TY - JOUR A1 - Morcillo, Dalia A1 - Winckelmann, Alexander A1 - Frick, Daniel A. A1 - Jacobsen, Lars A1 - Seger, Tino A1 - Florek, Stefan A1 - Richter, Silke A1 - Vogl, Jochen A1 - Recknagel, Sebastian A1 - Panne, Ulrich A1 - Abad Andrade, Carlos Enrique T1 - Lithium isotope ratio analysis of geological samples using atomic absorption spectrometry with improved spectral resolution N2 - This study introduces an improved spectrometric method with enhanced precision to determine isotope ratios in geological samples without chromatographic separation. Firstly, the improvement is achieved by increasing the spectral resolution of the spectrometer applied in well-known high-resolution continuum source atomic absorption spectrometry (HR-CS-AAS). The resulting resolving power and linear dispersion of the upgraded setup, which is denoted in the following as HR+CS-AAS, is well adapted to the line widths of the Li isotope components we investigated. Secondly, our proposed method combines optical absorption spectrometry with machine learning data analysis using an extreme gradient boosting algorithm (XGBoost). This method was applied to analyze certified geological reference materials with δLSVEC(7Li/6Li) (hereafter δ7Li) values ranging from −0.5 ‰ to 4.5 ‰. With a pixel related optical resolving power of λ/∆λ ≈ 780 000, we obtain precisions in δ7Li measurements from 1.0 ‰ to 2.5 ‰. The method is validated by comparing the results with multi-collector inductively coupled plasma mass spectrometry (MC-ICP-MS), confirming its metrological compatibility. This work presents a fast, robust, and reliable method for δ7Li measurement in geological samples. KW - Isotope KW - High-resolution continuum source atomic absorption spectroscopy KW - Lithium KW - Machine learning KW - Echelle spectrometer PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-611807 DO - https://doi.org/10.1016/j.sab.2024.107013 VL - 220 SP - 1 EP - 5 PB - Elsevier BV AN - OPUS4-61180 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - You, Zengchao A1 - Hoffmann, V. A1 - Morcillo, Dalia A1 - Agudo Jácome, Leonardo A1 - Leonhardt, Robert A1 - Winckelmann, Alexander A1 - Richter, Silke A1 - Recknagel, Sebastian A1 - Abad Andrade, Carlos Enrique T1 - Investigation of aluminum current collector degradation in lithium-ion batteries using glow discharge optical emission spectrometry N2 - In this work, we employed glow discharge optical emission spectrometry (GD-OES) depth profiling as a fast and semi-quantitative method to investigate the aluminum (Al) current collector degradation in commercial lithium cobalt oxide (LCO) pouch cells with no Al2O3 pretreatment. After battery aging, a heterogeneous deposit was found on the surface of the cathode. Gray hotspot areas within an extensive pale white region were formed. Consistent with energy dispersive X-ray (EDX) analysis of micro-cross sections milled via targeted focused ion beam (FIB), an Al-containing layer of approximately 3 µm can be observed using GD-OES. We attribute one main cause of this layer is the degradation of the Al current collector. The nonuniform growth of this layer was investigated by performing GD-OES depth profiling at different in-plane positions. We found that the gray area has a higher mass concentration of Al, probably in metallic form, whereas the white area was probably covered more homogeneously with Al2O3, resulting from the inhomogeneous distribution of the pitting positions on the current collector. Compared to FIB-EDX, GD-OES enables a faster and more convenient depth profile analysis, which allows the more productive characterization of lithium-ion batteries (LIBs), and consequently benefits the development of preferable battery materials. KW - GD-OES KW - depth profiles KW - Li-ion battery KW - battery aging mechanism KW - current collector corrosion PY - 2023 DO - https://doi.org/10.1016/j.sab.2023.106681 SN - 0584-8547 VL - 205 SP - 106681 PB - Elsevier B.V. CY - Amsterdam, Netherlands AN - OPUS4-57383 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Morcillo, Dalia A1 - Winckelmann, Alexander A1 - Oelze, Marcus A1 - Leonhardt, Robert A1 - Schmidt, Anita A1 - Richter, Silke A1 - Recknagel, Sebastian A1 - Vogl, Jochen A1 - Panne, Ulrich A1 - Abad Andrade, Carlos Enrique T1 - Exploring Age-Induced Lithium Isotope Fractionation in Lithium-Ion Batteries using Microwave-Induced Cold Nitrogen Plasma Mass Spectrometry N2 - This study explores Microwave-Inductively Coupled Atmospheric-pressure Plasma Mass Spectrometry (MICAP-MS) as a cost-effective alternative to Multi-Collector Inductively Coupled Plasma Mass Spectrometry (MC-ICP-MS) for analyzing lithium isotopic composition in lithium-ion batteries (LIBs). We investigate the performance of MICAP-MS in measuring Li isotope ratios in new and aged commercial lithium cobalt oxide (LCO) batteries. Our results show that MICAP-MS, operating under cold plasma conditions at 800 W with an 8 mm torch position, achieves results metrologically compatible with MC-ICP-MS, with a precision ranging from 0.6‰ to 3.4‰ for δ7Li values. MICAP-MS benefits from a dielectric resonator for uniform plasma, better ion velocity control, and higher energy efficiency. Optimal settings were identified with dwell times of 10 ms for 6Li and 1 ms for 7Li. The study of LIBs revealed that 6Li migrates towards the anode over multiple charge–discharge cycles, causing 7Li to accumulate in the cathode, a fractionation effect that becomes more pronounced with prolonged cycling. MICAP-MS provides a cost-effective, precise alternative to MC-ICP-MS, with lower operational costs and enhanced portability, advancing the study of isotopic fractionation and aging in lithium-ion batteries. KW - MICAP-MS KW - Lithium KW - Battery aging KW - Lithium isotopes KW - Nitrogen plasma KW - Isotope fractionation KW - lithium cobalt oxide KW - LCO PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-643777 DO - https://doi.org/10.1039/d4ja00324a SN - 0267-9477 SP - 1 EP - 11 PB - Royal Society of Chemistry (RSC) AN - OPUS4-64377 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - INPR A1 - Morcillo, Dalia A1 - Oelze, Marcus A1 - Seena Prem, Pranav A1 - de Oliveira Guilherme Buzanich, Ana A1 - Emmerling, Franziska A1 - Recknagel, Sebastian A1 - Panne, Ulrich A1 - Abad Andrade, Carlos Enrique T1 - Lithium isotope fractionation as an early indicator of degradation mechanisms in lithium-ion batteries N2 - Aging in lithium-ion batteries (LIBs) degrades performance and hinders sustainability, demanding advanced diagnostics for early failure prediction. We investigate lithium isotope fractionation (LIF) as an innovative probe of degradation in lithium cobalt oxide (LCO) coin cells aged over 0−700 cycles. High-precision multi-collector inductively coupled plasma mass spectrometry (MC-ICP-MS) quantified δ7Li variations across cell stages: non-cycled (0 cycles), newly formed (5 cycles), semi-aged (250 cycles), and fully aged (700 cycles). During early cycling (≤ 45 cycles), chemical processes drive 7Li enrichment at the anode (δ7Li vs LSVEC = +12 ‰) through solid electrolyte interphase (SEI) formation, while the cathode depletes in 7Li (δ7Li vs LSVEC = −0.7 ‰). Beyond 45 cycles, electric field-induced migration predominates, promoting 6Li intercalation into the anode and increasing the δ7Li of the cathode by 8.1 ‰. Mass balance verifies isotope conservation, attributing shifts to redistribution and trapping. Complementary electrochemical impedance spectroscopy (EIS) and X-ray absorption spectroscopy and diffraction confirm SEI expansion, cobalt oxidation, lattice shrinkage, and changes in electrode structure, corroborating LIF trends. Notably, a δ7Li inflection at approximately 270 cycles anticipates end-of-life by 70 cycles, surpassing traditional methods in sensitivity. LIF emerges as a predictive indicator of aging mechanisms, informing optimized designs for durable LIBs. KW - Lithium isotope fractionation KW - Lithium-ion batteries KW - Degradation mechanisms KW - LiCoO2 cathodes KW - LCO KW - Isotopic tracing KW - Lithium isotopes PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-650945 DO - https://doi.org/10.26434/chemrxiv-2025-16lvq SP - 1 EP - 19 AN - OPUS4-65094 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -