TY - JOUR A1 - Beyer, Katrin A1 - Kannengießer, Thomas A1 - Griesche, Axel A1 - Schillinger, B. T1 - Neutron radiography study of hydrogen desorption in technical iron N2 - The purpose of the present study is to show the feasibility of examining hydrogen desorption in technical iron samples using neutron radiography at the ANTARES facility of the FRM II research reactor, Technische Universität München. It has been shown that this method is appropriate for in situ determination of hydrogen Desorption for concentrations as low as 20 ppmH. Experiments were carried out in the temperature range from room temperature up to 260 °C. Measurement was based on direct comparison between electrochemically hydrogen-loaded iron samples and hydrogen-free reference samples at the same temperature. This enables the determination of hydrogen concentration as a function of time and temperature. Ex situ carrier gas hot extraction experiments using the same temperature–time profiles as the neutron radiography experiments have been used to calibrate the greyscale values of the radiographs to defined hydrogen concentrations. It can be stated that hydrogen desorption correlates with sample temperature. KW - Neutron radiography KW - Hydrogen PY - 2011 U6 - https://doi.org/10.1007/s10853-011-5450-7 SN - 0022-2461 SN - 1573-4803 VL - 46 IS - 15 SP - 5171 EP - 5175 PB - Springer Science + Business Media B.V. CY - Norwell, Mass. AN - OPUS4-25150 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Beyer, Katrin A1 - Kannengießer, Thomas A1 - Griesche, Axel A1 - Schillinger, B. T1 - Study of hydrogen effusion in austenitic stainless steel by time-resolved in-situ measurements using neutron radiography N2 - The purpose of the present study was to show the feasibility of measuring hydrogen effusion in austenitic stainless steel (1.4301) using neutron radiography at the facility ANTARES of the research reactor FRM II of the Technische Universität München. This method is appropriate to measure in-situ hydrogen effusion for hydrogen concentrations as small as 20 ppmH. Experiments were carried out in the temperature range from room temperature up to 533 K. The measurement principle is based on the parallel comparison of electrochemically hydrogen charged specimen with hydrogen-free reference specimen at the same temperature. This allows the determination of the hydrogen concentration in the specimens as a function of time and temperature. Separate hot carrier gas extraction experiments using the same temperature–time profiles as the radiography experiments have been used to calibrate the grey values of the neutron transmission images into hydrogen concentrations. It can be stated that the hydrogen effusion correlates with the specimen temperature. KW - Hydrogen effusion KW - Austenitic stainless steels KW - Neutron radiography PY - 2011 U6 - https://doi.org/10.1016/j.nima.2011.02.010 SN - 0168-9002 SN - 0167-5087 VL - 651 IS - 1 SP - 211 EP - 215 PB - North-Holland CY - Amsterdam AN - OPUS4-23401 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Griesche, Axel A1 - Beyer, Katrin A1 - Kannengießer, Thomas A1 - Calzada, E. T1 - Hydrogen diffusion measurements in steels using neutron imaging N2 - Revealing hydrogen embrittlement mechanisms in steels is of great interest to scientists and engineers. Neutron radiography makes it possible to measure in-situ hydrogen diffusion with high spatial and temporal resolution at concentrations as low as 20 ppm. We compare hydrogen-charged specimens with hydrogen-free reference specimens and use calibration standards to normalize the hydrogen concentrations. This allows quantitative tracking of the hydrogen concentration evolution as a function of time, space and temperature. Furthermore, a view into the material with 'neutron eyes' facilitates the detection of cavities that contain molecular hydrogen. KW - Hydrogen KW - Diffusion KW - Steel KW - Neutron radiography PY - 2012 UR - http://cdn.frm2.tum.de/fileadmin/stuff/information/documents/annualReports/Annual_Report_2011_online_version.pdf SP - 50 EP - 51 AN - OPUS4-25981 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Griesche, Axel A1 - Dabah, Eitan A1 - Hilger, A. A1 - Kardjilov, N. A1 - Manke, I. A1 - Kannengießer, Thomas T1 - Neutron imaging of hydrogen in steels T2 - Materials Science & Technology (MS&T) 2013 CY - Montreal, Quebec, Canada DA - 2013-10-27 KW - Neutron radiography KW - Hydrogen KW - Diffusion KW - Steel PY - 2013 SP - 945 EP - 950 PB - Curran CY - Red Hook, NY AN - OPUS4-29506 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Griesche, Axel A1 - Solórzano, E. A1 - Beyer, Katrin A1 - Kannengießer, Thomas T1 - The advantage of using in-situ methods for studying hydrogen mass transport: Neutron radiography vs. carrier gas hot extraction N2 - Neutron radiography (NR) is compared with the commonly used carrier gas hot extraction (CGHE) technique. We performed isothermal hydrogen effusion experiments at 623 K to study the mass transport kinetics. The investigated material was technical iron. The quantification of the hydrogen mass flow is done for NR by using concentration standards. The temporal hydrogen concentration evolution in the sample coincides well for both methods, i.e. NR and CGHE, and is in good agreement with literature. The advantages of the NR method are the non-destructive nature of measuring and the in-situ determination of hydrogen concentrations with high spatial and temporal resolution. Remaining hydrogen inside the sample can be identified directly by the NR method. KW - Hydrogen diffusion KW - In-situ KW - Neutron radiography KW - Carrier gas hot extraction KW - Imaging PY - 2013 U6 - https://doi.org/10.1016/j.ijhydene.2013.08.145 SN - 0360-3199 VL - 38 IS - 34 SP - 14725 EP - 14729 PB - Elsevier CY - Oxford AN - OPUS4-29413 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Dabah, Eitan A1 - Griesche, Axel A1 - Beyer, Katrin A1 - Solórzano, E. A1 - Kannengießer, Thomas ED - Kannengießer, Thomas ED - Babu, S. S. ED - Komizo, Y. ED - Ramirez, A.J. T1 - In situ measurements of hydrogen diffusion in duplex stainless steels by neutron radiography N2 - Hydrogen embrittlement (HE) is a widely known phenomenon and under investigation already for more than a century. This phenomenon, though thoroughly studied, is not yet completely understood, and so far, there are several suggested mechanisms that try to explain the occurrence of HE. One important factor of understanding the HE phenomenon and predicting hydrogen-assisted failure is the descent knowledge about the hydrogen transport behaviour in the material. Neutron radiography is a proven method for tracking hydrogen diffusion and it was applied successfully in various research studies. In the presented study, we examined the hydrogen effusion behaviour in duplex stainless steel by means of neutron radiography and calculated the effective diffusion coefficient from the obtained transmission images. KW - Neutron radiography KW - Hydrogen diffusion KW - Duplex stainless steels KW - Hydrogen embrittlement PY - 2014 SN - 978-3-319-06144-3 SN - 978-3-319-06145-0 U6 - https://doi.org/10.1007/978-3-319-06145-0_9 SP - 155 EP - 163 PB - Springer AN - OPUS4-31357 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Griesche, Axel A1 - Dabah, Eitan A1 - Kardjilov, N. A1 - Hilger, A. A1 - Manke, I. A1 - Kannengießer, Thomas T1 - Imaging of hydrogen in steels using neutrons N2 - We investigated the hydrogen distribution spatially and temporally in technical iron at room temperature. Samples were charged electrochemically and subsequently analysed by means of neutron radiography and tomography. The radiographic images allowed for a time-resolved analysis of hydrogen fluxes. The three-dimensional distribution of hydrogen measured by neutron tomography delivered valuable information for the damage analysis of hydrogen-induced cracks. For the first time hydrogen concentration gradients inside the material could be detect directly together with the cracks. The neutron radiography and tomography results were gained at the Research Reactor BER II of the HZB in Berlin. KW - Hydrogen embrittlement KW - Hydrogen diffusion KW - Neutron tomography KW - Blister PY - 2014 U6 - https://doi.org/10.3139/146.111043 SN - 1862-5282 VL - 105 IS - 7 SP - 640 EP - 644 PB - Carl Hanser CY - München AN - OPUS4-31084 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Griesche, Axel A1 - Dabah, Eitan A1 - Kannengießer, Thomas A1 - Kardjilov, N. A1 - Hilger, A. A1 - Manke, I. T1 - Three-dimensional imaging of hydrogen blister in iron with neutron tomography N2 - We investigated hydrogen embrittlement and blistering in electrochemically hydrogen-charged technical iron samples at room temperature. Hydrogen-stimulated cracks and blisters and the corresponding hydrogen distributions were observed by neutron tomography. Cold neutrons were provided by the research reactor BER II to picture the sample with a spatial resolution in the reconstructed three-dimensional model of ~25 µm. We made the unique observation that cracks were filled with molecular hydrogen and that cracks were surrounded by a 50 µm wide zone with a high hydrogen concentration. The zone contains up to ten times more hydrogen than the bulk material. The hydrogen enriched zone can be ascribed to a region of increased local defect density. Hydrogen also accumulated at the sample surface having the highest concentration at blistered areas. The surfaces of the brittle fractured cracks showed micropores visualized by scanning electron microscopy. The micropores were located at grain boundaries and were surrounded by stress fields detected by electron backscattered diffraction. The cracks clearly originated from the micropores. KW - Hydrogen embrittlement KW - Hydrogen diffusion KW - In situ KW - Neutron tomography KW - Iron PY - 2014 U6 - https://doi.org/10.1016/j.actamat.2014.06.034 SN - 1359-6454 SN - 1873-2453 VL - 78 SP - 14 EP - 22 PB - Elsevier Science CY - Kidlington AN - OPUS4-31068 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Laquai, René A1 - Schaupp, Thomas A1 - Müller, Bernd R. A1 - Griesche, Axel A1 - Bruno, Giovanni A1 - Kannengießer, Thomas T1 - 3D imaging of hydrogen assisted cracking using analyser-based imaging N2 - To better understand the mechanism of hydrogen assisted cracking (HAC), it is important to investigate the 3D structure of the cracks non-destructively. Since, cracks introduced by HAC are usually very small, conventional x-ray imaging methods often lack the required spatial resolution. However, the detection of those cracks can be enhanced by taking advantage of refraction at interfaces within the sample. To image this refractive deflection we employ analyser based imaging (ABI). In this work we aim at proving the enhanced crack detection of ABI by investigating an alluminum alloy weld. T2 - BESSY User Meeting 2015 CY - Berlin, Germany DA - 09.12.2015 KW - X-ray refraction KW - Synchrotron KW - Analyser-based imaging KW - Hydrogen assisted cracking KW - Welding PY - 2015 AN - OPUS4-38278 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Laquai, René A1 - Schaupp, Thomas A1 - Müller, Bernd R. A1 - Griesche, Axel A1 - Bruno, Giovanni A1 - Kannengießer, Thomas T1 - 3D imaging of hydrogen assisted cracking in metals using refraction enhanced synchrotron CT N2 - Hydrogen in metals can cause a degradation of the mechanical properties with possible subsequent hydrogen assisted cracking (HAC). Though, the mechanism of HAC is not completely understood yet and thus suitable methods for in situ investigations to characterise the crack formation are needed. X-ray computed tomography (CT) is a well-known tool for analysing these properties. However, the effective resolution of the detector system limits the detection of small defects by CT. Analyser based imaging (ABI) takes advantage of x-ray refraction at interfaces between volumes of different density, i.e. of cracks, pores, inclusions, etc., within the sample to detect defects smaller than the resolution of the detector system. In this study, measurements on an aluminium alloy weld showed that ABI allows us to resolve the 3D structure of cracks undetected by absorption based CT. Prospective investigations will analyse HAC in steels. T2 - NDT-CE 2015 - International symposium non-destructive testing in civil engineering CY - Berlin, Germany DA - 2015-09-15 KW - Wasserstoffversprödung KW - Wasserstoffunterstützte Rissbildung KW - Röntgenrefraktion KW - CT KW - Hydrogen embrittlement (HE) KW - Hydrogen assisted cracking (HAC) KW - Aluminium alloy KW - X-ray refraction KW - Analyser based imaging KW - Computed tomography (CT) KW - Synchrotron radiation PY - 2015 SN - 1435-4934 SP - 1217 EP - 1224 AN - OPUS4-34287 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -