TY - JOUR A1 - Griesche, Axel A1 - Dabah, Eitan A1 - Kannengießer, Thomas A1 - Kardjilov, N. A1 - Hilger, A. A1 - Manke, I. T1 - Three-dimensional imaging of hydrogen blister in iron with neutron tomography N2 - We investigated hydrogen embrittlement and blistering in electrochemically hydrogen-charged technical iron samples at room temperature. Hydrogen-stimulated cracks and blisters and the corresponding hydrogen distributions were observed by neutron tomography. Cold neutrons were provided by the research reactor BER II to picture the sample with a spatial resolution in the reconstructed three-dimensional model of ~25 µm. We made the unique observation that cracks were filled with molecular hydrogen and that cracks were surrounded by a 50 µm wide zone with a high hydrogen concentration. The zone contains up to ten times more hydrogen than the bulk material. The hydrogen enriched zone can be ascribed to a region of increased local defect density. Hydrogen also accumulated at the sample surface having the highest concentration at blistered areas. The surfaces of the brittle fractured cracks showed micropores visualized by scanning electron microscopy. The micropores were located at grain boundaries and were surrounded by stress fields detected by electron backscattered diffraction. The cracks clearly originated from the micropores. KW - Hydrogen embrittlement KW - Hydrogen diffusion KW - In situ KW - Neutron tomography KW - Iron PY - 2014 U6 - https://doi.org/10.1016/j.actamat.2014.06.034 SN - 1359-6454 SN - 1873-2453 VL - 78 SP - 14 EP - 22 PB - Elsevier Science CY - Kidlington AN - OPUS4-31068 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Griesche, Axel A1 - Dabah, Eitan A1 - Kannengießer, Thomas T1 - Neutron imaging of hydrogen in iron and steel N2 - Neutron radiography and tomography have been used for a time resolved in situ analysis and a 3D mapping of hydrogen diffusion in iron and steel. Samples were electrochemically charged with hydrogen and afterwards neutron transmission images were taken. Hydrogen diffusion coefficients in duplex stainless steel were determined at 623 K by measuring and comparing the sample's mean intensity with a hydrogen-free reference sample and subsequent normalisation to standards with known hydrogen content. In technical iron and in supermartensitic stainless steel the hydrogen distributions have been investigated. The radiographic images in iron show blisters, cracks and the distribution of molecular hydrogen inside cracks. The analysis of the diffusion behaviour of hydrogen out of a blister illustrates the capabilities of the method with respect to time and spatial resolution. The neutron tomography of supermartensitic tensile stressed samples illustrates the capability to visualise hydrogen distributions three-dimensionally. ------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------- On a utilisé la radiographie neutronique et la tomographie pour une analyse in situ à résolution temporelle et une cartographie 3D de la diffusion de l'hydrogène dans le fer et l'acier. On a chargé des échantillons par électrochimie avec de l'hydrogène et ensuite on a pris des images par émission de neutrons. On a déterminé les coefficients de diffusion de l’hydrogène dans l'acier inoxydable duplex à 623 K en mesurant et en comparant l'intensité moyenne de l'échantillon avec un échantillon de référence sans hydrogène et une normalisation subséquente à des échantillons références à teneur connue en hydrogène. On a examiné la distribution d'hydrogène dans le fer technique et dans l'acier inoxydable supermartensitique. Les images radiographiques du fer montrent des soufflures, des fissures, et la distribution de l'hydrogène moléculaire à l'intérieur des fissures. L'analyse du comportement de diffusion de l'hydrogène hors d'une soufflure illustre les possibilités de la méthode par rapport à la résolution temporelle et spatiale. La tomographie neutronique des échantillons supermartensitiques chargés en traction illustre la capacité de visualiser les distributions d'hydrogène en trois dimensions. KW - Neutron radiography KW - Hydrogen KW - Diffusion KW - Iron KW - Steel KW - Blister KW - Hydrogen assisted cracking PY - 2015 U6 - https://doi.org/10.1179/1879139514Y.0000000162 SN - 0008-4433 VL - 54 IS - 1 SP - 38 EP - 42 PB - Canadian Institute of Mining and Metallurgy CY - Montreal AN - OPUS4-32809 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -