TY - GEN A1 - Angst, U. A1 - Brem, M. A1 - Dauberschmidt, C. A1 - Ebell, Gino A1 - Eichler, T. A1 - Hariri, K. A1 - Harnisch, J. A1 - Keßler, S. A1 - Kosalla, M. A1 - Mayer, T. F. A1 - Mietz, Jürgen A1 - Pruckner, F. A1 - Sodeikat, C. T1 - Merkblatt B 12 Korrosionsmonitoring bei Stahl- und Spannbetonbauwerken N2 - Das Merkblatt B12 enthält alle gängigen und etablierten Monitoringverfahren für das Korrosionsmonitoring an Stahlbetonbauwerken. KW - Korrosion KW - Monitoring PY - 2018 SN - 978-3-940283-93-1 SP - 1 EP - 58 PB - DGZfP CY - Berlin AN - OPUS4-45235 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Ebell, Gino A1 - Burkert, Andreas A1 - Mietz, Jürgen T1 - Corrosion behavior of galvanized reinforcement in chloride containing mortar and carbonated mortar N2 - Korrosionseigenschaften von feuerverzinktem Betonstahl unterscheiden sich grundlegend von herkömmlichen Betonstahl. In diesem Vortrag sind Beispiele für das Korrosionsverhalten in chloridhaltigen und carbonatisierten Mörteln dargestellt T2 - Intergalva 2018 - 25th International Galvanizing Conference CY - Berlin, Germany DA - 17.06.2018 KW - Corrosion KW - Korrosion KW - Verzinkt KW - Betonstahl PY - 2018 SP - 301 EP - 309 AN - OPUS4-45240 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Burkert, Andreas A1 - Müller, Thoralf A1 - Lehmann, Jens A1 - Mietz, Jürgen T1 - Long-term corrosion behaviour of stainless steels in marine atmosphere N2 - Nine different stainless steel alloys were exposed for 5 years under marine environment and their corrosion behaviour was compared and assessed. The investigation of four different surface finishes for all alloys tested further enabled to consider industry-specific features of the surface finish for the material comparison. The results of the exposure tests yield conclusions regarding the influence of alloy composition, surface finish and exposure duration under marine environment. The three duplex stainless steels revealed excellent corrosion resistance even in case of crevices during the 5 years of exposure under the given exposure conditions. Also the molybdenum-alloyed ferritic steel 1.4521 showed good corrosion resistance comparable to the classical austenitic materials 1.4301 and 1.4404. KW - Corrosion KW - Free weathering KW - Marine atmosphere KW - Stainless steels PY - 2018 U6 - https://doi.org/10.1002/maco.201709636 SN - 0947-5117 SN - 1521-4176 VL - 69 IS - 1 SP - 20 EP - 28 PB - Wiley-VCH Verlag GmbH & Co KGaA CY - Weinheim AN - OPUS4-43625 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gluth, Gregor A1 - Hlavacek, Petr A1 - Reinemann, Steffi A1 - Ebell, Gino A1 - Mietz, Jürgen ED - Alexander, M.G. ED - Beushausen, H. ED - Dehn, F. ED - Moyo, P. T1 - Leaching, carbonation and chloride ingress in reinforced alkali-activated fly ash mortars N2 - Alkali-activated fly ash mortars were studied with regard to durability-relevant transport coefficients and the electrochemical behaviour of embedded carbon steel bars on exposure of the mortars to leaching, carbonation and chloride penetration environments. The transport coefficients differed considerably between different formulations, being lowest for a mortar with BFS addition, but still acceptable for one of the purely fly ash-based mortars. Leaching over a period of ~300 days in de-ionized water did not lead to observable corrosion of the embedded steel, as shown by the electrochemical data and visual inspection of the steel. Exposure to 100 % CO2 atmosphere caused steel depassivation within approx. two weeks; in addition, indications of a deterioration of the mortar were observed. The results are discussed in the context of the different reaction products expected in high- and low-Ca alkali-activated binders, and the alterations caused by leaching and carbonation. T2 - International Conference on Concrete Repair, Rehabilitation and Retrofitting (ICCRRR 2018) CY - Cape Town, South Africa DA - 19.11.2018 KW - Alkali-activated materials KW - Steel corrosion KW - Leaching KW - Carbonation PY - 2018 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-464381 VL - 199 SP - Article Number 02025 PB - EDP Sciences AN - OPUS4-46438 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ebell, Gino A1 - Burkert, Andreas A1 - Mietz, Jürgen T1 - Detection of reinforcement corrosion in reinforced concrete structures by potential mapping: Theory and practice N2 - Electrochemical potential mapping according to guideline B3 of DGZfP (German Society for Nondestructive Testing) is a recognized technique for the localization of corroding reinforcing steels. In reinforced concrete structures the measured potentials are not necessarily directly linked to the corrosion likelihood of the reinforcing steel. The measured values may be significantly affected, different from, e.g., stress measurement, by different influences on the potential formation at the phase boundary metal/concrete itself as well as the acquisition procedure. Due to the complexity of influencing factors there is a risk that the results are misinterpreted. Therefore, in a training concept firstly the theoretical basics of the test method should be imparted. Then, frequently occurring practical situations of various influencing factors will be made accessible to the participants by a model object specially designed for this purpose. The aim is to impart profound knowledge concerning the characteristics of potential mapping for detecting corrosion of reinforcing steel in order to apply this technique in practice as reliable and economical test method. KW - Corrosion KW - Potential mapping KW - Korrosion KW - Potentialfeldmessung PY - 2018 U6 - https://doi.org/10.1155/2018/3027825 SN - 1687-9333 SN - 1687-9325 VL - 2018 SP - Article 3027825, 1 EP - 6 PB - Hindawi AN - OPUS4-46206 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Babutzka, Martin A1 - Mietz, Jürgen A1 - Burkert, Andreas T1 - Investigation of the salinization of steel surfaces in marine environment N2 - The salinization and contamination of metal surfaces by chloride-containing aerosols is of great importance with regard to corrosion phenomena of damaged coated metal surfaces and stainless steels in the maritime sector and in offshore applications. Detailed questions have to be answered to clarify whether and to what extent salinization of the surface has an influence on the adhesion and durability of coatings in repairing applications and on pitting occurrence on stainless steels under atmospheric conditions. The questions arise which degree of salinization is reached after which period of time and how a defined and reproducible salinization can be simulated in the laboratory for further systematic investigations. The article is dedicated to these questions. Results of a field trial on the Island of Heligoland are presented and a simple procedure for a defined loading of metal surfaces with chlorides at a laboratory scale using a design of experiments (DoE) approach is introduced. KW - Maritime Atmosphäre KW - Versalzung KW - Maritime atmosphere KW - Salinization PY - 2018 U6 - https://doi.org/10.1002/maco.201810636 SN - 0947-5117 SN - 1521-4176 VL - 70 IS - 6 SP - 1016 EP - 1025 PB - Wiley-VCH Verlag CY - Weinheim AN - OPUS4-47727 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -