TY - JOUR A1 - Voss, Heike A1 - Knigge, Xenia A1 - Knapic, D. A1 - Weise, Matthias A1 - Sahre, Mario A1 - Hertwig, Andreas A1 - Sacco, A. A1 - Rossi, A. M. A1 - Radnik, Jörg A1 - Müller, Kai A1 - Wasmuth, Karsten A1 - Krüger, Jörg A1 - Hassel, A. W. A1 - Hodoroaba, Vasile-Dan A1 - Bonse, Jörn T1 - Picosecond laser processing of hierarchical micro–nanostructures on titanium alloy upon pre- and postanodization: morphological, structural, and chemical effects N2 - Recent publications indicate that the order of electrochemical anodization (before or after the laser processing step) plays an important role for the response of bone-forming osteoblasts—an effect that can be utilized for improving permanent dental or removable bone implants. For exploring these different surface functionalities, multimethod morphological, structural, and chemical characterizations are performed in combination with electrochemical pre- and postanodization for two different characteristic microspikes covered by nanometric laser-induced periodic surface structures on Ti–6Al–4V upon irradiation with near-infrared ps-laser pulses (1030 nm wavelength, ≈1 ps pulse duration, 67 and 80 kHz pulse repetition frequency) at two distinct sets of laser fluence and beam scanning parameters. This work involves morphological and topographical investigations by scanning electron microscopy and white light interference microscopy, structural material examinations via X-ray diffraction, and micro-Raman spectroscopy, as well as near-surface chemical analyses by X-ray photoelectron spectroscopy and hard X-ray photoelectron spectroscopy. The results allow to qualify the mean laser ablation depth, assess the spike geometry and surface roughness parameters, and provide new detailed insights into the near-surface oxidation that may affect the different cell growth behavior for pre- or postanodized medical implants. T2 - 2023 E-MRS Spring Meeting, Symposium L "Making light matter: lasers in material sciences and photonics" CY - Strasbourg, France DA - 29.05.2023 KW - Hierarchical micro-nanostructures KW - Laser-induced periodic surface structures (LIPSS) KW - Ultrashort laser pulses KW - Ti-6Al-4V alloy KW - X-ray photoelectron spectroscopy PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-601962 DO - https://doi.org/10.1002/pssa.202300920 SN - 1862-6319 SP - 1 EP - 11 PB - Wiley-VCH GmbH CY - Weinheim AN - OPUS4-60196 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - v. Woedtke, T. A1 - Abel, P. A1 - Krüger, Jörg A1 - Kautek, Wolfgang T1 - Subpicosecond-pulse laser microstructuring for enhanced reproducibility of biosensors N2 - Curved substrates can be micro-structured by laser ablation, which is not possible with standard lithographic methods. The novel femtosecond-pulse laser technique allows the production of defined and reproducible micro-perforations of originally analyte-impermeable membranes. The trans-membrane analyte flux can be controlled both by the variation of the laser focus diameter resulting in different areas of single perforations, and the number of perforations in arrays on small membrane areas. This leads to a higher degree of variability as well as reproducibility of the diffusion qualities of sensor membranes, and marks the main innovation with this technique compared to the hand-made mechanical perforation by specially grinded needles used up to now. Touchless micro-perforation of small membrane areas with negligible heat damage of the structures adjacent to the perforation allows the application of ‘analyte door’ membranes directly onto curved surfaces of miniaturized needle-sensors assigned for in vivo glucose monitoring, for the first time. KW - Biosensor KW - Glucose KW - Membrane perforation KW - Subpicosecond laser ablation KW - Reproducibility PY - 1997 DO - https://doi.org/10.1016/S0925-4005(97)80330-9 SN - 0925-4005 SN - 1873-3077 VL - 42 IS - 3 SP - 151 EP - 156 PB - Elsevier CY - Amsterdam [u.a.] AN - OPUS4-11513 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Urech, L. A1 - Lippert, T. A1 - Wokaun, A. A1 - Martin, Sven A1 - Mädebach, Heinrich A1 - Krüger, Jörg T1 - Removal of doped poly(methylmetacrylate) from tungsten and titanium substrates by femto- and nanosecond laser cleaning N2 - The influence of different laser pulse lengths on the removal of a polymer layer from metal substrates was investigated. As model systems, doped poly(methylmetacrylate) (PMMA) on titanium and tungsten substrates were selected. The ablation threshold and irradiation spot morphology of titanium and tungsten were compared for femtosecond (fs) and nanosecond (ns) laser irradiation and different pulse numbers. Nanosecond laser treatment resulted in a non-homogeneous surface morphology for both titanium and tungsten substrates. Femtosecond irradiation of tungsten revealed a homogeneous ablation spot with little changes in the surface morphology. For titanium, the formation of columnar structures within the irradiation spot was observed. Two different dopant concentrations were used for PMMA to achieve an equal linear absorption coefficient for the femto- and nanosecond laser wavelengths of 790 and 1064 nm. The best results were achieved for the removal of doped PMMA by femtosecond laser irradiation, where only a minimal modification of the metal surface was detected. In the case of nanosecond laser exposure, a pronounced change of the structure was observed, suggesting that damage-free cleaning of the selected metal may only be possible using femtosecond laser pulses. Different experimental parameters, such as laser fluence, pulse repetition rate and sample speed were also investigated to optimize the cleaning quality of doped PMMA from tungsten substrates with femtosecond laser pulses. KW - Poly(methylmetacrylate) KW - Laser treatment KW - Tungsten KW - Titanium KW - Femtosecond PY - 2006 DO - https://doi.org/10.1016/j.apsusc.2005.07.109 SN - 0169-4332 SN - 1873-5584 VL - 252 IS - 13 SP - 4754 EP - 4758 PB - North-Holland CY - Amsterdam AN - OPUS4-12368 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Tsibidis, G. D. A1 - Mimidis, A. A1 - Skoulas, E. A1 - Kirner, Sabrina V. A1 - Krüger, Jörg A1 - Bonse, Jörn A1 - Stratakis, E. T1 - Modelling periodic structure formation on 100Cr6 steel after irradiation with femtosecond-pulsed laser beams N2 - We investigate the periodic structure formation upon intense femtosecond pulsed irradiation of chrome steel (100Cr6) for linearly polarised laser beams. The underlying physical mechanism of the laser-induced periodic structures is explored, their spatial frequency is calculated and theoretical results are compared with experimental observations. The proposed theoretical model comprises estimations of electron excitation, heat transfer, relaxation processes, and hydrodynamics-related mass transport. Simulations describe the sequential formation of sub-wavelength ripples and supra-wavelength grooves. In addition, the influence of the laser wavelength on the periodicity of the structures is discussed. The proposed theoretical investigation offers a systematic methodology towards laser processing of steel surfaces with important applications. KW - Laser-induced periodic surface structures KW - Femtosecond laser ablation KW - Steel PY - 2018 UR - https://link.springer.com/article/10.1007/s00339-017-1443-y DO - https://doi.org/10.1007/s00339-017-1443-y SN - 0947-8396 SN - 1432-0630 VL - 124 IS - 1 SP - 27, 1 EP - 13 PB - Springer-Verlag AN - OPUS4-43626 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Symietz, Christian A1 - Lehmann, Erhard A1 - Gildenhaar, Renate A1 - Krüger, Jörg A1 - Berger, Georg T1 - Femtosecond laser induced fixation of calcium alkali phosphate ceramics on titanium alloy bone implant material N2 - Femtosecond lasers provide a novel method of attaching bioceramic material to a titanium alloy, thereby improving the quality of bone implants. The ultrashort 30 fs laser pulses (790 nm wavelength) penetrate a thin dip-coated layer of fine ceramic powder, while simultaneously melting a surface layer of the underlying metal. The specific adjustment of the laser parameters (pulse energy and number of pulses per spot) avoids unnecessary melting of the bioactive calcium phosphate, and permits a defined thin surface melting of the metal, which in turn is not heated throughout, and therefore maintains its mechanical stability. It is essential to choose laser energy densities that correspond to the interval between the ablation fluences of both materials involved: about 0.1-0.4 J cm-2. In this work, we present the first results of this unusual technique, including laser ablation studies, scanning electron microscopy and optical microscope images, combined with EDX data. KW - Bone implant KW - Bioceramic coating KW - Titanium KW - Calcium phosphate KW - Femtosecond laser PY - 2010 DO - https://doi.org/10.1016/j.actbio.2010.02.016 SN - 1742-7061 VL - 6 IS - 8 SP - 3318 EP - 3324 PB - Elsevier CY - Amsterdam AN - OPUS4-21446 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Symietz, Christian A1 - Lehmann, Erhard A1 - Gildenhaar, Renate A1 - Koter, Robert A1 - Berger, Georg A1 - Krüger, Jörg T1 - Fixation of bioactive calcium alkali phosphate on Ti6Al4V implant material with femtosecond laser pulses N2 - Bone implants made of metal, often titanium or the titanium alloy Ti6Al4V, need to be surface treated to become bioactive. This enables the formation of a firm and durable connection of the prosthesis with the living bone. We present a new method to uniformly cover Ti6Al4V with a thin layer of ceramics that imitates bone material. These calcium alkali phosphates, called GB14 and Ca10, are applied to the metal by dip coating of metal plates into an aqueous slurry containing the fine ceramic powder. The dried samples are illuminated with the 790 nm radiation of a pulsed femtosecond laser. If the laser fluence is set to a value just below the ablation threshold of the ceramic (ca. 0.4 J/cm²) the 30 fs laser pulses penetrate the partly transparent ceramic layer of 20–40 µm thickness. The remaining laser fluence at the ceramic–metal interface is still high enough to generate a thin metal melt layer leading to the ceramic fixation on the metal. The laser processing step is only possible because Ti6Al4V has a lower ablation threshold (between 0.1 and 0.15 J/cm²) than the ceramic material. After laser treatment in a fluence range between 0.1 and 0.4 J/cm², only the particles in contact with the metal withstand a post-laser treatment (ultrasonic cleaning). The non-irradiated rest of the layer is washed off. In this work, we present results of a successful ceramic fixation extending over larger areas. This is fundamental for future applications of arbitrarily shaped implants. KW - Bone implant KW - Bioceramic coating KW - Titanium KW - Calcium phosphate KW - Femtosecond laser PY - 2011 DO - https://doi.org/10.1016/j.apsusc.2010.10.046 SN - 0169-4332 SN - 1873-5584 VL - 257 IS - 12 SP - 5208 EP - 5212 PB - North-Holland CY - Amsterdam AN - OPUS4-23310 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Symietz, Christian A1 - Lehmann, Erhard A1 - Gildenhaar, Renate A1 - Hackbarth, Andreas A1 - Berger, Georg A1 - Krüger, Jörg T1 - Mechanical stability of Ti6Al4V implant material after femtosecond laser irradiation N2 - The surface of a titanium alloy (Ti6Al4V) implant material was covered with a bioactive calcium alkali phosphate ceramic with the aim to accelerate the healing and to form a stronger bond to living bone tissue. To fix the ceramic powder we used a femtosecond laser, which causes a thin surface melting of the metal. It is a requirement to prove that the laser irradiation would not reduce the lifetime of implants. Here we present the results of mechanical stability tests, determined by the rotating bending fatigue strength of sample rods. After describing the sample surfaces and their modifications caused by the laser treatment we give evidence for an unchanged mechanical stability. This applies not only to the ceramic fixation but also to a comparatively strong laser ablation. KW - Aluminium alloys KW - Bending strength KW - Bioceramics KW - Bone KW - Calcium compounds KW - Fatigue KW - Fatigue testing KW - High-speed optical techniques KW - Laser ablation KW - Melting KW - Orthopaedics KW - Prosthetics KW - Rods (structures) KW - Surface treatment KW - Titanium alloys KW - Vanadium alloys PY - 2012 DO - https://doi.org/10.1063/1.4737576 SN - 0021-8979 SN - 1089-7550 VL - 112 IS - 2 SP - 023103-1 - 023103-5 PB - American Institute of Physics CY - Melville, NY AN - OPUS4-26200 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Symietz, Christian A1 - Krüger, Jörg ED - Vilar, Rui T1 - Stability of laser surface modified implants N2 - A new technique to fix bioceramic powder on a titanium alloy by using femtosecond laser pulses is presented. It is shown that gentle fixation of a bioactive dielectric material on a metallic model implant is successful. This is potentially a new tool for the improvement of bone prostheses. An advantage of the ultrashort pulses is the very low heat influx into the whole sample. There is only a very thin interaction zone during the fixing, which is the metal surface in contact with the ceramic layer. Neither the fixed ceramic particles nor the major part of the metal suffer any modification. The stability of the model implant (ceramic on metal) is investigated by rotating bending fatigue tests. No indication of a reduction of the mechanical stability compared to untreated metallic reference samples was found. KW - Bone implant KW - Calcium phosphate coating KW - Femtosecond laser KW - Laser-induced fixation KW - Titanium alloy PY - 2016 SN - 978-0-08-100883-6 SN - 978-0-08-100942-0 DO - https://doi.org/10.1016/B978-0-08-100883-6.00004-6 SN - 2049-9485 IS - 111 SP - Chapter 4, 127 EP - 143 PB - Elsevier ET - 1st edition AN - OPUS4-36790 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Stratakis, E. A1 - Bonse, Jörn A1 - Heitz, J. A1 - Siegel, J. A1 - Tsibidis, G.D. A1 - Skoulas, E. A1 - Papadopoulos, A. A1 - Mimidis, A. A1 - Joel, A.-C. A1 - Comanns, P. A1 - Krüger, Jörg A1 - Florian, C. A1 - Fuentes-Edfuf, Y. A1 - Solis, J. A1 - Baumgartner, W. T1 - Laser engineering of biomimetic surfaces N2 - The exciting properties of micro- and nano-patterned surfaces found in natural species hide a virtually endless potential of technological ideas, opening new opportunities for innovation and exploitation in materials science and engineering. Due to the diversity of biomimetic surface functionalities, inspirations from natural surfaces are interesting for a broad range of applications in engineering, including phenomena of adhesion, friction, wear, lubrication, wetting phenomena, self-cleaning, antifouling, antibacterial phenomena, thermoregulation and optics. Lasers are increasingly proving to be promising tools for the precise and controlled structuring of materials at micro- and nano-scales. When ultrashort-pulsed lasers are used, the optimal interplay between laser and material parameters enables structuring down to the nanometer scale. Besides this, a unique aspect of laser processing technology is the possibility for material modifications at multiple (hierarchical) length scales, leading to the complex biomimetic micro- and nano-scale patterns, while adding a new dimension to structure optimization. This article reviews the current state of the art of laser processing methodologies, which are being used for the fabrication of bioinspired artificial surfaces to realize extraordinary wetting, optical, mechanical, and biological-active properties for numerous applications. The innovative aspect of laser functionalized biomimetic surfaces for a wide variety of current and future applications is particularly demonstrated and discussed. The article concludes with illustrating the wealth of arising possibilities and the number of new laser micro/nano fabrication approaches for obtaining complex high-resolution features, which prescribe a future where control of structures and subsequent functionalities are beyond our current imagination. KW - Biomimetic surfaces KW - Laser processing KW - Surface functionalization KW - Bioinspiration KW - Bionic materials PY - 2020 DO - https://doi.org/10.1016/j.mser.2020.100562 SN - 0927-796X VL - 141 SP - 100562-1 EP - 100562-47 PB - Elsevier B.V. AN - OPUS4-50927 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Stolzenberg, U. A1 - Schmitt Rahner, M. A1 - Pullner, B. A1 - Legall, Herbert A1 - Bonse, Jörn A1 - Kluge, M. A1 - Ortner, A. A1 - Hoppe, B. A1 - Krüger, Jörg T1 - X-ray emission hazards from ultrashort pulsed laser material processing in an industrial setting N2 - Interactions between ultrashort laser pulses with intensities larger than 10^13 W/cm^2 and solids during material processing can lead to the emission of X-rays with photon energies above 5 keV, causing radiation hazards to operators. A framework for inspecting X-ray emission hazards during laser material processing has yet to be developed. One requirement for conducting radiation protection inspections is using a reference scenario, i.e., laser settings and process parameters that will lead to an almost constant and high level of X-ray emissions. To study the feasibility of setting up a reference scenario in practice, ambient dose rates and photon energies were measured using traceable measurement equipment in an industrial setting at SCHOTT AG. Ultrashort pulsed (USP) lasers with a maximum average power of 220 W provided the opportunity to measure X-ray emissions at laser peak intensities of up to 3.3 × 10^15 W/cm^2 at pulse durations of ~1 ps. The results indicate that increasing the laser peak intensity is insufficient to generate high dose rates. The investigations were affected by various constraints which prevented measuring high ambient dose rates. In this work, a list of issues which may be encountered when performing measurements at USP-laser machines in industrial settings is identified. KW - X-ray emission hazards KW - Ultrashort pulsed laser KW - Radiation protection KW - Industrial applications KW - Protection housing PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-538632 DO - https://doi.org/10.3390/ma14237163 SN - 1996-1944 VL - 14 SP - 1 EP - 17 PB - MDPI CY - Basel AN - OPUS4-53863 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schwibbert, Karin A1 - Richter, Anja M. A1 - Krüger, Jörg A1 - Bonse, Jörn T1 - Laser-Textured Surfaces: A Way to Control Biofilm Formation? N2 - Bacterial biofilms pose serious problems in medical and industrial settings. One of the major societal challenges lies in the increasing resistance of bacteria against biocides used in antimicrobial treatments, e.g., via overabundant use in medicine, industry, and agriculture or cleaning and disinfection in private households. Hence, new efficient bacteria-repellent strategies avoiding the use of biocides are strongly desired. One promising route to achieve bacteria-repellent surfaces lies in the contactless and aseptic large-area laser-processing of technical surfaces. Tailored surface textures, enabled by different laser-processing strategies that result in topographic scales ranging from nanometers to micrometers may provide a solution to this challenge. This article presents a current state-of-the-art review of laser-surface subtractive texturing approaches for controlling the biofilm formation for different bacterial strains and in different environments. Based on specific properties of bacteria and laser-processed surfaces, the challenges of anti-microbial surface designs are discussed, and future directions will be outlined. KW - Antibacterial surfaces KW - Biofilms KW - Laser processing KW - Laser-induced periodic surface structures (LIPSS) KW - Microbial adhesions PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-588260 DO - https://doi.org/10.1002/lpor.202300753 SN - 1863-8899 SP - 1 EP - 41 PB - Wiley-VCH GmbH CY - Weinheim AN - OPUS4-58826 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schwibbert, Karin A1 - Menzel, F. A1 - Epperlein, N. A1 - Bonse, Jörn A1 - Krüger, Jörg T1 - Bacterial adhesion on femtosecond laser-modified polyethylene N2 - In this study, femtosecond laser-induced sub-micrometer structures are generated to modify polyethylene (PE) surface topographies. These surfaces were subjected to bacterial colonization studies with Escherichia coli and Staphylococcus aureus as test strains. The results reveal that the nanostructures do not influence S. aureus coverage, while the adhesion of E. coli is reduced. KW - Bacterial adhesion KW - Laser-modified surface KW - Polyethylene KW - Laser-induced nanostructures KW - Biofilm PY - 2019 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-492280 DO - https://doi.org/10.3390/ma12193107 VL - 12 IS - 19 SP - 3107 PB - MDPI CY - Basel, Schweiz AN - OPUS4-49228 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schmidt, Birgit Angelika A1 - Ziemann, M. A A1 - Pentzien, Simone A1 - Gabsch, T. A1 - Koch, W. A1 - Krüger, Jörg T1 - Technical analysis of a Central Asian wall painting detached from a Buddhist cave temple on the northern Silk Road N2 - A great number of Central Asian wall paintings, archeological materials, architectural fragments, and textiles, as well as painting fragments on silk and paper, make up the so called Turfan Collection at the Asian Art Museum in Berlin. The largest part of the collection comes from the Kucha region, a very important cultural center in the third to ninth centuries. Between 1902 and 1914, four German expeditions traveled along the northern Silk Road. During these expeditions, wall paintings were detached from their original settings in Buddhist cave complexes. This paper reports a technical study of a wall painting, existing in eight fragments, from the Buddhist cave no. 40 (Ritterhöhle). Its original painted surface is soot blackened and largely illegible. Grünwedel, leader of the first and third expeditions, described the almost complete destruction of the rediscovered temple complex and evidence of fire damage. The aim of this case study is to identify the materials used for the wall paintings. Furthermore, soot deposits as well as materials from conservation interventions were of interest. Non-invasive analyses were preferred but a limited number of samples were taken to provide more precise information on the painting technique. By employing optical and scanning electron microscopy, energy dispersive X-ray spectroscopy, micro X-ray fluorescence spectroscopy, X-ray diffraction analysis, and Raman spectroscopy, a layer sequence of earthen render, a ground layer made of gypsum, and a paint layer containing a variety of inorganic pigments were identified. KW - Wall paintings KW - Central Asia KW - Silk Road KW - Pigments KW - Microscopy PY - 2016 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-357297 DO - https://doi.org/10.1179/2047058414Y.0000000152 VL - 61 IS - 2 SP - 113 EP - 122 PB - Routledge Taylor & Francis Group CY - London AN - OPUS4-35729 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schmidt, Birgit Angelika A1 - Pentzien, Simone A1 - Conradi, Andrea A1 - Krüger, Jörg T1 - Femtosecond and nanosecond laser decontaminations of biocidal-loaded wooden artworks N2 - Until the end of the 1980s many wooden artworks underwent surface treatment by liquid preservatives, e.g. Hylotox-59. DDT (dichlorodiphenyltrichloroethane) crystal structures are formed on the wooden surfaces by the "blooming" of chlorine compounds by time. In addition to an aesthetic disturbance, it is assumed that DDT represents a health risk. Therefore, the removal of DDT crystals from the surfaces is requested. Contaminated wood with natural biocide ageing, gilded and wood carved elements and wooden samples with paint layers were provided by the Schlossmuseum Sondershausen, Germany. Laser cleaning on selected surface areas on the objects was done by means of femtosecond and nanosecond laser pulses. For the same object, cleaning results using 30-fs laser pulses at 800 nm wavelength are compared to findings utilizing 10-ns laser pulses at 1064 nm wavelength. Before and after laser treatment, chlorine measurements at the same surface position were done by X-ray fluorescence analysis (XRF) as an indicator for the presence of DDT. In this way, pointwise chlorine depletion rates can be obtained for the different pulse duration regimes and wavelengths. Additionally, the object surfaces were examined using optical microscopy and multi spectral imaging analysis. T2 - EMRS Spring Meeting 2017, Symposium X “New frontiers in laser interaction: from hard coatings to smart materials" CY - Strasbourg, France DA - 22.05.2017 KW - Laser cleaning KW - Decontamination KW - Wood KW - DDT KW - Femtosecond laser PY - 2017 DO - https://doi.org/10.1007/s00339-017-1316-4 SN - 0947-8396 SN - 1432-0630 VL - 123 IS - 11 SP - Article 696, 1 EP - 9 PB - Springer AN - OPUS4-42564 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schmid, M. A1 - Heidmann, B. A1 - Ringleb, F. A1 - Eylers, K. A1 - Ernst, O. A1 - Andree, Stefan A1 - Bonse, Jörn A1 - Boeck, T. A1 - Krüger, Jörg T1 - Locally grown Cu(In,Ga)Se2 micro islands for concentrator solar cells N2 - Light concentration opens up the path to enhanced material efficiency of solar cells via increased conversion efficiency and decreased material requirement. For true material saving, a fabrication method allowing local growth of high quality absorber material is essential. We present two scalable fs-laser based approaches for bottom-up growth of Cu(In,Ga)Se2 micro islands utilizing either site-controlled assembly of In(,Ga) droplets on laser-patterned substrates during physical vapor deposition, or laser-induced forward transfer of (Cu,In,Ga) layers for local precursor arrangement. The Cu(In,Ga)Se2 absorbers formed after selenization can deliver working solar devices showing efficiency enhancement under light concentration. T2 - SPIE OPTO, 2018 CY - San Francisco, USA DA - 29.01.2018 KW - Chalcopyrite KW - Cu(In,Ga)Se2 KW - Fs-laser patterning KW - Laser-induced forward transfer KW - Micro solar cell PY - 2018 SN - 978-1-5106-1540-3 SN - 0277-786X SN - 1996-756X VL - 10527 SP - 1052707-1 EP - 1052707-9 PB - SPIE CY - Bellingham, WA, USA AN - OPUS4-44450 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rudolph, Pascale A1 - Bonse, Jörn A1 - Krüger, Jörg A1 - Kautek, Wolfgang T1 - Femtosecond- and nanosecond-pulse laser ablation of bariumalumoborosilicate glass N2 - Laser ablation with femtosecond pulses (130 fs, wavelength 800 nm, repetition rate 2 Hz) was compared with nanosecond-pulse ablation (10 ns, wavelength 266 nm, repetition rate 2.5 Hz) of bariumalumoborosilicate glass in air using the direct focusing technique. Different ablation thresholds and heat-affected zones were observed. The lateral and vertical machining precision was evaluated. Single nanosecond laser pulses in the far UV resulted in a bubble or a circular hole in the centre of the illuminated spot, depending on the applied fluence. The ablation behaviour in the case of near-IR femtosecond pulses contrasted to this. Bubble formation was not detected. It needed repeated pulses at the same spot to modify the surface until material removal could be observed (incubation). Cavity dimensions of less than the beam diameter were achieved in this case. T2 - 5th International Conference on Laser Ablation ; COLA '99 CY - Göttingen, Germany DA - 1998-07-19 KW - Laser ablation KW - Bariumalumoborosilicate glass PY - 1999 DO - https://doi.org/10.1007/s003390051524 SN - 0947-8396 VL - 69 IS - 7 SP - S763 EP - S766 PB - Springer CY - Berlin AN - OPUS4-801 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rudenko, A. A1 - Colombier, J.-P. A1 - Höhm, S. A1 - Rosenfeld, A. A1 - Krüger, Jörg A1 - Bonse, Jörn A1 - Itina, T.E. T1 - Spontaneous periodic ordering on the surface and in the bulk of dielectrics irradiated by ultrafast laser: a shared electromagnetic origin N2 - Periodic self-organization of matter beyond the diffraction limit is a puzzling phenomenon, typical both for surface and bulk ultrashort laser processing. Here we compare the mechanisms of periodic nanostructure formation on the surface and in the bulk of fused silica. We show that volume nanogratings and surface nanoripples having subwavelength periodicity and oriented perpendicular to the laser polarization share the same electromagnetic origin. The nanostructure orientation is defined by the near-field local enhancement in the vicinity of the inhomogeneous scattering centers. The periodicity is attributed to the coherent superposition of the waves scattered at inhomogeneities. Numerical calculations also support the multipulse accumulation nature of nanogratings formation on the surface and inside fused silica. Laser surface processing by multiple laser pulses promotes the transition from the high spatial frequency perpendicularly oriented nanoripples to the low spatial frequency ripples, parallel or perpendicular to the laser polarization. The latter structures also share the electromagnetic origin, but are related to the incident field interference with the scattered far-field of rough non-metallic or transiently metallic surfaces. The characteristic ripple appearances are predicted by combined electromagnetic and thermo-mechanical approaches and supported by SEM images of the final surface morphology and by time-resolved pump-probe diffraction measurements. KW - Laser-induced periodic surface structures (LIPSS) KW - Femtosecond laser KW - Nanostructures KW - Dielectrics KW - Electromagnetic scattering PY - 2017 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-421747 UR - https://www.nature.com/articles/s41598-017-12502-4 DO - https://doi.org/10.1038/s41598-017-12502-4 SN - 2045-2322 VL - 7 SP - Article 12306, 1 EP - 14 PB - Springer Nature AN - OPUS4-42174 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rosenfeld, A. A1 - Rohloff, M. A1 - Höhm, S. A1 - Krüger, Jörg A1 - Bonse, Jörn T1 - Formation of laser-induced periodic surface structures on fused silica upon multiple parallel polarized double-femtosecond-laser-pulse irradiation sequences N2 - The formation of laser-induced periodic surface structures (LIPSS) upon irradiation of fused silica with multiple irradiation sequences of parallel polarized Ti:sapphire femtosecond laser pulse pairs (160 fs pulse duration, 800 nm central wavelength) was studied experimentally. For that purpose, a Michelson interferometer was used to generate near-equal-energy double-pulse sequences allowing the temporal pulse delay between the parallel-polarized individual fs-laser pulses to be varied between 0 and 40 ps with ~0.2 ps temporal resolution. The surface morphologies of the irradiated surface areas were characterized by means of scanning electron and scanning force microscopy. In the sub-ps delay range a strong decrease of the LIPSS periods and the ablation crater depths with the double-pulse delay was observed indicating the importance of the laser-induced free-electron plasma in the conduction band of the solids for the formation of LIPSS. KW - Laser-induced periodic surface structures (LIPSS) KW - Femtosecond laser ablation KW - Double-pulse experiments KW - Fused silica KW - Michelson interferometer PY - 2012 DO - https://doi.org/10.1016/j.apsusc.2011.09.076 SN - 0169-4332 SN - 1873-5584 VL - 258 IS - 23 SP - 9233 EP - 9236 PB - North-Holland CY - Amsterdam AN - OPUS4-26226 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rohloff, M. A1 - Das, S.K. A1 - Höhm, S. A1 - Grunwald, R. A1 - Rosenfeld, A. A1 - Krüger, Jörg A1 - Bonse, Jörn T1 - Formation of laser-induced periodic surface structures on fused silica upon multiple cross-polarized double-femtosecond-laser-pulse irradiation sequences N2 - The formation of laser-induced periodic surface structures (LIPSS) upon irradiation of fused silica with multiple irradiation sequences consisting of five Ti:sapphire femtosecond (fs) laser pulse pairs (150 fs, 800 nm) is studied experimentally. A Michelson interferometer is used to generate near-equal-energy double-pulse sequences with a temporal pulse delay from -20 to +20 ps between the cross-polarized individual fs-laser pulses (~0.2 ps resolution). The results of multiple double-pulse irradiation sequences are characterized by means of Scanning Electron and Scanning Force Microscopy. Specifically in the sub-ps delay domain striking differences in the surface morphologies can be observed, indicating the importance of the laser-induced free-electron plasma in the conduction band of the solids for the formation of LIPSS. KW - Atomic force microscopy KW - Conduction bands KW - High-speed optical techniques KW - Laser beam effects KW - Scanning electron microscopy KW - Silicon compounds KW - Surface morphology PY - 2011 DO - https://doi.org/10.1063/1.3605513 SN - 0021-8979 SN - 1089-7550 VL - 110 IS - 1 SP - 014910-1 - 014910-4 PB - American Institute of Physics CY - Melville, NY AN - OPUS4-24049 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ringleb, F. A1 - Eylers, K. A1 - Teubner, T. A1 - Schramm, H.-P. A1 - Symietz, Christian A1 - Bonse, Jörn A1 - Andree, Stefan A1 - Heidmann, B. A1 - Schmid, M. A1 - Krüger, Jörg A1 - Boeck, T. T1 - Growth and shape of indium islands on molybdenum at micro-roughened spots created by femtosecond laser pulses N2 - Indium islands on molybdenum coated glass can be grown in ordered arrays by surface structuring using a femtosecond laser. The effect of varying the molybdenum coated glass substrate temperature and the indium deposition rate on island areal density, volume and geometry is investigated and evaluated in a physical vapor deposition (PVD) process. The joined impact of growth conditions and spacing of the femtosecond laser structured spots on the arrangement and morphology of indium islands is demonstrated. The results yield a deeper understanding of the island growth and its precise adjustment to industrial requirements, which is indispensable for a technological application of such structures at a high throughput, for instance as precursors for the preparation of Cu(In,Ga)Se2 micro concentrator solar cells. KW - Indium islands KW - Femtosecond laser patterning KW - Diffusion KW - CIGSe micro solar cells PY - 2017 UR - http://www.sciencedirect.com/science/article/pii/S0169433216325764 DO - https://doi.org/10.1016/j.apsusc.2016.11.135 SN - 0169-4332 SN - 1873-5584 VL - 418 SP - 548 EP - 553 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-40551 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ringleb, F. A1 - Eylers, K. A1 - Teubner, T. A1 - Boeck, T. A1 - Symietz, Christian A1 - Bonse, Jörn A1 - Andree, Stefan A1 - Krüger, Jörg A1 - Heidmann, B. A1 - Schmid, M. A1 - Lux-Steiner, M. T1 - Regularly arranged indium islands on glass/molybdenum substrates upon femtosecond laser and physical vapor deposition processing N2 - A bottom-up approach is presented for the production of arrays of indium islands on a molybdenum layer on glass, which can serve as micro-sized precursors for indium compounds such as copper-indium-gallium-diselenide used in photovoltaics. Femtosecond laser ablation of glass and a subsequent deposition of a molybdenum film or direct laser processing of the molybdenum film both allow the preferential nucleation and growth of indium islands at the predefined locations in a following indium-based physical vapor deposition (PVD) process. A proper choice of laser and deposition parameters ensures the controlled growth of indium islands exclusively at the laser ablated spots. Based on a statistical analysis, these results are compared to the non-structured molybdenum surface, leading to randomly grown indium islands after PVD. KW - Femtosecond laser KW - Physical vapor deposition KW - Indium KW - Molybdenum substrate KW - Microconcentrator solar cell PY - 2016 DO - https://doi.org/10.1063/1.4943794 SN - 0003-6951 VL - 108 IS - 11 SP - 111904-1 EP - 111904-4 AN - OPUS4-35602 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ringleb, F. A1 - Andree, Stefan A1 - Heidmann, B. A1 - Bonse, Jörn A1 - Eylers, K. A1 - Ernst, O. A1 - Boeck, T. A1 - Schmid, M. A1 - Krüger, Jörg T1 - Femtosecond laser-assisted fabrication of chalcopyrite micro-concentrator photovoltaics N2 - Micro-concentrator solar cells offer an attractive way to further enhance the efficiency of planar-cell technologies while saving absorber material. Here, two laser-based bottom-up processes for the fabrication of regular arrays of CuInSe2 and Cu(In,Ga)Se2 microabsorber islands are presented, namely one approach based on nucleation and one based on laser-induced forward transfer. Additionally, a procedure for processing these microabsorbers to functioning micro solar cells connected in parallel is demonstrated. The resulting cells show up to 2.9% efficiency and a significant efficiency enhancement under concentrated Illumination. KW - Chalcopyrite KW - Femtosecond laser patterning KW - Laser-induced forward transfer KW - Micro-concentrator solar cell KW - Photovoltaics PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-470026 DO - https://doi.org/10.3762/bjnano.9.281 SN - 2190-4286 VL - 9 SP - 3025 EP - 3038 PB - Beilstein-Institut zur Förderung der Chemischen Wissenschaften CY - Frankfurt, M. AN - OPUS4-47002 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pentzien, Simone A1 - Rabin, Ira A1 - Hahn, Oliver A1 - Krüger, Jörg A1 - Kleber, F. A1 - Hollaus, F. A1 - Diem, M. A1 - Sablatnig, R. ED - Park, J.-I. ED - Kim, J. T1 - Can Modern Technologies Defeat Nazi Censorship? N2 - Censorship of parts of written text was and is a common practice in totalitarian regimes. It is used to destroy information not approved by the political power. Recovering the censored text is of interest for historical studies of the text. This paper raises the question, whether a censored postcard from 1942 can be made legible by applying multispectral imaging in combination with laser cleaning. In the fields of art conservation (e.g. color measurements), investigation (e.g. Analysis of underdrawings in paintings), and historical document analysis, multispectral imaging techniques have been applied successfully to give visibility to information hidden to the human eye. The basic principle of laser cleaning is to transfer laser pulse energy to a contamination layer by an absorption process that leads to heating and evaporation of the layer. Partial laser cleaning of postcards is possible; dirt on the surface can be removed and the obscured pictures and writings made visible again. We applied both techniques to the postcard. The text could not be restored since the original ink seems to have suffered severe chemical damage. T2 - ACCV 2012 Workshops, 11th Asian conference on computer vision CY - Daejeon, Korea DA - 05.11.2012 KW - Laser cleaning KW - Multispectral imaging KW - Image restoration KW - Image enhancement PY - 2013 SN - 978-3-642-37483-8 SN - 0302-9743 VL - II IS - LNCS 7729 SP - 13 EP - 24 PB - Springer CY - Berlin Heidelberg AN - OPUS4-28160 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pentzien, Simone A1 - Conradi, Andrea A1 - Koter, Robert A1 - Krüger, Jörg T1 - Cleaning of artificially soiled paper using nanosecond, picosecond and femtosecond laser pulses N2 - Cleaning of cultural assets, especially fragile organic materials like paper, is a part of the conservation process. Laser radiation as a non-contact tool offers prospects for that purpose. For the studies presented here, paper model samples were prepared using three different paper types (pure cellulose, rag paper, and wood-pulp paper). Pure cellulose serves as reference material. Rag and woodpulp paper represent essential characteristics of the basic materials of real-world artworks. The papers were mechanically soiled employing pulverized charcoal. Pure and artificially soiled paper samples were treated with laser pulses of 28 fs (800 nm wavelength) and 8–12 ns (532 nm) duration in a multi pulse approach. Additionally, the cellulose reference material was processed with 30 ps (532 nm) laser pulses. Damage and cleaning thresholds of pure and soiled paper were determined for the different laser regimes. Laser working ranges allowing for removal of contamination and avoiding permanent modification to the substrate were found. The specimens prior and after laser illumination were characterized by light-optical microscopy (OM) and scanning electron microscopy (SEM) as well as multi spectral imaging analysis. The work extends previous nanosecond laser cleaning investigations on paper into the ultra-short pulse duration domain. KW - Laser cleaning KW - Ablation KW - Laser impact on surfaces KW - Paper KW - Femtosecond laser PY - 2010 DO - https://doi.org/10.1007/s00339-010-5809-7 SN - 0947-8396 VL - 101 IS - 2 SP - 441 EP - 446 PB - Springer CY - Berlin AN - OPUS4-22155 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Martin, Sven A1 - Krüger, Jörg A1 - Hertwig, Andreas A1 - Fiedler, A. A1 - Kautek, Wolfgang T1 - Femtosecond laser interaction with protection materials N2 - Textile, aluminium and polyethylene used as components in laser protection curtains were investigated with respect to their ablation behaviour. Employing 33-fs pulses (800 nm wavelength, 1 kHz repetition rate), ex situ geometrical measurements of the ablation cavities and in situ acoustic investigations with a microphone were performed to determine the ablation thresholds in the single- and multi-pulse cases. The acoustical method proved advantageous for complex surface morphologies and/or single laser pulse interactions. Incubation phenomena can be observed for all the materials studied. Technically relevant multi-pulse ablation thresholds are presented and are compared with the single-pulse (1-on-1) irradiation. KW - Damage KW - Femtosecond laser ablation KW - Laser safety KW - Threshold KW - Aluminium KW - Textile PY - 2003 DO - https://doi.org/10.1016/S0169-4332(02)01392-2 SN - 0169-4332 SN - 1873-5584 VL - 208-209 SP - 333 EP - 339 PB - North-Holland CY - Amsterdam AN - OPUS4-11546 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Martin, Sven A1 - Hertwig, Andreas A1 - Lenzner, Matthias A1 - Krüger, Jörg A1 - Kautek, Wolfgang T1 - Spot-size dependence of the ablation threshold in dielectrics for femtosecond laser pulses N2 - The multi-pulse ablation threshold of barium borosilicate glass was measured using 30-fs pulses of a high repetition rate (1 kHz) laser system. The threshold fluence was found to decrease with increasing beam radius ranging from 20 to 400 m. Two existing models are applied by considering thermal accumulation and point defects, respectively . PY - 2003 DO - https://doi.org/10.1007/s00339-003-2213-6 SN - 0947-8396 VL - 77 IS - 7 SP - 883 EP - 884 PB - Springer CY - Berlin AN - OPUS4-6317 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mann, Guido A1 - Vogel, Jens A1 - Zoheidi, M. A1 - Eberstein, Markus A1 - Krüger, Jörg T1 - Breakdown limits of optical multimode fibers for the application of nanosecond laser pulses at 532 nm and 1064 nm wavelength N2 - For many applications, optical multimode fibers are used for the transmission of powerful laser radiation. High light throughput and damage resistance are desirable. Laser-induced breakdown at the end faces of fibers can limit their performance. Therefore, the determination of laser-induced damage thresholds (LIDT) at the surface of fibers is essential. Nanosecond (1064 nm and 532 nm wavelength) single-shot LIDT were measured according to the relevant standard on SiO2 glass preforms (Suprasil F300) as basic materials of the corresponding fibers. For 10 kinds of fused silica fibers (FiberTech) with core diameters between 180 µm and 600 µm, an illumination approach utilizing a stepwise increase of the laser fluence on a single spot was used. For both wavelengths, the LIDT values (0% damage probability) obtained by means of the two methods were compared. The influence of surface preparation (polishing) on damage resistance was investigated. For equal surface finishing, a correlation between drawing speed of the fibers and their surface LIDT values was found. In addition to the surface measurements, bulk LIDT were determined for the preform material. KW - Fiber waveguides KW - Physical radiation damage KW - Laser-beam impact phenomena KW - Glasses KW - Radiation treatment PY - 2009 DO - https://doi.org/10.1016/j.apsusc.2008.07.157 SN - 0169-4332 SN - 1873-5584 VL - 255 IS - 10 SP - 5519 EP - 5522 PB - North-Holland CY - Amsterdam AN - OPUS4-19036 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mann, Guido A1 - Vogel, Jens A1 - Preuß, Rüdiger A1 - Vaziri, Pouya A1 - Zoheidi, M. A1 - Eberstein, Markus A1 - Krüger, Jörg T1 - Nanosecond laser-induced surface damage of optical multimode fibers and their preforms N2 - High-power optical multimode fibers are essential components for materials processing and surgery and can limit the performance of expensive systems due to breakdown at the end faces. The aim of this paper is the determination of laser-induced damage thresholds (LIDT) of fibers (FiberTech) and preforms (Heraeus Suprasil F300). Preforms served as models. They were heated up to maximum temperatures of 1100, 1300 and 1500°C and cooled down to room temperature at rates of 10 K min-1 (oven) and ~105 K min-1 (quenched in air) to freeze in various structural states simulating different conditions similar to a drawing process during the production of fibers. Single- and multi-pulse LIDT measurements were done in accordance with the relevant ISO standards. Nd:YAG laser pulses with durations of 15 ns (1064 nm wavelength) and 8.5 ns (532 nm) at a repetition rate of 10 Hz were used. For the preforms, LIDT values (1-on-1) ranged from 220 to 350 J/cm² (1064 nm) and from 80 to 110 J/cm² (532 nm), respectively. A multi-pulse impact changed the thresholds to lower values. The LIDT (1064 nm wavelength) of the preforms can be regarded as a lower limit for those of the fibers. PY - 2008 DO - https://doi.org/10.1007/s00339-008-4576-1 SN - 0947-8396 VL - 92 IS - 4 SP - 853 EP - 857 PB - Springer CY - Berlin AN - OPUS4-17779 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mann, Guido A1 - Vogel, Jens A1 - Preuß, Rüdiger A1 - Vaziri, Pouya A1 - Zoheidi, M. A1 - Eberstein, Markus A1 - Krüger, Jörg T1 - Nanosecond laser damage resistance of differently prepared semi-finished parts of optical multimode fibers N2 - Optical multimode fibers are applied in materials processing (e.g. automotive industry), defense, aviation technology, medicine and biotechnology. One challenging task concerning the production of multimode fibers is the enhancement of laser-induced damage thresholds. A higher damage threshold enables a higher transmitted average power at a given fiber diameter or the same power inside a thinner fiber to obtain smaller focus spots. In principle, different material parameters affect the damage threshold. Besides the quality of the preform bulk material itself, the drawing process during the production of the fiber and the preparation of the fiber end surfaces influence the resistance. Therefore, the change of the laser-induced damage threshold of preform materials was investigated in dependence on a varying thermal treatment and preparation procedure. Single and multi-pulse laser-induced damage thresholds of preforms (F300, Heraeus) were measured using a Q-switched Nd:YAG laser at 1064 nm wavelength emitting pulses with a duration of 15 ns, a pulse energy of 12 mJ and a repetition rate of 10 Hz. The temporal and spatial shape of the laser pulses were controlled accurately. Laser-induced damage thresholds in a range from 150 J cm-2 to 350 J cm-2 were determined depending on the number of pulses applied to the same spot, the thermal history and the polishing quality of the samples, respectively. KW - Laser ablation KW - Optical fibers KW - Physical radiation damage KW - Radiation treatment KW - Glass transitions KW - Glasses PY - 2007 DO - https://doi.org/10.1016/j.apsusc.2007.09.032 SN - 0169-4332 SN - 1873-5584 VL - 254 IS - 4 SP - 1096 EP - 1100 PB - North-Holland CY - Amsterdam AN - OPUS4-16207 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mann, Guido A1 - Pentzien, Simone A1 - Krüger, Jörg T1 - Beam diameter dependence of surface damage threshold of fused silica fibers and preforms for nanosecond laser treatment at 1064 nm wavelength N2 - Optical fibers made of fused silica are a common method of transmitting high laser pulse energies. Failure of those fibers is a significant risk. The determination of laser-induced damage thresholds (LIDT) on fiber end facets according to ISO 21254 standard is needed. In the past, single pulse nanosecond laser experiments showed an improvement of LIDT with increasing fiber core diameter for 1064 nm wavelength and a constant beam diameter of 50 µm. This paper pays particular attention to the influence of the laser beam diameter on damage resistance. All-silica fiber types (LEONI) with different core diameters (100–600 µm) were investigated using beam diameters in a range from 30 µm to 100 µm. For comparison experiments on fused silica preform material (Heraeus F300) were performed. On one hand, surface LIDT of fused silica preform material decreases significantly with increasing beam size. A model considering a random distribution of point defects explains the experimental data qualitatively. On the other hand, LIDT of fiber end facets stays constant. White light microscopy results suggest that the point defect density on fiber end facets is lower compared to the preform surface due to an excellent surface polish quality. KW - Laser-induced damage threshold KW - Nanosecond laser KW - Optical fiber KW - Fused silica KW - Spot size KW - Defect model PY - 2013 DO - https://doi.org/10.1016/j.apsusc.2013.03.088 SN - 0169-4332 SN - 1873-5584 VL - 276 SP - 312 EP - 316 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-28310 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Mann, Guido A1 - Krüger, Jörg ED - Jitsuno, T. ED - Shao, J. ED - Rudolph, W. T1 - Nanosecond laser damage of optical multimode fibers N2 - For pulse laser materials processing often optical step index and gradient index multimode fibers with core diameters ranging from 100 to 600 μm are used. The design of a high power fiber transmission system must take into account limitations resulting from both surface and volume damage effects. Especially, breakdown at the fiber end faces and self-focusing in the fiber volume critically influence the fiber performance. At least operation charts are desirable to select the appropriate fiber type for given laser parameters. In industry-relevant studies the influence of fiber core diameter and end face preparation on laser-induced (surface) damage thresholds (LIDT) was investigated for frequently used all-silica fiber types (manufacturer LEONI). Experiments on preform material (initial fiber material) and compact specimens (models of the cladding and coating material) accompanied the tests performed in accordance with the relevant LIDT standards ISO 21254-1 and ISO 21254 2 for 1-on-1 and S-on-1 irradiation conditions, respectively. The relation beam diameter vs. LIDT was investigated for fused silica fibers. Additionally, laser-induced (bulk) damage thresholds of fused silica preform material F300 (manufacturer Heraeus) in dependence on external mechanical stress simulating fiber bending were measured. All experiments were performed with 10-ns laser pulses at 1064 and 532 nm wavelength with a Gaussian beam profile. T2 - Pacific Rim Laser Damage 2016 CY - Yokohama, Japan DA - 18.05.2016 KW - laser damage KW - optical fiber KW - nanosecond laser KW - fused silica PY - 2016 DO - https://doi.org/10.1117/12.2238515 VL - 9983 SP - 99830T AN - OPUS4-37140 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mann, Guido A1 - Jurke, Mathias A1 - Zoheidi, M. A1 - Krüger, Jörg T1 - Influence of mechanical stress on nanosecond laser-induced damage threshold of fused silica N2 - Optical multimode fibers made of fused silica are widely used for transmission of high power laser pulses. Bending of fibers creates mechanical stress inside the material. The bend stress of a fiber can be calculated from bend radius, geometrical fiber parameters and Young's Modulus of the fiber core material and reaches typically values of 220 MPa. A thermo-elastic model of Kusov et al. predicts a quadratic dependence of laser-induced damage threshold fluence with applied stress. In the present study, fiber preform material F300 (Heraeus) was loaded mechanically with pressures up to 220 MPa representing 20% of the pressure resistance of fused silica. Bulk laser-induced damage thresholds (LIDT) were evaluated using a longitudinal multimode Q-switched Nd:YAG laser (1064 nm) at a pulse duration of 12 ns with polarization states parallel and perpendicular to the stress direction. LIDT of fused silica samples of about 700 J/cm2 were found. LIDT did not show a dependence on mechanical pressure and polarization state which is a consequence of the small ratio of maximum applied stress (220 MPa) to Young's Modulus of fused silica (72.5 GPa). KW - Laser-induced damage threshold KW - LIDT KW - Nanosecond laser KW - Fused silica KW - Mechanical stress KW - Optical fiber PY - 2012 DO - https://doi.org/10.1016/j.apsusc.2012.01.049 SN - 0169-4332 SN - 1873-5584 VL - 258 IS - 23 SP - 9153 EP - 9156 PB - North-Holland CY - Amsterdam AN - OPUS4-26225 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mann, Guido A1 - Jurke, Mathias A1 - Zoheidi, M. A1 - Eberstein, Markus A1 - Krüger, Jörg T1 - Influence of core diameter and coating material on nanosecond laser-induced damage threshold of optical multimode fibers N2 - Single and multi pulse laser-induced damage thresholds (LIDT) of core, cladding, and coating materials of high-power optical multimode fibers were determined in accordance with ISO 11254 for 532 nm and 1064 nm wavelength in the 10-ns pulse duration regime with spatial Gaussian beam shape. For all-silica fibers, LIDT increases with rising core diameter in a range between 100-600 µm for a constant cladding-core ratio of 1.2. The damage resistance of the low refracting cladding (0.3 % fluorine doped fused silica) is comparable to the undoped SiO2 core. Coating materials show significantly lower LIDT than light-guiding parts of the fibers. KW - Fiber waveguides (42.81.Qb) KW - Physical radiation damage (61.80.-x) KW - Laser-beam impact phenomena (79.20.Ds) KW - Glasses (81.05.Kf) PY - 2010 SN - 1454-4164 VL - 12 IS - 3 SP - 711 EP - 714 PB - INOE & INFM CY - Bucharest AN - OPUS4-21083 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Lone, S. A. A1 - Muck, M. A1 - Fosodeder, P. A1 - Mardare, C.C. A1 - Florian, Camilo A1 - Weth, A. A1 - Krüger, Jörg A1 - Steinwender, C. A1 - Baumgartner, W. A1 - Bonse, Jörn A1 - Heitz, J. A1 - Hassel, A.W. T1 - Impact of Femtosecond Laser Treatment Accompanied with Anodization of Titanium Alloy on Fibroblast Cell Growth N2 - Herein, Ti6Al4V alloy is surface modified by femtosecond laser ablation. The microstructure image obtained by secondary electron microscopy reveals a combination of micrometer spikes or cones superimposed by nanoripples (laser‐induced periodic surface structures). To make the surface hydrophilic, anodization is performed resulting in further smoothness of microstructure and a final thickness of 35 ± 4 nm is estimated for oxide produced after anodization at 10 V (scan rate = 0.1 V s−1) versus standard hydrogen electrode. The obtained electrochemically active surface area (ECSA) is approximately 8 times larger compared with flat mirror polished Ti6Al4V surface. Combined chemical analysis by Pourbaix diagram and X‐ray photoelectron spectroscopy (XPS) analyses reveal that titanium and aluminum are passivating into TiO2 and Al2O3, but the dissolution of aluminum in the form of solvated ion is inevitable. Finally, cell seeding experiments on anodized and laser‐treated titanium alloy samples show that the growth of murine fibroblast cells is significantly suppressed due to unique surface texture of the laser‐treated and anodized titanium alloy sample. KW - Anodization KW - Femtosecond laser ablation KW - Laser-induced periodic surface structures, LIPSS KW - Ti6Al4V alloys KW - X-ray photoelectron spectroscopy PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-510263 DO - https://doi.org/https://doi.org/10.1002/pssa.201900838 SN - 1862-6300 SN - 1862-6319 VL - 217 IS - 13 SP - 1900838-1 EP - 1900838-9 PB - WILEY-VCH Verlag CY - Weinheim, Germany AN - OPUS4-51026 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Lenzner, Matthias A1 - Krüger, Jörg A1 - Sartania, S. A1 - Cheng, Z. A1 - Spielmann, Ch. A1 - Mourou, G. A1 - Kautek, Wolfgang A1 - Krausz, F. T1 - Femtosecond Optical Breakdown in Dielectrics N2 - We report measurements of the optical breakdown threshold and ablation depth in dielectrics with different band gaps for laser pulse durations ranging from 5 ps to 5 fs at a carrier wavelength of 780 nm. For tau <100 fs, the dominant channel for free electron generation is found to be either impact or multiphoton ionization (MPI) depending on the size of the band gap. The observed MPI rates are substantially lower than those predicted by the Keldysh theory. We demonstrate that sub-10-fs laser pulses open up the way to reversible nonperturbative nonlinear optics (at intensities greater than 1014 W/cm2 slightly below damage threshold) and to nanometer-precision laser ablation (slightly above threshold) in dielectric materials. PY - 1998 SN - 0031-9007 SN - 1079-7114 VL - 80 IS - 18 SP - 4076 EP - 4079 PB - American Physical Society CY - Ridge, NY AN - OPUS4-11518 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Legall, Herbert A1 - Schwanke, Christoph A1 - Pentzien, Simone A1 - Dittmar, G. A1 - Bonse, Jörn A1 - Krüger, Jörg T1 - X-ray emission as a potential hazard during ultrashort pulse laser material processing N2 - In laser machining with ultrashort laser pulses unwanted X-ray radiation in the keV range can be generated when a critical laser intensity is exceeded. Even if the emitted X-ray dose per pulse is low, high laser repetition rates can lead to an accumulation of X-ray doses beyond exposure safety limits. For 925 fs pulse duration at a center wavelength of 1030 nm, the X-ray emission was investigated up to an intensity of 2.6 × 10^14 W/cm2. The experiments were performed in air with a thin disk laser at a repetition rate of 400 kHz. X-ray spectra and doses were measured for various planar target materials covering a wide range of the periodic table from aluminum to tungsten. Without radiation shielding, the measured radiation doses at this high repetition rate clearly exceed the regulatory limits. Estimations for an adequate radiation shielding are provided. KW - Laser-induced X-ray emission KW - Ultrashort laser material interaction KW - Femtosecond laser KW - Radiation protection PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-448431 DO - https://doi.org/10.1007/s00339-018-1828-6 SN - 0947-8396 SN - 1432-0630 VL - 124 IS - 6 SP - Article 407, 1 EP - 8 PB - Springer AN - OPUS4-44843 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Legall, Herbert A1 - Schwanke, Christoph A1 - Bonse, Jörn A1 - Krüger, Jörg T1 - X-ray radiation protection aspects during ultrashort laser processing N2 - Ultrashort pulse laser processing of materials allows for precise machining with high accuracy. By increasing the repetition rate to several 100 kHz, laser machining becomes quick and cost-effective. Ultrafast laser processing at high repetition rates and peak intensities above 10^13 W/cm^2 can cause a potential hazard by generation of unwanted x-ray radiation. Therefore, radiation protection must be considered. For 925 fs pulse duration at a center wavelength of 1030 nm, the x-ray emission in air at a repetition rate of 400 kHz was investigated up to a peak intensity of 2.6 × 10^14 W/cm^2. Based on the presented measurements, the properties of potential shielding materials will be discussed. By extending our previous works, a scaling of the x-ray radiation emission to higher peak intensities up to 10^15 W/cm^2 is described, and emitted x-ray doses are predicted. KW - Laser ablation KW - Ultrashort pulse laser processing KW - Laser-induced x-ray emission KW - Radiation protection PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-505677 DO - https://doi.org/10.2351/1.5134778 VL - 32 IS - 2 SP - 022004 AN - OPUS4-50567 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Legall, Herbert A1 - Schwanke, Christoph A1 - Bonse, Jörn A1 - Krüger, Jörg T1 - The influence of processing parameters on X‑ray emission during ultra‑short pulse laser machining N2 - During ultra-short laser material processing at high laser pulse repetition rates unwanted X-ray radiation can be generated in a quantity that may constitute a potential risk for health. An adequate X-ray radiation protection requires a thoroughly understanding of the influence of the laser processing parameters on the generation of X-ray radiation. In the present work, the generated X-ray dose during laser machining was investigated in air for varying beam scanning conditions at a pulse duration of 925 fs, a center wavelength of 1030 nm and a laser peak intensity of 2.6 × 10^14 W/cm^2. The X-ray radiation dose and the corresponding spectral X-ray emission were investigated in dependence on the laser’s pulse repetition rate and on the beam scanning speed. The results show a strong dependence of the X-ray emission on these laser processing parameters. KW - Laser-induced X-ray emission KW - Ultrashort laser material interaction KW - Femtosecond laser KW - Radiation protection PY - 2019 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-486441 DO - https://doi.org/10.1007/s00339-019-2827-y SN - 0947-8396 SN - 1432-0630 VL - 125 IS - 8 SP - 570, 1 EP - 8 PB - Springer AN - OPUS4-48644 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Legall, Herbert A1 - Schwanke, Christoph A1 - Bonse, Jörn A1 - Krüger, Jörg T1 - X-ray emission during ultrashort pulse laser processing N2 - The industrial use of ultrashort laser pulses has made considerable progress in recent years. The reasons for this lie in the availability of high average powers at pulse repetition rates in the several 100 kHz range. The advantages of using ultrashort laser pulses in terms of processing precision can thus be fully exploited. However, high laser intensities on the workpiece can also lead to the generation of unwanted X-rays. Even if the emitted X-ray dose per pulse is low, the accumulated X-ray dose can become significant for high-repetition-rate laser systems so that X-ray exposure safety limits must be considered. The X-ray emission during ultrashort pulse laser processing was investigated for a pulse duration of 925 fs at 1030 nm wavelength and 400 kHz repetition rate. Industrially relevant materials such as steel,aluminum and glass were treated. Tungsten served as reference. X-ray spectra were recorded, and X-ray dose measurements were performed for laser treatment in air. For laser intensities > 2 × 10^13 W/cm2, X-ray doses exceeding the regulatory exposure limits for members of the public were found. Suitable X-ray protection strategies are proposed. T2 - SPIE Photonics West CY - San Francisco, USA DA - 02.02.2019 KW - Laser-induced X-ray emission KW - Ultrashort laser material interaction KW - Radiation protection PY - 2019 SN - 978-1-5106-2459-7 DO - https://doi.org/10.1117/12.2516165 SN - 0277-786X SN - 1996-756X VL - 10908 SP - 1090802-1 EP - 1090802-7 PB - SPIE - The international society for optics and photonics CY - Bellingham, WA, USA AN - OPUS4-47510 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Legall, Herbert A1 - Bonse, Jörn A1 - Krüger, Jörg T1 - Review of x-ray exposure and safety issues arising from ultra-short pulse laser material processing N2 - Laser processing with ultra-short laser pulses enables machining of materials with high accuracy and throughput. The development of novel laser Technologies with laser pulse repetition rates up to the MHz range opened the way for industrial manufacturing processes. From a radiological point of view this evolution is important, because x-ray radiation can be generated as an unwanted side effect in laser material processing. Even if the emitted x-ray dose per pulse is comparably low, the x-ray dose can become hazardous to health at high laser repetition rates. Therefore, radiation protection must be considered. This article provides an overview on the generation and detection of x-rays in laser material processing, as well as on the handling of this radiation risk in the framework of radiological protection. KW - Ultra-short pulse laser processing KW - Laser-induced x-ray emission KW - Radiation protection PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-522376 DO - https://doi.org/10.1088/1361-6498/abcb16 VL - 41 IS - 1 SP - R28 EP - R42 AN - OPUS4-52237 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Jörg A1 - Sorg, N. A1 - Reif, J. A1 - Kautek, Wolfgang T1 - In situ second harmonic generation measurements during the electrodeposition of Ni on n-Si(111) PY - 1993 SN - 0169-4332 SN - 1873-5584 VL - 69 SP - 388 EP - 392 PB - North-Holland CY - Amsterdam AN - OPUS4-11657 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Jörg A1 - Pentzien, Simone A1 - Conradi, Andrea T1 - Cleaning of artificially soiled paper with 532-nm nanosecond laser radiation N2 - Cleaning of paper is a challenging task due to the fact that a contamination should be removed and a fragile organic original material has to be preserved. Pulsed laser cleaning of artificially soiled Whatman© filter paper samples serving as models for historical paper was performed. Different cleaning strategies employing 8-ns laser pulses at 532 nm wavelength were applied to clean paper avoiding undesired effects like discoloration (yellowing) and mechanical deterioration of the substrate. Multi shot experiments with low-energy pulses were compared with single pulse investigations utilizing high pulse energies achieving a constant energy load incident on the samples in both cases. The cleaning efficiency and possible yellowing effects were evaluated by means of a multi spectral imaging system. An extensive microscopic analysis of the cleaned parts of the samples provided insight into the remaining soiling on the surface and in the bulk of the paper material after laser treatment. As a reference, a hard and a soft eraser were used to clean the samples. KW - Laser cleaning KW - Paper KW - Colorimetry PY - 2008 DO - https://doi.org/10.1007/s00339-008-4476-4 SN - 0947-8396 VL - 92 IS - 1 SP - 179 EP - 183 PB - Springer CY - Berlin AN - OPUS4-17331 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Jörg A1 - Niino, Hiroyuki A1 - Yabe, A. T1 - Investigation of excimer laser ablation threshold of polymers using a microphone N2 - KrF excimer laser ablation of polyethylene terephthalate (PET), polyimide (PI) and polycarbonate (PC) in air was studied by an in situ monitoring technique using a microphone. The microphone signal generated by a short acoustic pulse represented the etch rate of laser ablation depending on the laser fluence, i.e., the ablation “strength”. From a linear relationship between the microphone output voltage and the laser fluence, the single-pulse ablation thresholds were found to be 30 mJ cm-2 for PET, 37 mJ cm-2 for PI and 51 mJ cm-2 for PC (20-pulses threshold). The ablation thresholds of PET and PI were not influenced by the number of pulses per spot, while PC showed an incubation phenomenon. A microphone technique provides a simple method to determine the excimer laser ablation threshold of polymer films. KW - Laser ablation KW - Polymer KW - Treshold KW - Microphone KW - Acoustic measurement KW - Incubation PY - 2002 DO - https://doi.org/10.1016/S0169-4332(02)00418-X SN - 0169-4332 SN - 1873-5584 VL - 197-198 SP - 800 EP - 804 PB - North-Holland CY - Amsterdam AN - OPUS4-1920 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Jörg A1 - Meja, P. A1 - Autric, M. A1 - Kautek, Wolfgang T1 - Femtosecond pulse laser ablation of anodic oxide coatings on aluminium alloys with on-line acoustic observation N2 - The 125-fs laser ablation behaviour (800 nm) of aluminium and anodic oxide coatings on an AlMgSi1 alloy was investigated. The multi-pulse ablation threshold of aluminium at 1.2 J cm-2 was less than that of the oxides of 2–3 J cm-2. Aluminium exhibited a single pulse modification (melting) threshold of 0.3 J cm-2. These values derived from an evaluation of the crater geometry coincided with on-line acoustic measurements. The detected microphone voltage amplitude increased linearly with the laser fluence. The morphology of the ablation craters on aluminium indicated melt formation and displacement of a homogeneous melt phase due to the recoil action of the expanding metal vapour. The laser-processed ceramic oxide phases, on the other hand, showed a spongy resolidified melt layer, which denotes a collocated in-depth formation both of a melt and a gas phase. These phenomena are discussed in terms of the relative dominance of penetration depth of laser light and heat affected zones in the investigated materials with strongly varying optical and thermodynamical properties. KW - Laser ablation KW - Acoustic measurement KW - Microphone KW - Aluminium KW - Aluminium oxide PY - 2002 SN - 0169-4332 SN - 1873-5584 VL - 186 IS - 1-4 SP - 374 EP - 380 PB - North-Holland CY - Amsterdam AN - OPUS4-6324 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Jörg A1 - Martin, Sven A1 - Mädebach, Heinrich A1 - Urech, L. A1 - Lippert, T. A1 - Wokaun, A. A1 - Kautek, Wolfgang T1 - Femto- and nanosecond laser treatment of doped polymethylmethacrylate N2 - Femto- and nanosecond laser ablation of polymethylmethacrylate (PMMA) and PMMA doped with a linear absorber was investigated in the infrared spectral region. Ablation thresholds were determined and incubation phenomena were identified. The ‘degree’ of incubation was calculated employing a phenomenological model. The influence of the pulse duration on the machining quality of the polymers was examined. The presence of an absorbing chromophore is not a prerequisite for a controllable fs-laser structuring in contrast to the ns-treatment. Surface swelling always accompanied ablation. KW - Laser ablation KW - Laser beam machining KW - Doping thin films KW - Polymers-radiation effects PY - 2005 DO - https://doi.org/10.1016/j.apsusc.2005.01.078 SN - 0169-4332 SN - 1873-5584 VL - 247 SP - 406 EP - 411 PB - North-Holland CY - Amsterdam AN - OPUS4-7470 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Jörg A1 - Lenzner, Matthias A1 - Martin, Sven A1 - Lenner, M. A1 - Spielmann, Ch. A1 - Fiedler, A. A1 - Kautek, Wolfgang T1 - Single- and multi-pulse femtosecond laser ablation of optical filter materials N2 - Ablation experiments employing Ti:sapphire laser pulses with durations from 30 to 340 fs (centre wavelength 800 nm, repetition rate 1 kHz) were performed in air. Absorbing filters (Schott BG18 and BG36) served as targets. The direct focusing technique was used under single- and multi-pulse irradiation conditions. Ablation threshold fluences were determined from a semi-logarithmic plot of the ablation crater diameter versus laser fluence. The threshold fluence decreases for a shorter pulse duration and an increasing number of pulses. The multi-pulse ablation threshold fluences are similar to those of undoped glass material (~1 J cm-2). That means that the multi-pulse ablation threshold is independent on the doping level of the filters. For more than 100 pulses per spot and all pulse durations applied, the threshold fluence is practically constant. This leads to technically relevant ablation threshold values. KW - Damage KW - Femtosecond laser ablation KW - Filter KW - Incubation KW - Laser safety KW - Threshold PY - 2003 DO - https://doi.org/10.1016/S0169-4332(02)01389-2 SN - 0169-4332 SN - 1873-5584 VL - 208-209 SP - 233 EP - 237 PB - North-Holland CY - Amsterdam AN - OPUS4-11545 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Jörg A1 - Kautek, Wolfgang A1 - Niino, H. T1 - Biomaterial immobilization on polyurethane films by XeCl excimer laser processing N2 - Zusammenfassung The surface chemical modification of polyurethane (PU) films was performed by an UV laser-induced chemical reaction in a polysaccharide solution. This process may be applicable as hydrophilic packaging of implantable medical devices and in vivo sensors. When a PU film in contact with an aqueous alginic acid (AAC) solution was irradiated with a XeCl laser, the PU film turned hydrophilic. Contact angles of water on the film were reduced from 110° to 60°. Since light absorption of the AAC solution at 308 nm was negligibly small, reactive sites were generated solely on the PU surface. There, AAC could be immobilized by chemical bonds thus allowing for a nanometer-scaled grafting of this biomolecule. The mechanism was investigated by surface analyses with Fourier-transform infrared spectroscopy (FT-IR), dye staining, ultraviolet-visible (UV-VIS) spectroscopy, and scanning electron microscopy (SEM) techniques. A one-photon photochemical process could beidentified. PY - 2001 DO - https://doi.org/10.1007/s003390000617 SN - 0947-8396 VL - 72 IS - 1 SP - 53 EP - 57 PB - Springer CY - Berlin AN - OPUS4-926 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Jörg A1 - Kautek, Wolfgang A1 - Newesely, H. T1 - Femtosecond-pulse laser ablation of dental hydroxyapatite and single-crystalline fluoroapatite N2 - Laser microdrilling of healthy human enamel and dentine using 300 fs pulses at a wavelength of 615 nm and 3 Hz repetition rate leads to an enhanced structuring quality in comparison with nanosecond-laser results. Microcracking and damage to neighboring tissue can be reduced. Ablation threshold fluences for 100 laser pulses of 0.3 J cm-2 (human dentine), 0.6 J cm-2 (human enamel) and 0.8 J cm-2 (single crystalline fluoroapatite) could be determined. Ablation depths per pulse below 1 7m were observed. T2 - 5th International Conference on Laser Ablation ; COLA '99 CY - Göttingen, Germany DA - 1999-07-19 PY - 1999 DO - https://doi.org/10.1007/s003390051426 SN - 0947-8396 VL - 69 IS - 7 SP - S403 EP - S407 PB - Springer CY - Berlin AN - OPUS4-779 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Jörg A1 - Kautek, Wolfgang A1 - Lenzner, M. A1 - Sartania, S. A1 - Spielmann, Ch. A1 - Krausz, F. T1 - Laser micromachining of barium aluminium borosilicate glass with pulse durations between 20 fs and 3 ps KW - Laser micromachining KW - Subpicosecond laser ablation KW - Barium aluminium borosilicate glass PY - 1998 SN - 0169-4332 SN - 1873-5584 IS - 127-129 SP - 892 EP - 898 PB - North-Holland CY - Amsterdam AN - OPUS4-887 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Jörg A1 - Kautek, Wolfgang A1 - Lenzner, M. A1 - Krausz, F. T1 - Precision laser ablation of dielectrics in the 10-fs regime N2 - Zusammenfassung Laser pulses in the 10-fs domain provide a quality of micromachining of fused silica and borosilicate glass that is unobtainable with longer pulses in the range of several 100 femtoseconds up to picoseconds. The shortening of the pulses reduces the statistical behavior of the material removal and the ablation process thus attains a more deterministic and reproducible character. The improved reproducibility of ablation is accompanied by significantly smoother morphology. This offers the potential for lateral and vertical machining precision of the order of 100 nm and 10 nm, respectively. KW - Laser ablation PY - 1999 DO - https://doi.org/10.1007/s003390050906 SN - 0947-8396 VL - 68 IS - 3 SP - 369 EP - 371 PB - Springer CY - Berlin AN - OPUS4-825 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -