TY - JOUR A1 - Wiesholler, L. M. A1 - Frenzel, Florian A1 - Grauel, Bettina A1 - Würth, Christian A1 - Resch-Genger, Ute A1 - Hirsch, T. ED - Resch-Genger, Ute ED - Hirsch, Thomas T1 - Yb,Nd,Er-doped upconversion nanoparticles: 980 nm versus 808 nm excitation N2 - Yb,Nd,Er-doped upconversion nanoparticles (UCNPs) have attracted considerable interest as luminescent reporters for bioimaging, sensing, energy conversion/shaping, and anticounterfeiting due to their capability to convert multiple near-infrared (NIR) photons into shorter wavelength ultraviolet, visible or NIR luminescence by successive absorption of two or more NIR photons. This enables optical measurements in complex media with very little background and high penetration depths for bioimaging. The use of Nd3+ as substitute for the commonly employed sensitizer Yb3+ or in combination with Yb3+ shifts the excitation wavelength from about 980 nm, where the absorption of water can weaken upconversion luminescence, to about 800 nm, and laser-induced local overheating effects in cells, tissue, and live animal studies can be minimized. To systematically investigate the potential of Nd3+ doping, we assessed the performance of a set of similarly sized Yb3+,Nd3+,Er3+-doped core- and core–shell UCNPs of different particle architecture in water at broadly varied excitation power densities (P) with steady state and time-resolved fluorometry for excitation at 980 nm and 808 nm. As a measure for UCNPs performance, the P-dependent upconversion quantum yield (Φ) and its saturation behavior were used as well as particle brightness (B). Based upon spectroscopic measurements at both excitation wavelengths in water and in a lipid phantom and B-based calculations of signal size at different penetration depths, conditions under which excitation at 808 nm is advantageous are derived and parameters for the further optimization of triple-doped UCNPs are given. KW - Lanthanide KW - Upconversion KW - Nanoparticle KW - Photoluminescence KW - Quantum yield KW - Lifetime KW - Brightness KW - Nd excitation KW - Excitation power density KW - Modelling KW - NIR PY - 2019 U6 - https://doi.org/10.1039/C9NR03127H SN - 2040-3372 SN - 2040-3364 VL - 11 IS - 28 SP - 13440 EP - 13449 PB - Royal Society of Chemistry CY - London AN - OPUS4-48608 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Tietze, R. A1 - Panzer, R. A1 - Starzynski, T. A1 - Guhrenz, C. A1 - Frenzel, Florian A1 - Würth, Christian A1 - Resch-Genger, Ute A1 - Weigand, Jan J. A1 - Eychmüller, A. T1 - Synthesis of NIR-emitting InAs-based core/shell quantum dots with the use of tripyrazolylarsane as arsenic precursor N2 - Tris(3,5-dimethylpyrazolyl)arsane (1) is introduced as a low-cost and convenient to handle arsenic precursor for the straight Forward synthesis of InAs Quantum dots (QDs). Transamination of 1 with the solvent oleylamine (OLAH) gives trioleylarsane (As(OLA)3) which in the presence of the reducing agents diisobutylaluminum hydride (DIBAL-H) or trioleylphosphane (P(OLA)3) yields InAs QDs via a typical hot injection approach. The size of the obtained InAs core QDs are tuned by varying the reaction time, the amount of the applied reducing agent, or even more effectively by changing the Indium and/or zinc halide precursors, InX3, and ZnX2 (Cl, Br, or I). Passivation of the resulting InAs particles with a protective ZnS or ZnSe shell results in improved photoluminescence of the core/shell QDs covering a spectral range between 600 and 1150 nm. KW - Quantum dot KW - NIR KW - Near infrared PY - 2018 U6 - https://doi.org/10.1002/ppsc.201800175 SN - 0934-0866 SN - 1521-4117 VL - 35 IS - 9 SP - 1800175, 1 EP - 7 PB - Wiley AN - OPUS4-46076 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Frenzel, Florian A1 - Würth, Christian A1 - Dukhno, O. A1 - Przybilla, F. A1 - Wiesholler, L. M. A1 - Muhr, V. A1 - Horsch, T. A1 - Mély, Y. A1 - Resch-Genger, Ute T1 - Multiband emission from single β-NaYF4(Yb,Er) nanoparticles at high excitation power densities and comparison to ensemble studies N2 - Ensemble and single particle studies of the excitation power density (P)-dependent upconversion luminescence (UCL) of core and core–shell β-NaYF4:Yb,Er upconversion nanoparticles (UCNPs) doped with 20% Yb3+ and 1% or 3% Er3+ performed over a P regime of 6 orders of magnitude reveal an increasing contribution of the emission from high energy Er3+ levels at P > 1 kW/cm2. This changes the overall emission color from initially green over yellow to white. While initially the green and with increasing P the red emission dominate in ensemble measurements at P < 1 kW/cm2, the increasing population of higher Er3+ energy levels by multiphotonic processes at higher P in single particle studies results in a multitude of emission bands in the ultraviolet/visible/near infrared (UV/vis/NIR) accompanied by a decreased contribution of the red luminescence. Based upon a thorough analysis of the P-dependence of UCL, the emission bands activated at high P were grouped and assigned to 2–3, 3–4, and 4 photonic processes involving energy transfer (ET), excited-state absorption (ESA), cross-relaxation (CR), back energy transfer (BET), and non-radiative relaxation processes (nRP). This underlines the P-tunability of UCNP brightness and color and highlights the potential of P-dependent measurements for mechanistic studies required to manifest the population pathways of the different Er3+ levels. KW - Nano KW - Nanomaterial KW - Upconversion nanoparticle KW - Lanthanide KW - Photoluminescence KW - Quantum yield KW - Photophysics KW - Llifetime KW - Sensor KW - Excitation power density KW - Single particle KW - Brightness KW - NIR KW - Mechanism KW - Color tuning PY - 2021 U6 - https://doi.org/10.1007/s12274-021-3350-y SN - 1998-0124 VL - 14 IS - 11 SP - 4107 EP - 4115 PB - Nano Research AN - OPUS4-52364 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -