TY - JOUR A1 - Sturm, Patrick A1 - Gluth, Gregor A1 - Jäger, Christian A1 - Brouwers, H.J.H. A1 - Kühne, Hans-Carsten T1 - Sulfuric acid resistance of one-part alkali-activated mortars JF - Cement and Concrete Research N2 - One-part alkali-activated (geopolymer) mortars based on three different silica-rich starting materials and sodium aluminate, with and without ground granulated blast furnace slag (GGBFS) addition, were tested regarding sulfuric acid resistance according to DIN 19573:2016-03 (70 days at pH = 1). Corresponding pastes were characterized by XRD, SEM, chemical analysis, 29Si MAS NMR and 1H-29Si CPMAS NMR after water storage and after acid exposure. The mortars exhibited a high resistance against sulfuric acid attack, with the best ones conforming to the requirements of DIN 19573:2016-03. The analytical results showed that this was due to precipitation of silica gel at the acid-mortar interface, which formed a mechanically stable layer that protected the subjacent mortar and thus inhibited further degradation. The addition of GGBFS decreased the acid resistance via formation of expansive calcium sulfate phases. KW - Alkali activated materials KW - Acid resistance KW - Nuclear magnetic resonance KW - One-part geopolymers PY - 2018 DO - https://doi.org/10.1016/j.cemconres.2018.04.009 SN - 0008-8846 VL - 109 SP - 54 EP - 63 PB - Elsevier Ltd. AN - OPUS4-44722 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gluth, Gregor A1 - Sturm, Patrick A1 - Greiser, Sebastian A1 - Jäger, Christian A1 - Brouwers, H.J.H. A1 - Kühne, Hans-Carsten T1 - Einkomponentige alkaliaktivierte Bindemittel und Mörtel mit hohem Widerstand gegen Schwefelsäureangriff T2 - Tagung Bauchemie N2 - Einkomponentige alkaliaktivierte Bindemittel (AAB), d. h. AAB, bei denen der Aktivator als Feststoff im Bindemittel vorliegt, weisen Vorteile hinsichtlich der praktischen Anwendung im Bauwesen gegenüber konventionellen AAB auf. Einkomponentige AAB lassen sich als Gemische aus reaktiver Silica und Natriumaluminat herstellen, wobei die Reaktionsprodukte von der eingesetzten Silica und den Verhältnissen Na2O/Al2O3/SiO2/H2O abhängen: Während Mikrosilica und ähnliche Reststoffe zu zeolithreichen Produkten führen, erhält man aus Reisschalenasche vollständig amorphe Gele (sog. «Geopolymere »). Mörtel auf Basis solcher Bindemittel entsprechen den Anforderungen von DIN 19573:2016-03 hinsichtlich des Widerstands gegen Schwefelsäureangriff (Prüfung bei pH = 1 für 70 d) und sind damit potentiell als Reparatursysteme für Abwasserinfrastruktur geeignet. Untersuchungen mittels 29Si-MAS-NMR und 1H-29Si-Kreuzpolarisations(CP)-MAS-NMR sowie REM-Aufnahmen von erhärteten und dem Schwefelsäureangriff ausgesetzten AAB zeigen, dass der hohe Säurewiderstand v. a. auf die Fällung von Silicagel an der Grenzfläche Mörtel/Säure zurückzuführen ist, wodurch der Korrosionsfortschritt in darunterliegenden Schichten verlangsamt wird. T2 - Tagung Bauchemie der GDCh-Fachgruppe Bauchemie CY - Aachen, Germany DA - 30.09.2019 KW - Alkaliaktivierte Bindemittel KW - Biogene Schwefelsäurekorrosion KW - Abwasserinfrastruktur KW - Reparatursysteme PY - 2019 SP - 107 EP - 113 PB - Gesellschaft Deutscher Chemiker CY - Frankfurt am Main AN - OPUS4-49264 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Stuff, Maria A1 - Rübner, Katrin A1 - Prinz, Carsten A1 - Rische, N. A1 - Chronz, M. A1 - Kühne, Hans-Carsten ED - Siegesmund, S. ED - Middendorf, B. T1 - Towards a better understanding of tuff stone deterioration T2 - Monument Future: Decay and conservation of stone. - Proceedings of the 14th international congress on the deterioration and conservation of stone N2 - Stone deterioration is the result of a complex interaction of external physical, chemical and biological forces with the mineralogical-petrophysical properties of the stone. With a better understanding of how these properties are linked to material behavior and durability, more effective measures for stone conservation can be developed. Studying these interactions in tuff is particularly complex due to the naturally high heterogeneity of tuff rocks. The first aim of a current research project is to combine the results of recent and older studies on tuff deterioration. Furthermore, the literature overview is complemented by our own investigation of Weibern and Ettringen tuff, with a focus on pore structure characteristics. T2 - STONE - 14th international congress on the deterioration and conservation of stone CY - Meeting was canceled DA - 07.09.2020 KW - Pore structure KW - Weathering KW - Weibern tuff KW - Ettringen tuff PY - 2020 SN - 978-3-96311-172-3 SP - 805 EP - 810 PB - Mitteldeutscher Verlag CY - Halle (Saale) AN - OPUS4-51549 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gluth, Gregor A1 - Sturm, Patrick A1 - Greiser, Sebastian A1 - Jäger, Christian A1 - Kühne, Hans-Carsten ED - Wang, J. ED - Kriven, W. ED - Fey, T. ED - Colombo, P. ED - Weber, W.J. ED - Amoroso, J. ED - Fahrenholtz, W.G. ED - Shimamura, K. ED - Halbig, M. ED - Kirihara, S. ED - Wu, Y. ED - Shurgart, K. T1 - One-part geopolymers and aluminosilicate gel-zeolite composites: factors influencing microstructure and engineering properties T2 - Proceedings of the 42nd International Conference on Advanced Ceramics and Composites: Ceramic Engineering and Science Proceedings Volume 39, Issue 3 N2 - Mixing and curing of geopolymers and related alkali-activated materials without storage and handling of highly alkaline solutions possesses advantages regarding safety and economic viability. One possible approach is to produce these materials from solid silica feedstocks and solid sodium aluminate, and subsequent mixing with water. We present a comparison between geopolymers and aluminosilicate gel-zeolite composites synthesized by this route from different silica feedstocks (by-product silica from chlorosilane production, microsilica, rice husk ash) and with different SiO2/Al2O3 ratios, using results from XRD, NMR, SEM, thermal analysis, mechanical and acid resistance testing. The use of rice husk ash favors formation of a fully amorphous geopolymer with high strength. Utilization of the other silica feedstocks leads to formation of aluminosilicate gel-zeolite composites, the amount and kind of zeolites depending on the feedstock and the SiO2/Al2O3 ratio. These composites show beneficial dehydration behavior, viz. no distinct dehydration step of thermal strain, with the phase assemblage after heating to 1000°C controlled by the starting composition. Mortars produced from both, the geopolymers as well as the composites, exhibit high resistance to sulfuric acid attack, making them promising materials for the construction and the repair of industrial and sewer structures. T2 - 42nd International Conference on Advanced Ceramics and Composites CY - Daytona Beach, FL, USA DA - 21.01.2018 KW - Alkali-activated materials KW - One-part geopolymers KW - Sulfuric acid resistance KW - High-temperature resistance PY - 2019 DO - https://doi.org/10.1002/9781119543381.ch17 VL - 39 IS - 3 SP - 183 EP - 196 PB - John Wiley & Sons AN - OPUS4-47282 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -