TY - JOUR A1 - Schlegel, M.C. A1 - Stroh, Julia A1 - Malaga, K. A1 - Meng, Birgit A1 - Panne, Ulrich A1 - Emmerling, Franziska T1 - Pathway of a damaging mechanism - Analyzing chloride attack by synchrotron based X-ray diffraction JF - Solid state sciences N2 - Typically, the changes of the phase compositions due to the chemical attack are studied in-situ only by chemical analysis or microscopy. In this study, the chloride transport and binding in the cement matrix in different cementitious materials was analyzed by synchrotron based X-ray diffraction (SyXRD) and energy dispersive X-ray spectroscopy (EDX). Sample materials consisting of cement paste were embedded in high concentrated sodium chloride solution over different time spans. Afterwards, the phase and chemical compositions were determined. The high spatial resolution and the information about the chloride distribution offer a detailed view of chloride binding in the cement matrix and allow the conclusions about the degradation mechanisms. The results are discussed related to the influence of different supplementary cementitious materials on the damaging mechanism. KW - Portland cement KW - In-situ KW - X-Ray diffraction KW - EDX KW - Durability KW - Chloride attack PY - 2015 DO - https://doi.org/10.1016/j.solidstatesciences.2015.03.021 SN - 1293-2558 SN - 1873-3085 VL - 44 SP - 45 EP - 54 PB - Elsevier Masson SAS CY - Amsterdam AN - OPUS4-33171 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, Urs A1 - Miccoli, Lorenzo A1 - Malaga, K. T1 - A new grouting material for the repair of cracks in earthen structures T2 - Terra 2012 - 11th International conference on the study and conservation of earthen architecture heritage N2 - Traditional earthen structures of cultural value are often damaged by static or dynamic loads. This is usually manifested by the appearance of cracks. All too often these cracks are insufficiently or inappropriately repaired if at all because of lack of knowledge and/or technology. In particular, the behavior of crack repair by grouting poses a challenge in earthen materials and demands specific requirements for the grouting mortar, such as low water content, good water retention, low shrinkage, etc. If dynamic loads, e.g. induced by earthquakes, are expected, the grouting material requires additional specifications such as a compatible strength and modulus of elasticity as well as good adhesion to the earthen materials. The study presents results from the development of a grouting material based on hydraulic lime mortar suitable for the repair of cracks in a variety of earthen building techniques. The goal was to develop a material also compatible with earthen structures exposed to dynamic load. The grouting mortar was designed to be adaptable in strength properties and at the same time to have sufficient robustness for the use on the construction site. First results show a satisfactory performance of the grout concerning fresh and hardened mortar properties as well as injectability. The study is part of our work in the framework of the ongoing project NIKER, funded by the European Commission dealing with improving imovable Cultural Heritage assets against the risk of earthquakes. T2 - Terra 2012 - 11th International conference on the study and conservation of earthen architecture heritage CY - Lima, Peru DA - 2012-04-22 KW - Cracks KW - Grouting KW - Lime mortar KW - Earthen Structures KW - Cracks repair PY - 2012 SN - 978-9972-2885-5-5 IS - Theme 6 - t6_059 SP - 1 EP - 10 AN - OPUS4-30381 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -