TY - JOUR A1 - Friedrich, Jörg Florian A1 - Unger, Wolfgang A1 - Lippitz, Andreas A1 - Geng, Sh. A1 - Koprinarov, Ivaylo A1 - Kühn, Gerhard A1 - Weidner, Steffen T1 - Modelling plasma-induced reactions on polymer surfaces using aliphatic self-assembling and LB layers PY - 1998 SN - 0257-8972 VL - 98 SP - 1132 EP - 1141 PB - Elsevier Science CY - Lausanne AN - OPUS4-6999 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Holländer, A. A1 - Kühn, Gerhard T1 - Matrix-assisted Laser Desorption/Ionization Mass Spectrometry of C36- Alkane degradated by Vacuum Ultraviolet Radiation PY - 1997 SN - 0951-4198 SN - 1097-0231 VL - 11 SP - 447 EP - 450 PB - Wiley CY - Chichester AN - OPUS4-11095 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Friedrich, Jörg Florian A1 - Kühn, Gerhard T1 - Kontrolle der Plasmamodifizierung von Polymeroberflächen mittels ESCA PY - 1998 VL - 70 SP - 5 CY - Darmstadt AN - OPUS4-7285 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Kühn, Gerhard A1 - Friedrich, Jörg Florian T1 - Infrared-Matrix-assisted Laser Desorption/Ionization and Infrared-Laser Desorption/Ionization Investigations of Synthetic Polymers PY - 1998 SN - 0951-4198 SN - 1097-0231 VL - 12 SP - 1373 EP - 1381 PB - Wiley CY - Chichester AN - OPUS4-6988 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Weidner, Steffen A1 - Kühn, Gerhard A1 - Decker, Renate A1 - Roessner, D. A1 - Friedrich, Jörg Florian T1 - Influence of Plasma Treatment on the Molar Mass of Poly(ethylene terephthalate) Investigated by Different Chromatographic and Spectroscopic Methods N2 - The influence of different types of low and atmospheric pressure plasma on poly(ethylene terephthalate) (PET) has been studied in terms of changes in molar mass and molar mass distribution. Apart from a variation of plasma gases (oxygen, helium) different types of plasma (microwave, radio frequency, corona discharge) were used for the plasma surface modification. The changes in molar mass and types of functional end groups of lower molar mass products were investigated by means of matrix-assisted laser desorption/ionization time of flight mass spectrometry (MALDI-TOFMS), whereas the high-molar mass fraction was analyzed by means of size-exclusion chromatography (SEC). The formation of crosslinked products during exposure to a helium plasma, which emits preponderately energy-rich and intense ultraviolet radiation, was proved by means of thermal field-flow fractionation (ThFFF). This method combined with a multiangle laser light scattering (MALLS) detector allows detection of weakly crosslinked polymers and microgels. © 1998 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 36: 1639-1648, 1998 KW - Poly(ethylene terephthalate) KW - PET KW - Plasma PY - 1998 UR - http://www3.interscience.wiley.com/cgi-bin/abstract/36482/ABSTRACT DO - https://doi.org/10.1002/(SICI)1099-0518(19980730)36:10<1639::AID-POLA17>3.0.CO;2-H SN - 0360-6376 SN - 0887-624X VL - 36 IS - 10 SP - 1639 EP - 1648 PB - Wiley CY - Hoboken, NJ AN - OPUS4-6989 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Friedrich, Jörg Florian A1 - Möller, B. A1 - Kühn, Gerhard A1 - Unger, Wolfgang A1 - Krüger, P. T1 - Improvement of adhesion properties of polymers by producing oxyfluorinated surfaces PY - 2001 SN - 0016-4232 VL - 92 IS - 5 SP - 1334 EP - 1444 PB - Leuze CY - Saulgau, Württ. AN - OPUS4-6973 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kühn, Gerhard A1 - Retzko, Iris A1 - Lippitz, Andreas A1 - Unger, Wolfgang A1 - Friedrich, Jörg Florian T1 - Homofunctionalized polymer surfaces formed by selective plasma processes N2 - Several possibilities exist to produce a modified polymer surface with a high density of only one sort of functional group such as: (i) the plasma grafting of unfragmented monomer molecules and their polymerization forms OH, NH2, COOH groups, etc. in concentrations of approximately 25 groups per 100 C atoms; (ii) selective plasma bromination provides 10–25 CBr groups; (iii) the plasma oxidation of polymer surfaces in an O2 plasma followed by the chemical reduction of all O-containing groups to OH groups by diborane, vitride™ (Na complex) or LiAlH4 yields 9–14 OH groups per 100 carbon atoms; and (iv) the grafting of spacers with different endgroups onto OH or CBr groups produces 7–10 spacer molecules/100 C. This work was focused on the formation of thin plasma deposited polymer layers with a maximum of (homo)functional groups and with a minimum of chemical irregularities using the pulsed plasma technique. The monomers were allylalcohol, allylamine, acrylonitrile and acrylic acid. The further intent was to study the interactions of functional groups (OH, COOH, NH2) and deposited metals (Cr, Al, Ti). It was expected that more basic (NH2), weakly basic or neutral (OH) or more acidic (COOH) groups would show different interactions and chemical reactions with metal atoms. KW - Pulsed plasma polymerization KW - Functional groups KW - Long-term stability KW - Polymer-metal composites PY - 2001 DO - https://doi.org/10.1016/S0257-8972(01)01056-8 SN - 0257-8972 VL - 142-144 SP - 494 EP - 500 PB - Elsevier Science CY - Lausanne AN - OPUS4-6971 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Friedrich, Jörg Florian A1 - Schulz, Ulrich A1 - Kühn, Gerhard A1 - Erdmann, Jessica A1 - Möller, B. T1 - Glanzerhaltung von Autolacken - Verbessern der Lebensdauer eines 2K-Klarlacks durch Gasphasen-Fluorierung PY - 1999 SN - 0025-5300 VL - 41 SP - 375 EP - 378 PB - Carl Hanser Verlag CY - München AN - OPUS4-7284 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Friedrich, Jörg Florian A1 - Mix, Renate A1 - Kühn, Gerhard T1 - Functional groups bearing plasma homo and copolymer layers as adhesion promoters in metal-polymer composites N2 - Functional groups bearing monomers were pulsed plasma polymerised with a degree of retained functional groups of 55–91%. The following functional groups could be produced at a maximum of: 30 OH, 18 NH2, and 24 COOH per 100 C atoms. A plasma-initiated radical copolymerisation could also be realised using the functional group bearing monomers as a source of functionalities, olefins as ‘chain-extenders’ and dienes as ‘chemical cross-linkers’. The peel strengths of Al layers on such plasma polymers were correlated to the type and density of functional groups. KW - Functional groups KW - Adhesion promoters KW - Metal-polymer composites PY - 2003 DO - https://doi.org/10.1016/S0257-8972(03)00350-5 SN - 0257-8972 VL - 174-175 SP - 811 EP - 815 PB - Elsevier Science CY - Lausanne AN - OPUS4-2703 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Friedrich, Jörg Florian A1 - Kühn, Gerhard A1 - Mix, Renate A1 - Unger, Wolfgang T1 - Formation of Plasma Polymer Layers with Functional Groups of Different Type and Density at Polymer Surfaces and their Interaction with Al Atoms N2 - Monotype functionalizations with different types of functional groups (OH, NH2, COOH) on polypropylene and poly(tetrafluoroethylene) surfaces were synthesized using pulsed plasma-initiated homo- or copolymerization of functional group-carrying monomers. The maximum concentrations of functional groups were 31 OH, 18 NH2 or 24 COOH groups per 100 C atoms using allyl alcohol, allylamine or acrylic acid respectively as the monomer. The measured peel strengths of aluminium deposits increased linearly with the concentration of functional groups. Near the maximum concentration of OH (>27 OH/100 C atoms) or at moderate concentrations of COOH groups (>10 COOH/100 C atoms), constant (maximum) peel strengths were measured due to the mechanical collapse of one component in the composite (cohesive failure). Interface failures in Al-PP composites were found with COOH, NH2 and OH groups and cohesive failures were seen when higher concentrations of COOH groups were applied (>10 COOH/100 C atoms). PY - 2004 DO - https://doi.org/10.1002/ppap.200400008 SN - 1612-8850 SN - 1612-8869 VL - 1 IS - 1 SP - 28 EP - 50 PB - Wiley-VCH Verl. CY - Weinheim AN - OPUS4-4707 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -