TY - JOUR A1 - Höhm, S. A1 - Herzlieb, M. A1 - Rosenfeld, A. A1 - Krüger, Jörg A1 - Bonse, Jörn T1 - Dynamics of the formation of laser-induced periodic surface structures (LIPSS) upon femtosecond two-color double-pulse irradiation of metals, semiconductors, and dielectrics N2 - In order to address the dynamics and physical mechanisms of LIPSS formation for three different classes of materials (metals, semiconductors, and dielectrics), two-color double-fs-pulse experiments were performed on Titanium, Silicon and Fused Silica. For that purpose a Mach–Zehnder interferometer generated polarization controlled (parallel or cross-polarized) double-pulse sequences at 400 nm and 800 nm wavelength, with inter-pulse delays up to a few picoseconds. Multiple of these two-color double-pulse sequences were collinearly focused by a spherical mirror to the sample surfaces. The fluence of each individual pulse (400 nm and 800 nm) was always kept below its respective ablation threshold and only the joint action of both pulses lead to the formation of LIPSS. Their resulting characteristics (periods, areas) were analyzed by scanning electron microscopy. The periods along with the LIPSS orientation allow a clear identification of the pulse which dominates the energy coupling to the material. For strong absorbing materials (Silicon, Titanium), a wavelength-dependent plasmonic mechanism can explain the delay-dependence of the LIPSS. In contrast, for dielectrics (Fused Silica) the first pulse always dominates the energy deposition and LIPSS orientation, supporting a non-plasmonic formation scenario. For all materials, these two-color experiments confirm the importance of the ultrafast energy deposition stage for LIPSS formation. KW - Femtosecond laser ablation KW - Double-pulse experiments KW - Laser-induced periodic surface structures (LIPSS) KW - Mach-Zehnder interferometer KW - Ultrafast optical techniques PY - 2016 UR - http://www.sciencedirect.com/science/article/pii/S0169433215031347 U6 - https://doi.org/10.1016/j.apsusc.2015.12.129 SN - 0169-4332 SN - 1873-5584 VL - 374 SP - 331 EP - 338 PB - Elsevier CY - Amsterdam, Netherlands AN - OPUS4-35938 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Höhm, S. A1 - Herzlieb, M. A1 - Rosenfeld, A. A1 - Krüger, Jörg A1 - Bonse, Jörn T1 - Laser-induced periodic surface structures on fused silica upon cross-polarized two-color double-fs-pulse irradiation N2 - The dynamics of the formation of laser-induced periodic surface structures (LIPSS) on fused silica upon irradiation with linearly polarized fs-laser pulses (50 fs pulse duration) is studied by cross-polarized two-color double-fs-pulse experiments. In order to analyze the relevance of temporally distributed energy deposition in the early stage of LIPSS formation, a Mach-Zehnder interferometer was used for generating multiple double-pulse sequences at two different wavelengths (400 and 800 nm). The inter-pulse delay between the individual cross-polarized pulses of each sequence was systematically varied in the sub-ps range and the resulting LIPSS morphologies were characterized by scanning electron microscopy. It is found that the polarization of the first laser pulse arriving to the surface determines the orientation and the periodicity of the LIPSS. These two-color experiments further confirm the importance of the ultrafast energy deposition to the silica surface for LIPSS formation, particularly by the first laser pulse of each sequence. The second laser pulse subsequently reinforces the previously seeded spatial LIPSS characteristics (period, orientation). KW - Laser-induced periodic surface structures (LIPSS) KW - Femtosecond laser ablation KW - Double-pulse experiments KW - Ultrafast optical techniques KW - Mach-Zehnder interferometer PY - 2015 U6 - https://doi.org/10.1016/j.apsusc.2014.09.101 SN - 0169-4332 SN - 1873-5584 VL - 336 SP - 39 EP - 42 PB - North-Holland CY - Amsterdam AN - OPUS4-32860 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Höhm, S. A1 - Rosenfeld, A. A1 - Krüger, Jörg A1 - Bonse, Jörn T1 - Area dependence of femtosecond laser-induced periodic surface structures for varying band gap materials after double pulse excitation N2 - The formation of laser-induced periodic surface structures upon irradiation of titanium, silicon, and fused silica with multiple irradiation sequences consisting of parallel polarized Ti:sapphire femtosecond laser pulse pairs (pulse duration 50–150 fs, central wavelength ~800 nm) is studied experimentally. The temporal delay between the individual near-equal energy fs-laser pulses was varied between 0 and 5 ps with a temporal resolution of better than 0.2 ps. The surface morphology of the irradiated surface areas is characterized by means of scanning electron microscopy (SEM). In all materials a decrease of the rippled surface area is observed for increasing delays. The characteristic delay decay scale is quantified and related to material dependent excitation and energy relaxation processes. KW - Laser-induced periodic surface structures (LIPSS) KW - Femtosecond laser ablation KW - Double-pulse experiments KW - Ultrafast optical techniques KW - Mach-Zehnder interferometer PY - 2013 U6 - https://doi.org/10.1016/j.apsusc.2012.10.188 SN - 0169-4332 SN - 1873-5584 VL - 278 SP - 7 EP - 12 PB - North-Holland CY - Amsterdam AN - OPUS4-28601 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bonse, Jörn A1 - Krüger, Jörg A1 - Höhm, S. A1 - Rosenfeld, A. T1 - Femtosecond laser-induced periodic surface structures N2 - The formation of laser-induced periodic surface structures (LIPSS) in different materials (metals, semiconductors, and dielectrics) upon irradiation with linearly polarized fs-laser pulses (τ~30–150 fs, λ~800 nm) in air environment is studied experimentally and theoretically. In metals, predominantly low-spatial-frequency-LIPSS with periods close to the laser wavelength λ are observed perpendicular to the polarization. Under specific irradiation conditions, high-spatial-frequency-LIPSS with sub-100-nm spatial periods (~λ/10) can be generated. For semiconductors, the impact of transient changes of the optical properties to the LIPSS periods is analyzed theoretically and experimentally. In dielectrics, the importance of transient excitation stages in the LIPSS formation is demonstrated experimentally using (multiple) double-fs-laser-pulse irradiation sequences. A characteristic decrease of the LIPSS periods is observed for double-pulse delays of less than 2 ps. KW - Laser-induced periodic surface structures (LIPSS) KW - Femtosecond laser ablation KW - Ultrafast optical techniques KW - Silicon KW - Titanium KW - Silica PY - 2012 U6 - https://doi.org/10.2351/1.4712658 SN - 1042-346X SN - 1938-1387 VL - 24 IS - 4 SP - 042006-1 EP - 042006-7 PB - Laser Institute of America CY - Orlando, Fla., USA AN - OPUS4-26198 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rosenfeld, A. A1 - Rohloff, M. A1 - Höhm, S. A1 - Krüger, Jörg A1 - Bonse, Jörn T1 - Formation of laser-induced periodic surface structures on fused silica upon multiple parallel polarized double-femtosecond-laser-pulse irradiation sequences N2 - The formation of laser-induced periodic surface structures (LIPSS) upon irradiation of fused silica with multiple irradiation sequences of parallel polarized Ti:sapphire femtosecond laser pulse pairs (160 fs pulse duration, 800 nm central wavelength) was studied experimentally. For that purpose, a Michelson interferometer was used to generate near-equal-energy double-pulse sequences allowing the temporal pulse delay between the parallel-polarized individual fs-laser pulses to be varied between 0 and 40 ps with ~0.2 ps temporal resolution. The surface morphologies of the irradiated surface areas were characterized by means of scanning electron and scanning force microscopy. In the sub-ps delay range a strong decrease of the LIPSS periods and the ablation crater depths with the double-pulse delay was observed indicating the importance of the laser-induced free-electron plasma in the conduction band of the solids for the formation of LIPSS. KW - Laser-induced periodic surface structures (LIPSS) KW - Femtosecond laser ablation KW - Double-pulse experiments KW - Fused silica KW - Michelson interferometer PY - 2012 U6 - https://doi.org/10.1016/j.apsusc.2011.09.076 SN - 0169-4332 SN - 1873-5584 VL - 258 IS - 23 SP - 9233 EP - 9236 PB - North-Holland CY - Amsterdam AN - OPUS4-26226 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bonse, Jörn A1 - Rosenfeld, A. A1 - Krüger, Jörg T1 - Implications of transient changes of optical and surface properties of solids during femtosecond laser pulse irradiation to the formation of laser-induced periodic surface structures N2 - The formation of laser-induced periodic surface structures (LIPSS) upon irradiation of silicon wafer surfaces by linearly polarized Ti:sapphire femtosecond laser pulses (pulse duration 130 fs, central wavelength 800 nm) is studied experimentally and theoretically. In the experiments, so-called low-spatial frequency LIPSS (LSFL) were found with periods smaller than the laser wavelength and an orientation perpendicular to the polarization. The experimental results are analyzed by means of a new theoretical approach, which combines the widely accepted LIPSS theory of Sipe et al. with a Drude model, in order to account for transient (intra-pulse) changes of the optical properties of the irradiated materials. It is found that the LSFL formation is caused by the excitation of surface plasmon polaritons, SPPs, once the initially semiconducting material turns to a metallic state upon formation of a dense free-electron-plasma in the material and the subsequent interference between its electrical field with that of the incident laser beam resulting in a spatially modulated energy deposition at the surface. Moreover, the influence of the laser-excited carrier density and the role of the feedback upon the multi-pulse irradiation and its relation to the excitation of SPP in a grating-like surface structure is discussed. KW - Femtosecond laser ablation KW - Laser-induced periodic surface structures KW - (LIPSS) KW - Optical properties KW - Surface plasmon polaritons KW - Semiconductors KW - Silicon PY - 2011 U6 - https://doi.org/10.1016/j.apsusc.2010.11.059 SN - 0169-4332 SN - 1873-5584 VL - 257 IS - 12 SP - 5420 EP - 5423 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-23309 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bonse, Jörn A1 - Rosenfeld, A. A1 - Krüger, Jörg ED - Panchenko, V. ED - Mourou, G. ED - Zheltikov, A. M. T1 - Femtosecond laser-induced periodic surface structures: recent approaches to explain their sub-wavelength periodicities N2 - The formation of laser-induced periodic surface structures (LIPSS) upon irradiation of semiconductors and dielectrics by linearly polarized high-intensity Ti:sapphire fs-laser pulses (τ ~100 fs, λ ~800 nm) is studied experimentally and theoretically. In the experiments, two different types of LIPSS exhibiting very different spatial periods are observed (socalled LSFL – low spatial frequency LIPSS, and HSFL - high spatial frequency LIPSS), both having a different dependence on the incident laser fluence and pulse number per spot. The experimental results are analyzed by means of a new theoretical approach, which combines the generally accepted LIPSS theory of J. E. Sipe and co-workers [Phys. Rev. B 27, 1141-1154 (1983)] with a Drude model, in order to account for transient changes of the optical properties of the irradiated materials. The joint Sipe-Drude model is capable of explaining numerous aspects of fs-LIPSS formation, i.e., the orientation of the LIPSS, their fluence dependence as well as their spatial periods. The latter aspect is specifically demonstrated for silicon crystals, which show experimental LSFL periods Λ somewhat smaller than λ. This behaviour is caused by the excitation of surface plasmon polaritons, SPP, (once the initially semiconducting material turns to a metallic state upon formation of a dense free-electron-plasma in the material) and the subsequent interference between its electrical fields with that of the incident laser beam, resulting in a spatially modulated energy deposition at the surface. Upon multi-pulse irradiation, a feedback mechanism, caused by the redshift of the resonance in a grating-assisted SPP excitation, is further reducing the LSFL spatial periods. The SPP-based mechanism of LSFL successfully explains the remarkably large range of LSFL periods between ~0.6 λ and λ. T2 - LAT 2010 - International Conference on Lasers, Applications, and Technologies CY - Kazan, Russia DA - 23.08.2010 KW - Femtosecond laser ablation KW - Laser-induced periodic surface structures (LIPSS) KW - Surface plasmon polaritons KW - Second harmonic generation (SHG) KW - Silicon KW - Semiconductors KW - Dielectrics PY - 2011 U6 - https://doi.org/10.1117/12.879813 SN - 0277-786X N1 - Serientitel: Proceedings of SPIE – Series title: Proceedings of SPIE VL - 7994 SP - 79940M-1 EP - 79940M-10 CY - Bellingham, USA AN - OPUS4-23291 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bonse, Jörn A1 - Krüger, Jörg T1 - Probing the heat affected zone by chemical modifications in femtosecond pulse laser ablation of titanium nitride films in air N2 - A new approach is presented to quantify the so-called "heat affected zone" (HAZ) during femtosecond laser pulse processing. Ablation of titanium nitride (TiN) thin films (~3 μm thickness) by multiple femtosecond laser pulses (τ=130 fs, λ=800 nm) in air environment was studied by means of two different surface analytical methods both being sensitive to chemical alterations at the surface. Scanning Auger electron microscopy was applied for a visualization of the spatial distribution of specific elements (Ti, O) within the laser-modified areas. The chemical state of the irradiated surface was revealed by complementary x-ray photoelectron spectroscopy. Both methods were used for a depth-profiling chemical analysis (tracking the elements Ti, N, O, and C) using an Ar-ion beam for surface sputtering. In a narrow laser fluence range slightly below the ablation threshold of TiN significant superficial oxidation can be observed leading to the formation of substoichiometric TiO2-x. At fluences above the ablation threshold, an increased titanium concentration is observed within the entire ablation craters. Following upon sputter removal the elemental distribution into the depth of the nonablated material, the results allow an estimation of the heat-affected zone for femtosecond laser ablation in air environment. According to our analyses, the HAZ extends up to a few hundreds of nanometers into the nonablated material. KW - Femtosecond laser ablation KW - Heat affected zone KW - Titanium nitride KW - Scanning Auger electron microscopy KW - X-ray KW - Photoelektron spectroscopy PY - 2010 UR - http://link.aip.org/link/?JAP/107/054902 U6 - https://doi.org/10.1063/1.3311552 SN - 0021-8979 SN - 1089-7550 VL - 107 IS - 5 SP - 054902-1 - 054902-5 PB - American Institute of Physics CY - Melville, NY AN - OPUS4-20949 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bonse, Jörn A1 - Bachelier, G. A1 - Wiggins, S. M. A1 - Siegel, J. A1 - Solis, J. A1 - Krüger, Jörg A1 - Sturm, Heinz T1 - Femtosecond laser ablation of indium phosphide in air: dynamical, structural and morphological evolution N2 - The irradiation of single-crystalline indium phosphide (c-InP) by Ti:sapphire femtosecond laser pulses (130 fs, 800 nm) in air is studied by means of in-situ time resolved reflectivity measurements [fs-time-resolved microscopy (100 fs-10 ns) and point probing analysis (ns - µs)] and by complementary ex-situ surface analytical methods (Micro Raman Spectroscopy, Scanning Force, and Optical Microscopy). The dynamics of melting, ablation, and optical breakdown as well as structural changes resulting from rapid solidification are investigated in detail. Different laser-induced surface morphologies are characterized and discussed on the basis of recent ablation and optical breakdown models. KW - Femtosecond laser ablation KW - Optical breakdown KW - Time-resolved measurements KW - Semiconductor KW - Indium phosphide PY - 2010 SN - 1454-4164 VL - 12 IS - 3 SP - 421 EP - 426 PB - INOE & INFM CY - Bucharest AN - OPUS4-21082 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Bonse, Jörn A1 - Krüger, Jörg A1 - Kautek, Wolfgang A1 - Wrobel, J. M. T1 - Femtosecond pulse laser machining of InP wafers N2 - Ablation of indium phosphide wafers in air was performed with 130 fs laser pulses at a wavelength of 800 nm at a low repetition rate of 10 Hz. In order to evaluate the role of the incubation effects, the relationship between the number of laser pulses used for the ablation and the threshold fluence was studied. Particular attention was paid to the chemical composition, surface morphology and structural variations of the ablated area. T2 - 5th Laser Applications in Microelectronics and Optoelectronics Manufacturing Conference (LAMOM) CY - San José, CA, USA DA - 240.01.2000 KW - Femtosecond laser ablation KW - Indium phosphide KW - Auger electron spectroscopy PY - 2000 SN - 0-8194-3550-3 SN - 1605-7422 N1 - Serientitel: SPIE proceedings series – Series title: SPIE proceedings series IS - 3933 SP - 280 EP - 287 PB - SPIE CY - Bellingham, Wash. AN - OPUS4-937 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -