TY - JOUR A1 - Heuskin, D. A1 - Kargl, F. A1 - Griesche, Axel A1 - Stenzel, C. A1 - Mitschke, D. A1 - Bräuer, D. A1 - Meyer, A. T1 - MSL compatible isothermal furnace insert for high temperature shear-cell diffusion experiments N2 - For long-time diffusion experiments shear-cell techniques offer more favourable terms than the traditional long capillary techniques. Here, we present a further developed shear-cell that enables the measurement of diffusion coefficients up to temperatures of 1600 °C. Hence, diffusion experiments can be carried out at temperatures not accessible until now by conventional capillary or shear-cell techniques. The modified shear-cell, which can contain up to six samples of a total length of 90mm and a diameter of 1.5 mm, is built of 30 shear discs of 3mm thickness each. It is operated in an isothermal furnace insert which can be accommodated in the Materials Science Laboratory of the International Space Station. This provides the opportunity that the shear-cell can be applied to microgravity and to ground-based experiments, respectively. The heater insert with an overall length of 518mm and a diameter of 210mm consists of four heating zones with a total power of 3.5 kW. Temperature homogeneity along the graphite sample compartment is better than 2K at 1600°C. Details of the new design are discussed and results of first successfully performed heating and shearing cycles are presented. KW - Microgravity KW - Diffusion KW - Shear cell KW - Melt KW - Alloy PY - 2011 U6 - https://doi.org/10.1088/1742-6596/327/1/012053 SN - 1742-6588 SN - 1742-6596 VL - 327 IS - 012053 SP - 1 EP - 8 PB - IOP Publ. CY - Bristol, UK AN - OPUS4-24994 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kargl, F. A1 - Engelhardt, M. A1 - Yang, F. A1 - Weis, H. A1 - Schmakat, P. A1 - Schillinger, B. A1 - Griesche, Axel A1 - Meyer, A. T1 - In situ studies of mass transport in liquid alloys by means of neutron radiography N2 - When in situ techniques became available in recent years this led to a breakthrough in accurately determining diffusion coefficients for liquid alloys. Here we discuss how neutron radiography can be used to measure chemical diffusion in a ternary AlCuAg alloy. Neutron radiography hereby gives complementary information to x-ray radiography used for measuring chemical diffusion and to quasielastic neutron scattering used mainly for determining self-diffusion. A novel Al2O3 based furnace that enables one to study diffusion processes by means of neutron radiography is discussed. A chemical diffusion coefficient of Ag against Al around the eutectic composition Al68.6Cu13.8Ag17.6 at.% was obtained. It is demonstrated that the in situ technique of neutron radiography is a powerful means to study mass transport properties in situ in binary and ternary alloys that show poor x-ray contrast. KW - Neutron radiography KW - Diffusion KW - Liquid alloys KW - Shear cell PY - 2011 U6 - https://doi.org/10.1088/0953-8984/23/25/254201 SN - 0953-8984 SN - 1361-648X VL - 23 IS - 25 SP - 254201-1 EP - 254201-8 PB - IOP Publ. Ltd. CY - Bristol AN - OPUS4-23854 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Meyer, A. A1 - Kricheldorf, H. R. T1 - Sn(II)2-ethylhexanoate-catalyzed polymerizations of L-lactide in solution – Solution grown crystals of cyclic Poly(L-Lactide)s N2 - L-lactide (LA) was polymerized in toluene by means of neat tin(II) 2-ethylhexanoate (SnOct2). Concentration, time and temperature were varied. The isothermally crystallized polyLAs (PLA) were characterized in the virgin state with regard to topology, molar mass, melting temperature (Tm), crystal modification, high or low Tm morphology, crystallinity and crystal thickness. Even a small amount of solvent favored cyclization relative to polymerization in bulk, so that cyclic polylactides were obtained at 115 ◦C and even at 95 ◦C. At all temperatures the α-modification of PLA was obtained along with crystallinities up to 90%. With 6 M solution the high Tm morphology with Tm’s > 190 ◦C was obtained at 115 ◦C. The crystal thickness of crystallites grown from solution at 115 ◦C was on the average 10–20% higher than that of PLA polymerized in bulk. At a polymerization temperature of 75 ◦C cyclization was incomplete and fewer perfect crystallites were formed. A new hypothesis for the crystal growth of cyclic polyLAs is proposed. KW - Polylactide KW - MALDI-TOF MS KW - Crystalinity KW - Polymerization PY - 2022 U6 - https://doi.org/10.1016/j.polymer.2022.125142 SN - 0032-3861 VL - 255 SP - 1 EP - 9 PB - Elsevier CY - Oxford AN - OPUS4-55283 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. A1 - Weidner, Steffen A1 - Meyer, A. T1 - Ring-expansion polymerization (REP) of L-lactide with cyclic tin catalysts – About formation of extended ring crystals and optimization of Tm and ΔHm N2 - L-Lactide was polymerized in bulk at 140 °C with three different cyclic tin catalysts and the time was varied from 1 d up to 14 d. The MALDI TOF spectra confirmed the formation of cyclic polylactides (PLAs) and displayed a characteristic change of peak intensity distribution with formation of a “saw tooth pattern”. This pattern confirms a previous hypothesis that cyclic PLAs tend to form crystallites with extended ring conformation and relatively smooth surface. This type of crystallites is formed under thermodynamic control by transesterification on the surface of the crystallites. In this way PLAs with extraordinarily high melting temperatures (Tm's up to 200.6 °C) and extraordinarily high melting enthalpy were obtained (ΔHm's up to 105 J g−1). These ΔHm values require a revision of the maximum ΔHm value calculated in the literature for ideal PLA crystals. KW - Polylactide KW - MALDI-TOF MS KW - ring-expansion polymerization PY - 2022 U6 - https://doi.org/10.1016/j.polymer.2022.125516 SN - 0032-3861 VL - 263 SP - 125516 PB - Elsevier Ltd. AN - OPUS4-56338 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen A1 - Meyer, A. T1 - About the Influence of (Non-)Solvents on the Ring Expansion Polymerization of l-Lactide and the Formation of Extended Ring Crystals N2 - Ring-expansion polymerizations (REPs) catalyzed by two cyclic tin catalysts(2-stanna-1.3-dioxa-4,5,6,7-dibenzazepine [SnBiph] and 2,2-dibutyl-2-stanna-1,3-dithiolane [DSTL) are performed at 140 °C in bulk. Small amounts (4 vol%) of chlorobenzene or other solvents are added to facilitate transesterification reactions (ring–ring equilibration) in the solid poly(l-lactide)s. In the mass range up to m/z 13 000 crystalline PLAs displaying a so-called saw-tooth pattern in the MALDI-TOF mass spectra are obtained indicating the formation of extended-ring crystals. The characteristics of extended-ring crystallites and folded-ring crystallites are discussed. Furthermore, extremely high melting temperatures (Tm’s up to 201.2 °C) and melting enthalpies (𝚫Hm’s up to 106 J g−1)) are found confirming that 𝚫Hmmax, the 𝚫Hm of a perfect crystal, is around or above 115 J g−1 in contrast to literature data. KW - Polylactide KW - MALDI-TOF MS KW - Ring-expansion polymerization KW - Crystals PY - 2022 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-565038 SN - 1022-1352 SP - 1 EP - 8 PB - Wiley VHC-Verlag AN - OPUS4-56503 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen A1 - Meyer, A. T1 - Poly(L-lactide): Optimization of Melting Temperature and Melting Enthalpy N2 - Twice recrystallized L-lactide was polymerized with a dozen of different tin or bismuth catalysts in bulk at 160°C for 24 h and was annealed at 150°C afterwards. In two cases Tm values above 197.0°C were obtained. The parameters causing a scattering of the DSC data were studied and discussed. The samples prepared with SnCl2, 2,2-dibutyl-2-stanna-1,3-ditholane (DSTL) or cyclic tin(II) bisphenyldioxide (SnBiph) were subject to annealing programs with variation of time and temperatures, revealing that the Tm´s did not increase. However, an increase of Hm was achieved with maximum values in the range of 93-96 J g-1 corresponding to crystallinities off around 90%. Further studies were performed with once recrystallized L-lactide. Again, those samples directly crystallized from the polymerization process showed the highest Tm values. These data were compared with the equilibrium Tm0 and Hm0 data calculated by several research groups for perfect crystallites. A Tm0 of 213+/-2°C and a Hm0 of 106 J g-1 show the best agreement with the experimental data. The consequences of annealing for the thickness growth of crystallites are discussed on the basis of SAXS measurements. Finally, a comparison of cyclic and linear poly L-lactide)s is discussed. KW - Polylactide KW - MALDI-TOF MS KW - Transesterification PY - 2021 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-538656 SP - 1 EP - 10 PB - Royal Society for Chemistry AN - OPUS4-53865 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zocca, Andrea A1 - Wilbig, Janka A1 - Waske, Anja A1 - Günster, Jens A1 - Widjaja, Martinus A1 - Neumann, C. A1 - Clozel, M. A1 - Meyer, A. A1 - Ding, J. A1 - Zhou, Z. A1 - Tian, X. T1 - Challenges in the Technology Development for Additive Manufacturing in Space N2 - Instead of foreseeing and preparing for all possible scenarios of machine failures, accidents, and other challenges arising in space missions, it appears logical to take advantage of the flexibility of additive manufacturing for “in-space manufacturing” (ISM). Manned missions into space rely on complicated equipment, and their safe operation is a great challenge. Bearing in mind the absolute distance for manned missions to the Moon and Mars, the supply of spare parts for the repair and replacement of lost equipment via shipment from Earth would require too much time. With the high flexibility in design and the ability to manufacture ready-to-use components directly from a computer-aided model, additive manufacturing technologies appear to be extremely attractive in this context. Moreover, appropriate technologies are required for the manufacture of building habitats for extended stays of astronauts on the Moon and Mars, as well as material/feedstock. The capacities for sending equipment and material into space are not only very limited and costly, but also raise concerns regarding environmental issues on Earth. Accordingly, not all materials can be sent from Earth, and strategies for the use of in-situ resources, i.e., in-situ resource utilization (ISRU), are being envisioned. For the manufacturing of both complex parts and equipment, as well as for large infrastructure, appropriate technologies for material processing in space need to be developed. KW - Additive manufacturing KW - Space KW - Process PY - 2022 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-549204 SN - 2772-6657 VL - 1 IS - 1 SP - 1 EP - 13 PB - Elsevier Ltd. AN - OPUS4-54920 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Meyer, A. A1 - Weidner, Steffen T1 - High Tm Poly(l-lactide)s by Means of Bismuth Catalysts? N2 - One series of BiSub-catalyzed ring-opening polymerizations (ROPs) is per-formed at 160 °C for 3 days with addition of difunctional cocatalysts to find out, if poly(l-lactide) crystallizes directly from the reaction mixture. An analogous series is performed with monofunctional cocatalysts. High Tm crystal-lites (Tm > 190 °C) are obtained from all bifunctional cocatalysts, but not from all monofunctional ones. It is shown by means of SAXS measurements that the high Tm values are mainly a consequence of a transesterification–homogenization process across the lamellar surfaces resulting in thickness and smoothing of the surfaces. An unusual enthalpy-driven modification of the molecular weight distribution is found for samples that have crystallized during the polymerization. A third series of ROPs is performed at 170 °C for 2 h followed by annealing at 120 °C (2 h) to induce crystallization. Complete transformation of the resulting low Tm crystallites (Tm < 180 °C) into the high Tm crystallites by annealing at 170 °C for 1 d is not achieved, despite variation of the cocatalyst. KW - Polylactide KW - MALDI-TOF MS KW - Crystallization PY - 2021 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-522777 SN - 1022-1352 VL - 222 IS - 8 SP - 19 PB - Wiley AN - OPUS4-52277 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Meyer, A. A1 - Kricheldorf, H. R. A1 - Weidner, Steffen T1 - ROPs of L-lactide catalyzed by neat Tin(II)2-ethylhexanoate - Influence of the reaction conditions on Tm and ΔHm N2 - L-Lactide was polymerized by means of neat SnOct2 with variation of LA/Cat ratio, temperature and time. The resulting cyclic polylactides crystallized spontaneously at 160 °C or below, but needed nucleation via mechanical stress at 165 or 170 °C. All the crystalline polylactides obtained directly from ROP above 120 °C had melting temperatures (Tm) above 189 °C (up to 194.5 °C). SnOct2 also enabled transformation of low Tm poly(L-lactide)s (Tm <180 °C) into the high Tm m1odification by annealing, due to the impact of transesterification reactions in the interphase between the crystallites. The influence of crystallization temperature and annealing time on the crystal thickness was studied via SAXS measurements. A comparison with the crystallization and annealing experiments reported by Pennings and coworkers and Tsuji and Ikada is discussed, and a satisfactory agreement has been found, because those authors also studied polyLA samples containing SnOct2 in its active form. It is also demonstrated in this work that the high Tm modification cannot be obtained when the catalyst is removed or poisoned as it is true for commercial polylactides. KW - Polylactide KW - MALDI-TOF MS KW - Crystallization PY - 2021 U6 - https://doi.org/10.1016/j.polymer.2021.124122 SN - 0032-3861 VL - 231 SP - 1 EP - 10 PB - Elsevier CY - Oxford AN - OPUS4-53194 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Meyer, A. A1 - Falkenhagen, Jana A1 - Kricheldorf, H. R. T1 - SnOct2-catalyzed and alcohol-initiated ROPs of L-lactide – About the influence of initiators on chemical reactions in the melt and the solid state N2 - SnOct2 (Sn(II) 2-ethylhexanoate) catalyzed ROPs of L-lactide were performed in bulk with eight different alcohols as initiators. The time was varied between 1 h and 24 h for all initiators. For two initiators the temperature was also lowered to 115 ◦C. Even-numbered chains were predominantly formed in all polymerizations at short times, but the rate of transesterification (e.g. even/odd equilibration) and the molecular weight distribution were found to depend significantly on the nature of the initiator. Observed transesterification reactions also continued in solid poly (L-lactide), and with the most active initiator, almost total equilibration was achieved even at 130 ◦C. This means that all chains including those of the crystallites were involved in transesterification reactions proceeding across the flat surfaces of the crystallites. The more or less equilibrated crystalline polylactides were characterized by DSC and SAXS measurements with regard to their melting temperature (Tm), crystallinity and crystal thickness. KW - Polylactide KW - MALDI-TOF MS KW - Crystallization KW - Catalysts KW - SAXS PY - 2021 U6 - https://doi.org/10.1016/j.eurpolymj.2021.110508 VL - 153 SP - 110508 PB - Elsevier Ltd. AN - OPUS4-52633 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rosemann, Paul A1 - Müller, Christina A1 - Meyer, A. A1 - Halle, T. T1 - Influence of nitrogen on the corrosion resistance of martensitic stainless steels N2 - The corrosion resistance of martensitic stainless steels (MSS) depends strongly on the chemical composition and the applied heat treatment. Both determines the distribution of the alloying elements in the microstructure and the resulting material properties. The addition of nitrogen is known to be beneficial for the pitting corrosion resistance of stainless steels. In case of MSS this effect is not only connected to nitrogen itself because nitrogen can be used to substitute carbon which also influences the result of the heat treatment process. This paper shows the effect of nitrogen on the corrosion resistance in relation to the hardening process of MSS. Therefore the effects of austenitization duration, austenitization temperature and cooling rate on microstructure, hardness and corrosion resistance were studied on the MSS X30CrMoN15 1 and X50CrMoV15. The effect of different cooling rates was studied in the range of > 100 K/s down to 1 K/s using the jominy end quench test. The changes in corrosion resistance were detected with electrochemical potentiodynamic reactivation (EPR) and by the determination of critical pitting potentials. Besides this experimental approach thermodynamic calculations with the software thermocalc will be presented and used for the interpretation of the effect of nitrogen on the corrosion resistance of MSS. T2 - 18th Chemnitz Seminar on Materials Engineering – 18. Werkstofftechnisches Kolloquium CY - Chemnitz, Germany KW - Martensitic stainless steels KW - Corrosion resistance KW - Heat treatment PY - 2016 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-366956 VL - 118 IS - 1 SP - 19 EP - 19 PB - IOP Publishing AN - OPUS4-36695 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rosemann, Paul A1 - Müller, C. A1 - Meyer, A. A1 - Halle, T. ED - Lampke, T. ED - Wagner, G. ED - Wagner, M.F.-X. T1 - Einfluss von Stickstoff auf Mikrostruktur und Korrosionsverhalten martensitischer nichtrostender Stähle N2 - Die Korrosionsbeständigkeit martensitischer nichtrostender Stähle (MNS) wird wesentlich von der chemischen Zusammensetzung und dem Wärmebehandlungszustand beeinflusst. Beides bestimmt die Verteilung der Legierungselemente im Gefüge und die daraus resultierenden Werkstoffeigenschaften. Das Legieren mit Stickstoff bewirkt im Allgemeinen eine Verbesserung der Lochkorrosionsbeständigkeit von nichtrostenden Stählen. Bei martensitischen nichtrostenden Stählen ist dieser Effekt nicht nur auf den Stickstoffgehalt selbst zurückzuführen, sondern auch auf den gleichzeitig verringerten Kohlenstoffgehalt, der ebenfalls das Ergebnis der Wärmebehandlung beeinflusst. In dieser Arbeit wird der Einfluss von Stickstoff auf die Korrosionsbeständigkeit in Bezug zum Härtungsprozess von MNS dargestellt. Dazu wird vergleichend der Effekt von Austenitisierungsdauer, -temperatur und Abkühlgeschwindigkeit auf Gefüge, Härte und Korrosionsbeständigkeit der MNS X50CrMoV15 und X30CrMoN15 1 untersucht. Die Abkühlgeschwindigkeit wurde mit dem Stirnabschreckversuch gezielt variiert, um den Einfluss von Abkühlgeschwindigkeiten von > 100 K/s bis 1 K/s zu charakterisieren. Die Veränderungen der Korrosionsbeständigkeit werden durch die elektrochemisch potentiodynamische Reaktivierung (EPR) und durch die Bestimmung kritischer Lochkorrosionspotentiale dokumentiert. Neben diesem experimentellen Ansatz werden auch die Ergebnisse von thermodynamischen Berechnungen mit der Software Thermocalc vorgestellt und abschließend auch zur Interpretation des Einflusses von Stickstoff auf die Korrosionsbeständigkeit martensitischer nichtrostender Stähle genutzt. T2 - 18. Werkstofftechnisches Kolloquium der TU Chemnitz CY - Chemnitz, Germany DA - 10.03.2016 KW - Korrosionsbeständigkeit KW - Corrosion resistance KW - Wärmebehandlung KW - Heat treatment KW - Nichtrostende Stähle KW - Stainless steels KW - Thermocalc KW - Thermocalc PY - 2016 SN - 978-3-00-052212-3 SN - 1439-1597 VL - 59 SP - 325 EP - 336 PB - TU Chemnitz, Fakultät für Maschinenbau, Institut für Werkstoffwissenschaft und Werkstofftechnik CY - Chemnitz AN - OPUS4-37263 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Menzel, M. A1 - Scharf, O. A1 - Novak, S. A1 - Radtke, Martin A1 - Reinholz, Uwe A1 - Hischenhuber, P. A1 - Buzanich, Günter A1 - Meyer, A. A1 - Lopez, V. A1 - McIntosh, K. A1 - Streli, C. A1 - Havrilla, G. A1 - Fittschen, U. T1 - Shading in TXRF: calculations and experimental validation using a color X-ray camera N2 - Absorption effects in total reflection X-ray fluorescence (TXRF) analysis are important to consider, especially if external calibration is to be applied. With a color X-ray camera (CXC), that enables spatially and energy resolved XRF analysis, the absorption of the primary beam was directly visualized for mL-droplets and an array of pL-droplets printed on a Si-wafer with drop-on-demand technology. As expected, deposits that are hit by the primary beam first shade subsequent droplets, leading to a diminished XRF signal. This shading effect was quantified with enhanced precision making use of sub-pixel analysis that improves the spatial resolution of the camera. The measured absorption was compared to simulated results using three different model calculations. It was found they match very well (average deviation < 10%). Thus errors in quantification due to absorption effects can be accounted for in a more accurate manner. KW - absorption KW - X-ray Fluorescence analysis PY - 2015 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-359000 IS - 10 SP - 2184 EP - 2193 PB - Royal Society of Chemistry CY - Cambridge AN - OPUS4-35900 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Griesche, Axel A1 - Engelhardt, M. A1 - Kargl, F. A1 - Meyer, A. A1 - Weis, H. A1 - Yang, F. T1 - Diffusion measurements with neutron radiography KW - Diffusion KW - Metal KW - Semiconductor KW - Melt KW - In-situ KW - Radiography KW - Darken KW - Capillary PY - 2009 IS - Chapter 4.1.5 SP - 214 EP - 215 AN - OPUS4-21449 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Meyer, A. A1 - Kricheldorf, H. R. T1 - Ring–Ring Equilibration in Solid, Even-Numbered Cyclic Poly(l-lactide)s and their Stereocomplexes N2 - Even-numbered cyclic poly(d-lactide) and poly(l-lactide) are prepared by ringexpansion polymerization. The cyclic pol(l-lactide) is annealed either at 120 or at 160 °C for several days. The progress of transesterification in the solid state is monitored by the formation of odd-numbered cycles via matrix-assisted laser desorption/ionization-time of flight mass spectrometry. The changes of the crystallinity are monitored by differential scanning calorimetry, wideand small-angle x-ray scattering (WAXS and SAXS) measurements. Despite total even-odd equilibration at 160 °C, the crystallinity of poly(l-lactide) is not reduced. Furthermore, the crystallinity of the stereocomplexes of both cyclic polylactides do not decrease or vanish, as expected, when a blocky or random stereosequence is formed by transesterification. This conclusion is confirmed by 13C NMR spectroscopy. These measurements demonstrate that transesterification is a ring–ring equilibration involving the loops on the surfaces of the lamellar crystallites thereby improving crystallinity and 3D packing of crystallites without significant broadening of the molecular weight distribution. KW - Polylactide KW - MALDI-TOF MS KW - Cyclization PY - 2020 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-506458 VL - 221 IS - 9 SP - 2000012 PB - Wiley-VCH Verlag AN - OPUS4-50645 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen A1 - Meyer, A. T1 - High Tm poly(L-lactide)s via REP or ROPPOC of L-lactide N2 - A new kind of high melting (HTm) pol(L-lactide) was discovered when cyclic poly(L-lactide)s were prepared by ring-expansion polymerization with cyclic tin catalysts at 130–160 °C in bulk. By DSC measurements with 10 K min−1 melting temperatures (Tm) in the range of 190–196 °C were found. The WAXS and SAXS measurements evidenced that not a new crystal lattice but a well-ordered morphology and a higher perfection of the crystallites are responsible for the high Tm values and high crystallinities. Under identical reaction conditions SnOct2-catalyzed and alcohol-initiated ROPs do not yield these crystallites. Furthermore, it was found that the standard crystallites are kinetically favored upon rapid crystallization, whereas the high melting form of poly(L-lactide) is thermodynamically more stable. KW - Polylactide KW - MALDI-TOF MS KW - ROPPOC PY - 2020 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-507477 VL - 11 IS - 12 SP - 2182 EP - 2193 PB - Royal Society of Chemistry AN - OPUS4-50747 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Meyer, A. A1 - Chatti, S. A1 - Kricheldorf, H. R. T1 - About the transformation of low Tm into high Tm poly(L-lactide)s by annealing under the influence of transesterification catalysts N2 - Cyclic polylactides were prepared in bulk at 170 °C, crystallized at 120 °C and then annealed at temperatures between 130 and 170 C with variation of catalyst, catalyst concentration and annealing time. The transformation of the initially formed low melting (LTm) crystallites, having melting temperatures (Tm) <180 °C into high melting (HTm) crystallites having Tm values > 189 °C was monitored by means of DSC measurements and characterized in selected cases by SAXS measurements. It was confirmed that the formation of HTm crystallites involves a significant growth of the thickness of the lamellar crystallites along with smoothing of their surface. Annealing at 170 °C for 1 d or longer causes thermal degradation with lowering of the molecular weights, a gradual transition of cyclic into linear chains and a moderate decrease of lamellar thickness. An unexpected result revealed by MALDI TOF mass spectrometry is a partial reorganization of the molecular weight distribution driven by a gain of crystallization enthalpy. KW - Polylactide KW - MALDI-TOF MS KW - Crystallization KW - Annealing PY - 2021 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-521062 VL - 11 IS - 5 SP - 2872 EP - 2883 PB - Royal Society of Chemistry AN - OPUS4-52106 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Meyer, A. A1 - Weidner, Steffen A1 - Kricheldorf, H. T1 - Stereocomplexation of cyclic polylactides with each other and with linear poly(L-lactide)s N2 - Two kinds of cyclic poly(D- and L-lactide)s were synthesized, namely CI labeled samples mainly consisting of even-numbered cycles with low dispersity and CII, CIII or CIV-labeled ones consisting of equal amounts of even and odd-numbered cycles with high dispersity and igher molecular weights (Mw up to 300 000). Furthermore, linear poly L-lactide)s were prepared by initiation with ethanol and in both series the molecular weight was varied. The formation of stereocomplexes from cyclic poly(D-lactide)s and all kinds of poly L-lactide)s was performed in dichloromethane/toluene mixtures. The stereocomplexes crystallized from the reaction mixture were characterized in the virgin state and after annealing at 205 °C. Stereocomplexes free of stereohomopolymers with crystallinities up to 80% were obtained from all experiments in yields ranging from 60 to 80%. Despite the high annealing temperature (maintained for 1 h), little transesterification was observed and the crystallinity slightly increased. KW - Polylactide KW - MALDI-TOF MS KW - Stereocomplex KW - Cyclic PY - 2019 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-496693 VL - 10 SP - 6191 EP - 6199 PB - Royal Society for Chemistry AN - OPUS4-49669 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen A1 - Meyer, A. T1 - High Tm linear poly(L-lactide)s prepared via alcohol-initiated ROPs of L-lactide N2 - Alcohol-initiated ROPs of L-lactide were performed in bulk at 160 °C for 72 h with variation of the catalyst or with variation of the initiator (aliphatic alcohols). Spontaneous crystallization was only observed when cyclic Sn(II) compounds were used as a catalyst. Regardless of initiator, high melting crystallites with melting temperatures (Tm) of 189–193 °C were obtained in almost all experiments with Sn(II) 2,2′-dioxybiphenyl (SnBiph) as catalyst, even when the time was shortened to 24 h. These HTm poly(lactide)s represent the thermodynamically most stable form of poly(L-lactide). Regardless of the reaction conditions, such high melting crystallites were never obtained when Sn(II) 2-ethylhexanoate (SnOct2) was used as catalyst. SAXS measurements evidenced that formation of HTm poly(L-lactide) involves growth of the crystallite thickness, but chemical modification of the crystallite surface (smoothing) seems to be of greater importance. A hypothesis, why the “surface smoothing” is more effective for crystallites of linear chains than for crystallites composed of cycles is discussed. KW - Polylactide KW - MALDI-TOF MS KW - Ring-opening polymerization PY - 2021 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-524330 VL - 11 IS - 23 SP - 14093 EP - 14102 PB - Royal Society of Chemistry AN - OPUS4-52433 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. R. A1 - Weidner, Steffen A1 - Meyer, A. T1 - About the Influence of (Non-)Solvents on the Ring Expansion Polymerization of l-Lactide and the Formation of Extended Ring Crystals N2 - Ring-expansion polymerizations (REPs) catalyzed by two cyclic tin catalysts (2-stanna-1.3-dioxa-4,5,6,7-dibenzazepine [SnBiph] and 2,2-dibutyl-2-stanna-1,3-dithiolane [DSTL]) are performed at 140 °C in bulk. Small amounts (4 vol%) of chlorobenzene or other solvents are added to facilitate transesterification reactions (ring–ring equilibration) in the solid poly(l-lactide)s. In the mass range up to m/z 13 000 crystalline PLAs displaying a so-called saw-tooth pattern in the MALDI-TOF mass spectra are obtained indicating the formation of extended-ring crystals. The characteristics of extended-ring crystallites and folded-ring crystallites are discussed. Furthermore, extremely high melting temperatures (Tm’s up to 201.2 °C) and melting enthalpies (𝚫Hm’s up to 106 J g−1)) are found confirming that 𝚫Hm max, the 𝚫Hm of a perfect crystal, is around or above 115 J g−1 in contrast to literature data. KW - Polylactide KW - MALDI-TOF MS KW - Ring-expansion polymerization KW - Biobased PY - 2023 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-573063 VL - 224 IS - 5 SP - 1 EP - 8 PB - Wiley VHC-Verlag AN - OPUS4-57306 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Meyer, A. A1 - Kricheldorf, H. R. T1 - Alcohol-initiated and Tin(II) 2-ethylhexanoate-catalyzed polymerization of L-lactide in bulk – About separate crystallization of cyclic and linear Poly (L-lactide)s N2 - Alcohol-initiated ROPs of L-Lactide were performed at 140 ◦C in bulk with variation of the initiator/catalyst ratio and time. Lower ratios favor the formation of cycles which upon annealing display a change of the MALDI mass peak distribution towards a new maximum with a “saw-tooth pattern” of the mass peaks representing the cycles. Such a pattern was not observed for the mass peak of the linear chains. The coexistence of these patterns indicate that linear and cyclic poly (L-lactide)s (PLA) crystallize in separate crystals, and that the crystallites of the cycles are made up by extended rings. High Tm and ΔHm values confirm that these extended-ring crystallites represent a thermodynamically optimized form of PLA. Experiments with preformed cyclic and linear PLAs support this interpretation. KW - Polylactide KW - MALDI-TOF MS KW - Crystalinity KW - Polymerization PY - 2023 U6 - https://doi.org/10.1016/j.polymer.2023.126355 VL - 285 IS - 126355 SP - 1 EP - 9 PB - Elsevier Ltd. AN - OPUS4-58355 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. A1 - Weidner, Steffen A1 - Meyer, A. T1 - Syntheses of Polyglycolide via Polycondensation: A Reinvestigation N2 - The Na salt of chloroacetic acid is condensed in suspension. Furthermore,glycolic acid is condensed in bulk or in concentrated solution by means of SnCl2 or 4-toluene sulfonic acid (TSA) as catalysts. The temperatures are varied from 160 to 200°C and the time from 1 to 5 days. Low molar mass cyclic poly(glycolic acid) (PGA) is detected by means of matrix-assisted laser desorption ionization time-of-flight (MALDI TOF) mass spectrometry in most PGAs. A predominance of certain cycles having an even number of repeat units is observed suggesting a thermodynamically favored formation of extended-ring crystals. Extremely high melting temperatures (up to 237.5°C)and high melting enthalpies are found for polycondensations with TSA in 1,2-dichlorobenzene. KW - MALDI TOF MS KW - Polycondensation KW - Polyglycolide KW - Cyclization PY - 2024 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-596856 IS - 2300397 SP - 1 EP - 7 PB - Wiley VHC-Verlag AN - OPUS4-59685 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Meyer, A. A1 - Kricheldorf, H. T1 - Cyclic polyglycolides via ring-expansion polymerization with cyclic tin catalysts N2 - Glycolide was polymerized in bulk with two cyclic catalysts − 2,2-dibutyl-2-stanna-1,3-dithiolane (DSTL) and 2-stanna-1,3-dioxa-4,5,6,7-dibenzepane (SnBiph). The monomer/initiator ratio, temperature (140 – 180 °C) and time (1–––4 days) were varied. The MALDI TOF mass spectra exclusively displayed peaks of cyclic polyglycolide (PGA) and revealed an unusual “saw-tooth pattern” in the mass range below m/z 2 500 suggesting formation of extended ring crystallites. The DSC measurements indicated increasing crystallinity with higher temperature and longer time, and after annealing for 4 d at 160 °C a hitherto unknown and unexpected glass transition was found in the temperature range of 170–185 °C. Linear PGAs prepared by means of metal alkoxides under identical conditions did not show the afore-mentioned features of the cyclic PGAs, neither in the mass spectra nor in the DSC measurements. All PGAs were also characterized by SAXS measurements, which revealed relatively small L-values suggesting formation of thin crystallites in all cases with little influence of the reaction conditions. KW - Polyglycolide KW - MALDI-TOF MS KW - Ring-expansion polymerization KW - Crystals PY - 2024 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-595541 SN - 0014-3057 VL - 207 SP - 1 EP - 9 PB - Elsevier Ltd. AN - OPUS4-59554 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Meyer, A. A1 - Kricheldorf, H. T1 - Transformation of poly(L-lactide) crystals composed of linear chains into crystals composed of cycles N2 - A poly(L-lactide) with a trifluoroethyl ester end group and an average degree of polymerization (DP) of 50 was synthesized by ROP of L-lactide initiated with trifluoroethanol. Small-angle X-ray scattering (SAXS) in combination with differential scanning calorimetry (DSC) measurements revealed an average crystal thickness of 13 nm, corresponding to 45 repeat units. This suggests that most crystallites were formed by extended PLA chains, and both flat surfaces were covered by CF3 groups. The crystalline PLAs were annealed at 140 or 160 °C in the presence of two catalysts: tin(II) 2-ethylhexanoate, (SnOct2) or dibutyltin bis(pentafluorophenoxide) (BuSnPhF). The chemical reactions, such as polycondensation and cyclization, proceeded in the solid state and were monitored by matrix-assisted laser desorption/ionization time-offlight (MALDI TOF) mass spectrometry and gel permeation chromatography (GPC) measurements. Under optimal conditions a large fraction of linear chains was transformed into crystallites composed of extended cycles. Additionally, MALDI TOF MS analysis of GPC fractions from samples annealed for 28 or 42 days detected chain elongation of the linear species up to a factor of 20. KW - Polylactide KW - MALDI-TOF MS KW - Crystalinity KW - Transesterification PY - 2024 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-597250 SN - 1759-9954 VL - 15 IS - 12 SP - 1173 EP - 1181 PB - Royal Society for Chemistry AN - OPUS4-59725 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Meyer, A. A1 - Falkenhagen, Jana A1 - Kricheldorf, H. R. T1 - Polycondensations and Cyclization of Poly(L-lactide) Ethyl Esters in the Solid State N2 - The usefulness of seven different Tin catalysts, Bismuth subsalicylate and Titan tetra(ethoxide) for the polycondensation of ethyl L-lactate (ELA) was examined at 150 °C/6 d. Dibutyltin bis(phenoxides) proved to be particularly effective. Despite the low reactivity of ELA, weight average molecular masses (Mw) up to 12 500 were found along with partial crystallization. Furthermore, polylactides (PLAs) of similar molecular masses were prepared via ELA-initiated ROPs of L-lactide by means of the four most effective polycondensation catalysts. The crystalline linear PLAs were annealed at 140 or 160 °C in the presence of these catalysts. The consequences of the transesterification reactions in the solid PLAs were studied by means of matrix-assisted laser desorption/ionization (MALDI TOF) mass spectrometry, gel permeation chromatography (GPC) and small-angle X-ray scattering (SAXS). The results indicate that polycondensation and formation of cycles proceed in the solid state via formation of loops on the surface of the crystallites. In summary, five different transesterification reactions are required to explain all results. KW - Polylactide KW - MALDI-TOF MS KW - Crystalinity PY - 2024 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-592934 SN - 1759-9962 VL - 15 IS - 2 SP - 71 EP - 82 PB - RSC Publ. CY - Cambridge AN - OPUS4-59293 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kricheldorf, H. A1 - Weidner, Steffen A1 - Meyer, A. T1 - Syntheses of high molecular mass polyglycolides via ring-opening polymerization with simultaneous polycondensation(ROPPOC) by means of tin and zinc catalysts N2 - Glycolide was polymerized in bulk by means of four different ROPPOC catalysts: tin(II) 2-ethylhexanoate (SnOct2), dibutyltin bis(pentafluoro-phenoxide) (BuSnOPF),zinc biscaproate (ZnCap), and zinc bis(pentafluoro-phenyl sulfide) (ZnSPF). The temperature was varied between 110 and 180°C and the time between 3 h and 7 days. For the few polyglycolides (PGAs) that were soluble extremely high molecular masses were obtained. The MALDI TOF mass spectra had all a low signal-to-noise ration and displayed the peaks of cyclic PGAs with a“saw-tooth pattern ”indicating formation of extended-ring crystallites in the mass range below m/z 2500. The shape of DSC curves varied considerably with catalyst and reaction conditions, whereas the long-distance values measured by SAXS were small and varied little with the polymeriza-tion conditions. KW - MALDI TOF MS KW - Polyglycolide KW - Crystalinity PY - 2024 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-598221 VL - 35 IS - 4 SP - 1 EP - 10 PB - John Wiley & Sons Ltd. AN - OPUS4-59822 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -