TY - JOUR A1 - Blaeß, Carsten A1 - Müller, Ralf T1 - Sintering and foaming of bioactive glasses N2 - Sintering, crystallization, and foaming of 44.8SiO2–2.5P2O3–36.5CaO–6.6Na2O–6.6K2O–3.0CaF2 (F3) and 54.6SiO2–1.7P2O3–22.1CaO–6.0Na2O–7.9K2O–7.7MgO (13–93) bioactive glass powders milled in isopropanol and CO2 were studied via heating microscopy, differential thermal analysis, vacuum hot extraction (VHE), Infrared spectroscopy, and time-of-flight secondary ion mass spectrometry. Full densification was reached in any case and followed by significant foaming. VHE studies show that foaming is driven by carbon gases and carbonates were detected by Infrared spectroscopy to provide the major foaming source. Carbonates could be detected even after heating to 750◦C, which hints on a thermally very stable species or mechanical trapping. Otherwise, dark gray compact colors for milling in isopropanol indicate the presence of residual carbon as well. Its significant contribution to foaming, however, could not be proved and might be limited by the diffusivity of oxygen needed for carbon oxidation to carbon gas. KW - Bioactive Glass KW - Crystallization KW - Foaming KW - Sintering PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-552454 DO - https://doi.org/10.1111/jace.18626 SN - 0002-7820 SP - 1 EP - 11 PB - Wiley online library AN - OPUS4-55245 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Winkel, A. A1 - Meszaros, R. A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Travitzky, N. A1 - Fey, T. A1 - Greil, P. A1 - Wondraczek, L. T1 - Sintering of 3D-printed glass/HAp composites N2 - We report the sintering of 3D-printed composites of 13-93 bioactive glass and hydroxyapatite (HAp) powders. The sintering process is characterized on conventionally produced powder compacts with varying HAp content. A numeric approximation of the densification kinetics is then obtained on the basis of Frenkel, Mackenzie–Shuttleworth, and Einstein–Roscoe models, and optimized sintering conditions for 3D-printed structures are derived. Fully isotropic sintering of complex cellular composites is obtained by continuous heating to 750°C at a rate of 2 K/min for a HAp content of 40 wt%. The approach can readily be generalized for printing and sintering of similar glass-ceramic composites. KW - Sintering glass composit bio material PY - 2012 DO - https://doi.org/10.1111/j.1551-2916.2012.05368.x SN - 0002-7820 SN - 1551-2916 VL - 95 IS - 11 SP - 3387 EP - 3393 PB - Blackwell Publishing CY - Malden AN - OPUS4-27053 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Eberstein, Markus A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Deubener, J. A1 - Schiller, Wolfgang Arno T1 - Sintering of glass matrix composites with small rigid inclusions KW - Glass ceramics KW - Inclusions KW - Sintering KW - Mixing KW - Powders KW - Solid-state reaction PY - 2009 DO - https://doi.org/10.1016/j.jeurceramsoc.2009.02.007 SN - 0955-2219 SN - 1873-619X VL - 29 IS - 12 SP - 2469 EP - 2479 PB - Elsevier CY - Oxford AN - OPUS4-19570 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schiller, Wolfgang Arno A1 - Müller, Ralf A1 - Eberstein, Markus A1 - Reinsch, Stefan A1 - Rabe, Torsten T1 - Sintering of LTCC N2 - Low Temperature Co-fired Ceramic materials (LTCC) have attracted growing interest in recent years since they are promising candidates for highly integrated ceramic packaging. This paper surveys materials concepts of related glass ceramic composites (GCC) and discusses unsolved problems and challenges. The densification of GCC based on "viscous sintering" may be affected by steric effects and partial dissolution of dispersed crystal particles, crystallization and phase boundary reactions. KW - Sintering KW - Glass ceramic composites KW - Viscosity KW - Densification KW - Modelling PY - 2008 SN - 0173-9913 SN - 0196-6219 VL - 85 IS - 13 SP - 12 EP - 17 PB - Göller CY - Baden-Baden AN - OPUS4-19086 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kiefer, P. A1 - Deubener, J. A1 - Müller, Ralf A1 - Behrens, H. T1 - Statistical analysis of propagation rates of indentation-induced radial cracks N2 - Due to the stochastic nature of crack nucleation by Vickers indentation, a statistical analysis of propagation rates of 185 radial cracks was performed. Crack growth was observed directly using a video camera with high Image acquisition rate. It is found that propagation rates are controlled by the environmental reactions at the crack-tip shortly after their initiation (< 1 s). Calibration of the stress intensity KI showed that the residual stress factor χ and the exponent n of the equation KI==χPc−n (with P==load and c==crack length) are broadly distributed among the 185 analyzed cracks, ranging from 10−16 to 104 and from 0.1 to 5, respectively. For the most frequent crack, the equation KI==0.052Pc−1.47 holds. The results show that correlations of indentation-induced crack length to stress intensity necessitate the use of statistical significant data that are calibrated by the environmental reactions at the crack-tip. KW - Stress intensity factor KW - Vickers indentation KW - Subcritical crack growth KW - Soda-lime-silica glass PY - 2019 DO - https://doi.org/10.1016/j.jnoncrysol.2019.119739 VL - 527 SP - 119739 PB - Elsevier B.V. AN - OPUS4-50393 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Behrens, H. A1 - Bauer, U. A1 - Reinsch, Stefan A1 - Kiefer, P. A1 - Müller, Ralf A1 - Deubener, J. T1 - Structural relaxation mechanisms in hydrous sodium borosilicate glasses N2 - Borosilicate glasses (16Na2O–10B2O3–74SiO2, NBS) with water contents up to 22 mol% H2O were prepared to study the effect of water on structural relaxation using DTA, viscometry and internal friction measurements. The results show that the glass transition temperature Tg of DTA and the isokom temperature T12, of viscometry are in excellent agreement, confirming the equivalence of enthalpy and viscous relaxation for NBS glass. Combining Tg data with water speciation data demonstrates that OH groups are mainly responsible for the decrease of Tg with increasing hydration, while molecular water plays only a minor role. Internal friction spectra at 7.125 Hz confirm the decisive influence of water on mechanical relaxation. The temperature range of α-relaxation (glass transition) strongly decreases while two β-relaxation peaks (sub-Tg) progressively appear with increasing water content. A high temperature β-relaxation peak, attributed to the presence of OH groups, shifts from 670 to 450 K as total water content increases from 0.01 to 5 wt%. A low temperature β-relaxation peak, attributed to molecular water, appears at 380 K and 330 K in glasses containing 3 and 5 wt% H2O, respectively. These findings suggest that relaxation mechanism of different hydrous species at low temperature may contribute to fatigue of stressed glasses. KW - Borosilicate glass KW - Water KW - Relaxation KW - Internal friction KW - Glass transition PY - 2018 DO - https://doi.org/10.1016/j.jnoncrysol.2018.05.025 VL - 497 SP - 30 EP - 39 PB - Elsevier B.V. AN - OPUS4-45608 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Akatsuka, C. A1 - Honma, T. A1 - Müller, Ralf A1 - Reinsch, Stefan A1 - Tanaka, S. A1 - Komatsu, T. T1 - Surface crystallization and gas bubble formation during conventional heat treatment in Na2MnP2O7 glass N2 - The crystallization behavior of sodium ion conductive Na2MnP2O7 glass was examined to clarify the crystallization mechanism. The formation of thermodynamically metastable phase, layered Na2MnP2O7, at the surface of the glass occurred. Heat treatment at 430 °C for 3 h lead to surface crystals of Na2MnP2O7 oriented with the (101) direction perpendicular to the sample surface. As the heat treatment temperature increased, the glass-ceramic samples deformed, and the presence numerous micro bubbles due to dissolved water was detected. KW - Glass-ceramic KW - Crystallization KW - Sodium ion batteries KW - Bubble formation KW - Phosphate PY - 2019 DO - https://doi.org/10.1016/j.jnoncrysol.2019.01.030 VL - 510 SP - 36 EP - 41 PB - Elsevier B.V. AN - OPUS4-49618 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Scheffler, Franziska A1 - Fleck, Mirjam A1 - Busch, Richard A1 - Casado, Santiago A1 - Gnecco, Enrico A1 - Tielemann, Christopher A1 - Brauer, Delia S. A1 - Müller, Ralf T1 - Surface Crystallization of Barium Fresnoite Glass: Annealing Atmosphere, Crystal Morphology and Orientation N2 - Controlled oriented crystallization of glass surfaces is desired for high precision applications, since the uppermost crystal layer significantly influences the properties of the material. In contrast to previous studies, the data presented here deal with separated crystals growing at defect-free surfaces in four atmospheres with different degrees of humidity (ambient/dry air, argon and vacuum). A glass with the composition 2 BaO–TiO2–2.75 SiO2 was heat-treated at 825 °C until fresnoite (Ba2TiSi2O8) grew to a significant size. The crystal growth rate is found to increase with increasing humidity. The morphology of the crystals changes from highly distorted dendrites in the driest atmosphere (vacuum) to circular/spear-head-shaped crystals in the wettest atmosphere (ambient air), which we attribute to a decrease in viscosity of the glass surface due to water uptake. The least distorted crystals appear in the form of depressions of up to 6 µm. This has an influence on the observed crystal orientation, as measured by electron backscatter diffraction (EBSD). The pulled-in crystals change the orientation during growth relative to the flat glass surface due to an enrichment in SiO2 at the crystal fronts. This confirms that the orientation of crystals is not fixed following nucleation. KW - Fresnoite KW - Surface crystallization KW - Crystal growth KW - Crystal morphology KW - Crystal orientation KW - EBSD PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-587230 DO - https://doi.org/10.3390/cryst13030475 VL - 13 IS - 3 SP - 1 EP - 17 PB - MDPI AG CY - Basel AN - OPUS4-58723 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schmelzer, J.W.P. A1 - Potapov, O. V. A1 - Fokin, V. M. A1 - Müller, Ralf A1 - Reinsch, Stefan T1 - The effect of elastic stress and relaxation on crystal nucleation in lithium disilicate glass N2 - In the framework of a general theoretical approach recently developed, the effect of elastic stresses on the rate of nucleation of crystallites of critical sizes in the process of crystallization of lithium disilicate glasses is studied. Hereby both the evolution of elastic stresses – due to changes in the specific volume of the crystallizing system (i.e., differences in the densities of the melt and the crystal) – and their relaxation – connected with viscous flow – are taken into consideration. If the classical theory of nucleation is employed for the determination of the nucleation rates (modified by taking into account elastic stresses), elastic stresses may lead, for the system under consideration, to a decrease of the nucleation rate by up to two orders of magnitude. As shown, the theory allows an at least qualitatively correct incorporation of the effect of elastic stresses and stress relaxation into the description of nucleation phenomena in glass-forming melts. PY - 2004 DO - https://doi.org/10.1016/j.jnoncrysol.2003.10.002 SN - 0022-3093 VL - 333 IS - 2 SP - 150 EP - 160 PB - North-Holland Publ. Co. CY - Amsterdam AN - OPUS4-6236 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Balzer, R. A1 - Behrens, H. A1 - Schuth, S. A1 - Waurischk, Tina A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Fechtelkord, M. A1 - Deubener, J. T1 - The influence of H2O and SiO2 on the structure of silicoborate glasses N2 - To understand the impact of dissolved water on structure and properties, four boron-rich glasses of molar compositions 15-x Na2O x CaO 15 SiO2 70 B2O3 (with x=0, 7.5, 10) and 10 Na2O 15 SiO2 75 B2O3 were prepared and subsequently hydrated (up to 8 wt% H2O). Density measurements show a non-linear trend upon hydration implying large structural changes in particular at water contents<2 wt%. Near-infrared spectroscopy shows hydroxyl groups are the dominant species in all glasses upon the entire range of water content. Molecular H2O is detectable only at total water contents>2 wt%. 11B MAS NMR spectra show that the abundance of BO4 species is mainly controlled by ratio of (Na2O+CaO)/B2O3 while incorporation of water plays a minor role. Compared to borate glasses, the efficiency of formation of BO4 tetrahedra is favored by crosslinking of the network by SiO4-units. The glass transition temperatures, determined by differential thermal analysis, decreases continuously with water content due to breakage of B-O-B bonds by hydrolysis. However, compared to Silicates and aluminosilicates, the effect of dissolved water is less pronounced which can be explained by weaker B-O-B bonds in comparison to Si-O-Si bonds. KW - High pressure KW - Water speciation KW - Silicoborate glasses KW - Infrared spectroscopy KW - NMR spectroscopy PY - 2019 DO - https://doi.org/10.1016/j.jnoncrysol.2019.05.030 VL - 519 SP - 38 EP - 51 PB - Elsevier B.V. AN - OPUS4-48748 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schmelzer, J.W.P. A1 - Müller, Ralf A1 - Möller, J. A1 - Gutzow, I.S. T1 - Theory of nucleation in viscoelastic media: application to phase formation in glassforming melts N2 - Glassforming melts behave, in the vicinity of the temperature of vitrification Tg, as viscoelastic bodies. A general theory of nucleation in a viscoelastic body developed elsewhere is applicable to the description of phase formation processes in such systems. The present contribution is directed to the demonstration of the relevance of this proposed general theory to describing phase transformation processes in glassforming melts. The application of the theory is shown to explain a number of experimental results on crystallization of glassforming melts, which have not found a satisfactory interpretation so far. PY - 2003 DO - https://doi.org/10.1016/S0022-3093(02)01428-X SN - 0022-3093 VL - 315 SP - 144 EP - 160 PB - North-Holland Publ. Co. CY - Amsterdam AN - OPUS4-2078 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ried, Peter A1 - Gaber, Martin A1 - Beyer, Katrin A1 - Müller, Ralf A1 - Kipphardt, Heinrich A1 - Kannengießer, Thomas T1 - Thermo Analytic Investigation of Hydrogen Effusion Behavior - Sensor Evaluation and Calibration N2 - The well established carrier gas analysis (CGA) method was used to test different hydrogen detectors comprising a thermal conductivity detector (TCD) and a metal oxide semiconducting (MOx) sensor. The MOx sensor provides high hydrogen sensitivity and selectivity, whereas the TCD exhibits a much shorter response time and a linear hydrogen concentration dependency. Therefore, the TCD was used for quantitative hydrogen concentration measurements above 50?µmol/mol. The respective calibration was made using N2/H2 gas mixtures. Furthermore, the hydrogen content and degassing behaviour of titanium hydride (TiH2-x) was studied. This material turned out to be a potential candidate for a solid sample calibration. Vacuum hot extraction (VHE) coupled with a mass spectrometer (MS) was then calibrated with TiH2-x as transfer standard. The calibration was applied for the evaluation of the hydrogen content of austenitic steel samples (1.4301) and the comparison of CGA-TCD and VHE-MS. KW - Hydrogen KW - Steel KW - Vacuum hot extraction KW - Carrier gas analysis KW - Titanium hydride KW - Gas calibration PY - 2011 DO - https://doi.org/10.1002/srin.201000237 SN - 1611-3683 SN - 0177-4832 VL - 82 IS - 1 SP - 14 EP - 19 PB - Verl. Stahleisen CY - Düsseldorf AN - OPUS4-23202 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Deubener, J. A1 - Allix, M. A1 - Davis, M.J. A1 - Duran, A. A1 - Höche, T. A1 - Honma, T. A1 - Komatsu, T. A1 - Krüger, S. A1 - Mitra, I. A1 - Müller, Ralf A1 - Nakane, S. A1 - Pascual, M.J. A1 - Schmelzer, J.W. A1 - Zanotto, E.D. A1 - Zhou, S. T1 - Updated definition of glass-ceramics N2 - Glass-ceramics are noted for their unusual combination of properties and manifold commercialized products for consumer and specialized markets. Evolution of novel glass and ceramic processing routes, a plethora of new compositions, and unique exotic nano- and microstructures over the past 60 years led us to review the Definition of glass-ceramics. Well-established and emerging processing methods, such as co-firing, additive manufacturing, and laser patterning are analyzed concerning the core requirements of processing glass-ceramics and the Performance of the final products. In this communication, we propose a revised, updated definition of glass-ceramics, which reads “Glass-ceramics are inorganic, non-metallic materials prepared by controlled crystallization of glasses via different processing methods. They contain at least one type of functional crystalline phase and a residual glass. The volume fraction crystallized may vary from ppm to almost 100%”. KW - Glass-ceramics definition PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-464711 DO - https://doi.org/10.1016/j.jnoncrysol.2018.01.033 SN - 0022-3093 SN - 1873-4812 VL - 501 SP - 3 EP - 10 PB - Elsevier B.V. AN - OPUS4-46471 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Waurischk, Tina A1 - Reinsch, Stefan A1 - Rouxel, T. A1 - Behrens, H. A1 - Deubener, J. A1 - Müller, Ralf T1 - Vacuum crack growth in alkali silicate glasses N2 - Crack growth velocity in alkali silicate glasses was measured in vacuum across 10 orders of magnitude with double cantilever beam technique. Measured and literature crack growth data were compared with calculated intrinsic fracture toughness data obtained from Young´s moduli and the theoretical fracture surface energy estimated from chemical bond energies. Data analysis reveals significant deviations from this intrinsic brittle fracture behavior. These deviations do not follow simple compositional trends. Two opposing processes may explain this finding: a decrease in the apparent fracture surface energy due to stress-induced chemical changes at the crack tip and its increase due to energy dissipation during fracture. KW - Silicate glass KW - Brittle fracture KW - Crack growth KW - Calculated intrinsic fracture toughness PY - 2021 DO - https://doi.org/10.1016/j.jnoncrysol.2021.121094 SN - 0022-3093 VL - 572 SP - 1 EP - 8 PB - Elsevier CY - Amsterdam AN - OPUS4-53144 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Deubener, J. A1 - Bornhöft, H. A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Lumeau, J. A1 - Glebova, L.N. A1 - Glebov, L.B. T1 - Viscosity, relaxation and elastic properties of photo-thermo-refractive glass KW - Ultrasonic relaxation KW - Silicates KW - Rheology KW - Structural relaxation KW - Viscosity PY - 2009 DO - https://doi.org/10.1016/j.noncrysol.2008.10.002 SN - 0022-3093 VL - 355 SP - 126 EP - 131 PB - North-Holland Publ. Co. CY - Amsterdam AN - OPUS4-18671 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Blaeß, Carsten A1 - Müller, Ralf T1 - Viscous healing of Vickers indentation–induced cracks in glass N2 - AbstractViscous healing of cracks induced by the Vickers indentation in a soda lime magnesium silicate, a soda borosilicate, and a soda aluminosilicate glass (NAS) was studied by laser scanning microscopy. Plots of the crack length, width, and depth normalized to the initial crack length versus time over viscosity merge into single master curves of each of these quantities for each glass. Despite glass properties do not differ strikingly from each other, however, these master curves strongly differ among the glasses. This finding was attributed to a different interplay of various crack healing phenomena. Lateral cracks were found to be responsible for the bulging of the sample surface around the Vickers imprint, which in turn promotes radial crack widening as the main cause of healing delay. The most rapid healing of lateral cracks was observed in NAS in which bulging and crack widening were least pronounced. KW - Crack healing KW - Glass KW - Vickers indentation PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-587295 DO - https://doi.org/10.1111/jace.19245 SN - 0002-7820 VL - 106 IS - 10 SP - 5795 EP - 5805 PB - Wiley AN - OPUS4-58729 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Deubener, Joachim A1 - Müller, Ralf A1 - Behrens, H. A1 - Heide, G. T1 - Water and the glass transition temperature of silicate melts N2 - Literature data on the effect of water on the glass transition in silicate melts are gathered for a broad range of total water content cw from 3 × 10-4 to 27 wt%. In terms of a reduced glass transition temperature Tg*=Tg/TgGN, where TgGN is Tg of the melt containing cw?0.02 wt% total water, a uniform dependence of Tg* on total water content (cw) is evident for silicate melts. Tg* decreases steadily with increasing water content, most strongly at the lowest water content where H2O is dominantly dissolved as OH. For water-rich melts, the variation of Tg* is less pronounced, but it does not vanish even at the largest water contents reported (?27 wt%). Tg* vs. cw is fitted by a three-component model. This approach accounts for different transition temperatures of the dry glass, hydroxyl and molecular water predicting Tg* as a weighted linear combination of these temperatures. The required but mostly unknown water speciation in the glasses was estimated using IR-spectroscopy data for hydrous sodium trisilicate and rhyolite. PY - 2003 DO - https://doi.org/10.1016/S0022-3093(03)00472-1 SN - 0022-3093 VL - 330 SP - 268 EP - 273 PB - North-Holland Publ. Co. CY - Amsterdam AN - OPUS4-3120 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Balzer, R. A1 - Behrens, H. A1 - Waurischk, Tina A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Kiefer, P. A1 - Deubener, J. A1 - Fechtelkord, M. T1 - Water in Alkali Aluminosilicate Glasses N2 - To understand the influence of water and alkalis on aluminosilicate glasses, three polymerized glasses with varying ratios of Na/K were synthesized [(22. 5-x)Na2O-xK2O-22.5 Al2O3-55 SiO2 with x = 0, 7.5, and 11.25]. Subsequently, these glasses were hydrated (up to 8 wt% H2O) in an internally heated gas pressure vessel. The density of hydrous glasses linearly decreased with water content above 1 wt%, consistent with the partial molar volume of H2O of 12 cm3/mol. Near-infrared spectroscopy revealed that hydroxyl groups are the dominant species at water content of <4 wt%, and molecular water becomes dominating at water content of >5 wt%. The fraction of OH is particularly high in the pure Na-bearing glass compared to the mixed alkali glasses. 27Al magic angle spinning-NMR spectroscopy shows that aluminum is exclusively fourfold coordinated with some variations in the local geometry. It appears that the local structure around Al becomes more ordered with increasing K/Na ratio. The incorporation of H2O reinforces this effect. The differential thermal analysis of hydrous glasses shows a significant mass loss in the range of glass transition already during the first upscan, implying the high mobility of water in the glasses. This observation can be explained by the open structure of the aluminosilicate network and by the low dissociation enthalpy of H2O in the glasses (≈ 8 kJ/mol). The effect of the dissolved H2O on the glass transition temperature is less pronounced than for other aluminosilicate glasses, probably because of the large fraction of Al in the glasses. KW - NMR spectroscopy KW - Alkali aluminosilicate glasses KW - Water speciation KW - Glass transition KW - Infrared spectroscopy PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-509497 DO - https://doi.org/10.3389/fmats.2020.00085 VL - 7 SP - 85 AN - OPUS4-50949 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Ralf A1 - Gaber, Martin A1 - Gottschling, Peter T1 - Water release and crystallisation of glass powders T2 - Physics and Chemistry of Glasses / VII Symposium on Crystallization in Glasses in Liquids CY - Sheffield, England, UK DA - 2004-07-06 PY - 2004 SN - 1753-3562 SN - 0017-1050 SN - 0031-9090 SN - 1750-6697 VL - 45 IS - 2 SP - 1 EP - 5 PB - Society of Glass Technology CY - Sheffield AN - OPUS4-6237 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Reinsch, Stefan A1 - Rössler, C. A1 - Bauer, Ute A1 - Müller, Ralf A1 - Deubener, J. A1 - Behrens, H. T1 - Water, the other network modifier in borate glasses N2 - In the present study we have investigated whether the effect of water on properties of borate glasses resembles that of alkali oxide. Soda-lime-borate glasses with nominal compositions of x Na2O, 10 CaO, (90-x) B2O3 (x = 5, 15 and 25 mol%) were doped with up to 8 wt.% H2O by processing glass powder + distilled water in platinum capsules in an internally heated gas pressure vessel at 1523 K and 500 MPa. The water content of hydrous glasses was determined by Karl-Fischer titration and near-infrared spectroscopy. The glass transition temperature T-g. was derived from DTA and micropenetration experiments for which the effect of water loss at the surface of the hydrous glasses was studied. Heating glass samples at 10 K min(-1) in the DTA resulted in T-g values which are close to T-12 isokom temperatures confirming the equivalence of enthalpy relaxation and viscous relaxation for borate glasses. For all three glass series it is shown that T-g strongly decreases whereas the liquid fragility strongly increases upon the addition of water. These findings reveal that H2O primarily causes breaking of B-O-B bonds rather than supporting 4-fold coordinated boron as it is well-known for alkali oxides in this concentration range. (C) 2015 Elsevier B.V. All rights reserved. KW - Wasserhaltige Gläser KW - Viskosität KW - Boratgläser KW - Thermische Analyse KW - Viscosity KW - Borate glasses KW - Thermal analysis KW - Water-bearing glasses PY - 2016 DO - https://doi.org/10.1016/j.jnoncrysol.2015.10.010 SN - 0022-3093 VL - 432 SP - 208 EP - 217 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-35123 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -