TY - JOUR A1 - Bonse, Jörn A1 - Rudolph, Pascale A1 - Krüger, Jörg A1 - Baudach, Steffen A1 - Kautek, Wolfgang T1 - Femtosecond pulse laser processing of TiN on silicon N2 - Ultrashort pulse laser microstructuring (pulse duration 130 fs, wavelength 800 nm, repetition rate 2 Hz) of titanium nitride (TiN) films on silicon substrates was performed in air using the direct focusing technique. The lateral and vertical precision of laser ablation was evaluated. The TiN ablation threshold changed with the number of pulses applied to the surface due to an incubation effect. An ablation depth per pulse below the penetration depth of light was observed. Columnar structures were formed in the silicon substrate after drilling through the TiN layer. KW - Femtosecond laser ablation KW - Titanium nitride KW - Silicon KW - Optical properties PY - 2000 U6 - https://doi.org/10.1016/S0169-4332(99)00481-X SN - 0169-4332 SN - 1873-5584 VL - 154-155 SP - 659 EP - 663 PB - North-Holland CY - Amsterdam AN - OPUS4-802 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Bonse, Jörn A1 - Baudach, Steffen A1 - Krüger, Jörg A1 - Kautek, Wolfgang ED - Phipps, C. T1 - Femtosecond laser micromachining of technical materials N2 - Micromachining experiments were performed with Ti:sapphire laser pulses (130 fs - 150 fs, 800 nm, approximately 10 Hz) in air. Employing the direct focusing technique, highly absorbing titanium nitride (TiN) and weakly absorbing polyimide (PI) and polymethylmethacrylate (PMMA) served as target materials. The lateral and vertical precision of the laser ablation and morphological features were characterized by scanning force (SFM), scanning electron (SEM) and optical microscopy. For TiN, incubation can be observed, i.e. the single-pulse surface damage threshold (0.26 J/cm2) is by a factor of two greater than the threshold for 100 pulses. Ablation rates below 10 nm per pulse can be achieved. The evolution of sub-wavelength ripples is presented in dependence on pulse number and laser fluence, respectively. The incubation behavior of the polymers can be described by an accumulation model as for TiN. Experiments on PI with varying focal lengths result in the same modification thresholds. Different polarization states of light (linear, circular) lead to a variation of the ablation rate and to various morphological patterns in the ablation craters (wavelength ripples, cones). Swelling of PMMA occurred at fluences below the ablation threshold. T2 - 3rd SPIE's International Conference on High-Power Laser Ablation CY - Santa Fe, NM, USA DA - 24.04.2000 KW - Ablation KW - Femtosecond pulse laser KW - Laser processing KW - Micromachining KW - Polymer KW - Titanium nitride KW - Ripples PY - 2000 SN - 0-8194-3700-X U6 - https://doi.org/10.1117/12.407346 SN - 1605-7422 N1 - Serientitel: SPIE proceedings series – Series title: SPIE proceedings series IS - 4065 SP - 161 EP - 172 PB - SPIE CY - Bellingham, Wash. AN - OPUS4-967 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -