TY - CONF A1 - Wilsch, Gerd A1 - Gottlieb, Cassian A1 - Günther, Tobias A1 - Millar, Steven A1 - Völker, Tobias T1 - Laser-Induced Breakdown Spectroscopy (LIBS) Automated 2D chemical analysis of chloride content in concrete structures N2 - The application of a LIBS system is presented. A diode-pumped low energy laser (3 mJ, 1.5 ns, 100 Hz) and a compact NIR spectrometer are used. A scanner allows the two-dimensional element mapping. For the quantitative analysis calibration of the system is carried out with reference samples in a concentration range of chlorine of 0.05 wt.% to 2.5 wt.%. To determine the 2D distribution of harmful elements (Cl, C), concrete cores were drilled, split and analyzed directly. By comparing the chloride ingress and the carbonation, the interaction of both processes can be visualized in one measurement that takes less than 10 minutes with a drill core of 50 mm x 100 mm. Results obtained were compared and verified with standard measurements. T2 - Concrete Solutions 2019 CY - Cluj Napoca, Romania DA - 30.09.2019 KW - Chloride KW - Beton KW - LIBS KW - Schädigung PY - 2019 AN - OPUS4-51703 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Duffner, Eric A1 - Munzke, Dorit A1 - Mair, Georg A1 - Szczepaniak, Mariusz A1 - Schukar, Marcus T1 - Lebensdauerversuche an Faserverbund-Druckbehältern überwacht mittels Schallemissionsprüfung und optischen Fasern N2 - Kurzfassung. Die meisten Faserverbundbehälter, die in Europa für den Transport gefährlicher Stoffe oder als Speicherbehälter für Wasserstoff oder Erdgas in Fahrzeugen Verwendung finden, werden für eine nicht begrenzte Lebensdauer ausgelegt. In regelmäßigen Abständen sind für diese Druckbehälter wiederkehrende Prüfungen vorgeschrieben, die in der Regel aus visuellen Inspektionen und hydraulischen Innendruckprüfungen bestehen [1]. Die wiederkehrenden Prüfungen sind jedoch weder geeignet, die sichere Betriebsdauer festzulegen noch den Alterungszustand der Druckbehälter zu beurteilen. Aufgrund des weiter steigenden Drucks zur Kosten- und Gewichtsreduktion von Faserverbundbehältern und der damit einhergehenden Ausnutzung der existierenden Sicherheitsmargen gewinnen Methoden zur Beurteilung des Alterungsverhaltens dieser Druckbehälter immer mehr an Bedeutung. Vor diesem Hintergrund wurde in der BAM das orhaben „Alterungsverhalten von Composite-Druckgefäßen mit Carbonfaser-Compositen unter gekoppelten Beanspruchungen (COD-AGE)“ gestartet, um die Alterung von Faserverbundbehältern mittels verschiedener zerstörungsfreier Prüfverfahren zu untersuchen. Die hier vorgestellten Ergebnisse wurden an einem Typ 4 Hybridbehälter mit Kunststoffliner gewonnen, in den im Rahmen des Herstellungsprozesses optische Glasfasern in verschiedenen Schichten integriert wurden. Der Behälter wurde mittels hydraulischem Innendruck und erhöhter Umgebungstemperatur zyklisch bis zum Lebensende belastet. Zwischen den einzelnen Lastsequenzen erfolgte eine an die wiederkehrende Prüfung im Betrieb angelehnte hydraulische Druckbelastung. Sowohl die hydraulische Alterung als auch die Druckrampen wurden mittels Schallemissionsprüfung (SEP) und verteilter faseroptischer Sensorik mit dem Ziel einer frühzeitigen Versagensvorhersage überwacht. Durch die Schallemissionsanalyse sollte untersucht werden, ob zum Lebensende hin ein signifikanter Anstieg der Schallemissionsaktivität und -intensität, unterteilt in verschiedene Lastbereiche, beobachtet werden kann. Zusätzlich zum kontinuierlichen Monitoring der Zyklierung sollten die Druckrampen separat untersucht werden, um hier Potenziale für die wiederkehrende Prüfung zu erkennen. T2 - 22. Kolloquium Schallemission und 3. Anwenderseminar Zustandsüberwachung mit geführten Wellen CY - Karlsruhe, Germany DA - 27.03.2019 KW - Faserverbund KW - Druckbehältern KW - Lebensdauerversuche KW - Schallemissionsprüfung KW - Optische Fasern PY - 2019 AN - OPUS4-47955 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wilsch, Gerd A1 - Günther, Tobias A1 - Völker, Tobias T1 - LIBS for the analysis of concrete N2 - Special features and examples of using LIBS on concrete. T2 - Workshop on tandem LIBS/LA-ICP-MS CY - Berlin, Germany DA - 18.11.2019 KW - Mobile system KW - LIBS KW - Concrete KW - Damage KW - Chloride KW - Sulphate KW - Mapping PY - 2019 AN - OPUS4-51710 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wilsch, Gerd A1 - Günther, Tobias A1 - Völker, Tobias T1 - LIBS – Betonanalytik mir dem Laser N2 - Es wird ein alternatives Verfahren zur schnellen zweidimensionalen Analyse der chemischen Zusammensetzung von Baustoffen vorgestellt. Dieses beruht auf der Kombination des Abtrags einer geringen Materialmenge durch einen gepulsten Laser, der Plasmaerzeugung und der Analyse der Lichtemission des Plasmas mittels optischer Spektroskopie. Es können prinzipiell alle Elemente gleichzeitig nachgewiesen werden. Damit ist es möglich einerseits Informationen über den Baustoff an sich als auch über den Eintrag potentiell schädigender Elemente (z. B. Cl, C, Na, K, S) zu gewinnen. Das Verfahren kann automatisiert im Labor oder als mobile Version direkt vor Ort eingesetzt werden. Es liefert zweidimensionale Bilder der Elementverteilung in Echtzeit. Es kann ohne große Probenvorbereitung z. B. direkt an der Querschnittsfläche eines Bohrkernes gemessen werden. Die Messung dauert nur wenige Minuten. Das Prinzip der Messung, die Vor- und die Nachteile, sowie die verfügbare Gerätetechnik für den Einsatz im Labor oder direkt am Bauwerk werden vorgestellt. Abschließend werden praktische Beispiele für die Anwendung des LIBS-Verfahrens zur Erfassung des Chlorid-Eintrages, der Karbonatisierung und der Verteilung von Schwefel präsentiert. T2 - 9. Betonfachtagung CY - Berlin, Germany DA - 12.11.2019 KW - Chloride KW - Beton KW - LIBS KW - Schädigung PY - 2019 AN - OPUS4-51673 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gaal, Mate A1 - Heckel, Thomas A1 - Brackrock, Daniel T1 - Linear and matrix phased array inspection of complex thin wall components N2 - The application of phased arrays in either linear or matrix arrangement in combination with signal processing opens the door for the mechanized inspection of different thin wall materials itself as well as their joining methods. Modern lightweight components are typically manufactured by a composition of different types of e.g. steels, metals, fiber reinforced plastics and glass. Dependent on the material combinations e.g. welding, brazing, bonding, cladding or coating may be applied during the manufacturing process to join different semi-finished products to form the component. The resulting complex material composition and different damage mechanisms pose new challenges to non-destructive testing with ultrasound due to the different material properties and the overall arrangement of the materials employed. The sound field variation capabilities of array probes may be helpful to overcome some of these challenges if adapted to the specific inspection task. Examples for the non-destructive mechanized phased array inspection of different types of materials and joining methods will be presented. T2 - KINT Symposium CY - Amsterdam, The Netherlands DA - 30.10.2019 KW - Matrix array KW - Phased array KW - Joints PY - 2019 AN - OPUS4-49538 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Evsevleev, Sergei A1 - Mishurova, Tatiana A1 - Sevostianov, Igor A1 - Garcés, Gerardo A1 - Requena, Guillermo A1 - Cabeza, Sandra A1 - Bruno, Giovanni T1 - Load transfer and damage evolution in multiphase Al alloy matrix composites under uniaxial compression N2 - Aluminum alloys are extensively used in the automotive industry. Particularly, squeeze casting production of Al-Si alloys is employed in the conception of metal matrix composites (MMC) for combustion engines. Such materials are of a high interest since they allow combining improved mechanical properties and reduced weight and hence improve efficiency. We investigate two types of MMCs, which can be potentially used for production of combustion engine pistons: 1) a near-eutectic cast AlSi12CuMgNi alloy reinforced with 15%vol. Al2O3 random planar oriented short fibers and 2) the same alloy reinforced with 7%vol. Al2O3 random planar oriented short fibers + 15%vol. SiC particles. Complex 3D microstructure of the samples in as-cast condition, consisting of four and five phases (Al matrix, eutectic Si, intermetallics, Al2O3 fibers and SiC particles) was investigated by synchrotron computed tomography (CT). Advanced methods based on machine learning were applied for segmentation of all phases. This allowed extracting quantitative information such as volume fraction, shape and interconnectivity of every phase. In-situ compression tests during neutron diffraction experiments were used to track the load transfer among phases, while CT on pre-strained samples to monitor and quantify damage. A micromechanical model was developed to simulate the evolution of the internal stress of each phase during uniaxial compression. We showed that in composites with the Al2O3 fiber mat plane perpendicular to the load axis the Al-alloy matrix presents a large hydrostatic stress component, i.e. undergoes compression also in the direction transverse to the external load. This feature holds with and without the addition of SiC ceramic reinforcement and is absent in the case when the Al2O3 fiber mat plane is parallel to the load axis. We show, that the intermetallics play a decisive role at very high loads, when all other reinforcement phases suffer (extensive) damage. The addition of SiC particles does alleviate the load on the Al2O3 fibers, on the eutectic Si, and on the intermetallic phases in both cases of parallel and orthogonal (to the load axis) Al2O3 fiber orientation. Apart from the beneficial addition of ceramic reinforcement, the presence of intermetallic phase and eutectic silicon, forming an interconnected network even at high loads, when single particles break, confers peculiar properties to these multi-phase composites. T2 - The 3rd International Conference on Light Materials CY - Manchester, UK DA - 05.11.2019 KW - Aluminum alloy KW - Metal Matrix Composite KW - Computed tomography KW - Neutron diffraction KW - Stress analysis KW - Load partition PY - 2019 AN - OPUS4-49640 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Avila, Luis A1 - Rehmer, Birgit A1 - Skrotzki, Birgit A1 - Graf, B. A1 - Rethmeier, Michael A1 - Ulbricht, Alexander T1 - Low cycle fatigue behavior and failure mechanisms of additively manufactured Ti-6Al-4V N2 - Despite of the significant advances in AM process optimization there is still a lack of experimental results and understanding regarding the mechanical behavior and microstructural evolution of AMparts, especially in loading conditions typical for safety-relevant applications e.g. in the aerospace or power engineering. Within the scope of the presented investigations, a characterization of the fatigue behavior of additively manufactured Ti-6Al-4V in the low cycle fatigue regime was carried out in the range of 0.3 to 1.0 % strain amplitude at room temperature, 250°C and 400°C. The Ti-6Al-4V specimens are machined out of lean cylindrical rods, which were fabricated using powder laser metal deposition (LMD) with an improved build-up strategy. The improved strategy incorporates variable track overlap ratios to achieve a constant growth in the shell and core area. The low-cycle-fatigue behavior is described based on cyclic deformation curves and strain-based fatigue life curves. The lifetimes are fitted based on the Manson-Coffin-Basquin relationship. A characterization of the microstructure and the Lack-of-Fusion (LoF)-defect-structure in the as-built state is performed using optical light microscopy and high-resolution computed tomography (CT) respectively. The failure mechanism under loading is described in terms of LoF-defects-evolution and crack growth mechanism based on an interrupted LCF test with selected test parameters. After failure, scanning electron microscopy, digital and optical light microscopy and CT are used to describe the failure mechanisms both in the longitudinal direction and in the cross section of the specimens. The fatigue lives obtained are comparable with results from previous related studies and are shorter than those of traditionally manufactured (wrought) Ti-6Al-4V. In this study new experimental data and understanding of the mechanical behavior under application-relevant loading conditions (high temperature, cyclic plasticity) is gained. Furthermore, a better understanding of the role of LoFdefects and AM-typical microstructural features on the failure mechanism of LMD Ti-6Al-4V is achieved. T2 - First European Conference on Structural Integrity of Additively Manufactured Materials (ESIAM19) CY - Trondheim, Norway DA - 09.09.2019 KW - High Temperature Testing KW - Titanium KW - Ti-6Al-4V KW - Additive Manufacturing KW - Computed Tomography KW - Microstructure KW - Tensile Properties KW - Low Cycle Fatigue PY - 2019 AN - OPUS4-49492 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Waske, Anja T1 - Magnetocaloric materials for cooling and harvesting of low-grade waste heat N2 - To date, there are very few technologies available for the conversion of low-temperature waste heat into electricity. Thermomagnetic generators are one approach proposed more than a century ago. Such devices are based on a cyclic change of magnetization with temperature. For thermomagnetic materials, we used a commercial magnetocaloric alloy with a transition temperature of 300 K. T2 - Symposiumsorganisation und Vortrag CY - Stockholm, Sweden DA - 05.09.2019 KW - X-Ray imaging KW - Energy harvesting KW - Additive Manufacturing KW - Magnetocaloric KW - Material Science KW - Non-Destructive testing PY - 2019 AN - OPUS4-50178 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schob, D. A1 - Sagradov, I. A1 - Roszak, R. A1 - Sparr, H. A1 - Franke, R. A1 - Ziegenhorn, M. A1 - Kupsch, Andreas A1 - Léonard, Fabien A1 - Müller, Bernd R. A1 - Bruno, Giovanni T1 - Material and damage behaviour of 3D printed PA12 under cyclic loading N2 - The material and damage behaviour of additively manufactured polyamide 12 (PA12) under dynamic loading was characterized by cyclic tests and microstructure analysis. The results were used to develop a numerical material and damage model. In a recent study, it was shown that the material and damage behaviour of 3D printed PA12 under quasistatic loading is simulated in a realistic way by coupling the material model by Chaboche and the damage model by Gurson-Tvergaard-Needleman (GTN). Using microscopy, X-ray refraction, and computed tomography, a porosity of about 5% was evaluated. These results served as a starting point for the present work. For the dynamic load, both the previously used Chaboche model and the GTN model were extended. Furthermore, the temperature was measured during the experiment and the self-heating effect was observed. Therefore, a temperaturedependent material parameters for the simulation were introduced. Considering the results of mechanical experiments, microstructural investigations, and self-heating effects, a good agreement between Experiment and numerical simulation could be achieved. T2 - VI International Conference on Computational Modeling of Fracture and Failure of Materials and Structures CY - Brunswick, Germany DA - 12.06.2019 KW - Polyamide 12 KW - Selective Laser Sintering (SLS) KW - Viscoplasticity KW - Chaboche model KW - GTN model KW - X-ray refraction KW - Computed tomography PY - 2019 AN - OPUS4-48335 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kupsch, Andreas A1 - Müller, Bernd R. A1 - Bruno, Giovanni A1 - Lange, A. A1 - Hentschel, M.P. A1 - Laquai, René T1 - Materialcharakterisierung mittels bildgebender Röntgenstreuverfahren N2 - Die herkömmliche Bildgebung mit Röntgenstrahlung beruht auf unterschiedlicher Absorption durch verschiedene Materialien im Volumen eines Körpers. Es entsteht ein "Massebild". Die hier vorgestellten Verfahren benutzen die Brechung und Beugung von Röntgenstrahlen, um innere Oberflächen oder die Molekulartextur von Materialien und Bauteilen abzubilden. Im Vortrag werden die entsprechenden Messtechniken an der BAM im Labormaßstab sowie an Großforschungseinrichtungen vorgestellt und anhand einiger Anwendungsbeispiele die zusätzlichen Informationen zur herkömmlichen Durchstrahlung diskutiert. T2 - 243. Sitzung DGZfP-Arbeitskreis Thüringen CY - Ilmenau, Germany DA - 11.04.2019 KW - Röntgenrefraktion KW - Röntgenbeugung KW - Diffraction Enhanced Imaging KW - Keramik KW - Polyethylen KW - Metall-Matrix-Komposit PY - 2019 AN - OPUS4-49859 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -