TY - JOUR A1 - Dümichen, Erik A1 - Braun, Ulrike A1 - Kraemer, R. A1 - Deglmann, P. A1 - Senz, R. T1 - Thermal extraction combined with thermal desorption: A powerful tool to investigate the thermo-oxidative degradation of polyamide 66 materials N2 - Using thermogravimetric analysis (TGA) with a solid-phase adsorber for thermal extraction, followed by subsequently analysing the adsorber with thermo-desorption gas chromatography mass spectrometry (TDS-GC–MS) enables measurement of polymer degradation under oxidizing atmosphere, and the identification of certain complex hydrocarbon degradation products by chromatographic separation and defined mass patterns. This technique, thermal-extraction desorption gas chromatography mass spectrometry (TED-GC–MS) was used to investigate the thermo-oxidative degradation of PA 66 and PA 66 doped with 2 wt% of metal oxide particles. In TGA pure PA 66 formed more residue under an oxidizing atmosphere than an inert one. In contrast to the measurements under inert atmosphere, several condensed aromatic species containing nitrogen could be identified in thermo-oxidative measurements. These degradation products were formed through condensation reactions of primary amides originating from imide hydrolysis. The formation of such highly condensed species also causes higher char formation. Four metal oxides have shown an impact on the thermo-oxidative degradation of PA 66: Fe2O3 on η-Al2O3 < pure Fe2O3 = Fe2O3 on γ-Al2O3 < pure ZnO. For ZnO even a char-stabilizing effect could be observed. A catalytic effect of these metal oxides causes more condensed cyclopentanone and pyridine derivates. Thus, more water is formed and released, resulting in increased hydrolysis of the imides and degradation at lower temperatures. KW - PA 66 KW - Metal oxide particles KW - Thermo-oxidation KW - Thermogravimetry KW - Solid-phase extraction PY - 2015 U6 - https://doi.org/10.1016/j.jaap.2015.08.006 SN - 0165-2370 SN - 1873-250X VL - 115 SP - 288 EP - 298 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-34338 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Dümichen, Erik A1 - Braun, Ulrike A1 - Sturm, Heinz A1 - Kraemer, R. A1 - Deglmann, P. A1 - Gaan, S. A1 - Senz, R. T1 - A new molecular understanding of the thermal degradation of PA 66 doped with metal oxides: Experiment and computation N2 - The thermal molecular degradation of polyamide 66 (PA 66) doped with (partially supported) metal oxide particles (Fe2O3, ZnO, Al2O3) was investigated qualitatively and quantitatively using common analysis techniques like thermogravimetry coupled with IR-spectroscopic evolved gas analysis (TGA-FTIR). Using pyrolysis coupled with gas chromatography mass spectrometry (Py-GC-MS), qualitative conclusions were drawn about the complex hydrocarbon products. However, the combination of TGA with solid-phase extraction, followed by thermal desorption gas chromatography mass spectrometry (TED-GC-MS), allows qualitative and even semi-quantitative conclusions about the decomposition pathway of PA 66 in the presence of various metal oxide particles. The investigations under inert conditions showed that the presence of metal particles increases the rate of decarboxylation and deamination reactions, as well as the formation rate of cyclopentanone and pyridine derivatives. These species are a consequence of various condensation reactions. The condensation reactions release a large amount of water, thus triggering the hydrolysis of PA 66. Molecular thermal degradation mechanisms were developed for the main decomposition as well as for the condensation reactions and supported by quantum chemical calculations. The catalytic effect of the metal oxides in PA 66 increases in the following order: PA 66 = PA 66 – Al2O3 < PA 66 – Fe2O3 < PA 66 – ZnO. KW - PA 66 KW - Metal oxide particles KW - Thermal degradation KW - Solid-phase extraction KW - Molecular modeling PY - 2015 U6 - https://doi.org/10.1016/j.polymdegradstab.2015.07.011 SN - 0141-3910 SN - 1873-2321 VL - 120 SP - 340 EP - 356 PB - Elsevier Ltd. CY - London AN - OPUS4-33806 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -