TY - JOUR A1 - Altenkirch, J. A1 - Gibmeier, J. A1 - Kostov, V. A1 - Kromm, Arne A1 - Kannengießer, Thomas A1 - Doyle, S. A1 - Wanner, A. T1 - Time- and temperature-resolved synchrotron X-ray diffraction: observation of phase transformation and strain evolution in novel low temperature transformation weld filler materials JF - The journal of strain analysis for engineering design N2 - Solid-state phase transformations and the evolution of thermal and elastic strains in novel low temperature transformation (LTT) weld filler materials in the near surface region are monitored in real time by means of an innovative experimental set-up at the PDIFF (powder diffraction) beamline at the synchrotron light source ANKA (Angströmquelle Karlsruhe) at the KIT (Karlsruhe Institute for Technology). The key components of the diffraction set-up are two fast microstrip line detectors, which enables the strain evolution to be followed as a function of time and temperature for a 0.5?s counting time. During controlled heating and cooling cycles, as well as during near welding cycles, the martensite–austenite–martensite phase transitions are analysed. The transformation kinetics are monitored during resistance heating of small chips of the pure LTT alloys and during gas tungsten arc welding of simplified LTT welds using a specially designed welding rig for in-situ studies on the diffraction instruments. Under the mechanically unconstrained condition allowing free thermal expansion and shrinkage, the LTT alloys are found to exhibit decreasing transformation temperatures Ac and MS and increasing phase fraction of retained austenite for increasing Ni content. The strain evolution during welding reveals increased compressive stresses upon welding, which is attributed to the martensite formation upon cooling, which counteracts the thermal contraction strains. Comparison of the transformation temperatures reveals higher values than in the pure LTT alloys, but no variation between the different alloys. On the one hand, this is attributed to preferred grain orientation affecting the diffraction measurements and the determination of the transformation temperatures. On the other hand, it is possible that with the different chemical compositions of the LTT alloys and the mechanical constraints during welding, the evolution of the residual strain and stress may vary and result in counteracting affects with respect to lowered martensite start temperatures. KW - In-situ synchrotron X-ray diffraction KW - Low temperature transformation KW - Welding PY - 2011 DO - https://doi.org/10.1177/0309324711413190 SN - 0309-3247 SN - 2041-3130 VL - 46 IS - 7 SP - 563 EP - 579 PB - Sage CY - London AN - OPUS4-24683 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Altenkirch, J. A1 - Gibmeier, J. A1 - Kromm, Arne A1 - Kannengießer, Thomas A1 - Nitschke-Pagel, T. A1 - Hofmann, M. T1 - In situ study of structural integrity of low transformation temperature (LTT)-welds JF - Materials science and engineering A N2 - We discuss the stability of weld residual strain under static and quasi cyclic transverse tensile loading in the elastic and elastic–plastic region. The test welds were joined with low transformation temperature weld filler materials with 10 wt% Cr and varying Ni-content from 8 to 12 wt%. Using neutron diffraction the residual lattice strain in the martensitic α'- and austenitic γ-phase in the fusion zone as well as the ferritic α-phase in the heat affected zone and base metal as induced by welding, superimposed by stepwise tensile loading and after unloading was measured. The amount of retained austenite in the fusion zone increases with increasing Ni-content, but it decreases with increasing load level due to stress induced martensite formation. In the as-welded condition the transverse macroscopic residual lattice strain was found to be in low compression in the fusion zone in each weld, while the heat affected zone was in tension. Local plastic deformation of the γ-phase as a result of yielding during tensile loading in combination with the change in phase fraction resulted in increased macroscopic compression in the fusion zone. The reduced yield strength in the heat affected zone resulted in plastic deformation and a considerable shift into compression. Comparison with the cross weld distribution of the hardness and FWHM of the neutron diffraction interference lines supported the assumption of plastic deformation of the γ- and α-phase in the fusion and heat affected zone, respectively, while the α'-phase in the fusion zone was stressed within the elastic regime only. Microstructural observations as well as measurement of the local γ-phase fraction by means of laboratory X-ray diffraction in the fusion zone strengthen these observations. KW - Low transformation temperature KW - Residual stress KW - Neutron diffraction PY - 2011 DO - https://doi.org/10.1016/j.msea.2011.03.091 SN - 0921-5093 SN - 1873-4936 VL - 528 IS - 16-17 SP - 5566 EP - 5575 PB - Elsevier CY - Amsterdam AN - OPUS4-24359 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Kromm, Arne A1 - Kannengießer, Thomas A1 - Gibmeier, J. A1 - Genzel, C. A1 - Mee, V. van der T1 - Determination of Residual Stresses in Low Transformation Temperature (LTT-) Weld Metals using X-ray and High Energy Synchrotron Radiation T2 - IIW Document KW - Filler material KW - Low transformation temperature KW - Synchrotron radiation KW - Phase specific residual stresses KW - Energy dispersive diffraction PY - 2007 IS - II-1658r1-07 SP - 1 EP - 17 PB - International Institute of Welding CY - Paris AN - OPUS4-15716 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kromm, Arne A1 - Kannengießer, Thomas A1 - Gibmeier, J. A1 - Genzel, C. A1 - Van der Mee, V. T1 - Determination of residual stresses in low transformation temperature (LTT -) welds metals using X-rayand high energy synchrotron radiation JF - Welding in the world N2 - Crack and fatigue resistance are relevant evaluation criteria for welded joints and are decreased by tensile residual stresses resulting from the welding and cooling process, while compressive residual stresses can have a positive influence on the characteristics mentioned. In order to generate compressive residual stresses, a set of post weld treatment procedures is available, like shot peening, hammering, etc. These procedures have the disadvantage that they are time and cost extensive and have to be applied after welding. As another point, such technologies can only produce compressive stresses at the top surface, i.e. can only contribute to the reduction of the risk of cracks initiated at the surface, like fatigue cracks. A chance to generate compressive stresses over the complete weld joint during the welding procedure is offered by the so-called Low Transformation Temperature (LTT -) filler wires. Compared to conventional wires, these materials show lower phase transformation temperatures, which can work against coolingrelated tensile stresses, resulting from respective shrinkage restraint. In consequence, distinct compressive residual stresses can be observed within the weld and adjacent areas. The strength of these fillers makes them potentially applicable to high-strength steel welding. Welds produced with different LTT – filler wires have shown different levels and distributions of the resulting residual stresses depending on the specific transformation temperature. The transformation temperatures are determined by temperature measurement. Classical X-ray diffraction as well as diffraction methods using high energy synchrotron radiation have been used for residual stress analysis. By means of high energy synchrotron diffraction in reflection mode residual stress depth gradients can be determined nondestructively. The phase selective nature of the diffraction measurements enables the simultaneous determination of the phase specific residual stresses of all contributing crystalline phases within one experiment. The application of white beam diffraction implies recording of a multitude of diffraction lines within the energy range of the provided energy spectrum of the white beam. By this means phase specific residual stress depth distributions up to distances of 150 ìm below the surface can be analysed for steel using the energy dispersive set-up of the HMI-beamline EDDI at the Bessy site, Berlin, providing an energy range between 20-150 keV. As a side effect quantitative phase analysis can be carried out using white energy dispersive diffraction e.g. the determination of the content of retained austenite in the weld. KW - Filler materials KW - Low temperature KW - Reference lists KW - Residual stresses KW - Temperature KW - Transformation KW - Synchrotron radiation KW - Phase specific residual stresses KW - Energy dispersive diffraction PY - 2009 SN - 0043-2288 SN - 1878-6669 VL - 53 IS - 1/2 SP - 3 EP - 16 PB - Springer CY - Oxford AN - OPUS4-19214 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kromm, Arne A1 - Kannengießer, Thomas A1 - Gibmeier, J. T1 - In-situ observation of phase transformations during welding of low transformation temperature filler material JF - Materials science forum KW - LTT filler material KW - In-situ observation KW - Energy dispersive diffraction KW - Transformation temperature KW - Residual stress PY - 2010 DO - https://doi.org/10.4028/www.scientific.net/MSF.638-642.3769 SN - 0255-5476 VL - 638-642 SP - 3769 EP - 3774 PB - Trans Tech Publications CY - Aedermannsdorf, Switzerland AN - OPUS4-20725 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kannengießer, Thomas A1 - Kromm, Arne A1 - Gibmeier, J. A1 - Rethmeier, Michael T1 - In-situ-Analyse der Phasenumwandlungskinetik während des Schweißens JF - MP materials testing N2 - Zugeigenspannungen, wie sie beim Schweißprozess durch inhomogene Temperaturverteilungen und Schrumpfungen hervorgerufen werden, können die Lebensdauer geschweißter Verbindungen signifikant herabsetzen. Eine neue und außerordentlich attraktive Methode, um Druckeigenspannungen bereits während des Schweißens gezielt einzustellen, gelingt mit sogenannten LTT (Low Transformation Temperature)-Legierungen. LTT-Legierungen weisen eine martensitische Phasenumwandlung bei relativ niedrigen Temperaturen auf, wobei die damit verbundene Volumenexpansion zu einer Reduktion der Schrumpfeigenspannungen bzw. Erzeugung von Druckeigenspannungen führt. Zum direkten Nachweis der Phasenumwandlungen und der damit verbundenen resultierenden Schweißeigenspannungen wurden erstmals In-situ-Schweißexperimente unter Nutzung hoch energetischer, polychromatischer Synchrotronstrahlung (Weißstrahl) realisiert, um die Umwandlungskinetik während eines realen Schweißprozesses und die daraus resultierenden Schweißeigenspannungen zu analysieren. Es wird gezeigt, dass mit LTT-Legierungen signifikante Druckeigenspannungen in der Schweißnaht erreicht werden. PY - 2010 SN - 0025-5300 VL - 52 IS - 4 SP - 204 EP - 210 PB - Hanser CY - München AN - OPUS4-21219 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gibmeier, J. A1 - Obelode, E. A1 - Altenkirch, J. A1 - Kromm, Arne A1 - Kannengießer, Thomas T1 - Residual stress in steel fusion welds joined using low transformation temperature (LTT) filler material JF - Materials science forum N2 - Welding residual stress is of major concern for structural integrity assessment in industrial components. Shear and volume strains resulting from the austenite-martensite-transformation affect the development of residual stress during welding. Controlling the phase transformation allows adjustment of the welding residual stress. Low transformation temperature (LTT) weld filler materials exhibiting reduced MS-temperatures allow postponing the phase transformation. The associated strain arising from the delayed transformation compensates for the thermal contraction strains and as such may reduce tensile or even introduce compressive residual stress. In this article we discuss the tri-axial residual stress distribution in 15 mm S690Q steel plates joined with LTT filler materials with 10 wt% Cr and a Ni-content that varies from 8 to 12 wt%. Using complementary synchrotron X-ray and neutron diffraction stress analysis the macroscopic residual stress was derived from the phase specific lattice strain and phase fraction of martensite and retained austenite, respectively. The local phase specific unstrained lattice parameters were determined using stress relieved combs. The investigation revealed increasing phase fraction of retained austenite with increasing Ni-content. Further, independent of the Ni-content in each weld in the fusion zone, significant compressive residual stresses were found in the longitudinal direction, which are balanced by tensile residual stresses in the heat affected zone (HAZ). In the weld transverse and normal direction the stress distribution is qualitatively similar but less in magnitude. The increased amount of retained austenite reduces the compressive stress arising from shear and volume strains during the delayed phase transformation and therefore no significant increase in compression was observed for decreasing MS-temperatures. KW - Welding residual stresses KW - Neutron diffraction KW - LTT filler materials PY - 2014 DO - https://doi.org/10.4028/www.scientific.net/MSF.768-769.620 SN - 0255-5476 VL - 768-769 SP - 620 EP - 627 PB - Trans Tech Publications CY - Aedermannsdorf, Switzerland AN - OPUS4-29706 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Held, E. A1 - Ohl, H. A1 - Gibmeier, J. A1 - Dixneit, Jonny A1 - Kromm, Arne A1 - Kannengießer, Thomas ED - Petzow, G. T1 - Mikrostruktur- und Härteentwicklung in Schweißnähten mit neuartigen LTT-Schweißzusatzwerkstoffen T2 - Fortschritte in der Metallographie - Vortragstexte der 47. Metallographie-Tagung T2 - 47. Metallographie-Tagung CY - Friedrichshafen, Germany DA - 2013-09-18 PY - 2013 SN - 978-3-88355-398-6 VL - 45 SP - 297 EP - 302 AN - OPUS4-29710 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kromm, Arne A1 - Thomas, Maximilian A1 - Kannengießer, Thomas A1 - Gibmeier, J. A1 - Vollert, F. T1 - Assessment of the Solidification Cracking Susceptibility of Welding Consumables in the Varestraint Test by Means of an Extended Evaluation Methodology JF - Advanced Engineering Materials N2 - Various test methods are available for assessing the susceptibility of materials to solidification cracking during welding. In the widely used Varestraint test, the crack length is selected as a criterion as a function of the applied bending strain. Unfortunately, the crack length does not characterize the material behavior alone but depends to varying degrees on the individual test parameters used, which makes the interpretation of the results difficult. In addition, the crack length is not comparable under different test conditions. To overcome these disadvantages, we have developed a novel evaluation methodology that decouples the machine influence from the material behavior. The measured crack length is related to the maximum possible value specified by welding speed and deformation time. This relative crack length is calculated numerically, considering the orientation of the cracks. Experiments on two high-alloy martensitic welding consumables show that, in contrast to the conventional evaluation, a comparison of different welding parameters becomes possible. Furthermore, the strain rate proved to be a suitable crack criterion in agreement with Prokhorov's hot cracking model. KW - Welding KW - Solidification cracking KW - Varestraint test PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-545780 DO - https://doi.org/10.1002/adem.202101650 SN - 1438-1656 SP - 2101650 PB - Wiley online library AN - OPUS4-54578 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gibmeier, J. A1 - Held, A. A1 - Altenkirch, J. A1 - Kromm, Arne A1 - Kannengießer, Thomas A1 - Buslaps, T. T1 - Real time monitoring of phase transformation and strain evolution in LTT weld filler material using EDXRD JF - Journal of materials processing technology N2 - For a newly developed 10% Cr and 10% Ni low transformation temperature (LTT) weld filler material, the local phase transformation kinetics and the strain evolution during gas tungsten arc welding (GTAW) under real welding conditions was studied. An experimental set-up and a measuring and evaluation strategy are presented to gain a real time insight into the welding process. The experiments were carried out at the beam line ID15@ESRF using a two detector EDXRD (energy dispersive X-ray diffraction) set-up and high energy synchrotron X-rays. The time-resolved diffraction analysis during welding was carried out locally throughout the weld in longitudinal as well as in transverse direction to the weld line to examine the interdependence of the strain state and the transformation kinetics. This comprehension is crucial for the optimization of the weld process, and thus for the tailoring of the resulting residual stress states, which is one of the main issues for the application of LTT alloys. Using the herein proposed approach EDXRD diffraction pattern can be monitored during real welding with a counting rate of 5 Hz. By means of the time resolved diffraction data the local transformation temperatures and times were determined and the local phasespecific strain evolutions are discussed with respect to the transformation rates and the time-delayed phase transformations. KW - In situ synchrotron X-ray diffraction KW - Low transformation temperature KW - Welding PY - 2014 DO - https://doi.org/10.1016/j.jmatprotec.2014.06.008 SN - 0924-0136 SN - 1873-4774 VL - 214 IS - 11 SP - 2739 EP - 2747 PB - Elsevier CY - Amsterdam AN - OPUS4-30955 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -