TY - JOUR A1 - Al-Falahat, A M A1 - Kardjilov, N A1 - Woracek, R A1 - Boin, M A1 - Markötter, Henning A1 - Kuhn, L T A1 - Makowska, M A1 - Strobl, M A1 - Pfretzschner, B A1 - Banhart, J A1 - Manke, I T1 - Temperature dependence in Bragg edge neutron transmission measurements N2 - A systematic study has been carried out to investigate the neutron transmission signal as a function of sample temperature. In particular, the experimentally determined wavelength-dependent neutron attenuation spectra for a martensitic steel at temperatures ranging from 21 to 700°C are compared with simulated data. A theoretical description that includes the Debye–Waller factor in order to describe the temperature influence on the neutron cross sections was implemented in the nxsPlotter software and used for the simulations. The analysis of the attenuation coefficients at varying temperatures shows that the missing contributions due to elastic and inelastic scattering can be clearly distinguished: while the elastically scattered intensities decrease with higher temperatures, the inelastically scattered intensities increase, and the two can be separated from each other by analysing unique sharp features in the form of Bragg edges. This study presents the first systematic approach to quantify this effect and can serve as a basis , for example, to correct measurements taken during in situ heat treatments, in many cases being a prerequisite for obtaining quantifiable results. KW - Neutron Bragg edge imaging KW - Debye–Waller factor KW - Temperature-dependent neutron transmission KW - Super martensitic stainless steel PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-556896 DO - https://doi.org/10.1107/S1600576722006549 VL - 55 IS - Pt 4 SP - 919 EP - 928 PB - International Union of Crystallography AN - OPUS4-55689 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Al-Falahat, A. A1 - Kardjilov, N. A1 - Markötter, Henning A1 - Kupsch, Andreas A1 - Woracek, R. A1 - Alrwashdeh, S. A1 - Manke, I. T1 - Investigation of detector backlighting and other effects in neutron darkfield images N2 - Neutron imaging can provide unique contrast mechanisms. In order to yield reliable and reproducible attenuation coefficients for quantification, one needs to fully understand and characterize the experimental set-up. One effect that has been largely overlooked in scintillator-camera based neutron imaging systems is the backlight scattering or back illumination in the detection system which can significantly affect the quantification of attenuation coefficients and lead to severe errors and image artifacts. Herein, backlighting is investigated by varying the illuminated detector area and the magnitude of the attenuation. The attenuation coefficient of multiple metal plates was determined by polychromatic neutrons bu the CONRAD V7 instrument. The strength of the back illumination strongly depends upon the sample absorption. While it is relatively moderate (a few percent) for weak absorbing samples, it can be severe when the sample is a strong absorber or thick. KW - Attenuation coefficient KW - Neutron imaging KW - Neutron scattering KW - Polycromatic neutrons KW - Scintillator PY - 2024 SN - 1073-9149 DO - https://doi.org/10.1080/10739149.2024.2380772 SP - 1 EP - 11 PB - Taylor & Francis AN - OPUS4-60752 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hilger, A. A1 - Kardjilov, N. A1 - Lange, A. A1 - Kupsch, Andreas A1 - Hentschel, M. P. A1 - Manke, I. T1 - Neutron darkfield imaging of fiber composites N2 - While X-ray based darkfield imaging with grating interferometers is already widely used, darkfield imaging with neutrons has still a relatively small user community focused mostly on magnetic materials. Here, we demonstrate the application of neutron darkfield imaging byTalbot-Lau type grating interferometry to fiber reinforced plastics. Common carbon and glass fiber composites have been investigated including characteristic damage structures. The darkfield images show a strong signal response caused by fiber delamination, suitable fiber direction, particles, pores and cracks. The basic principles of neutron darkfield imaging applied to fiber composites are highlighted. KW - Neutron radiography KW - Darkfield imaging KW - Talbot-Lau interferometer KW - Fiber composites KW - Non-destructive testing PY - 2021 DO - https://doi.org/10.1515/mt-2020-0103 SN - 2195-8572 SN - 0025-5300 VL - 63 IS - 7 SP - 623 EP - 629 PB - De Gruyter CY - Berlin AN - OPUS4-53077 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hoffmann, H A1 - Paulisch, M C A1 - Gebhard, M A1 - Osiewacz, J A1 - Kutter, M A1 - Hilger, A A1 - Arlt, T A1 - Kardjilov, N A1 - Ellendorff, B A1 - Beckmann, F A1 - Markötter, Henning A1 - Luik, M A1 - Turek, T A1 - Manke, I A1 - Roth, C T1 - Development of a Modular Operando Cell for X-ray Imaging of Strongly Absorbing Silver-Based Gas Diffusion Electrodes N2 - Metal-based gas diffusion electrodes are utilized in chlor-alkali electrolysis or electrochemical reduction of carbon dioxide, allowing the reaction to proceed at high current densities. In contrast to planar electrodes and predominantly 2D designs, the industrially required high current densities can be achieved by intense contact between the gas and liquid phase with the catalytically active surfaces. An essential asset for the knowledge-based design of tailored electrodes is therefore in-depth information on electrolyte distribution and intrusion into the electrode’s porous structure. Lab-based and synchrotron radiography allow for monitoring this process operando. Herein, we describe the development of a cell design that can be modularly adapted and successfully used to monitor both the oxygen reduction reaction and the electrochemical reduction of CO2 as exemplary and currently very relevant examples of gas-liquid reactions by only minor modifications to the cell set-up. With the reported cell design, we were able to observe the electrolyte distribution within the gas diffusion electrode during cell operation in realistic conditions. KW - X-Ray imaging KW - Gas diffusion electrodes KW - Operando cell PY - 2022 DO - https://doi.org/10.1149/1945-7111/ac6220 VL - 169 IS - 4 SP - 044508 PB - IOP science AN - OPUS4-55027 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jamro, R. A1 - Mente, Tobias A1 - Kardjilov, N. A1 - Markötter, Henning A1 - Al-Falahat, Ala'A. M. A1 - Woracek, R. A1 - Manke, I. A1 - Griesche, Axel T1 - Temperature distribution during welding measured by neutron imaging N2 - This study was carried out to investigate the neutron transmission signal as a function of sample temperature during a welding process. A theoretical description that includes the Debye-Waller factor was used to describe the temperature influence on the neutron crosssections. Neutron imaging using a monochromatic beam helps to observe transmission variations related to the material temperature. In-situ neutron imaging of welding experiments show the distribution of the temperature in bulk steel samples. The performed finite element modelling of expected temperature distributions shows good agreement with the obtained experimental data. KW - Neutron imaging KW - Debye-Waller-Faktor PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-586268 DO - https://doi.org/10.1088/1742-6596/2605/1/012026 VL - 2605 SP - 1 EP - 10 PB - IOP Publishing Ltd. AN - OPUS4-58626 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kardjilov, N A1 - Manke, I A1 - Hilger, A A1 - Arlt, T A1 - Bradbury, R A1 - Markötter, Henning A1 - Woracek, R A1 - Strobel, M A1 - Treimer, W A1 - Banhart, J T1 - The Neutron Imaging Instrument CONRAD — Post‐Operational Review N2 - The neutron imaging instrument CONRAD was operated as a part of the user program of the research reactor BER‐II at Helmholtz‐Zentrum Berlin (HZB) from 2005 to 2020. The Instrument was designed to use the neutron flux from the cold source of the reactor, transported by a curved neutron guide. The pure cold neutron spectrum provided a great advantage in the use of different neutron optical components such as focusing lenses and guides, solid‐state polarizers, Monochromators and phase gratings. The flexible setup of the instrument allowed for implementation of new methods including wavelength‐selective, dark‐field, phase‐contrast and imaging with polarized neutrons. In summary, these developments helped to attract a large number of scientists and industrial customers, who were introduced to neutron imaging and subsequently contributed to the Expansion of the neutron imaging community. KW - Neutron imaging KW - Neutron scattering KW - Neutron instrument KW - Tomography PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-534190 DO - https://doi.org/10.3390/ jimaging7010011 VL - 7 IS - 11 SP - 7010011 PB - MDPI AN - OPUS4-53419 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mohseninia, A A1 - Eppler, M A1 - Kartouzian, D A1 - Markötter, Henning A1 - Kardjilov, N A1 - Wilhelm, F A1 - Scholta, J A1 - Manke, I T1 - PTFE Content in Catalyst Layers and Microporous Layers: Effect on Performance and Water Distribution in Polymer Electrolyte Membrane Fuel Cells N2 - This work describes the effects of catalyst layers (CLs) consisting of hydrophobic PTFE on the performance and water management of PEM fuel cells. Catalyst inks with various PTFE contents were coated on Nafion membranes and characterized using contact angle measurements, SEX-EDX, and mercury porosimetry. Fuel cell tests and electrochemical impedance spectroscopy (EIS) were conducted under varying operating conditions for the prepared materials. At dry conditions, CLs with 5 wt.% PTFE were advantageous for cell performance due to improved membrane hydration, whereas under humid conditions and high air flow rates CLs with 10 wt.% PTFE improved the performance in high current density region. Higher PTFE contents (⩾20 wt.%) increased the mass transport resistance due to reduced porosity of the CLs structure. Operando neutron radiography was utilized to study the effects of hydrophobicity gradients within CLs and cathode microporous layer (MPLC) on liquid water distribution. More hydrophobic CLs increased the water content in adjacent layers and improved performance, especially at dry conditions. MPLC with higher PTFE contents increased the overall liquid water within the CLs and GDLs and escalated the water transfer to the anode side. Furthermore, the role of back-diffusion transport mechanism on water distribution was identified for the investigated cells. KW - Neutron imaging KW - Polymer Electrolyte Membrane Fuel Cell KW - Catalyst Layer KW - Microporous Layer KW - Water Distribution PY - 2021 DO - https://doi.org/10.1149/1945-7111/abec53 VL - 168 IS - 3 SP - 034509 PB - IOP Science AN - OPUS4-52402 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, R. A1 - Boenke, T. A1 - Dörfler, S. A1 - Abendroth, T. A1 - Härtel, P. A1 - Althues, H. A1 - Kaskel, S. A1 - Kardjilov, N. A1 - Markötter, Henning A1 - Sintschuk, Michael A1 - Hilger, A. A1 - Manke, I. A1 - Risse, S. T1 - Multimodal Operando Analysis of Lithium Sulfur Multilayer Pouch Cells: An In-Depth Investigation on Cell Component Design and Performance N2 - This study presents an innovative operando analysis of lithium-sulfur (Li/S) multilayer pouch cells, employing a combination of lab-source and synchrotron x-ray imaging to investigate sulfur crystallite dissolution and lithium dendrite formation. By integrating advanced X-ray imaging, impedance spectroscopy, and simultaneous monitoring of temperature and pressure, the research uncovers critical insights into the behavior of active and inactive cell components. The analysis reveals significant degradation increments, primarily driven by side product accumulation and the deterioration of lithium microstructures, which contribute to performance loss over cycling. Additionally, temperature distribution analysis shows a strong correlation between joule heating, polarization resistance, and the observed endothermic processes during crystallization. These findings provide a comprehensive understanding of the mechanistic processes within industrially relevant pouch cells, highlighting opportunities for optimizing Li/S cell designs and advancing high-energy-density battery systems for commercial applications. KW - Current collector perforation KW - Impedance spectroscopy KW - Lthium sulfur batteries KW - Multilayer pouch cells KW - X-ray imaging PY - 2025 DO - https://doi.org/10.1002/aenm.202404256 SP - 1 EP - 12 PB - Wiley VHC-Verlag AN - OPUS4-62436 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pacheco, V. A1 - Marattukalam, J. J. A1 - Karlsson, D. A1 - Dessieux, L. A1 - Tran, K. V. A1 - Beran, P. A1 - Manke, I. A1 - Kardjilov, N. A1 - Markötter, Henning A1 - Sahlberg, M. A1 - Woracek, R. T1 - On the relationship between laser scan strategy, texture variations and hidden nucleation sites for failure in laser powder-bed fusion N2 - While laser powder-bed fusion has overcome some of the design constraints of conventional manufacturing methods, it requires careful selection of process parameters and scan strategies to obtain favorable properties. Here we show that even simple scan strategies, complex ones being inevitable when printing intricate designs, can inadvertently produce local alterations of the microstructure and preferential grain orientation over small areas – which easily remain unnoticed across the macroscale. We describe how a combined usage of neutron imaging and electron backscatter diffraction can reveal these localized variations and explain their origin within cm-sized parts. We explain the observed contrast variations by linking the neutron images to simulated data, pole figures and EBSD, providing an invaluable reference for future studies and showing that presumably minor changes of the scan strategy can have detrimental effects on the mechanical properties. In-situ tensile tests reveal that fracture occurs in a region that was re-melted during the building process. KW - Laser powder-bed fusion KW - Texture KW - Preferential orientation KW - Diffraction contrast neutron imaging KW - Bragg-edge PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-568054 DO - https://doi.org/10.1016/j.mtla.2022.101614 VL - 26 SP - 1 EP - 9 PB - Elsevier B.V. AN - OPUS4-56805 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Peruzzi, N. A1 - Galli, S. A1 - Helmholz, H. A1 - Kardjilov, N. A1 - Krüger, D. A1 - Markötter, Henning A1 - Moosmann, J. A1 - Orlov, D. A1 - Prgomet, Z. A1 - Willumeit-Römer, R. A1 - Wennerberg, A. A1 - Bech, M. T1 - Multimodal ex vivo methods reveal that Gd-rich corrosion byproducts remain at the implant site of biodegradable Mg-Gd screws N2 - Extensive research is being conducted on magnesium (Mg) alloys for bone implant manufacturing, due to their biocompatibility, biodegradability and mechanical properties. Gadolinium (Gd) is among the most promising alloying elements for property control in Mg alloy implants; however, its toxicity is contro- versial. Investigating Gd behavior during implant corrosion is thus of utmost importance. In this study, we analyzed the degradation byproducts at the implant site of biodegradable Mg-5Gd and Mg-10Gd implants after 12 weeks healing time, using a combination of different imaging techniques: histology, energy-dispersive x-ray spectroscopy (EDX), x-ray microcomputed tomography (μCT) and neutron μCT. The main finding has been that, at the healing time in exam, the corrosion appears to have involved only the Mg component, which has been substituted by calcium and phosphorus, while the Gd remains localized at the implant site. This was observed in 2D by means of EDX maps and extended to 3D with a novel application of neutron tomography. X-ray fluorescence analysis of the main excretory organs also did not reveal any measurable accumulation of Gd, further reinforcing the conclusion that very limited or no removal at all of Gd-alloy happened during degradation. KW - Magnesium-gadolinium alloy KW - Biodegradable implant KW - Multimodal analysis KW - Energy-dispersive x-ray spectroscopy KW - Micro-computed tomography PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-535910 DO - https://doi.org/10.1016/j.actbio.2021.09.047 SN - 1742-7061 SP - 1 EP - 10 PB - Elsevier Ltd. AN - OPUS4-53591 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -