TY - JOUR A1 - Merino, E. A1 - Cere, S. A1 - Özcan Sandikcioglu, Özlem A1 - Dimper, Matthias A1 - Sobrados, I. A1 - Durán, A. A1 - Castro, Y. T1 - Influence of the BF3·O(C2H5)2 on the corrosion resistance of hybrid silica sol-gel coatings deposited on flash-PEO-treated Mg alloy N2 - Achieving highly cross-linked sol-gel coatings to provide effective corrosion protection of Mg alloys remains a challenging task. The aim of this work is to evaluate the effect boron trifluoride diethyl etherate (BF3·O(C2H5)2) as catalyst to epoxy group in a GPTMS/TEOS/SiO2 sol and assesses its effect on the structure and corrosion resistance properties of Flash-PEO coated pre-treated Mg alloy. 29Si MAS NMR and 13C CPMAS-NMR demonstrated that (BF3·O(C2H5)2) efficiently promotes the epoxy polymerization of the GPTMS and the formation of a hybrid silica network. However, the amount of (BF3·O(C2H5)2) should be optimized to minimize the formation of undesirable byproducts such as ethyl ether terminal units. Therefore, GPTMS/TEOS/SiO2 sols containing different amounts of (BF3·O(C2H5)2) were synthesized and deposited onto the Flash-PEO coated Mg alloy, leading to bilayer systems with a total thickness of ⁓8 μm. The corrosion behavior of the bilayer coatings in 3.5 wt% NaCl solution was evaluated by electrochemical impedance spectroscopy (EIS) and Scanning Kelvin probe microscope (SKPFM). The results revealed that the barrier properties of the coatings with enhanced cross-linked structure showed impedance modulus (│Z│f:0.1 Hz) approximately four orders of magnitude higher than the bare magnesium alloy and two orders of magnitude higher than the F-PEO coated sample. A suitable compromise between (BF3·O(C2H5)2) amount and sol-gel film structure is required to obtain a more durable barrier coating capable to extend the protective lifespan of the magnesium alloy. KW - Sol-gel KW - Corrosion KW - AZ31B Mg alloy KW - Chemical structure KW - SKPFM PY - 2026 DO - https://doi.org/10.1016/j.surfcoat.2025.133055 SN - 0257-8972 VL - 522 SP - 1 EP - 13 PB - Elsevier B.V. AN - OPUS4-65416 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Valet, Svenja A1 - Bohlmann, Tatjana A1 - Ebell, Gino A1 - Burkert, Andreas T1 - pH sensitive gel pads for the visualization of anodes and cathodes on zinc N2 - Zinc and zinc alloys have many applications. Zinc corrosion takes place in the atmosphere and is assumed to follow the water drop theory (a macroelement), in which the anode is at the centre of the drop and is surrounded by a cathode. This paper is the first to use gel electrolytes made of agar to visualize anodic and cathodic areas on zinc samples in order to examine the water drop theory. For that, agar gels were added with universal pH indicators, as the anode and cathode exhibit different pH values. In this paper, different amounts of pH indicators were tested to determine whether the indicator influences the potential, the impedance, phase shift, corrosion current and potential and corrosion layer resistance. KW - Corrosion KW - Zinc KW - Gel electrolyte PY - 2026 DO - https://doi.org/10.1016/j.electacta.2026.148134 SN - 0013-4686 VL - 551 SP - 1 EP - 21 PB - Elsevier Ltd. AN - OPUS4-65308 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Heyn, A. A1 - Kotula, Stefan A1 - Ebell, Gino A1 - Babutzka, M. T1 - Results of a Round Robin Test for the Determination of Polarization Resistances on Differently Weathered Zinc Samples Using Gel Electrolytes N2 - This article presents the results of a round robin test throughout Germany with 19 participating institutions. Corrosion productlayer resistances (RL ) were determined on two differently weathered pure zinc samples and a sample activated with NaOH bymeans of electrochemical measurement of the linear polarization resistance (LPR) using agar‐based gel electrolytes. The roundrobin test was organized by the Bundesanstalt für Materialforschung und ‐prüfung (BAM) in Berlin. The measurements werecarried out by the participants in the period from May to July 2021. The results are summarized in this article comprising anassessment of the reproducibility and repeatability of the measurements. The methodology is suitable for distinguishing zincsurfaces after exposure to different atmospheres based on the corrosion product layer resistances (RL). In addition, possibleproblems in the application of the method were identified, and solutions for improving reproducibility and repeatability arediscussed. The results and knowledge from the round robin test are incorporated into a new test standard (DIN 50023:2024‐07)for this measurement method KW - Corrosion PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-630546 DO - https://doi.org/10.1002/maco.202414696 SN - 1521-4176 SP - 1 EP - 12 PB - Wiley AN - OPUS4-63054 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ebell, Gino A1 - Seifert, Lando A1 - Burkert, Andreas T1 - Innovative Korrosionsprüfung für Beton- und Spannstähle T1 - Test methods for corrosion testing of reinforcing and prestressing steels N2 - Korrosion ist einer der maßgeblichen Schädigungsmechanis-men im Stahlbetonbau und limitiert die Nutzungsdauer vonInfrastrukturbauwerken zum Teil erheblich. Dabei differenziertman zwischen verschiedenen Korrosionsvarianten, Korrosioninfolge Karbonatisierung des Betons, chloridinduzierte Korro-sion an Meerwasserbauwerken oder durch Tausalzbelastungund im Fall von Spannstahlbauwerken kann zusätzlich was-serstoffinduzierte Spannungsrisskorrosion (SpRK) auftreten.Für den Einsatz alternativer Betonstähle wie nichtrostenderBetonstahl gilt es, die Höhe des kritischen korrosionsaus-lösenden Chloridgehalts zu bestimmen. Um diesen für diejeweiligen Betonstähle zu ermitteln, fehlen bislang jedochnormativ geregelte Prüfverfahren. Die Empfindlichkeit vonSpannstählen gegenüber SpRK bedarf gemäß aktueller Nor-mung Langzeit-Auslagerungstests, die eine werkseigeneProduktionskontrolle aufgrund der langen Prüfzeiten nahezuunmöglich machen. Ein neu entwickeltes Prüfverfahren unterAnwendung kathodischer Polarisation, das inzwischen imneusten Entwurf der DIN EN ISO 15630–3 aufgenommenwurde, ermöglicht eine Bewertung der SpRK-Empfindlichkeitfür Spanndrähte innerhalb von 24 Stunden. Die Ergebnissetragen zur Verbesserung der Lebensdauerabschätzung undzur Weiterentwicklung von Normen für korrosionsbeständigeBetonstähle und der Robustheitsbewertung von Spannstählenbei. N2 - Corrosion is a primary damage mechanism in reinforced concrete construction, significantly reducing the service life of infrastructure. A categorisation of corrosion is imperative for the comprehension of the subject. The corrosion of concrete can be attributed to the carbonation process, whilst chloride-induced corrosion is prevalent in structures exposed to seawater or by de-icing salt. Additionaly to the former corrosion processe, prestressing steel structures could be also highly susceptible to hydrogen-induced stress corrosion cracking (SCC). In order to utilise alternative reinforcing steels, such as stainless reinforcing steel, it is necessary to ascertain the level of critical chloride threshold that can induce corrosion. Nevertheless, there is an absence of standardised test methods for determining this for the respective reinforcing steels to date. Acc. to current standardization, the sensitivity of prestressing steels to chromium content necessitates long-term ageing tests, which impede in-house production control due to the extended testing times. However, a newly developed test method using cathodic polarization, which has now been included in the latest draft of DIN EN ISO 15630–3, makes it possible to assess the susceptibility of prestressing steels to corrosion cracking within 24 hours. The results of this study will contribute to the improvement of service life estimation and the further development of standards for corrosion-resistant reinforcing steels and the robustness assessment of prestressing steels. KW - Korrosion KW - Spannstahl KW - Nichtrostender Betonstahl KW - Corrosion KW - Prestressing steel KW - Stainless reinforcing steel KW - Wasserstoff KW - Spannungsrisskorrosion KW - Lochkorrosion KW - Hydrogen KW - Stress corrosion cracking KW - Pitting corrosion PY - 2025 DO - https://doi.org/10.1002/best.202500025 SN - 0005-9900 SN - 1437-1006 SP - 1 EP - 8 PB - Ernst CY - Berlin AN - OPUS4-63305 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ebell, Gino A1 - Tannert, S. A1 - Lehmann, Jens A1 - Müller, H. T1 - Offshore Weathering Campaign on a North Sea Wind Farm Part One: Corrosivity Categories N2 - The aim of this study is to investigate the corrosion behavior of materials and coatings in offshore environments, with a focus on determining the corrosivity categories at different locations on wind turbines. The collaboration between the authors enabled a 3‐year weathering campaign at the Hohe See and Albatros offshore wind farms in the North Sea. Metal panels were installed on two wind turbines to assess the corrosivity of different atmospheric conditions. Preliminary results indicate significant variations in corrosivity depending on location and material used, suggesting that current standards may not fully reflect real‐world conditions. The results of the study will help to optimize material selection and corrosion protection strategies for offshore wind farms, potentially extending their lifetime and reducing operating costs. KW - Corrosion KW - Offshore KW - Wind PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-628995 DO - https://doi.org/10.1002/maco.202414711 SN - 1521-4176 SP - 1 EP - 10 PB - Wiley CY - Weinheim AN - OPUS4-62899 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Manzoni, Anna Maria A1 - Mohring, Wencke A1 - Schneider, Mike A1 - Laplanche, Guillaume A1 - Hagen, Sebastian Peter A1 - Stephan‐Scherb, Christiane T1 - High‐Temperature Oxidation of the CrFeNi Medium‐Entropy Alloy N2 - The isothermal high‐temperature oxidation behavior of the equiatomic CrFeNi medium‐entropy alloy is a key issue that determines whether this material is suited for high‐temperature application. In this view, the understanding of the long‐term behavior is even more crucial than short‐term corrosion effects. Herein, a single‐phase CrFeNi alloy of the face‐centered‐cubic structure is exposed to synthetic air at 1000, 1050, and 1100 °C for 24, 100, and 1000 h and its oxidation behavior is systematically compared to that of 316L steel, which shows a surprising initial oxidation stabilization during early stages. The oxidation rate of CrFeNi is parabolic at 1000 °C (with a parabolic constant kp = 1.4·10−5 mg−2 cm−4 s−1) and 1050 °C (kp = 2.7·10−5 mg−2 cm−4 s−1), but breakaway oxidation occurs at 1100 °C after 4 h of exposure. In all cases, the oxide scales are found to (at least) partially spall off. Chromium diffuses outward to form a Cr2O3 layer at the gas/oxide interface, and a thin layer of (Cr, Fe, Ni)3O4 is identified at the oxide/alloy interface. Unlike the 316L alloy, which contains more Mn and Fe, the CrFeNi alloy does not show any catastrophic oxidation behavior at the investigated conditions. KW - Corrosion KW - Medium-entropy alloy KW - Scanning electron microscopy PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-636672 DO - https://doi.org/10.1002/adem.202500400 SN - 1438-1656 SP - 1 EP - 14 PB - Wiley VHC-Verlag AN - OPUS4-63667 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Malefioudaki, Mariella A1 - Misra, Archismita A1 - Sbeity, Nadja A1 - Zueco-Vincelle, Juan A1 - Laguna-Bercero, Miguel A. A1 - Koerdt, Andrea A1 - Martín-Rapún, Rafael A1 - Mitchell, Scott G. T1 - Multifunctional polyoxomolybdate ionic liquid coatings for mitigating microbiologically influenced corrosion N2 - Corrosion of metals and other materials in marine environments poses significant economic, operational, safety, and environmental challenges across the oil and gas industry, the renewable energy sector, and maritime infrastructure. Microbiologically influenced corrosion (MIC) accounts for a substantial portion of this corrosion, with sulfate-reducing bacteria (SRB) and methanogenic archaea (MA) being key contributors. Conventional methods such as cathodic polarization have proven insufficient in mitigating the colonization of corrosive microbial communities in real marine environments, requiring the development of alternative, broad-spectrum antimicrobial strategies to prevent such biofilm formation. Recently, molybdate has emerged as a potential alternative to traditional biocides and nitrate. Our hypothesis is polyoxometalate-ionic liquids (POM-ILs), which exhibit antimicrobial and anticorrosion properties, could have a broader spectrum of antimicrobial activity than demonstrated until now and could be capable of shielding and protecting sensitive metal surfaces from the extreme acidic environments produced by MIC microorganisms. Here we show how two prototype polyoxomolybdate-based POM-ILs, [(CH3(CH2)6)4N]2[Mo6O19] and [(CH3(CH2)6)4N]4[Mo8O26], demonstrated antimicrobial activity at microgram per millilitre concentrations, prevented biofilm formation on metal surfaces, and provided resistance to corrosive acidic environments. Furthermore, impedance measurements were commensurate with electron microscopy studies showing that POM-IL-coated brass coupons withstood extremely corrosive environments. These proof-of-concept results demonstrate how multi-functional POM-IL coatings represent promising MIC mitigation solutions by providing a hydrophobic acid-resistant and biocidal protective layer that prevents biocolonisation and acidic corrosion by MIC microorganisms. KW - Polyoxometalates KW - Ionic liquid KW - Microbiologically influenced corrosion KW - Corrosion KW - Heritage preservation PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-631951 DO - https://doi.org/10.1039/d5mh00373c SN - 2051-6347 VL - 12 IS - 13 SP - 4648 EP - 4661 PB - Royal Society of Chemistry (RSC) CY - Cambridge AN - OPUS4-63195 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Tidblad, Johan A1 - Moya Núñez, Alice A1 - de la Fuente, Daniel A1 - Ebell, Gino A1 - Flatlandsmo Berglen, Tore A1 - Grøntoft, Terje A1 - Hans, Ulrik A1 - Christodoulakis, Ioannis A1 - Kajánek, Daniel A1 - Kreislová, Kateřina A1 - Kwiatkowski, Lech A1 - La Torreta, Teresa A1 - Lutze, Rafał A1 - Pinar Larrubia, Guadalupe A1 - Pintus, Valentina A1 - Prange, Michael A1 - Spezzano, Pasquale A1 - Varotsos, Costas A1 - Verney-Carron, Aurélie A1 - Vuorio, Tiina A1 - Yates, Tim T1 - Corrosion and Soiling in the 21st Century: Insights from ICP Materials and Impact on Cultural Heritage N2 - This paper reviews results published by the International Co-operative Programme on Effects on Materials including Historic and Cultural Monuments (ICP Materials) with emphasis on those obtained after the turn of the century. Data from ICP Materials come from two main sources. The first is through exposures of materials and collection of environmental data in a network of atmospheric exposure test sites mainly distributed across Europe. Corrosion of carbon steel has continued to decrease during the period 2000–2020 but corrosion of zinc only up until 2014, and the trend in zinc corrosion is only visible when examining four-year data. Surface recession of limestone as well as soiling of modern glass show no decreasing trend during 2000–2020. The second is through case studies performed at heritage sites across Europe. Risk analysis of corrosion and soiling for twenty-six sites indicate that currently soiling is a more significant maintenance trigger than corrosion. Costs for maintaining heritage sites are substantial and costs attributable to air pollution is estimated from 40% to as much as 80% of the total cost. Future directions of the program are work on effects of particulate matter, improving the scientific basis for the work, and making the monitoring data publicly available. KW - Corrosion KW - Atmospheric corrosion KW - Soiling PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-644651 DO - https://doi.org/10.3390/cmd6040054 SN - 2624-5558 VL - 6 IS - 4 SP - 1 EP - 25 PB - MDPI AG AN - OPUS4-64465 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pfennig, Anja A1 - Mohring, Wencke A1 - Wolf, Marcus T1 - The insignificant improvement of corrosion and corrosion fatigue behavior in geothermal environment applying Boehmit coatings on high alloyed steels N2 - The efficacy of alumina-sol based coatings in a water-free atmosphere at high temperatures suggests a potential solution for enhancing the corrosion resistance of high-alloyed steels in Carbon Capture and Storage (CCS) environments. In this study, coupons of X20Cr13, designed for use as injection pipes with 13% Chromium and 0.20% Carbon (1.4021, AISI 420), were sol-gel coated with water and ethanol-based alumina. These coated coupons were then exposed to CO2-saturated saline aquifer water, simulating conditions in the Northern German Basin, for 1000 h at ambient pressure and 60 °C. Corrosion fatigue experiments were also conducted using specimens of X5CrNiMoCuNb16-4 (1.4542, AISI 630), a suitable candidate for geothermal applications, to assess the impact of the ethanol-based coating on the number of cycles to failure at different stress amplitudes. Unfortunately, the coating exhibited early spallation, resulting in corrosion kinetics and corrosion fatigue data identical to those of uncoated specimens. Consequently, the initially promising Boehmit coating is deemed unsuitable for CCS applications and further research therefore not advisable. KW - Alumina coating KW - High alloyed steel KW - Pitting KW - Surface corrosion KW - CO2 KW - Pipeline KW - Corrosion KW - CCS KW - CO2-storage PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-623786 DO - https://doi.org/10.3390/app14041575 SN - 2076-3417 VL - 14 IS - 4 SP - 1 EP - 12 PB - MDPI CY - Basel AN - OPUS4-62378 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zhang, Runze A1 - Sur, Debashish A1 - Li, Kangming A1 - Witt, Julia A1 - Black, Robert A1 - Whittingham, Alexander A1 - Scully, John R. A1 - Hattrick-Simpers, Jason T1 - Bayesian assessment of commonly used equivalent circuit models for corrosion analysis in electrochemical impedance spectroscopy N2 - Electrochemical Impedance Spectroscopy (EIS) is a crucial technique for assessing corrosion of metallic materials. The analysis of EIS hinges on the selection of an appropriate equivalent circuit model (ECM) that accurately characterizes the system under study. In this work, we systematically examined the applicability of three commonly used ECMs across several typical material degradation scenarios. By applying Bayesian Inference to simulated corrosion EIS data, we assessed the suitability of these ECMs under different corrosion conditions and identified regions where the EIS data lacks sufficient information to statistically substantiate the ECM structure. Additionally, we posit that the traditional approach to EIS analysis, which often requires measurements to very low frequencies, might not be always necessary to correctly model the appropriate ECM. Our study assesses the impact of omitting data from low to medium-frequency ranges on inference results and reveals that a significant portion of low-frequency measurements can be excluded without substantially compromising the accuracy of extracting system parameters. Further, we propose simple checks to the posterior distributions of the ECM components and posterior predictions, which can be used to quantitatively evaluate the suitability of a particular ECM and the minimum frequency required to be measured. This framework points to a pathway for expediting EIS acquisition by intelligently reducing low-frequency data collection and permitting on-the-fly EIS measurements. KW - Electrochemical Impedance Spectroscopy (EIS) KW - MAPz@BAM KW - Bayesian Inference KW - Corrosion PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-623392 DO - https://doi.org/10.1038/s41529-024-00537-8 VL - 8 SP - 120 PB - Springer Materials AN - OPUS4-62339 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Frenck, Johanna-Maria A1 - Frenck, Georg A1 - Degener, Sebastian A1 - Vollmer, Malte A1 - Niendorf, Thomas T1 - Interrelationships of stress-induced martensitic phase transformation and pitting corrosion in iron-based shape memory alloys N2 - Orientation dependence of stress-induced martensitic transformation under compression and the influence of a corrosion attack on superelastic properties were investigated for Fe42.7Mn34.7Al13.4Ni7.7Cr1.5 (at.−%) single crystals. The results of incremental strain tests show that the crystallographic orientation has a considerable impact on the superelastic performance, eventually resulting from the formation of twinned or detwinned martensite to accommodate strain as well martensite variant interaction. In order to investigate the effect of a corrosive environment on the mechanical performance and martensitic transformation, compression specimens were immersed in a 5.0 wt.−% NaCl solution for 24 h before tested in incremental strain tests. The immersion of the compression specimens revealed a partial surface corrosion attack including localized pitting corrosion. The localized corrosion attack increased the number of active martensite plates, most probably due to an induced multiaxial stress state. Further investigations on specimens subjected to −6% compressive strain revealed that areas with retransformed martensite serve as nucleation zones for corrosion damage. Stress-induced corrosion cracks developed, which eventually deteriorate functional response. KW - Shape memory alloy (SMA) KW - In situ characterization KW - Corrosion KW - Austenite-to-martensite phase transformation PY - 2024 DO - https://doi.org/10.1016/j.mtla.2023.102001 VL - 33 SP - 1 EP - 11 PB - Elsevier BV AN - OPUS4-61283 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kingsbery, P. A1 - Manzoni, Anna Maria A1 - Suárez Ocano, Patricia A1 - Többens, D. M. A1 - Stephan-Scherb, C. T1 - High‐temperature KCl‐induced corrosion of high Cr and Ni alloys investigated by in‐situ diffraction N2 - High‐temperature KCl‐induced corrosion in laboratory air was observed in situ utilizing X‐ray diffraction. High Cr‐containing model alloys (Fe‐13Cr, Fe‐18Cr‐12Ni, and Fe‐25Cr‐20Ni) were coated with KCl and exposed to dry air at 560°C. KCl‐free alloys were studied in the equivalent atmosphere as a reference. After exposure to KCl‐free environments, all alloys showed the formation of very thin oxide layers, indicating good corrosion resistance. In contrast, KCl‐bearing alloys showed distinct damage after exposure. KW - Corrosion KW - In-situ diffraction KW - High-temperature corrosion PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-600831 DO - https://doi.org/10.1002/maco.202314224 SN - 0947-5117 SP - 1 EP - 10 PB - Wiley VHC-Verlag AN - OPUS4-60083 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Heyn, A. A1 - Meist, M. A1 - Michael, O. A1 - Babutzka, M. A1 - Valet, Svenja A1 - Ebell, Gino T1 - Electrochemical characterization of surfaces of galvanized steels under different exposure conditions using gel electrolytes N2 - The corrosion behavior of galvanized steels and zinc components under atmospheric exposure depends mostly on the corrosion product‐based cover layer formation under the prevailing conditions. The use of agar‐based gel electrolytes makes it possible to use electrochemical methods to obtain a characteristic value from these cover layers that describe their current and future protective capacity. It is shown here that different states of galvanized steel can be distinguished very well under laboratory conditions and that this method is also suitable for use under practical conditions. Based on the characteristic values and assuming future time of wetness, it is very easy to draw up a forecast for the future corrosion rate, which provides plausible values. KW - Materials Chemistry KW - Metals and Alloys KW - Surfaces, Coatings and Films KW - Mechanical Engineering KW - Mechanics of Materials KW - Environmental Chemistry KW - Corrosion KW - Znc PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-599234 DO - https://doi.org/10.1002/maco.202414389 SP - 1 EP - 16 PB - Wiley VHC-Verlag AN - OPUS4-59923 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Koerdt, Andrea A1 - Gerengi, Husnu A1 - Kaya, Ertugrul A1 - M. Solomon, Moses A1 - Snape, Matthew T1 - Advances in the Mitigation of Microbiologically Influenced Concrete Corrosion: A Snapshot N2 - Concrete, a versatile construction material, faces pervasive deterioration due to microbiologically influenced corrosion (MIC) in various applications, including sewer systems, marine engineering, and buildings. MIC is initiated by microbial activities such as involving sulfate-reducing bacteria (SRB), sulfur-oxidizing bacteria (SOB), etc., producing corrosive substances like sulfuric acid. This process significantly impacts structures, causing economic losses and environmental concerns. Despite over a century of research, MIC remains a debated issue, lacking standardized assessment methods. Microorganisms contribute to concrete degradation through physical and chemical means. In the oil and gas industry, SRB and SOB activities may adversely affect concrete in offshore platforms. MIC challenges also arise in cooling water systems and civil infrastructures, impacting concrete surfaces. Sewer systems experience biogenic corrosion, primarily driven by SRB activities, leading to concrete deterioration. Mitigation traditionally involves the use of biocides and surface coatings, but their long-term effectiveness and environmental impact are questionable. Nowadays, it is important to design more eco-friendly mitigation products. The microbial-influenced carbonate precipitation is one of the green techniques and involves incorporating beneficial bacteria with antibacterial activity into cementitious materials to prevent the growth and the formation of a community that contains species that are pathogenic or may be responsible for MIC. These innovative strategies present promising avenues for addressing MIC challenges and preserving the integrity of concrete structures. This review provides a snapshot of the MIC in various areas and mitigation measures, excluding underlying mechanisms and broader influencing factors. KW - MIC KW - Corrosion KW - Concrete KW - Environment PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-619218 DO - https://doi.org/10.3390/ma17235846 VL - 17 IS - 23 SP - 1 EP - 19 PB - MDPI AN - OPUS4-61921 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wetzel, Annica A1 - Morell, Daniel A1 - von der Au, Marcus A1 - Wittstock, Gunther A1 - Özcan Sandikcioglu, Özlem A1 - Witt, Julia T1 - Transpassive Metal Dissolution vs. Oxygen Evolution Reaction: Implication for Alloy Stability and Electrocatalysis T1 - Transpassive Metallauflösung vs. Sauerstoffentwicklung: Auswirkungen auf Legierungsstabilität und Elektrokatalyse N2 - Multi-principal element alloys (MPEAs) are gaining interest in corrosion and electrocatalysis research due to their electrochemical stability across a broad pH range and the design flexibility they offer. Using the equimolar CrCoNi alloy, we observe significant metal dissolution in a corrosive electrolyte (0.1 M NaCl, pH 2) concurrently with the oxygen evolution reaction (OER) in the transpassive region despite the absence of hysteresis in polarization curves or other obvious corrosion indicators. We present a characterization scheme to delineate the contribution of OER and alloy dissolution, using scanning electrochemical microscopy (SECM) for OER-onset detection, and quantitative chemical analysis with inductively coupled-mass spectrometry (ICP-MS) and ultraviolet visible light (UV-Vis) spectroscopy to elucidate metal dissolution processes. In-situ electrochemical atomic force microscopy (EC-AFM) revealed that the transpassive metal dissolution on CrCoNi is dominated by intergranular corrosion. These results have significant implications for the stability of MPEAs in corrosion systems, emphasizing the necessity of analytically determining metal ions released from MPEA electrodes into the electrolyte when evaluating Faradaic efficiencies of OER catalysts. The release of transition metal ions not only reduces the Faradaic efficiency of electrolyzers but may also cause poisoning and degradation of membranes in electrochemical reactors. N2 - Multi-Hauptelement-Legierungen (MPEAs) gewinnen in der Korrosions- und Elektrokatalyseforschung aufgrund ihrer elektrochemischen Stabilität über einen breiten pH-Bereich und der Vielfalt der möglichen chemischen Zusammensetzungen zunehmend an Interesse. In unseren Untersuchungen mit der äquimolaren CrCoNi-Legierung in einem sauren Elektrolyten (0.1 M NaCl, pH 2) beobachteten wir eine signifikante Metallauflösung, die mit der Sauerstoffentwicklungsreaktion (OER) im transpassiven Bereich einhergeht, obwohl in zyklischen Polarisationskurven keine Hysterese auftrat oder andere offensichtliche Korrosionsindikatoren vorlagen. In diesem Artikel wird ein Charakterisierungskonzept eingeführt, dass die Beiträge der OER und der Legierungsauflösung differenziert. Hierfür kommt die elektrochemische Rastermikroskopie (SECM) zum Nachweis des Beginns der OER und die quantitative chemische Analyse mit induktiv gekoppelter Massenspektrometrie (ICP-MS) und UV/Vis-Spektrometrie zur Aufklärung der Metallauflösungsprozesse zum Einsatz. Die elektrochemische In situ-Atomkraftmikroskopie (EC-AFM) zeigte, dass die intergranulare Korrosion der dominierende Mechanismus der transpassive Metallauflösung von CrCoNi ist. Diese Ergebnisse besitzen erhebliche Auswirkungen für die Beurteilung der Stabilität von MPEAs in Korrosionssystemen und der Stromausbeute von OER-Katalysatoren auf der Basis von MPEAs. Die Daten unterstreichen die Notwendigkeit der analytischen Bestimmung von Metallionen, die von MPEA-Elektroden freigesetzt werden. Die Freisetzung von Übergangsmetallionen verringert nicht nur die Stromausbeute von Elektrolyseuren, sondern kann zu einer Schädigung von Membranen in elektrochemischen Reaktoren führen. KW - Transpassive dissolution KW - Corrosion KW - Multi-prinicpal element alloys (MPEAs) KW - Passivation PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-597045 DO - https://doi.org/10.1002/anie.202317058 SP - 1 EP - 8 PB - Wiley VHC-Verlag AN - OPUS4-59704 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wetzel, Annica A1 - Morell, Daniel A1 - von der Au, Marcus A1 - Witt, Julia A1 - Özcan Sandikcioglu, Özlem T1 - Transpassive Behavior of Equimolar CrMnFeCoNi and CrCoNi Multi‐Principal Element Alloys in an Alkaline NaCl Electrolyte N2 - AbstractWe investigated the corrosion properties and transpassive behavior of CrMnFeCoNi and CrCoNi multi‐principal element alloys (MPEAs) in a 0.1 M NaCl electrolyte at pH 12. By using SECM‐based tip substrate voltammetry (TSV) in combination with the chemical analysis of the electrolyte, we were able to differentiate between anodic metal dissolution and oxygen evolution in the transpassive range. Our investigations have shown that CrCoNi has a significantly higher corrosion resistance compared to CrMnFeCoNi. In the studied alkaline environment, a transpassive oxide film is formed on the surface of CrCoNi during secondary passivation. This transpassive oxide film appears to play a significant role in oxygen evolution, as the increase in TSV currents at the microelectrode coincides with the corresponding current density plateau of the voltametric current trace. The formation of the transpassive oxide film was not observed in previous studies conducted in acidic environments. Moreover, the alkaline electrolyte induced a positive hysteresis and mild pitting corrosion, in addition to intergranular corrosion, which was the sole corrosion process observed at acidic pH levels. These findings enhance the understanding of the processes governing the transpassivity of CrMnFeCoNi and CrCoNi MPEAs in alkaline environments and have potential implications for the development of application‐tailored corrosion‐resistant MPEAs. KW - Multi-principal element alloys KW - MPEA KW - Corrosion KW - Oxygen evolution reaction KW - Transpassive region PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-611594 DO - https://doi.org/10.1002/celc.202400346 SN - 2196-0216 SP - 1 EP - 9 PB - Wiley AN - OPUS4-61159 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mehri Sofiani, F A1 - Chaudhuri, Somsubhro A1 - Elahi, S.A. A1 - Hectors, K. A1 - De Waele, W. T1 - Quantitative Analysis of the Correlation between Geometric Parameters of Pits and Stress Concentration Factors for a Plate Subject to Uniaxial Tensile Stress N2 - The offshore environment is inherently corrosive. Consequently, pits may nucleate on exposed steel surfaces. Corrosion pits can be a source of crack initiation when the structure is subject to fatigue loading. The criticality of a corrosion pit with respect to the structural integrity depends on its shape and size and can be quantified using a stress concentration factor (𝐾𝑡). In this work, a parametric 3D finite element model is developed to perform stress analysis of a pitted plate subjected to uniaxial tensile stress. The model is used for an extensive parameter study in which 𝐾𝑡 is determined for various pit configurations. It is demonstrated that each one of the geometrical parameters holds a substantial influence on the location of the Most Critical Region (MCR). It is shown that 𝐾𝑡 increases as the pit gets narrower. Pits with an elliptical mouth yield higher 𝐾𝑡 values when the angle between the load direction and the pit mouth major axis increases. Moreover, 𝐾𝑡 increases with the increase in the localized thickness loss which is more pronounced for relatively wider pits. Finally, a regression model is presented for estimating 𝐾𝑡 based on the geometric parameters of a pit. KW - FEM KW - Corrosion KW - SCF KW - Pitting corrosion PY - 2023 DO - https://doi.org/10.1016/j.tafmec.2023.104081 SN - 0167-8442 VL - 127 SP - 1 EP - 27 PB - Elsevier Ltd. AN - OPUS4-58284 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Matamoros-Veloza, A. A1 - Stawski, Tomasz A1 - Vargas, S. A1 - Neville, A. T1 - Study of a Local Structure at the Interface between Corrosion Films and Carbon Steel Surface in Undersaturated CO2 Environments N2 - Industries transporting CO2 gas-saturated fluids have infrastructures made of carbon steel. This is a good material with great mechanical properties but prone to corrosion and potential failure. Corrosion in sweet environments involves the formation of FeCO3 as a corrosion film, which is recognized to play a protective role under certain conditions. This work on the dissolution of corrosion films in sweet environments, under acidic and undersaturated conditions, demonstrates that the effects on the integrity of steel are far more significant than the damage observed on the surface of the corrosion film. Our results prove that dissolution of FeCO3 involved the presence of an amorphous phase, the intermediate formation of FeCl2 or FeCl+, and the presence of a phase with short distance atom–atom correlations. The amorphous phase was identified as a mixture of retained γ-Fe and Fe3C. Partially broken α-Fe and Fe3C structures were identified to prove the damage on the material, confirming the interface zone without evident damage on the corrosion film. Dissolution affected both the α-Fe and FeCO3, with the lattice [102̅] from the FeCO3 crystalline structure being the fastest to dissolve. The damage of steel at the molecular scale was evident at the macroscale with pit depths of up to 250 μm. The impact on the integrity of steel can be, therefore, more drastic than frequently reported in industrial operations of CO2 transport industries that use cleaning procedures (e.g., acid treatment, pigging) as part of their operational activities. KW - Steel KW - Corrosion KW - Siderite KW - Diffraction KW - Pair distribution function KW - Synchrotron PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-572156 DO - https://doi.org/10.1021/acsomega.2c07631 SN - 2470-1343 VL - 8 IS - 9 SP - 8497 EP - 8504 PB - ACS AN - OPUS4-57215 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ebell, Gino A1 - Mayer, T. F. A1 - Harnisch, J. A1 - Dauberschmidt, Ch. T1 - Corrosion monitoring of reinforced concrete structures:The DGZfP specification B12 Collaboration N2 - Corrosion monitoring of reinforced or prestressed concrete structures has becomeincreasingly important in recent years. Areas of application include componentsthat are no longer accessible after completion or where potential fieldmeasurements cannot be carried out due to existing coatings. Corrosion monitoringcan also be used to monitor the progress of corrosion in corroding systems, e.g. to prove the success of repair measures according to repair principle 8 in accordancewith EN 1504‐9 or repair method 8.3 in accordance with the DIBt repair guideline.It also could be used to prove the functionality of cathodic corrosion protectionsystems in accordance with ISO 12696. Despite the increasing importance ofcorrosion monitoring, no guidelines orrecommendations existed until 2018. Thisgap was closed by the English version of specification B12,“Corrosion Monitoringof Reinforced and Prestressed Concrete Structures,”of the German Society for Non‐Destructive Testing, which was published in 2021. This article introducesspecification B12 by explaining the basicmeasurement principles and illustratingthe potential of corrosion monitoring in new and existing buildings. KW - Corrosion KW - Monitoring PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-580982 DO - https://doi.org/10.1002/maco.202313934 SN - 0947-5117 SP - 1 EP - 9 PB - Wiley VHC-Verlag AN - OPUS4-58098 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Valet, Svenja A1 - Bohlmann, Tatjana A1 - Burkert, Andreas A1 - Ebell, Gino T1 - Zinc acetate containing gel pads for electrochemical measurements of Zn samples N2 - Agar gel pads have been used for electrochemical measurements for some time. For zinc in particular, a standard method for measuring the stability of the corrosion product layer is being established. The main interpretation factor is the corrosion product layer resistance RL, as it is easy to determine and interpret. A high corrosion product layer resistance indicates a high level of protection. However, it is not yet known how low the corrosion product layer resistance is for freshly produced zinc samples. As zinc is highly active, it reacts immediately with the environment to form a corrosion product layer, which affects the corrosion product layer resistance. The addition of zinc acetate to the agar gel pads prevents the formation of a surface layer and destroys existing ones. This makes it possible to measure an almost corrosion product-free zinc surface. This is important in defining the range of corrosion product layer resistance for a protective surface. KW - Electrochemistry KW - General Chemical Engineering KW - Analytical Chemistry KW - Corrosion KW - Zinc KW - Korrosion PY - 2023 DO - https://doi.org/10.1016/j.jelechem.2023.117814 SN - 1572-6657 VL - 948 SP - 1 EP - 8 PB - Elsevier B.V. AN - OPUS4-59079 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bäßler, Ralph A1 - Bettge, Dirk A1 - Bender, R. A1 - Féron, D. A1 - Mills, D. A1 - Ritter, S. A1 - de Graeve, I. A1 - Dugstad, A. A1 - Grassini, S. A1 - Hack, T. A1 - Halama, M. A1 - Han, E.-H. A1 - Harder, T. A1 - Hinds, G. A1 - Kittel, J. A1 - Krieg, R. A1 - Leygraf, C. A1 - Martinelli, L. A1 - Mol, A. A1 - Neff, D. A1 - Nilsson, J.-O. A1 - Odnevall, I. A1 - Paterson, S. A1 - Paul, S. A1 - Prosek, T. A1 - Raupach, M. A1 - Revilla, R. I. A1 - Ropital, F. A1 - Schweigart, H. A1 - Szala, E. A1 - Therryn, H. A1 - Tidblad, J. A1 - Virtanen, S. A1 - Volovitch, P. A1 - Watkinson, D. A1 - Wilms, M. A1 - Winning, G. A1 - Zheludkevich, M. T1 - La corrosion: un défi pour une société durable N2 - Une transition mondiale vers des systèmes énergétiques plus durables, abordables et fiables a été initiée par l’accord de Paris et l’Agenda 2030 des Nations unies pour un développement durable. Il s’agit là d’un défi industriel majeur car les systèmes et infrastructures énergétiques résilients au changement climatique exigent de se positionner pour le long terme. Se pencher sur le comportement dans la durée des matériaux structurels - principalement des métaux et des alliages - s’impose alors comme une nécessité. Dans cette optique, « La corrosion : un défi pour une société durable »présente une série de cas montrant l’importance de la tenue à la corrosion et de la protection anticorrosion des métaux et des alliages pour le développement de systèmes durables, économiques et fiables de production d’énergie. KW - Corrosion KW - Coûts de la corrosion KW - Protection KW - Anticorrosion KW - Stratégies deprévention PY - 2023 DO - https://doi.org/10.51257/a-v1-cor2000 SN - 2555-5383 VL - 2023 IS - Avril SP - 1 EP - 23 CY - Saint-Denis, France AN - OPUS4-57927 LA - fra AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - de Oliveira Guilherme Buzanich, Ana A1 - Radtke, Martin A1 - Yusenko, Kirill A1 - Stawski, Tomasz A1 - Kulow, Anicó A1 - Cakir, Cafer Tufan A1 - Röder, Bettina A1 - Naese, Christoph A1 - Britzke, Ralf A1 - Sintschuk, Michael A1 - Emmerling, Franziska T1 - BAMline - A real-life sample materials research beamline N2 - With increasing demand and environmental concerns, researchers are exploring new materials that can perform as well or better than traditional materials while reducing environmental impact. The BAMline, a real-life sample materials research beamline, provides unique insights into materials’ electronic and chemical structure at different time and length scales. The beamline specializes in x-ray absorption spectroscopy, x-ray fluorescence spectroscopy, and tomography experiments. This enables real-time optimization of material properties and performance for various applications, such as energy transfer, energy storage, catalysis, and corrosion resistance. This paper gives an overview of the analytical methods and sample environments of the BAMline, which cover non-destructive testing experiments in materials science, chemistry, biology, medicine, and cultural heritage. We also present our own synthesis methods, processes, and equipment developed specifically for the BAMline, and we give examples of synthesized materials and their potential applications. Finally, this article discusses the future perspectives of the BAMline and its potential for further advances in sustainable materials research. KW - Extended X-ray absorption fine structure KW - Energy storage KW - Environmental impacts KW - Nondestructive testing techniques KW - X-ray fluorescence spectroscopy KW - Corrosion KW - Near edge X-ray absorption fine structure spectroscopy KW - X-ray absorption spectroscopy PY - 2023 DO - https://doi.org/10.1063/5.0157194 VL - 158 IS - 24 SP - 1 EP - 22 PB - AIP Publishing AN - OPUS4-57824 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Henning, Ricky A1 - Sturm, Patrick A1 - Keßler, S. A1 - Gluth, Gregor T1 - Corrosion of hybrid alkaline cements in saline solution simulating evaporite rock – effect of the Portland clinker content N2 - Two hybrid alkaline cements (HAC) based on Portland clinker, ground granulated blast furnace slag (GGBFS), fly ash and sodium sulfate, as well as an alkali-activated GGBFS/fly ash blend and a Portland cement paste were exposed to a saturated saline solution for 70 days. The combined chemical attack of chloride, magnesium and sulfate ions and the associated changes of the phase assemblage of the materials were studied by X-ray diffraction, thermal analysis and spatially resolved X-ray fluorescence spectroscopy. The experimental results revealed dissolution of ettringite, C-N-A-S-H and calcite, and the formation of gypsum, Kuzel's salt and Friedel's salt; thermodynamic modeling indicated the formation of M-S-H. The resistance of the HAC against attack by the saline solution increased with Portland clinker fraction. The capacity of portlandite to maintain pH at values above 10 is found to be a major factor controlling the resistance of HAC against corrosion in the saline solution. KW - Hybrid cements KW - Alkali-activated materials KW - Magnesium chloride KW - Corrosion KW - Salt attack PY - 2023 DO - https://doi.org/10.1016/j.cemconres.2023.107215 SN - 0008-8846 SN - 1873-3948 VL - 172 SP - 1 EP - 14 PB - Elsevier Ltd. AN - OPUS4-57638 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Cakir, Cafer Tufan A1 - Piotrowiak, T. A1 - Reinholz, Uwe A1 - Ludwig, A. A1 - Emmerling, Franziska A1 - Streli, C. A1 - de Oliveira Guilherme Buzanich, Ana A1 - Radtke, Martin T1 - Exploring the Depths of Corrosion: A Novel GE-XANES Technique for Investigating Compositionally Complex Alloys N2 - In this study, we propose the use of nondestructive, depth-resolved, element-specific characterization using grazing exit X-ray absorption near-edge structure spectroscopy (GE-XANES) to investigate the corrosion process in compositionally complex alloys (CCAs). By combining grazing exit X-ray fluorescence spectroscopy (GE-XRF) geometry and a pnCCD detector, we provide a scanning-free, nondestructive, depth-resolved analysis in a sub-micrometer depth range, which is especially relevant for layered materials, such as corroded CCAs. Our setup allows for spatial and energy-resolved measurements and directly extracts the desired fluorescence line, free from scattering events and other overlapping lines. We demonstrate the potential of our approach on a compositionally complex CrCoNi alloy and a layered reference sample with known composition and specific layer thickness. Our findings indicate that this new GE-XANES approach has exciting opportunities for studying surface catalysis and corrosion processes in real-world materials. KW - Degradation mechanisms KW - Grazin exit XANES KW - Depth resolved XANES KW - Compositional complex alloys KW - Corrosion PY - 2023 DO - https://doi.org/10.1021/acs.analchem.3c00404 VL - 95 SP - 4810 EP - 4818 PB - ACS Publications AN - OPUS4-57823 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pfennig, A. A1 - Kranzmann, Axel T1 - Understanding the Anomalous Corrosion Behaviour of 17% Chromium Martensitic Stainless Steel in Laboratory CCS-Environment—A Descriptive Approach N2 - To mitigate carbon dioxide emissions CO2 is compressed and sequestrated into deep geological layers (Carbon Capture and Storage CCS). The corrosion of injection pipe steels is induced when the metal is in contact with CO2 and at the same time the geological saline formation water. Stainless steels X35CrMo17 and X5CrNiCuNb16-4 with approximately 17% Cr show potential as injection pipes to engineer the Northern German Basin geological onshore CCS-site. Static laboratory experiments (T = 60 ◦C, p = 100 bar, 700–8000 h exposure time, aquifer water, CO2-flow rate of 9 L/h) were conducted to evaluate corrosion kinetics. The anomalous surface corrosion phenomena were found to be independent of heat treatment prior to exposure. The corrosion process is described as a function of the atmosphere and diffusion process of ionic species to explain the precipitation mechanism and better estimate the reliability of these particular steels in a downhole CCS environment. KW - Corrosion KW - Steel KW - High alloyed steel KW - Corrosion mechanism KW - CCS PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-545700 DO - https://doi.org/10.3390/cleantechnol4020014 VL - 4 IS - 2 SP - 239 EP - 257 PB - MDPI AN - OPUS4-54570 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bulling, Jannis A1 - Jurgelucks, B. A1 - Prager, Jens A1 - Walther, A. T1 - Defect reconstruction in a two-dimensional semi-analytical waveguide model via derivative-based optimization N2 - This paper considers an indirect measurement approach to reconstruct a defect in a two-dimensional waveguide model for a non-destructive ultrasonic inspection via derivative-based optimization. The propagation of the mechanical waves is simulated by the scaled boundary finite element method that builds on a semi-analytical approach. The simulated data are then fitted to given data associated with the reflected waves from a defect which is to be reconstructed. For this purpose, we apply an iteratively regularized Gauss-Newton method in combination with algorithmic differentiation to provide the required derivative information accurately and efficiently. We present numerical results for three kinds of defects, namely, a crack, delamination, and corrosion. The objective function and the properties of the reconstruction method are investigated. The examples show that the parameterization of the defect can be reconstructed efficiently as well as robustly in the presence of noise. KW - Mechanical waves KW - Corrosion KW - Finite-element analysis KW - Ultrasonic testing KW - Nondestructive testing techniques KW - Symbolic computation KW - Materials analysis KW - MATLAB KW - Newton Raphson method PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-565485 DO - https://doi.org/10.1121/10.0013574 VL - 152 IS - 2 SP - 1217 EP - 1229 PB - AIP Publ. CY - Melville, NY AN - OPUS4-56548 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Babutzka, Martin A1 - Grabowski, Sven A1 - Sahrhage, H. A1 - Lampke, T. T1 - Electrochemical corrosion investigations on binary and ternary zinc alloy coatings using gel electrolytes N2 - Novel agar-based test electrolytes are used to perform electrochemical corrosion investigations on ZnFe and ZnNi binary as well as ZnFeMo ternary zinc coatings. The objectives of the electrochemical investigations include the characterization of the corrosion behavior, the description of the protective effect of the coatings as well as the investigation of the layer formation and degradation under artificial aging. ZnFe and ZnFeMo coatings are applied with varying iron content as well as an additional passivation layer, respectively, to study the effect on corrosion resistance. The results show that the protective effect of the coatings is not negatively influenced by different iron contents or the addition of molybdenum. Additional passivation of the ZnFe-containing coatings by means of a passivating agent leads to a significant improvement in the protective effect. Artificial aging leads to slight degradation of the additional passivation layer whereas coatings without post-treatment enhance their protective effect by the formation of corrosion product layers. KW - Binary zinc alloys KW - Ternary zinc alloys KW - Corrosion testing KW - Gel electrolytes KW - Corrosion PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-543013 DO - https://doi.org/10.1002/adem.202101336 SN - 1438-1656 SP - 1 EP - 14 PB - Wiley-VCH CY - Weinheim AN - OPUS4-54301 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Steger, S. A1 - Horn, Wolfgang A1 - Eggert, G. A1 - Krekel, C. T1 - Are cellulose ethers safe for the conservation of artwork? New insights in their VOC activity by means of Oddy testing N2 - Cellulose ethers, like methyl cellulose (MC) or hydroxypropyl cellulose (HPC), are widely used in conservation. They also occur as additives and rheology modifiers in various products like dispersions or gels. Do such products release harmful volatile organic compounds (VOC) during their accelerated aging? A mass testing series utilizing the Oddy test of 60 commercial cellulose ethers ranks the products in safe for permanent use (P, no corrosion), only for temporary use (T, slight corrosion), and unsuitable at all (F, heavy corrosion). Results show that 55% of the products passed the test whereas 33% are for temporary use as slight corrosion occurred on at least one metal coupon and only 11% failed the Oddy test. Raman measurements of the corrosion products identified oxides like massicot, litharge, cuprite, and tenorite among carbonates (hydrocerussite, plumbonacrite), and acetates like basic lead acetate, lead acetate trihydrate as well as lead formate as main phases. For example, commercial, industrial Klucel® G (HPC) scored a T rating through slight corrosion on the lead coupon. Basic lead acetate among other phases indicates the presence of acetic acid. Additional measurements of the sample with thermal desorption GC–MS utilizing the BEMMA scheme confirm the high acetic acid outgassing and reveal the presence of a small amount of formaldehyde. KW - Cellulose ether KW - Corrosion KW - Oddy test KW - VOC KW - BEMMA PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-547591 DO - https://doi.org/10.1186/s40494-022-00688-4 SN - 2050-7445 VL - 10 IS - 1 SP - 1 EP - 12 PB - Springer Open AN - OPUS4-54759 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schwarz, W. A1 - Wilsch, Gerd A1 - Katsumi, N. A1 - Ebell, Gino A1 - Völker, Tobias T1 - Ion distribution in concrete overlay, mapped by laser induced breakdown spectroscopy (LIBS), modified by an embedded zinc anode N2 - Galvanic corrosion protection by embedded zinc anodes is an accepted technique for the corrosion protection of reinforcing steel in concrete. Galvanic currents flow between the zinc anode and the steel reinforcement due to the potential difference that is in the range of a few hundred mV. The ion distribution was studied on two steel reinforced concrete specimens admixed with 3 wt.% chloride/wt. cement and galvanically protected by a surface applied EZ-anode. On both specimens, a zinc anode was embedded and glued to the concrete surface by a geo-polymer-based chloride-free binder. At one specimen, the EZ-anode was operated for 2,5 years, the EZ-anode at the other specimen was not electrically connected to the reinforcement, this specimen serves as a reference. Both specimens have been stored under identical conditions. The ion distribution between the anode (EZ-ANODE) and cathode (steel reinforcement) was studied by laser-induced breakdown spectroscopy (LIBS) after 7 months, 12 months, and 2,5 years. Results of the LIBS studies on the specimen with activated EZ-anode after 7 months, 12 months, and 2,5 years and of the reference specimen after 2,5 years are reported. Results show that diffusion of ions contributes to the changes in the ion distribution but migration, especially of chlorides towards the EZ-anode is significant despite the weak electric field – several hundred millivolts - generated by the galvanic current. Results show that chloride ions accumulate near the zinc-anode as in water-insoluble zinc-hydroxy chlorides - Simonkollite. T2 - ICCRRR 2022 CY - Capetown, South Africa KW - Corrosion KW - LIBS KW - Zinc KW - Anode PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-560576 DO - https://doi.org/10.1051/matecconf/202236404023 SN - 2261-236X VL - 364 SP - 1 EP - 7 PB - EDP Sciences CY - Les Ulis AN - OPUS4-56057 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Manzoni, Anna Maria A1 - Mohring, Wencke A1 - Hesse, René A1 - Agudo Jácome, Leonardo A1 - Stephan-Scherb, C. T1 - Early material damage in equimolar CrMnFeCoNi in mixed oxidizing/sulfiding hot gas atmosphere N2 - The challenges to use more varied fuels at medium and high temperatures above 500 °C need to be addressed by tuning the materials toward a better resistance against increased corrosion. As a first step the corrosion processes need to be better understood, especially in the case of the unavoidable and highly corrosive sulfur-based gases. Herein, oxidation/sulfidation of an equimolar CrMnFeCoNi high-entropy alloy is studied at an early stage after hot gas exposure at 600 °C for 6 h in 0.5% SO2 and 99.5% Ar. The oxidation process is studied by means of X-ray diffraction, scanning and transmission electron microscopy, and supported by thermodynamic calculations. It is found that the sulfur does not enter the bulk material but interacts mainly with the fast-diffusing manganese at grain boundary triple junctions at the alloy surface. Submicrometer scaled Cr–S–O-rich phases close to the grain boundaries complete the sulfur-based phase formation. The grains are covered in different Fe-, Mn-, and Cr-based spinels and other oxides. KW - High entropy alloy KW - Sulfiding KW - Corrosion KW - Transmission electron microscopy PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-543495 DO - https://doi.org/10.1002/adem.202101573 SN - 1527-2648 SP - 1 EP - 8 PB - Wiley-VCH CY - Weinheim AN - OPUS4-54349 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kromer, C. A1 - Schwibbert, Karin A1 - Gadicherla, A. K. A1 - Thiele, Dorothea A1 - Nirmalananthan-Budau, Nithiya A1 - Laux, P. A1 - Resch-Genger, Ute A1 - Luch, A. A1 - Tschiche, H. R. T1 - Monitoring and imaging pH in biofilms utilizing a fluorescent polymeric nanosensor N2 - Biofilms are ubiquitous in nature and in the man-made environment. Given their harmful effects on human health, an in-depth understanding of biofilms and the monitoring of their formation and growth are important. Particularly relevant for many metabolic processes and survival strategies of biofilms is their extracellular pH. However, most conventional techniques are not suited for minimally invasive pH measurements of living biofilms. Here, a fluorescent nanosensor is presented for ratiometric measurements of pH in biofilms in the range of pH 4.5–9.5 using confocal laser scanning microscopy. The nanosensor consists of biocompatible polystyrene nanoparticles loaded with pH-inert dye Nile Red and is surface functionalized with a pH-responsive fluorescein dye. Its performance was validated by fluorometrically monitoring the time-dependent changes in pH in E. coli biofilms after glucose inoculation at 37 °C and 4 °C. This revealed a temperature-dependent decrease in pH over a 4-h period caused by the acidifying glucose metabolism of E. coli. These studies demonstrate the applicability of this nanosensor to characterize the chemical microenvironment in biofilms with fluorescence methods. KW - Dye KW - Fluorescence KW - Signal enhancement KW - Sensor KW - Quantum yield KW - Synthesis KW - Nanoparticle KW - Nano KW - Polymer KW - Ph KW - Biofilm KW - MIC KW - Corrosion KW - Microorganism KW - Bacteria PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-550751 DO - https://doi.org/10.1038/s41598-022-13518-1 SN - 2045-2322 VL - 12 IS - 1 SP - 1 EP - 10 PB - Nature Publishing Group CY - London AN - OPUS4-55075 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hattrick-Simpers, J. A1 - Li, K. A1 - Greenwood, M. A1 - Black, R. A1 - Witt, Julia A1 - Kozdras, M. A1 - Pang, X. A1 - Özcan Sandikcioglu, Özlem T1 - Designing durable, sustainable, high-performance materials for clean energy infrastructure N2 - Civilization and modern societies would not be possible without manmade materials. Considering their production volumes, their supporting role in nearly all industrial processes, and the impact of their sourcing and production on the environment, metals and alloys are and will be of prominent importance for the clean energy transition. The focus of materials discovery must move to more specialized, application-tailored green alloys that outperform the legacy materials not only in performance but also in sustainability and resource efficiency. This white paper summarizes a joint Canadian-German initiative aimed at developing a materials acceleration platform (MAP) focusing on the discovery of new alloy families that will address this challenge. We call our initiative the “Build to Last Materials Acceleration Platform” (B2L-MAP) and present in this perspective our concept of a three-tiered self-driving laboratory that is composed of a simulation-aided pre-selection module (B2L-select), an artificial intelligence (AI)-driven experimental lead generator (B2L-explore), and an upscaling module for durability assessment (B2L-assess). The resulting tool will be used to identify and subsequently demonstrate novel corrosion-resistant alloys at scale for three key applications of critical importance to an offshore, wind-driven hydrogen plant (reusable electrical contacts, offshore infrastructure, and oxygen evolution reaction catalysts). KW - Material Acceleration Platforms (MAPs) KW - Self-driving-labs (SDLs) KW - Automation KW - Artificial Intelligence (AI) KW - Elektrolyse KW - Structural Materials KW - Corrosion PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-568452 DO - https://doi.org/10.1016/j.xcrp.2022.101200 SN - 2666-3864 VL - 4 IS - 1 SP - 1 EP - 11 PB - Cell Press ; Elsevier CY - Maryland Heights, MO AN - OPUS4-56845 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bender, R. A1 - Féron, D. A1 - Mills, D. A1 - Ritter, S. A1 - Bäßler, Ralph A1 - Bettge, Dirk A1 - de Graeve, I. A1 - Dugstad, A. A1 - Grassini, S. A1 - Hack, T. A1 - Halama, M. A1 - Han, E.-H. A1 - Harder, T. A1 - Hinds, G. A1 - Kittel, J. A1 - Krieg, R. A1 - Leygraf, C. A1 - Martinelli, L. A1 - Mol, A. A1 - Neff, D. A1 - Nilsson, J.-O. A1 - Odnevall, I. A1 - Paterson, S. A1 - Paul, S. A1 - Prošek, T. A1 - Raupach, M. A1 - Revilla, R. I. A1 - Ropital, F. A1 - Schweigart, H. A1 - Szala, E. A1 - Terryn, H. A1 - Tidblad, J. A1 - Virtanen, S. A1 - Volovitch, P. A1 - Watkinson, D. A1 - Wilms, M. A1 - Winning, G. A1 - Zheludkevich, M. T1 - Corrosion challenges towards a sustainable society N2 - A global transition towards more sustainable, affordable and reliable energy systems is being stimulated by the Paris Agreement and the United Nation's 2030 Agenda for Sustainable Development. This poses a challenge for the corrosion industry, as building climate‐resilient energy systems and infrastructures brings with it a long‐term direction, so as a result the long‐term behaviour of structural materials (mainly metals and alloys) becomes a major prospect. With this in mind “Corrosion Challenges Towards a Sustainable Society” presents a series of cases showing the importance of corrosion protection of metals and alloys in the development of energy production to further understand the science of corrosion, and bring the need for research and the consequences of corrosion into public and political focus. This includes emphasis on the limitation of greenhouse gas emissions, on the lifetime of infrastructures, implants, cultural heritage artefacts, and a variety of other topics. KW - Corrosion KW - Corrosion costs KW - Corrosion protection KW - Preventive strategies PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-554801 DO - https://doi.org/10.1002/maco.202213140 SN - 1521-4176 VL - 73 IS - 11 SP - 1730 EP - 1751 PB - Wiley-VCH CY - Weinheim AN - OPUS4-55480 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wetzel, Annica A1 - von der Au, Marcus A1 - Dietrich, P. M. A1 - Radnik, Jörg A1 - Özcan Sandikcioglu, Özlem A1 - Witt, Julia T1 - The comparison of the corrosion behavior of the CrCoNi medium entropy alloy and CrMnFeCoNi high entropy alloy N2 - This work presents the determination of the corrosion characteristics of CrCoNi (medium entropy alloy) and CrMnFeCoNi (high entropy alloy) in 0.1 M NaCl and 0.1 M H2SO4. The morphology and chemical composition of the oxide layers formed on CrCoNi and CrMnFeCoNi were comparatively analyzed by scanning Kelvin probe microscopy (SKPFM) and scanning electron microscopy (SEM) and supported with chemical analysis by means of inductively coupled plasma mass spectrometry (ICP-MS) and X-Ray photoelectron spectroscopy (XPS). The analysis of the 3p core level peaks showed that the oxide layer (native and after anodic passivation) on CrCoNi consisted mainly of Cr oxides, while the oxide layer on CrMnFeCoNi was primarily composed of a mixture of Cr and Fe oxides. In addition, XPS was utilized to assess the oxide layer thicknesses. These results were compared to the thicknesses obtained by means of electrochemical impedance spectroscopy (EIS), with both approaches yielding values up to about 4 nm depending on the electrolyte and the alloy. Cyclic polarization measurements indicated superior corrosion resistance of CrCoNi in both aqueous environments compared to CrMnFeCoNi, as well as to AISI 304 stainless steel. KW - Medium entropy alloy KW - High entropy alloy KW - SKPFM KW - XPS KW - Passivation KW - Corrosion PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-559902 DO - https://doi.org/10.1016/j.apsusc.2022.154171 SN - 0169-4332 VL - 601 SP - 1 EP - 10 PB - Elsevier B.V. AN - OPUS4-55990 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pfennig, Anja A1 - Wolf, Marcus A1 - Kranzmann, Axel T1 - Corrosion and corrosion fatigue of steels in downhole CCS environment - A summary N2 - Static immersion tests of potential injection pipe steels 42CrMo4, X20Cr13, X46Cr13, X35CrMo4, and X5CrNiCuNb16-4 at T = 60 °C and ambient pressure, as well as p = 100 bar were performed for 700–8000 h in a CO₂-saturated synthetic aquifer environment similar to CCS sites in the Northern German Basin (NGB). Corrosion rates at 100 bar are generally lower than at ambient pressure. The main corrosion products are FeCO₃ and FeOOH with surface and local corrosion phenomena directly related to the alloy composition and microstructure. The appropriate heat treatment enhances corrosion resistance. The lifetime reduction of X46Cr13, X5CrNiCuNb16-4, and duplex stainless steel X2CrNiMoN22-5-3 in a CCS environment is demonstrated in the in situ corrosion fatigue CF experiments (axial push-pull and rotation bending load, 60 °C, brine: Stuttgart Aquifer and NGB, flowing CO₂: 30 L/h, +/- applied potential). Insulating the test setup is necessary to gain reliable data. S-N plots, micrographic-, phase-, fractographic-, and surface analysis prove that the life expectancy of X2CrNiMoN22-5-3 in the axial cyclic load to failure is clearly related to the surface finish, applied stress amplitude, and stress mode. The horizontal grain attack within corrosion pit cavities, multiple fatigue cracks, and preferable deterioration of austenitic phase mainly cause fatigue failure. The CF life range increases significantly when a protective potential is applied. KW - Steel KW - High alloyed steel KW - Corrosion KW - Corrosion fatigue KW - Carbon capture and storage PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-531391 DO - https://doi.org/10.3390/pr9040594 SN - 2227-9717 VL - 9 IS - 4 SP - 1 EP - 33 PB - MDPI CY - Basel AN - OPUS4-53139 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pfennig, Anja A1 - Wolf, M. A1 - Kranzmann, Axel T1 - Corrosion and Corrosion Fatigue of Steels in Downhole CCS Environment—A Summary N2 - Static immersion tests of potential injection pipe steels 42CrMo4, X20Cr13, X46Cr13, X35CrMo4, and X5CrNiCuNb16-4 at T = 60°C and ambient pressure, as well as p = 100 bar were performed for 700–8000 h in a CO2-saturated synthetic aquifer environment similar to CCS sites in the Northern German Basin (NGB). Corrosion rates at 100 bar are generally lower than at ambient pressure. The main corrosion products are FeCO3 and FeOOH with surface and local corrosion phenomena directly related to the alloy composition and microstructure. The appropriate heat treatment enhances corrosion resistance. The lifetime reduction of X46Cr13, X5CrNiCuNb16-4, and duplex stainless steel X2CrNiMoN22-5-3 in a CCS environment is demonstrated in the in situ corrosion fatigue CF experiments (axial push-pull and rotation bending load, 60°C , brine: Stuttgart Aquifer and NGB, flowing CO2: 30 L/h, +/- applied potential). Insulating the test setup is necessary to gain reliable data. S-N plots, micrographic-, phase-, fractographic-, and surface analysis prove that the life expectancy of X2CrNiMoN22-5-3 in the axial cyclic load to failure is clearly related to the surface finish, applied stress amplitude, and stress mode. The horizontal grain attack within corrosion pit cavities, multiple fatigue cracks, and preferable deterioration of austenitic phase mainly cause fatigue failure. The CF life range increases significantly when a protective potential is applied. KW - Carbon capture and storage KW - Steel KW - High alloyed steel KW - Corrosion KW - Corrosion fatigue KW - CCS PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-523948 DO - https://doi.org/10.3390/pr9040594 VL - 9 IS - 4 SP - 594 PB - MDPI CY - Basel, Switzerland AN - OPUS4-52394 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Valet, Svenja A1 - Burkert, Andreas A1 - Ebell, Gino A1 - Babutzka, Martin T1 - Determination of the corrosion product layer resistance on zinc and electrolytically galvanized steel samples by using gel electrolytes N2 - Although zinc and zinc coatings have been widely used for corrosion protection for decades new zinc coatings are constantly being developed. Characterizing the corrosion protectiveness of these new coatings, however, should not be underestimated. While exposure tests are time intensive, cyclic tests can only be used for a very limited field of application. Thus, electrochemical measurements provide both an efficient and an effective alternative. Conventional aqueous bulk electrolytes influence the surface layers of a tested zinc coating and are therefore not reliable. Gel electrolytes, however, have evolved over the last few years, are minimally invasive and provide reliable results. This work describes experiments with gel electrolytes made of agar. Unlike previous work, it proposes a composition of gel electrolyte for minimally invasive description of the protective power of naturally formed oxide layers on zinc and zinc coatings. Therefore, as a first part, the gel electrolyte made of agar is verified as a method for zinc and zinc-coated samples. Afterwards, this paper introduces the corrosion product layer resistance RL as a promising parameter to evaluate the protective power of zinc coatings. Results are verified with EIS and FTIR measurements. An example on a representative zinc coating demonstrates the practical application. KW - Gel electrolytes KW - Agar KW - Zinc coatings KW - Atmospheric exposure KW - Corrosion PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-526053 DO - https://doi.org/10.1016/j.electacta.2021.138191 SN - 0013-4686 VL - 385 SP - 138191 PB - Elsevier Ltd. AN - OPUS4-52605 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Stoljarova, A. A1 - Regenspurg, S. A1 - Bäßler, Ralph A1 - Mathiesen, T. A1 - Braüner Nielsen, J. T1 - Effect of lead and copper containing brine on steel materials for geothermal applications – A corrosion study N2 - Geothermal brines often contain high amounts of lead and copper ions that can precipitate as native Cu and Pb as consequence of galvanic corrosion when brines react with carbon steel materials. This contribution evaluates which materials could overcome the problem of galvanic corrosion at geothermal environment. The behavior of these materials in water containing high chloride concentration (> 100 g/L NaCl) as well as various amounts of dissolved bCl2 and/or CuCl2 was characterized by electrochemical and exposure measurements. Both methods reveal carbon steel suffers corrosion susceptibility, accompanied by Cu◦ and/or Pb◦ precipitation on the surface. Electrochemical measurements on stainless steels result in significant difference in corrosion and repassivation potentials (Ecorr = -189 mV, Erep = 70 mV), indicating a good corrosion resistance. KW - Copper KW - Lead KW - Corrosion KW - Steel KW - Geothermal energy PY - 2021 DO - https://doi.org/10.1016/j.geothermics.2020.102024 SN - 0375-6505 VL - 91 SP - NIL_75 EP - NIL_85 PB - Elsevier CY - Amsterdam AN - OPUS4-51976 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Aristia, Gabriela A1 - Le, Quynh Hoa A1 - Nofz, Marianne A1 - Sojref, Regine A1 - Bäßler, Ralph T1 - Study of Al2O3 Sol-Gel Coatings on X20Cr13 in Artificial North German Basin Geothermal Water at 150 °C N2 - Al2O3 has been widely used as a coating in industrial applications due to its excellent chemical and thermal resistance. Considering high temperatures and aggressive mediums exist in geothermal systems, Al2O3 can be a potential coating candidate to protect steels in geothermal applications. In this study, γ-Al2O3 was used as a coating on martensitic steels by applying AlOOH sol followed by a heat treatment at 600 °C. To evaluate the coating application process, one-, two-, and three-layer coatings were tested in the artificial North German Basin (NGB), containing 166 g/L Cl−, at 150 °C and 1 MPa for 168 h. To reveal the stability of the Al2O3 coating in NGB solution, three-layer coatings were used in exposure tests for 24, 168, 672, and 1296 h, followed by surface and cross-section characterization. SEM images show that the Al2O3 coating was stable up to 1296 h of exposure, where the outer layer mostly transformed into boehmite AlOOH with needle-like crystals dominating the surface. Closer analysis of cross-sections showed that the interface between each layer was affected in long-term exposure tests, which caused local delamination after 168 h of exposure. In separate experiments, electrochemical impedance spectroscopy (EIS) was performed at 150 °C to evaluate the changes of coatings within the first 24 h. Results showed that the most significant decrease in the impedance is within 6 h, which can be associated with the electrolyte penetration through the coating, followed by the formation of AlOOH. Here, results of both short-term EIS measurements (up to 24 h) and long-term exposure tests (up to 1296 h) are discussed. KW - Al2O3 KW - Geothermal KW - Martensitic steels KW - Behmite KW - Corrosion PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-525551 DO - https://doi.org/10.3390/coatings11050526 SN - 2079-6412 VL - 11 IS - 5 SP - 526 PB - MDPI CY - Basel AN - OPUS4-52555 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Le, Quynh Hoa A1 - Bäßler, Ralph A1 - Bettge, Dirk A1 - Buggisch, E. A1 - Schiller, Bernadette Nicole A1 - Beck, M. T1 - Corrosion Study on Wellbore Materials for the CO2 Injection Process N2 - For reliability and safety issues of injection wells, corrosion resistance of materials used needs to be determined. Herein, representative low-cost materials, including carbon steel X70/1.8977 and low alloyed steel 1.7225, were embedded in mortar to mimic the realistic casing-mortar interface. Two types of cement were investigated: (1) Dyckerhoff Variodur commercial Portland cement, representing a highly acidic resistant cement and (2) Wollastonite, which can react with CO2 and become stable under a CO2 stream due to the carbonation process. Exposure tests were performed under 10 MPa and at 333 K in artificial aquifer fluid for up to 20 weeks, revealing crevice corrosion and uniform corrosion instead of expected pitting corrosion. To clarify the role of cement, simulated pore water was made by dispersing cement powder in aquifer fluid and used as a solution to expose steels. Surface analysis, accompanied by element mapping on exposed specimens and their crosssections, was carried out to trace the chloride intrusion and corrosion process that followed. KW - Carbon capture storage KW - CCS KW - Carbon dioxide KW - Corrosion KW - Carbon steel KW - Aquifer fluid KW - Cement KW - Casing KW - Pitting PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-519774 DO - https://doi.org/10.3390/pr9010115 SN - 2227-9717 VL - 9 IS - 1 SP - 115 PB - MDPI CY - Basel AN - OPUS4-51977 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wurzler, Nina A1 - Sobol, Oded A1 - Altmann, Korinna A1 - Radnik, Jörg A1 - Özcan Sandikcioglu, Özlem T1 - Preconditioning of AISI 304 stainless steel surfaces in the presence of flavins—Part I: Effect on surface chemistry and corrosion behavior N2 - Stainless steel AISI 304 surfaces were studied after a mild anodic polarization for oxide growth in the presence and absence of two derivatives of vitamin B2 (riboflavin and flavin mononucleotide) that can be secreted by metal‐reducing bacteria and act as a chelating agent for iron species. The alterations in oxide chemistry were studied by means of surface‐sensitive techniques such as X‐ray photoelectron spectroscopy and time‐of‐flight secondary ion mass spectrometry analysis. The complementary electrochemical characterization revealed a preferential growth of an oxide/hydroxide iron‐rich film that is responsible for an altered pit initiation and nucleation behavior. These findings suggest that as the corrosion behavior is determined by the interplay of the chemical and electronic properties, only a mild anodic polarization in the presence of redox‐active molecules is able to alter the chemical and electronic structure of the passive film formed on stainless steel AISI 304. This helps to achieve a profound understanding of the mechanisms of microbially influenced corrosion (MIC) and especially the possible effects of the redox‐active biomolecules, as they may play an important role in the corrosion susceptibility of stainless steel surfaces. KW - Corrosion KW - Stainless steel KW - Surface analysis PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-528117 DO - https://doi.org/10.1002/maco.202012191 VL - 72 IS - 6 SP - 974 EP - 982 PB - Wiley AN - OPUS4-52811 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Blank, Robin A1 - Nitschke, Heike A1 - Saliwan Neumann, Romeo A1 - Kranzmann, Axel T1 - Materialographic Preparation of Salt N2 - Molten salt containing systems gain in importance for sustainable energy use and production. For research and development, interactions of molten salts with potential container materials are of major interest. This article introduces preparation procedures to display an intact metal and salt microstructure and their interface using light optical microscopy and scanning electron microscopy. The exemplary material combination is the ternary salt mixture NaCl-KCl-MgCl2 and the low alloyed steel 1.4901 (T92) with a maximum service temperature of 550 °C. These are potential elements/materials for use in latent heat thermal energy storages. KW - Molten salt KW - Corrosion KW - Steel KW - Aging KW - Dry preparation PY - 2021 DO - https://doi.org/10.1515/pm-2022-0058 VL - 59 IS - 10 SP - 628 EP - 640 PB - De Gruyter AN - OPUS4-56048 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Aristia, Gabriela A1 - Bäßler, Ralph A1 - Nofz, Marianne A1 - Sojref, Regine A1 - Kohl, Anka T1 - Short-term exposure tests of ɣ-Al2O3 Sol-gel coating on X20Cr13 in artificial geothermal waters with different pH N2 - The suitability of an Al2O3 coating for corrosion protection on X20Cr13 was evaluated in various artificial geothermal brines, focusing on the influence of different pH (4, 6 and 8) and their chemical compositions on the coating properties. All experiments were performed in the laboratory using autoclaves at 150 ◦C and 1 MPa in deaerated condition for 1 and 7 days. Results showed that the pH of geothermal waters is the most detrimental factor in the transformation of ɣ-Al2O3 and its protective abilities. Delaminations were found in the Coating exposed to geothermal brines with pH 4. FTIR spectra indicated a transformation of ɣ-Al2O3 to boehmite AlOOH after exposure to pH 4 and 6, and bayerite Al(OH)3 was formed after exposure to pH 8. Different Crystal structures of the hydrated Al2O3 also contribute to the stability of the coatings, observed by the SEM- EDX of the surface and cross-section of coatings. This study indicated that ɣ-Al2O3 sol-gel coating presents a promising aspect of corrosion protection in geothermal environment with a neutral pH. KW - Al2O3 KW - Corrosion KW - Coating KW - Martensitic steel PY - 2021 DO - https://doi.org/10.1016/j.geothermics.2021.102193 SN - 0375-6505 VL - 96 SP - 102193 PB - Elsevier Ltd. CY - Amsterdam AN - OPUS4-52931 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Haller, T. A1 - Völker, Christoph A1 - Hartmann, T. T1 - Machine learning based multi-sensor fusion for the nondestructive testing of corrosion in concrete N2 - Half-cell potential mapping (HP) is the most popular non-destructive testing method (NDT) for locating corrosion damage in concrete. It is generally accepted that HP is susceptible to environmental factors caused by salt-related deterioration, such as different moisture and chloride gradients. Additional NDT methods are able to identify distinctive areas but are not yet used to estimate more accurate test results. We present a Supervised Machine Learning (SML) based approach to data fusion of seven different signal features to obtain higher quality information. SMLs are methods that explore (or learn) relationships between different (sensor) data from predefined data labels. To obtain a representative, labelled data set we conducted a comprehensive experiment simulating the deterioration cycle of a chloride exposed device in the laboratory. Our data set consists of 18 measurement campaigns, each containing HP, Ground Penetrating- Radar, Microwave Moisture and Wenner resistivity data. We compare the performance of different ML approaches. Many outperform the best single method, HP. We describe the intrinsic challenges posed by a data-driven approach in NDT and show how future work can help overcome them. T2 - SMAR2019 - 5th International Conference on Smart Monitoring, Assessment and Rehabilitation of Civil Structures CY - Potsdam, Germany DA - 27.08.2019 KW - Machine Learning KW - NDT KW - Half-Cell Potential Mapping KW - Corrosion KW - Reinforced Concrete KW - Data Fusion PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-498563 UR - http://www.ndt.net/?id=24890 VL - 25 IS - 1 SP - 24890-1 EP - 24890-8 PB - NDT.net CY - Kirchwald AN - OPUS4-49856 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Boschmann Käthler, C. A1 - Angst, U. A1 - Ebell, Gino A1 - Elsener, B. T1 - Chloride-induced reinforcement corrosion in cracked concrete: the influence of time of wetness on corrosion propagation N2 - Literature data on the influence of concrete cracks on corrosion propagation of reinforcing steel are contradictory. This might be due to very different exposure and test conditions but also to a lack of time-resolved data in cyclic wetting–drying exposure. Here, the influence of the environmental conditions on the corrosion rates in cracked concrete is studied experimentally. The results show that the corrosion rate in cracked concrete depends on the duration of wetting and drying phases and the relative humidity (RH) during the drying phase. The lower the ambient RH in the drying phase, the faster the cracks dry, which depresses the corrosion rate in the periods between the wetting events. A model is proposed to estimate corrosion rates in cracked concrete cyclic wetting/drying exposure. KW - Korrosion KW - Corrosion KW - Concrete PY - 2020 DO - https://doi.org/10.1080/1478422X.2020.1789371 SP - 1 EP - 11 PB - Taylor Francis Online CY - London AN - OPUS4-50986 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Babutzka, Martin A1 - Müller, Thoralf A1 - Mietz, Jürgen A1 - Burkert, Andreas T1 - Investigation of the influence of iron‐containing abrasives on the corrosion behaviour of the aluminium alloy AlSi1.2Mg0.4 N2 - The corrosion resistance of aluminium surfaces is closely linked to the surfacecstate after a grinding process. For years, iron‐containing abrasive materials were suspected to lead to increased corrosion susceptibility after processing of aluminium surfaces. To prove a possible correlation between the iron content of an abrasive and the corrosion behaviour of aluminium components, scientific investigations and experimentally practical corrosion tests are necessary. For the current investigation, specimens of a technical Al‐Si alloy from the same batch were used. The test specimens were mechanically ground with various resin‐bonded model abrasives containing different iron contents. The performed corrosion tests did not reveal a negative influence of the different iron‐containing abrasives on the corrosion behaviour of the Al–Si alloy. However, the most sensitive measuring method (electrochemical noise) showed differences in the surface activity depending on the type of abrasive. KW - Aluminium KW - Corrosion KW - Corrosion testing KW - Grinding PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-506762 DO - https://doi.org/10.1002/maco.202011657 SN - 0947-5117 SN - 1521-4176 VL - 71 IS - 10 SP - 1667 EP - 1679 PB - Wiley‐VCH Verlag GmbH & Co. KGaA CY - Weinheim AN - OPUS4-50676 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kratzig, A. A1 - Le, Quynh Hoa A1 - Bettge, Dirk A1 - Menneken, M. A1 - Bäßler, Ralph T1 - Early Stage of Corrosion Formation on Pipeline Steel X70 Under Oxyfuel Atmosphere at Low Temperature N2 - The early stage of corrosion formation on X70 pipeline steel under oxyfuel atmosphere was investigated by applying a simulated gas mixture (CO2 containing 6700 ppmv O2, 100 ppmv NO2, 70 ppmv SO2 and 50 ppmv H2O) for 15 h at 278 K and ambient pressure. Short-term tests (6 h) revealed that the corrosion starts as local spots related to grinding marks progressing by time and moisture until a closed layer was formed. Acid droplets (pH 1.5), generated in the gas atmosphere, containing a mixture of H2SO4 and HNO3, were identified as corrosion starters. After 15 h of exposure, corrosion products were mainly X-ray amorphous and only partially crystalline. In-situ energy-dispersive X-ray diffraction (EDXRD) results showed that the crystalline fractions consist primarily of water-bearing iron sulfates. Applying Raman spectroscopy, water-bearing iron nitrates were detected as subordinated phases. Supplementary long-term tests exhibited a significant increase in the crystalline fraction and formation of additional water-bearing iron sulfates. All phases of the corrosion layer were intergrown in a nanocrystalline network. In addition, numerous globular structures have been detected above the corrosion layer, which were identified as hydrated iron sulphate and hematite. As a type of corrosion, shallow pit formation was identified, and the corrosion rate was about 0.1 mma−1. In addition to in-situ EDXRD, SEM/EDS, TEM, Raman spectroscopy and interferometry were used to chemically and microstructurally analyze the corrosion products. KW - Corrosion KW - CCUS KW - In-situ ED-XRD KW - CO2 pipeline transport KW - Oxyfuel KW - Carbon steel KW - Impurities PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-506303 DO - https://doi.org/10.3390/pr8040421 SN - 2227-9717 VL - 8 IS - 4 SP - 421-1 EP - 421-19 PB - MDPI CY - Basel AN - OPUS4-50630 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bäßler, Ralph T1 - Review: Science, Technology and Applications of Metals in Additive Manufacturing N2 - Often 3D‐printing and additive manufacturing are mentioned as the 3rd industrial revolution. In this conjunction this book provides a brief overview on additively manufactured metal pieces. This book fulfills its intension to serve as an educational guide, providing a holistic picture encompassing science, technology and applications for the real‐life use of Metal Additive Manufacturing. KW - Additive manufacturing KW - Corrosion KW - Material properties PY - 2020 DO - https://doi.org/10.1002/maco.202070114 SN - 1521-4176 SN - 0947-5117 VL - 71 IS - 11 SP - 1929 EP - 1930 PB - WILEY‐VCH Verlag GmbH & Co. KGaA CY - Weinheim AN - OPUS4-51514 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Seifert, Lando T1 - Review: Steel‐Reinforced Concrete Str‐uctures: Assessment and Repair of Corrosion N2 - In 2019 CRC Press published the "Steel‐Reinforced Concrete Structures" as a paperback. This book does not vary in terms of content from the hardback publication of 2008. But it is first reviewed here in corrosion news. The book provides eight of nine chapters in which the author discusses technical aspects of assessment and repair of steel‐reinforced concrete structures. To sum up, this book is recommended for students and people involved with the assessment and repair of reinforced‐concrete structures, who want to get a quick introduction into the different aspects of the field. Readers also learn much about the economic interactions besides the topic. However, for experienced technicians and corrosion experts, this book may not be exact enough in both the electrochemical description of deterioration processes and the practical aspects of repair and control methods. Despite that, the discussions of the author are scientifically correct. KW - Concrete KW - Corrosion PY - 2020 DO - https://doi.org/10.1002/maco.202070084 SN - 1521-4176 SN - 0947-5117 VL - 71 IS - 8 SP - 1408 EP - 1409 PB - WILEY‐VCH Verlag GmbH & Co. KGaA CY - Weinheim AN - OPUS4-51075 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Faes, W. A1 - Lecompte, S. A1 - van Bael, J. A1 - Salenbien, R. A1 - Bäßler, Ralph A1 - Bellemans, I. A1 - Cools, P. A1 - de Geyter, N. A1 - Morent, R. A1 - Verbeken, K. A1 - de Paepe, M. T1 - Corrosion behaviour of different steel types in artificial geothermal fluids N2 - Geothermal energy is an interesting alternative to polluting fossil energy sources. Therefore, in Belgium, two wells have been drilled for a deep geothermal power plant. However, the environment to which the installations are exposed is challenging. The geothermal brine has 165 g/l total dissolved solids (of which 90% are sodium and chlorine) and the production temperature can be up to 130 °C. To assess their suitability to be used in a geothermal power plant, the corrosivity of the artificial brine to three common construction materials was investigated with exposure and electrochemical tests. The metals under consideration are a low-alloyed carbon steel (S235JR), an austenitic stainless steel (UNS S31603) and a duplex stainless steel (UNS S31803). The carbon steel, that was found to corrode uniformly, could be considered as a constructional material if a sufficient wall thickness is chosen. The austenitic stainless steel and the duplex stainless steel demonstrate very low uniform corrosion rates. They are however susceptible to pitting and crevice corrosion. To guarantee safe operation of the geothermal power plant, the susceptibility of the alloys to stress corrosion cracking should be tested and in situ experiments should be performed. KW - Geothermal energy KW - Corrosion KW - Carbon dioxide KW - Carbon steel KW - Stainless steel PY - 2019 DO - https://doi.org/10.1016/j.geothermics.2019.05.018 SN - 0375-6505 VL - 82 IS - 11 SP - 182 EP - 189 PB - Elsevier Ltd. AN - OPUS4-48759 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -