TY - JOUR A1 - Sieg, H. A1 - Braeuning, C. A1 - Kunz, B. M. A1 - Daher, H. A1 - Kästner, C. A1 - Krause, B.-C. A1 - Meyer, T. A1 - Jalili, P. A1 - Kogeveen, K. A1 - Böhmert, L. A1 - Lichtenstein, D. A1 - Burel, A. A1 - Chevance, S. A1 - Jungnickel, H. A1 - Tentschert, J. A1 - Laux, P. A1 - Braeuning, A. A1 - Gauffre, F. A1 - Fessard, V. A1 - Meijer, J. A1 - Estrela-Lopis, I. A1 - Thünemann, Andreas A1 - Luch, A. A1 - Lampen, A. T1 - Uptake and molecular impact of aluminum-containing nanomaterials on human intestinal caco-2 cells N2 - Aluminum (Al) is one of the most common elements in the earth crust and increasingly used in food, consumer products and packaging. Its hazard potential for humans is still not completely understood. Besides the metallic form, Al also exists as mineral, including the insoluble oxide, and in soluble ionic forms. Representatives of these three species, namely a metallic and an oxidic species of Al-containing nanoparticles and soluble aluminum chloride, were applied to human intestinal cell lines as models for the intestinal barrier. We characterized physicochemical particle parameters, protein corona composition, ion release and cellular uptake. Different in vitro assays were performed to determine potential effects and molecular modes of Action related to the individual chemical species. For a deeper insight into signaling processes, microarray transcriptome analyses followed by bioinformatic data analysis were employed. The particulate Al species showed different solubility in biological media. Metallic Al nanoparticles released more ions than Al2O3 nanoparticles, while AlCl3 showed a mixture of dissolved and agglomerated particulate entities in biological media. The protein corona composition differed between both nanoparticle species. Cellular uptake, investigated in transwell experiments, occurred predominantly in particulate form, whereas ionic Al was not taken up by intestinal cell lines. Transcellular transport was not observed. None of the Al species showed cytotoxic effects up to 200 mg Al/mL. The transcriptome analysis indicated mainly effects on oxidative stress pathways, xenobiotic metabolism and metal homeostasis. We have shown for the first time that intestinal cellular uptake of Al occurs preferably in the particle form, while toxicological effects appear to be ion-related. KW - Small-angle x-ray scattering KW - SAXS KW - Nanopatricle PY - 2018 DO - https://doi.org/10.1080/17435390.2018.1504999 SN - 1743-5390 VL - 12 IS - 9 SP - 992 EP - 1013 PB - Taylor & Francis AN - OPUS4-47432 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Radunz, Sebastian A1 - Schavkan, A. A1 - Wahl, Sebastian A1 - Würth, Christian A1 - Tschiche, H. R. A1 - Krumrey, M. A1 - Resch-Genger, Ute T1 - Evolution of Size and Optical Properties of Upconverting Nanoparticles during High-Temperature Synthesis N2 - We investigated the growth of β-phase NaYF4:Yb3+,Er3+ upconversion nanoparticles synthesized by the thermal decomposition method using a combination of in situ and offline analytical methods for determining the application-relevant optical properties, size, crystal phase, and chemical composition. This included in situ steady state luminescence in combination with offline time-resolved luminescence spectroscopy as well as small-angle X-ray scattering (SAXS) transmission electron microscopy (TEM), X-ray diffraction analysis (XRD), and inductively coupled Plasma optical emission spectrometry (ICP-OES). For assessing the suitability of our optical monitoring approach, the in situ-collected spectroscopic data, which reveal the luminescence evolution during nanocrystal synthesis, were compared to measurements done after cooling of the reaction mixture of the as-synthesized particles. The excellent correlation of the in situ and time-resolved upconversion luminescence with the nanoparticle sizes determined during the course of the reaction provides important insights into the various stages of nanoparticle growth. This study highlights the capability of in situ luminescence monitoring to control the efficiency of UCNP synthesis, particularly the reaction times at elevated temperatures and the particle quality in terms of size, shape, and crystal structure, as well as luminescence lifetime and upconversion quantum yield. KW - Rare earth nanoparticles KW - Upconversion KW - TEM KW - SAXS PY - 2018 UR - https://pubs.acs.org/doi/pdf/10.1021/acs.jpcc.8b09819 DO - https://doi.org/10.1021/acs.jpcc.8b09819 VL - 50 IS - 122 SP - 28958 EP - 28967 PB - American Chemical Society CY - Washington, DC AN - OPUS4-47169 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Brandl, F. A1 - Thünemann, Andreas A1 - Beuermann, S. T1 - Poly(meth)acrylate-PVDF core–shell particles from emulsion polymerization: preferential formation of the PVDF β crystal phase N2 - A facile and convenient approach for the synthesis of core–shell particles via emulsion polymerization is presented. The shell consists of poly(vinylidene fluoride) (PVDF) and the core of poly(methyl methacrylate) (PMMA), poly(glycidyl methacrylate) (PGMA) or poly(methyl acrylate) (PMA). In a first step, a non-fluorinated (meth)acrylate monomer is polymerized in the emulsion to produce poly(meth)acrylate core particles. Secondly, vinylidene fluoride (VDF) is directly added to the reactor and polymerized for shell formation. Small-angle X-ray scattering (SAXS) was employed to characterize the structure of the core–shell particles. Interestingly, the particles’ core contains fluorinated and non-fluorinated polymers, whereas the shell of the particles consists only of PVDF. The resulting particles with a diameter of around 40 nm show a significantly higher PVDF β phase content than the PVDF homopolymer obtained by emulsion polymerization KW - Small-angle x-ray scattering KW - SAXS KW - Nanopatricle KW - Polymer PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-465910 DO - https://doi.org/10.1039/C8PY01236A SN - 1759-9954 SN - 1759-9962 VL - 9 IS - 44 SP - 5359 EP - 5369 PB - The Royal Society of Chemistry AN - OPUS4-46591 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Smales, Glen Jacob A1 - Pauw, Brian Richard A1 - Thünemann, Andreas T1 - THE MAUS: A GI-/ULTRA-/W/SAXS Instrument of the future N2 - The Multi-scale Analyzer for Ultrafine Structures or the “MAUS” for short, is a SAXS instrument that combines a multitude of features that make it both unique, and one of the most adaptable instruments around. T2 - SAS2018 CY - Traverse City, MI, USA DA - 07.10.2018 KW - SAXS KW - MAUS KW - Small-angle scattering KW - DAWN KW - Grazing incidence PY - 2018 AN - OPUS4-46523 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Saadeh, Qais A1 - Pauw, Brian Richard A1 - Thünemann, Andreas A1 - Günster, Jens T1 - In-Situ SAXS Techniques N2 - Our project's aim is to enhance the capabilities of additive manufacturing techniques, where enabling a Two-Photon-Polymerization (TPP) 3D printer of producing arrays of precisely aligned nanoparticles is of an enormous value. As heterogeneous functional nanostructures with arrays of oriented nanoparticles are very promising in many fields; electrochemistry, energy storage, nanoelectronics among other vital fields. The feasibility and the convenience of orienting nanoparticles using magnetic, electric fields and ultrasonic vibrations will be systematically investigated, using Small Angle X-ray Scattering (SAXS), since SAXS can provide detailed information about the orientation characteristics of nano-Ensembles. Corresponding to our prerequisites, a set ad hoc functional sample holders, sample stages and other In-Situ SAXS solutions were developed, and incorporated to be compatible with a state-of-the-arts SAXS machine, called Multi-scale Analyzer for Ultrafine Structures (MAUS). The MAUS has been customized and engineered to serve as a miniaturized synchrotron, and that is exactly what we need. Experiments attempting to orient superparamagnetic nanoparticles will be discussed, where the outcomes will not only help in understanding the mechanics of field-particle interactions, it will also help in further developing the adequate needed set of corrections to the SAXS data, that is especially regards oriented samples. T2 - XVII International Small Angle Scattering Conference – SAS 2018 CY - Traverse City, Michigan, USA DA - 07.10.2018 KW - In-Situ Techniques KW - SAXS KW - Magnetic nano-particles PY - 2018 AN - OPUS4-46443 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Saloga, Patrick E. J. T1 - SAXS in Analysis of Ultra-small Size-adjustable Zinc Oxide Nanoparticles for Controlled Band Gap Engineering N2 - Zinc oxide (ZnO) as a wide-bandgap II-VI semiconductor finds application in areas like optoelectronics, photocatalysis as well as in detection systems. While band-gap engineering in macroscopic ZnO can be performed by alloying, the band-gap of ZnO nanoparticles is also dependent on their size. Since small-angle X-ray scattering (SAXS) provides a much higher resolution in terms of ultra-small nanoparticle size analysis compared to other techniques, it allows for a careful examination of the correlation between particle size and band-gap. We report on the microwave-assisted synthesis of oleate-capped, photoluminescent zinc oxide nanoparticles with adjustable size as dispersions in organic solvents. The spherical particles were obtained by hydrolysis of the metal precursor in presence of a strong base at temperatures above the solvent’s boiling point. Hence, the reaction is dramatically accelerated and within seconds – instead of hours at lower temperatures –, narrowly dispersed particle systems are yielded. The particles’ sizes as derived from SAXS strongly depend on the reaction temperature and time. Choosing the right reaction conditions, the particle size and thus their band gap can be finely tuned. A size increase can be achieved both by increasing the reaction temperature and the reaction time. See Figure 1 for an exemplary comparison of five-minute syntheses at different temperatures. Here, the yielded particles display diameters between 5.0 and 7.6 nm and corresponding band-gaps of 3.32 up to 3.41 eV. The size increase is accompanied by a red-shift of the UV/Vis absorption edges and fluorescence emission. Furthermore, these particles can be transferred into water by coating with polysorbates. T2 - SAS2018 XVII International Small Angle Scattering Conference CY - Traverse City, Michigan, USA DA - 07.10.2018 KW - SAXS KW - Zinc oxide nanoparticles KW - Microwave synthesis PY - 2018 AN - OPUS4-46348 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hollamby, M. J. A1 - Holmes, A. T. A1 - Blackburn, E. A1 - Danks, A. A1 - Jellyman, E. A1 - Pauw, Brian Richard A1 - Rogers, S. A1 - Grillo, I. A1 - Saeki, A. A1 - Nakanishi, T. T1 - Formation and magnetic alignment of a photoconductive organogel formed by an alkyl-C60 hydrophobic amphiphile N2 - The formation and alignment of gel fibres in alkanes (solvents) was investigated. The gel fibres consist of small amphiphilic molecules containing a C60 molecule and a small ligand chain. Under the right conditions, these self-assemble in core-shell micelles, which themselves pack into micron-sized fibre-like structures. These can be aligned using a strong magnetic field, as investigated using SANS with a 17T superconducting magnet at a range of field strengths. T2 - 7th EuCheMS Chemistry Congress CY - Liverpool, UK DA - 26.08.2018 KW - Small-angle scattering KW - Alignment KW - SANS KW - SAXS PY - 2018 AN - OPUS4-46101 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Thünemann, Andreas T1 - Characterization of (bio)macromolecules and polymeric materials with modern scattering methods N2 - The analysis of polymers, biopolymers and polymeric materials is of great interest in biomaterials science. Here small-angle x-ray scattering (SAXS), static light scatterin (SLS) and dynamic light scattering (DLS) are described. Current efforts for digitalization of this methods are explaind with respect to modern data science in biomedical research. T2 - MacroBio Summer School 2018: Biomaterial Science in View of Digitalization CY - Teltow, Germany DA - 24.09.2018 KW - Small-angle x-ray scattering KW - SAXS KW - Static light scattering KW - SLS KW - Dynamic light scattering KW - DLS KW - Biomaterials PY - 2018 AN - OPUS4-46051 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Radunz, Sebastian A1 - Schavkan, A. A1 - Wahl, S. A1 - Tschiche, Harald Rune A1 - Würth, Christian A1 - Krumrey, M. A1 - Resch-Genger, Ute T1 - Investigation of upconverting nanoparticle growth utilizing in-situ luminescence monitoring in combination with offline small-angle X-ray scattering (SAXS) and transmission electron microscopy (TEM) N2 - - UCNPs were succesfully synthesized and characterized - Various stages of UCNP growth were tracked using different analytical methods including real time in-situ & time-resolved luminescence spectroscopy, SAXS and TEM measurements - Additional size determination will be performed using inductively coupled plasma - mass spectrometry (ICP-MS) T2 - BAM-PTB-Nanoworkshop CY - PTB, Berlin, Germany DA - 14.05.2018 KW - Rare earth nanoparticles KW - Upconversion KW - TEM KW - SAXS PY - 2018 AN - OPUS4-45884 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kästner, Claudia A1 - Saloga, Patrick E. J. A1 - Thünemann, Andreas T1 - Kinetic monitoring of glutathione-induced silver nanoparticle disintegration N2 - We report on etching of polyacrylic acid-stabilised silver nanoparticles in the presence of glutathione (GSH). The initial particles with a radius of 3.2 nm and consisting of ∼8100 silver atoms dissolve in a two-step reaction mechanism while in parallel smaller silver particles with a radius of 0.65 nm and consisting of 60 to 70 silver atoms were formed. The kinetics of the etching of the initial particles, accompanied by formation of smaller silver particles was interpreted based on in situ, time-resolved small-angle X-ray scattering (SAXS) experiments. KW - Small-angle X-ray scattering KW - SAXS KW - Silver nanoparticles PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-452464 DO - https://doi.org/10.1039/c8nr02369g SN - 2040-3372 VL - 10 IS - 24 SP - 11485 EP - 11490 PB - The Royal Society of Chemistry AN - OPUS4-45246 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kästner, Claudia A1 - Böhmert, Linda A1 - Braeuning, Albert A1 - Lampen, Alfonso A1 - Thünemann, Andreas T1 - Fate of fluorescence labels - Their adsorption and desorption kinetics to silver nanoparticles N2 - Silver nanoparticles are among the most widely used and produced nanoparticles. Because of their frequent application in consumer products, the assessment of their toxicological potential has seen a renewed importance. A Major difficulty is the traceability of nanoparticles in in vitro and in vivo experiments. Even if the particles are labeled, for example, by a fluorescent marker, the dynamic exchange of ligands often prohibits their spatial localization. Our study provides an insight into the adsorption and desorption kinetics of two different fluorescent labels on silver nanoparticles with a core radius of 3 nm by dynamic light scattering, small-angle X-ray scattering, and fluorescence spectroscopy. We used BSA-FITC and tyrosine as examples for common fluorescent ligands. It is shown that the adsorption of BSA-FITC takes at least 3 days, whereas tyrosine adsorbs immediately. The quantitative amount of stabilizer on the particle surface was determined by fluorescence spectroscopy and revealed that the particles are stabilized by a monolayer of BSA-FITC (corresponding to 20 ± 9 molecules), whereas tyrosine forms a multilayered structure consisting of 15900 ± 200 molecules. Desorption experiments show that the BSA-FITC-stabilized particles are ideally suited for application in in vitro and in vivo experiments because the ligand desorption takes several days. Depending on the BSA concentration in the particles surroundings, the rate constant is k = 0.2 per day or lower when applying first order kinetics, that is, 50% of the BSAFITC molecules are released from the particle’s surface within 3.4 days. For illustration, we provide a first application of the fluorescence-labeled particles in an uptake study with two different commonly used cell lines, the human liver cell model HepG2 and the human intestinal cell model of differentiated Caco-2 cells. KW - Small-angle X-ray scattering KW - SAXS KW - Nanoparticle KW - Silver nanoparticles PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-452166 DO - https://doi.org/10.1021/acs.langmuir.8b01305 SN - 1520-5827 SN - 0743-7463 VL - 34 IS - 24 SP - 7153 EP - 7160 PB - American Chemical Society AN - OPUS4-45216 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Thünemann, Andreas T1 - Challenges of synthesis and analysis of core-shell nanoparticles for reference materials N2 - Core-shell nanoparticles are widespread in nature, industrial applications and nanotechnology research. Facile ways of modern synthesis will be discussed and possibilities to reveal their structures with small-angle X-ray scattering (SAXS). A recent review on using block copolymer templates as one of the most reliable routes for tuning size and shape of nanoparticles is provided by Li et al.1 Ferritin and apoferritin are archetypical examples for protein-based core-shell nanoparticles. Their structures are easily accessed by synchrotron SAXS2 but also with commercial instruments and allow fast performance tests.3 SASfit4 is a suitable program tool based on classical curve fitting and McSAS5 is a complementary program based on a Monte Carlo technique. Detailed refinements of SAXS data evaluation are on the way for better data analysis.6 A sub nanometer resolution is state-of-the-art for quantification of the size distribution of polyacrylic acid stabilized silver nanoparticles.3 Such particles are useful in catalysis.7 It was observed that the catalytic activity can be tuned easily by varying the shell material of the particles. T2 - NanoWorkshop 2018 (Workshop on reference nanomaterials, current situation and needs: development, measurement, standardization) CY - Berlin, Germany DA - 14.05.2018 KW - Small-angle X-ray scattering KW - SAXS KW - Nanoparticle PY - 2018 AN - OPUS4-44903 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Saadeh, Qais A1 - Pauw, Brian Richard A1 - Thünemann, Andreas A1 - Günster, Jens T1 - In-situ SAXS techniques N2 - This project studies the orientation of nanoparticles under the influence of external stimuli such as electric fields, magnetic fields and ultra-sonic vibrations. A set of functional sample holders that fit inside the sample chamber of a state-of-the-art Small Angle X-ray Scattering (SAXS) machine, called the “Multi-scale Analyzer for Ultrafine Structures” (MAUS). The MAUS has been custom engineered to serve as a miniaturized Synchrotron, thus enabling standard material to be characterized to a high standard. Our work is needed to detail the fine characterization of reference nano-particles, not only on the nano-scale, but also coupled with external agents. A second aim of this project is to verify a few proof-of-concept designs for the alignment of nano-particles. Where the alignment of nano-particles In-Situ is intended to further develop 3D printing technologies, and SAXS is an ideal choice to study the alignment of an oriented ensemble. For more information about the MAUS; https://www.bam.de/Content/DE/Pressemitteilungen/2018/AnalyticalSciences/2018-01-31-mit-maus-an-die-spitze-der-nano-forschung.html T2 - NanoWorkshop 2018 (Workshop on Reference Nanomaterials. Current situation and needs: development, measurement, standardization) CY - Berlin, Germany DA - 14.05.2018 KW - SAXS KW - Nano-particles alignment KW - Magnetic nano-particles PY - 2018 AN - OPUS4-44912 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kästner, Claudia A1 - Sieg, H. A1 - Böhmert, L. A1 - Braeuning, A. A1 - Lampen, A. A1 - Thünemann, Andreas T1 - Creating the silver standard: Development and applications of a silver nanoparticle reference material N2 - The utilization of silver nanoparticles in consumer related products has significantly increased over the last decade, especially due to their antimicrobial properties. Today they are used in a high variety of products ranging from food containers over children toys and textiles. Therefore, research on the toxicological potential of silver nanoparticles becomes increasingly important for a high amount of studies. Unfortunately, the results of these studies are extremely diverse and do not lead to a consistent evaluation. The central problem lies in the use of a wide range of silver nanoparticles, which show a broad size distribution. To overcome this problem we report on the synthesis and application of small silver nanoparticles with a narrow size distribution (R = 3.1 nm, σ = 0.6 nm). The poly(acrylic acid) stabilized particles are thoroughly characterized by small-angle X-ray scattering, dynamic light scattering and UV/Vis spectroscopy. The particles are highly stable and show no aggregation for more than six months. It is foreseen to use these thoroughly characterized nanoparticles as reference material to compare the catalytic and biological properties of functionalized silver nanoparticles. As a first step the particles are used in the first world-wide inter-laboratory comparison of SAXS. Furthermore, the stabilizing ligand PAA can be easily exchanged by biomolecules to modify the surface functionality. Replacements of PAA with glutathione (GSH) and bovine serum albumin (BSA) have been performed as examples. With this flexible system first applications regarding biological application in an artificial digestion procedure have been performed. Thereby the changes in size distribution and aggregation state were monitored by SAXS. Additionally these particles show a high catalytic activity of (436 ± 24) L g-1 s-1 in the reduction of 4- nitrophenol to 4-aminophenol. This activity is two orders of magnitude higher than for other silver particles in the literature. T2 - NanoWorkshop 2018 CY - Berlin, Germany DA - 14.05.2018 KW - Silver nanoparticles KW - SAXS KW - Artificial digestion KW - Catalysis PY - 2018 AN - OPUS4-44911 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Saloga, Patrick E. J. A1 - Kästner, Claudia A1 - Thünemann, Andreas T1 - Microwave-assisted high-speed silver nanoparticle synthesis N2 - Ever since increasing a reaction’s yield while shortening the reaction time is the main objective in synthesis optimization. Microwave reactors meet these demands. In literature however their usage is under discussion due to claims of the existence of non-thermal effects resulting from the microwave radiation. Especially for nano-reference-material syntheses it is of crucial importance to be aware of influences on the reaction pathway. Therefore, we compare ultra-small silver nanoparticles with mean radii of 3 nm, synthesized via conventional and microwave heating. We employed a versatile one-pot polyol synthesis of poly(acrylic acid) (PAA) stabilized silver nanoparticles, which display superior catalytic properties. No microwave specific effects in terms of particle size distribution characteristics, as derived by small-angle X-ray scattering (SAXS) and dynamic light scattering (DLS), are revealed. Due to the microwave reactor’s characteristics of a closed system, syntheses can be carried out at temperatures beyond the solvent’s boiling point. Particle formation was accelerated by a factor of 30 by increasing the reaction temperature from 200 °C to 250 °C. The particle growth process follows a cluster coalescence mechanism. A post-synthetic incubation step at 250 °C induces a further growth of the particles while the size distribution broadens. Thus, utilization of microwave reactors enables an enormous decrease of the reaction time as well as the opportunity of tuning the particles’ size. Possibly, decomposition of the stabilizing ligand at elevated temperatures results in reduced yields. A temperature of 250 °C and a corresponding reaction time of 30 s represent a compromise between short reaction times and high yields. T2 - NanoWorkshop 2018 (Workshop on Reference Nanomaterials. Current situation and needs: development, measurement, standardization) CY - Berlin, Germany DA - 14.05.2016 KW - SAXS KW - Microwave synthesis KW - Silver nanoparticles PY - 2018 AN - OPUS4-44904 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Liebig, Ferenc A1 - Moreno, Silvia A1 - Thünemann, Andreas A1 - Temme, Achim A1 - Appelhans, Dietmar A1 - Koetz, Joachim T1 - Toxicological investigations of “naked” and polymer-entrapped AOT-based gold nanotriangles N2 - tNegatively charged ultrathin gold nanotriangles (AuNTs) were synthesized in a vesicular dioctyl sodiumsulfosuccinate (AOT)/phospholipid-based template phase. These “naked” AuNTs with localized surfaceplasmon resonances in the NIR region at about 1300 nm and special photothermal properties are ofparticular interest for imaging and hyperthermia of cancerous tissues. For these kinds of applicationsthe toxicity and the cellular uptake of the AuNTs is of outstanding importance. Therefore, this studyfocuses on the toxicity of “naked” AOT-stabilized AuNTs compared to polymer-coated AuNTs. Poly-meric coating consisted of non-modified hyperbranched poly(ethyleneimine) (PEI), maltose-modifiedpoly(ethyleneimine) (PEI-Mal) and heparin. The toxicological experiments were carried out with twodifferent cell lines (embryonic kidney carcinoma cell line HEK293T and NK-cell leukemia cell line YTS).This study revealed that the heparin-coating of AuNTs improved biocompatibility by a factor of 50 whencompared to naked AuNTs. Of note, the highest nontoxic concentration of the AuNTs coated with PEI andPEI-Mal is drastically decreased. Overall, this is mainly triggered by the different surface charges of poly-meric coatings. Therefore, AuNTs coated with heparin were selected to carry out uptake studies. Theirpromising high biocompatibility and cellular uptake may open future studies in the field of biomedicalapplications. KW - Small-angle X-ray scattering KW - SAXS KW - Nanoparticle PY - 2018 DO - https://doi.org/10.1016/j.colsurfb.2018.04.059 SN - 0927-7765 VL - 167 SP - 560 EP - 567 PB - Elsevier AN - OPUS4-44844 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krause, B. A1 - Meyer, T. A1 - Sieg, H. A1 - Kästner, Claudia A1 - Reichardt, P. A1 - Tentschert, J. A1 - Jungnickel, H. A1 - Estrela-Lopis, I. A1 - Burel, A. A1 - Chevance, S. A1 - Gauffre, F. A1 - Jalili, P. A1 - Meijer, J. A1 - Böhmert, L. A1 - Braeuning, A. A1 - Thünemann, Andreas A1 - Emmerling, Franziska A1 - Fessard, V. A1 - Laux, P. A1 - Lampen, A. A1 - Luch, A. T1 - Characterization of aluminum, aluminum oxide and titanium dioxide nanomaterials using a combination of methods for particle surface and size analysis N2 - The application of appropriate analytical techniques is essential for nanomaterial (NM) characterization. In this study, we compared different analytical techniques for NM analysis. Regarding possible adverse health effects, ionic and particulate NM effects have to be taken into account. As NMs behave quite differently in physiological media, special attention was paid to techniques which are able to determine the biosolubility and complexation behavior of NMs. Representative NMs of similar size were selected: aluminum (Al0) and aluminum oxide (Al2O3), to compare the behavior of metal and metal oxides. In addition, titanium dioxide (TiO2) was investigated. Characterization techniques such as dynamic light scattering (DLS) and nanoparticle tracking analysis (NTA) were evaluated with respect to their suitability for fast characterization of nanoparticle dispersions regarding a particle's hydrodynamic diameter and size distribution. By application of inductively coupled plasma mass spectrometry in the single particle mode (SP-ICP-MS), individual nanoparticles were quantified and characterized regarding their size. SP-ICP-MS measurements were correlated with the information gained using other characterization techniques, i.e. transmission electron microscopy (TEM) and small angle X-ray scattering (SAXS). The particle surface as an important descriptor of NMs was analyzed by X-ray diffraction (XRD). NM impurities and their co-localization with biomolecules were determined by ion beam microscopy (IBM) and confocal Raman microscopy (CRM). We conclude advantages and disadvantages of the different techniques applied and suggest options for their complementation. Thus, this paper may serve as a practical guide to particle characterization techniques. KW - Small-angle X-ray scattering KW - SAXS PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-447057 DO - https://doi.org/10.1039/C8RA00205C SN - 2046-2069 VL - 8 IS - 26 SP - 14377 EP - 14388 PB - The Royal Society of Chemistry AN - OPUS4-44705 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Liebig, F. A1 - Sarhan, R. M. A1 - Prietzel, C. A1 - Thünemann, Andreas A1 - Bargheer, M. A1 - Koetz, J. T1 - Undulated Gold Nanoplatelet Superstructures: In Situ Growth of Hemispherical Gold Nanoparticles onto the Surface of Gold Nanotriangles N2 - Negatively charged flat gold nanotriangles, formed in a vesicular template phase and separated by an AOT-micelle-based depletion flocculation, were reloaded by adding a cationic polyelectrolyte, that is, a hyperbranched polyethylenimine (PEI). Heating the system to 100 °C in the presence of a gold chloride solution, the reduction process leads to the formation of gold nanoparticles inside the polymer shell surrounding the nanoplatelets. The gold nanoparticle formation is investigated by UV−vis spectroscopy, small-angle X-ray scattering, and dynamic light scattering measurements in combination with transmission electron microscopy. Spontaneously formed gold clusters in the hyperbranched PEI shell with an absorption maximum at 350 nm grow on the surface of the nanotriangles as hemispherical particles with diameters of ∼6 nm. High-resolution micrographs show that the hemispherical gold particles are crystallized onto the {111} facets on the bottom and top of the platelet as well as on the edges without a grain boundary. Undulated gold nanoplatelet superstructures with special properties become available, which show a significantly modified performance in SERS-detected photocatalysis regarding both reactivity and enhancement factor. KW - Small-angle X-ray scattering KW - SAXS KW - gold KW - nanoparticle PY - 2018 DO - https://doi.org/10.1021/acs.langmuir.7b02898 SN - 0743-7463 VL - 34 IS - 15 SP - 4584 EP - 4594 PB - American Chemical Society AN - OPUS4-44704 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Juling, S. A1 - Böhmert, L. A1 - Lichtenstein, D. A1 - Oberemm, A. A1 - Creutzenberg, O. A1 - Thünemann, Andreas A1 - Braeuning, A. A1 - Lampen, A. T1 - Comparative proteomic analysis of hepatic effects induced by nanosilver, silver ions and nanoparticle coating in rats N2 - The presence of nano-scaled particles in food and food-related products has drawn attention to the oral uptake of nanoparticles and their interactions with biological systems. In the present study, we used a toxicoproteomics approach to allow for the untargeted experimental identification and comparative analysis of cellular Responses in rat liver after repeated-dose treatment with silver nanoparticles, ions, and the coating matrix used for particle stabilization. The proteomic analysis revealed treatment-related effects caused by exposure to silver in particulate and ionic form. Both silver species induced similar patterns of signaling and metabolic alterations. Silver-induced cellular alterations comprised, amongst others, proteins involved in metal homeostasis, oxidative stress response, and energy metabolism. However, we discovered that secondary nano-scaled structures were formed from ionic silver. Furthermore, also the coating matrix alone gave rise to the formation of nano-scaled particles. The present data confirm, complement, and extend previous knowledge on silver toxicity in rodent liver by providing a comprehensive proteomic data set. The observation of secondary particle formation from nonparticle controls underlines the difficulties in separating particle-, ion-, and matrix coating-related effects in biological systems. Awareness of this issue will support proper evaluation of nanotoxicology-related data in the future. KW - Silver nanoparticles KW - Small-angle X-ray scattering KW - SAXS PY - 2018 DO - https://doi.org/10.1016/j.fct.2018.01.056 SN - 0278-6915 SN - 1873-6351 VL - 113 SP - 255 EP - 266 PB - Elsevier AN - OPUS4-44563 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Saloga, Patrick E. J. T1 - Messdatenauswertung mittels Origin in der Nanopartikelanalyse N2 - Die Anwendung der Software Origin zur Datenauswertung in der Nanopartikelanalyse wird anhand eines Beispiels vom Importieren der Daten über deren Verarbeitung bis zur graphischen Ausgabe demonstriert. T2 - ADDITIVE Origin Anwendertage 2018 CY - Berlin, Germany DA - 12.03.2018 KW - Silbernanopartikel KW - Origin KW - SAXS PY - 2018 AN - OPUS4-44458 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -