capture and storage technology (CCS) require resistance against the corrosive environment of a potential CCS-site, e.g. heat, pressure, salinity of the aquifer, CO2-partial pressure. Samples of different mild and high alloyed stainless injection-pipe steels partially heat treated: 42CrMo4, X20Cr13, X46Cr13, X35CrMo4 as well as X5CrNiCuNb16-4 were kept at T=60 °C and ambient pressure as well as p=100 bar for 700 h - 8000 h in a CO2-saturated synthetic aquifer environment similar to possible geological on-shore CCS-sites in the northern German Basin. Main corrosion products are FeCO3 and FeOOH. Corrosion rates obtained at 100 bar are generally much lower than those measured at ambient pressure. Highest surface corrosion rates are 0.8 mm/year for 42CrMo4 and lowest 0.01 mm/year for X5CrNiCuNb16-4 in the vapour phase at ambient pressure. At 100 bar the highest corrosion rates are 0.01 mm/year for 42CrMo4, X20Cr13 (liquid phase), X46Cr13 and less than 0.01 mm/year for X35CrMo4 and X5CrNiCuNb16-4 after 8000 h of exposure with no regard to atmosphere. Martensitic microstructure offers good corrosion resistance. T2 - 8th International Conference on Future Environment and Energy (ICFEE 2018) CY - Phuket, Thailand DA - 10.01.2018 KW - CCS KW - CO2 corrosion KW - Pipeline PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-465896 DO - https://doi.org/10.1088/1755-1315/150/1/012012 VL - 150 SP - 81 EP - 90 PB - IOP Publ. AN - OPUS4-46589 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -