TY - JOUR A1 - Valet, Svenja A1 - Bohlmann, Tatjana A1 - Ebell, Gino A1 - Burkert, Andreas T1 - pH sensitive gel pads for the visualization of anodes and cathodes on zinc N2 - Zinc and zinc alloys have many applications. Zinc corrosion takes place in the atmosphere and is assumed to follow the water drop theory (a macroelement), in which the anode is at the centre of the drop and is surrounded by a cathode. This paper is the first to use gel electrolytes made of agar to visualize anodic and cathodic areas on zinc samples in order to examine the water drop theory. For that, agar gels were added with universal pH indicators, as the anode and cathode exhibit different pH values. In this paper, different amounts of pH indicators were tested to determine whether the indicator influences the potential, the impedance, phase shift, corrosion current and potential and corrosion layer resistance. KW - Corrosion KW - Zinc KW - Gel electrolyte PY - 2026 DO - https://doi.org/10.1016/j.electacta.2026.148134 SN - 0013-4686 VL - 551 SP - 1 EP - 21 PB - Elsevier Ltd. AN - OPUS4-65308 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Tidblad, Johan A1 - Moya Núñez, Alice A1 - de la Fuente, Daniel A1 - Ebell, Gino A1 - Flatlandsmo Berglen, Tore A1 - Grøntoft, Terje A1 - Hans, Ulrik A1 - Christodoulakis, Ioannis A1 - Kajánek, Daniel A1 - Kreislová, Kateřina A1 - Kwiatkowski, Lech A1 - La Torreta, Teresa A1 - Lutze, Rafał A1 - Pinar Larrubia, Guadalupe A1 - Pintus, Valentina A1 - Prange, Michael A1 - Spezzano, Pasquale A1 - Varotsos, Costas A1 - Verney-Carron, Aurélie A1 - Vuorio, Tiina A1 - Yates, Tim T1 - Corrosion and Soiling in the 21st Century: Insights from ICP Materials and Impact on Cultural Heritage N2 - This paper reviews results published by the International Co-operative Programme on Effects on Materials including Historic and Cultural Monuments (ICP Materials) with emphasis on those obtained after the turn of the century. Data from ICP Materials come from two main sources. The first is through exposures of materials and collection of environmental data in a network of atmospheric exposure test sites mainly distributed across Europe. Corrosion of carbon steel has continued to decrease during the period 2000–2020 but corrosion of zinc only up until 2014, and the trend in zinc corrosion is only visible when examining four-year data. Surface recession of limestone as well as soiling of modern glass show no decreasing trend during 2000–2020. The second is through case studies performed at heritage sites across Europe. Risk analysis of corrosion and soiling for twenty-six sites indicate that currently soiling is a more significant maintenance trigger than corrosion. Costs for maintaining heritage sites are substantial and costs attributable to air pollution is estimated from 40% to as much as 80% of the total cost. Future directions of the program are work on effects of particulate matter, improving the scientific basis for the work, and making the monitoring data publicly available. KW - Corrosion KW - Atmospheric corrosion KW - Soiling PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-644651 DO - https://doi.org/10.3390/cmd6040054 SN - 2624-5558 VL - 6 IS - 4 SP - 1 EP - 25 PB - MDPI AG AN - OPUS4-64465 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ebell, Gino A1 - Seifert, Lando A1 - Burkert, Andreas T1 - Innovative Korrosionsprüfung für Beton- und Spannstähle T1 - Test methods for corrosion testing of reinforcing and prestressing steels N2 - Korrosion ist einer der maßgeblichen Schädigungsmechanis-men im Stahlbetonbau und limitiert die Nutzungsdauer vonInfrastrukturbauwerken zum Teil erheblich. Dabei differenziertman zwischen verschiedenen Korrosionsvarianten, Korrosioninfolge Karbonatisierung des Betons, chloridinduzierte Korro-sion an Meerwasserbauwerken oder durch Tausalzbelastungund im Fall von Spannstahlbauwerken kann zusätzlich was-serstoffinduzierte Spannungsrisskorrosion (SpRK) auftreten.Für den Einsatz alternativer Betonstähle wie nichtrostenderBetonstahl gilt es, die Höhe des kritischen korrosionsaus-lösenden Chloridgehalts zu bestimmen. Um diesen für diejeweiligen Betonstähle zu ermitteln, fehlen bislang jedochnormativ geregelte Prüfverfahren. Die Empfindlichkeit vonSpannstählen gegenüber SpRK bedarf gemäß aktueller Nor-mung Langzeit-Auslagerungstests, die eine werkseigeneProduktionskontrolle aufgrund der langen Prüfzeiten nahezuunmöglich machen. Ein neu entwickeltes Prüfverfahren unterAnwendung kathodischer Polarisation, das inzwischen imneusten Entwurf der DIN EN ISO 15630–3 aufgenommenwurde, ermöglicht eine Bewertung der SpRK-Empfindlichkeitfür Spanndrähte innerhalb von 24 Stunden. Die Ergebnissetragen zur Verbesserung der Lebensdauerabschätzung undzur Weiterentwicklung von Normen für korrosionsbeständigeBetonstähle und der Robustheitsbewertung von Spannstählenbei. N2 - Corrosion is a primary damage mechanism in reinforced concrete construction, significantly reducing the service life of infrastructure. A categorisation of corrosion is imperative for the comprehension of the subject. The corrosion of concrete can be attributed to the carbonation process, whilst chloride-induced corrosion is prevalent in structures exposed to seawater or by de-icing salt. Additionaly to the former corrosion processe, prestressing steel structures could be also highly susceptible to hydrogen-induced stress corrosion cracking (SCC). In order to utilise alternative reinforcing steels, such as stainless reinforcing steel, it is necessary to ascertain the level of critical chloride threshold that can induce corrosion. Nevertheless, there is an absence of standardised test methods for determining this for the respective reinforcing steels to date. Acc. to current standardization, the sensitivity of prestressing steels to chromium content necessitates long-term ageing tests, which impede in-house production control due to the extended testing times. However, a newly developed test method using cathodic polarization, which has now been included in the latest draft of DIN EN ISO 15630–3, makes it possible to assess the susceptibility of prestressing steels to corrosion cracking within 24 hours. The results of this study will contribute to the improvement of service life estimation and the further development of standards for corrosion-resistant reinforcing steels and the robustness assessment of prestressing steels. KW - Korrosion KW - Spannstahl KW - Nichtrostender Betonstahl KW - Corrosion KW - Prestressing steel KW - Stainless reinforcing steel KW - Wasserstoff KW - Spannungsrisskorrosion KW - Lochkorrosion KW - Hydrogen KW - Stress corrosion cracking KW - Pitting corrosion PY - 2025 DO - https://doi.org/10.1002/best.202500025 SN - 0005-9900 SN - 1437-1006 SP - 1 EP - 8 PB - Ernst CY - Berlin AN - OPUS4-63305 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Heyn, A. A1 - Kotula, Stefan A1 - Ebell, Gino A1 - Babutzka, M. T1 - Results of a Round Robin Test for the Determination of Polarization Resistances on Differently Weathered Zinc Samples Using Gel Electrolytes N2 - This article presents the results of a round robin test throughout Germany with 19 participating institutions. Corrosion productlayer resistances (RL ) were determined on two differently weathered pure zinc samples and a sample activated with NaOH bymeans of electrochemical measurement of the linear polarization resistance (LPR) using agar‐based gel electrolytes. The roundrobin test was organized by the Bundesanstalt für Materialforschung und ‐prüfung (BAM) in Berlin. The measurements werecarried out by the participants in the period from May to July 2021. The results are summarized in this article comprising anassessment of the reproducibility and repeatability of the measurements. The methodology is suitable for distinguishing zincsurfaces after exposure to different atmospheres based on the corrosion product layer resistances (RL). In addition, possibleproblems in the application of the method were identified, and solutions for improving reproducibility and repeatability arediscussed. The results and knowledge from the round robin test are incorporated into a new test standard (DIN 50023:2024‐07)for this measurement method KW - Corrosion PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-630546 DO - https://doi.org/10.1002/maco.202414696 SN - 1521-4176 SP - 1 EP - 12 PB - Wiley AN - OPUS4-63054 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ebell, Gino A1 - Tannert, S. A1 - Lehmann, Jens A1 - Müller, H. T1 - Offshore Weathering Campaign on a North Sea Wind Farm Part One: Corrosivity Categories N2 - The aim of this study is to investigate the corrosion behavior of materials and coatings in offshore environments, with a focus on determining the corrosivity categories at different locations on wind turbines. The collaboration between the authors enabled a 3‐year weathering campaign at the Hohe See and Albatros offshore wind farms in the North Sea. Metal panels were installed on two wind turbines to assess the corrosivity of different atmospheric conditions. Preliminary results indicate significant variations in corrosivity depending on location and material used, suggesting that current standards may not fully reflect real‐world conditions. The results of the study will help to optimize material selection and corrosion protection strategies for offshore wind farms, potentially extending their lifetime and reducing operating costs. KW - Corrosion KW - Offshore KW - Wind PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-628995 DO - https://doi.org/10.1002/maco.202414711 SN - 1521-4176 SP - 1 EP - 10 PB - Wiley CY - Weinheim AN - OPUS4-62899 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Frenck, Johanna-Maria A1 - Frenck, Georg A1 - Degener, Sebastian A1 - Vollmer, Malte A1 - Niendorf, Thomas T1 - Interrelationships of stress-induced martensitic phase transformation and pitting corrosion in iron-based shape memory alloys N2 - Orientation dependence of stress-induced martensitic transformation under compression and the influence of a corrosion attack on superelastic properties were investigated for Fe42.7Mn34.7Al13.4Ni7.7Cr1.5 (at.−%) single crystals. The results of incremental strain tests show that the crystallographic orientation has a considerable impact on the superelastic performance, eventually resulting from the formation of twinned or detwinned martensite to accommodate strain as well martensite variant interaction. In order to investigate the effect of a corrosive environment on the mechanical performance and martensitic transformation, compression specimens were immersed in a 5.0 wt.−% NaCl solution for 24 h before tested in incremental strain tests. The immersion of the compression specimens revealed a partial surface corrosion attack including localized pitting corrosion. The localized corrosion attack increased the number of active martensite plates, most probably due to an induced multiaxial stress state. Further investigations on specimens subjected to −6% compressive strain revealed that areas with retransformed martensite serve as nucleation zones for corrosion damage. Stress-induced corrosion cracks developed, which eventually deteriorate functional response. KW - Shape memory alloy (SMA) KW - In situ characterization KW - Corrosion KW - Austenite-to-martensite phase transformation PY - 2024 DO - https://doi.org/10.1016/j.mtla.2023.102001 VL - 33 SP - 1 EP - 11 PB - Elsevier BV AN - OPUS4-61283 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Heyn, A. A1 - Meist, M. A1 - Michael, O. A1 - Babutzka, M. A1 - Valet, Svenja A1 - Ebell, Gino T1 - Electrochemical characterization of surfaces of galvanized steels under different exposure conditions using gel electrolytes N2 - The corrosion behavior of galvanized steels and zinc components under atmospheric exposure depends mostly on the corrosion product‐based cover layer formation under the prevailing conditions. The use of agar‐based gel electrolytes makes it possible to use electrochemical methods to obtain a characteristic value from these cover layers that describe their current and future protective capacity. It is shown here that different states of galvanized steel can be distinguished very well under laboratory conditions and that this method is also suitable for use under practical conditions. Based on the characteristic values and assuming future time of wetness, it is very easy to draw up a forecast for the future corrosion rate, which provides plausible values. KW - Materials Chemistry KW - Metals and Alloys KW - Surfaces, Coatings and Films KW - Mechanical Engineering KW - Mechanics of Materials KW - Environmental Chemistry KW - Corrosion KW - Znc PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-599234 DO - https://doi.org/10.1002/maco.202414389 SP - 1 EP - 16 PB - Wiley VHC-Verlag AN - OPUS4-59923 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Valet, Svenja A1 - Bohlmann, Tatjana A1 - Burkert, Andreas A1 - Ebell, Gino T1 - Zinc acetate containing gel pads for electrochemical measurements of Zn samples N2 - Agar gel pads have been used for electrochemical measurements for some time. For zinc in particular, a standard method for measuring the stability of the corrosion product layer is being established. The main interpretation factor is the corrosion product layer resistance RL, as it is easy to determine and interpret. A high corrosion product layer resistance indicates a high level of protection. However, it is not yet known how low the corrosion product layer resistance is for freshly produced zinc samples. As zinc is highly active, it reacts immediately with the environment to form a corrosion product layer, which affects the corrosion product layer resistance. The addition of zinc acetate to the agar gel pads prevents the formation of a surface layer and destroys existing ones. This makes it possible to measure an almost corrosion product-free zinc surface. This is important in defining the range of corrosion product layer resistance for a protective surface. KW - Electrochemistry KW - General Chemical Engineering KW - Analytical Chemistry KW - Corrosion KW - Zinc KW - Korrosion PY - 2023 DO - https://doi.org/10.1016/j.jelechem.2023.117814 SN - 1572-6657 VL - 948 SP - 1 EP - 8 PB - Elsevier B.V. AN - OPUS4-59079 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ebell, Gino A1 - Mayer, T. F. A1 - Harnisch, J. A1 - Dauberschmidt, Ch. T1 - Corrosion monitoring of reinforced concrete structures:The DGZfP specification B12 Collaboration N2 - Corrosion monitoring of reinforced or prestressed concrete structures has becomeincreasingly important in recent years. Areas of application include componentsthat are no longer accessible after completion or where potential fieldmeasurements cannot be carried out due to existing coatings. Corrosion monitoringcan also be used to monitor the progress of corrosion in corroding systems, e.g. to prove the success of repair measures according to repair principle 8 in accordancewith EN 1504‐9 or repair method 8.3 in accordance with the DIBt repair guideline.It also could be used to prove the functionality of cathodic corrosion protectionsystems in accordance with ISO 12696. Despite the increasing importance ofcorrosion monitoring, no guidelines orrecommendations existed until 2018. Thisgap was closed by the English version of specification B12,“Corrosion Monitoringof Reinforced and Prestressed Concrete Structures,”of the German Society for Non‐Destructive Testing, which was published in 2021. This article introducesspecification B12 by explaining the basicmeasurement principles and illustratingthe potential of corrosion monitoring in new and existing buildings. KW - Corrosion KW - Monitoring PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-580982 DO - https://doi.org/10.1002/maco.202313934 SN - 0947-5117 SP - 1 EP - 9 PB - Wiley VHC-Verlag AN - OPUS4-58098 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bäßler, Ralph A1 - Bettge, Dirk A1 - Bender, R. A1 - Féron, D. A1 - Mills, D. A1 - Ritter, S. A1 - de Graeve, I. A1 - Dugstad, A. A1 - Grassini, S. A1 - Hack, T. A1 - Halama, M. A1 - Han, E.-H. A1 - Harder, T. A1 - Hinds, G. A1 - Kittel, J. A1 - Krieg, R. A1 - Leygraf, C. A1 - Martinelli, L. A1 - Mol, A. A1 - Neff, D. A1 - Nilsson, J.-O. A1 - Odnevall, I. A1 - Paterson, S. A1 - Paul, S. A1 - Prosek, T. A1 - Raupach, M. A1 - Revilla, R. I. A1 - Ropital, F. A1 - Schweigart, H. A1 - Szala, E. A1 - Therryn, H. A1 - Tidblad, J. A1 - Virtanen, S. A1 - Volovitch, P. A1 - Watkinson, D. A1 - Wilms, M. A1 - Winning, G. A1 - Zheludkevich, M. T1 - La corrosion: un défi pour une société durable N2 - Une transition mondiale vers des systèmes énergétiques plus durables, abordables et fiables a été initiée par l’accord de Paris et l’Agenda 2030 des Nations unies pour un développement durable. Il s’agit là d’un défi industriel majeur car les systèmes et infrastructures énergétiques résilients au changement climatique exigent de se positionner pour le long terme. Se pencher sur le comportement dans la durée des matériaux structurels - principalement des métaux et des alliages - s’impose alors comme une nécessité. Dans cette optique, « La corrosion : un défi pour une société durable »présente une série de cas montrant l’importance de la tenue à la corrosion et de la protection anticorrosion des métaux et des alliages pour le développement de systèmes durables, économiques et fiables de production d’énergie. KW - Corrosion KW - Coûts de la corrosion KW - Protection KW - Anticorrosion KW - Stratégies deprévention PY - 2023 DO - https://doi.org/10.51257/a-v1-cor2000 SN - 2555-5383 VL - 2023 IS - Avril SP - 1 EP - 23 CY - Saint-Denis, France AN - OPUS4-57927 LA - fra AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Henning, Ricky A1 - Sturm, Patrick A1 - Keßler, S. A1 - Gluth, Gregor T1 - Corrosion of hybrid alkaline cements in saline solution simulating evaporite rock – effect of the Portland clinker content N2 - Two hybrid alkaline cements (HAC) based on Portland clinker, ground granulated blast furnace slag (GGBFS), fly ash and sodium sulfate, as well as an alkali-activated GGBFS/fly ash blend and a Portland cement paste were exposed to a saturated saline solution for 70 days. The combined chemical attack of chloride, magnesium and sulfate ions and the associated changes of the phase assemblage of the materials were studied by X-ray diffraction, thermal analysis and spatially resolved X-ray fluorescence spectroscopy. The experimental results revealed dissolution of ettringite, C-N-A-S-H and calcite, and the formation of gypsum, Kuzel's salt and Friedel's salt; thermodynamic modeling indicated the formation of M-S-H. The resistance of the HAC against attack by the saline solution increased with Portland clinker fraction. The capacity of portlandite to maintain pH at values above 10 is found to be a major factor controlling the resistance of HAC against corrosion in the saline solution. KW - Hybrid cements KW - Alkali-activated materials KW - Magnesium chloride KW - Corrosion KW - Salt attack PY - 2023 DO - https://doi.org/10.1016/j.cemconres.2023.107215 SN - 0008-8846 SN - 1873-3948 VL - 172 SP - 1 EP - 14 PB - Elsevier Ltd. AN - OPUS4-57638 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schwarz, W. A1 - Wilsch, Gerd A1 - Katsumi, N. A1 - Ebell, Gino A1 - Völker, Tobias T1 - Ion distribution in concrete overlay, mapped by laser induced breakdown spectroscopy (LIBS), modified by an embedded zinc anode N2 - Galvanic corrosion protection by embedded zinc anodes is an accepted technique for the corrosion protection of reinforcing steel in concrete. Galvanic currents flow between the zinc anode and the steel reinforcement due to the potential difference that is in the range of a few hundred mV. The ion distribution was studied on two steel reinforced concrete specimens admixed with 3 wt.% chloride/wt. cement and galvanically protected by a surface applied EZ-anode. On both specimens, a zinc anode was embedded and glued to the concrete surface by a geo-polymer-based chloride-free binder. At one specimen, the EZ-anode was operated for 2,5 years, the EZ-anode at the other specimen was not electrically connected to the reinforcement, this specimen serves as a reference. Both specimens have been stored under identical conditions. The ion distribution between the anode (EZ-ANODE) and cathode (steel reinforcement) was studied by laser-induced breakdown spectroscopy (LIBS) after 7 months, 12 months, and 2,5 years. Results of the LIBS studies on the specimen with activated EZ-anode after 7 months, 12 months, and 2,5 years and of the reference specimen after 2,5 years are reported. Results show that diffusion of ions contributes to the changes in the ion distribution but migration, especially of chlorides towards the EZ-anode is significant despite the weak electric field – several hundred millivolts - generated by the galvanic current. Results show that chloride ions accumulate near the zinc-anode as in water-insoluble zinc-hydroxy chlorides - Simonkollite. T2 - ICCRRR 2022 CY - Capetown, South Africa KW - Corrosion KW - LIBS KW - Zinc KW - Anode PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-560576 DO - https://doi.org/10.1051/matecconf/202236404023 SN - 2261-236X VL - 364 SP - 1 EP - 7 PB - EDP Sciences CY - Les Ulis AN - OPUS4-56057 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bender, R. A1 - Féron, D. A1 - Mills, D. A1 - Ritter, S. A1 - Bäßler, Ralph A1 - Bettge, Dirk A1 - de Graeve, I. A1 - Dugstad, A. A1 - Grassini, S. A1 - Hack, T. A1 - Halama, M. A1 - Han, E.-H. A1 - Harder, T. A1 - Hinds, G. A1 - Kittel, J. A1 - Krieg, R. A1 - Leygraf, C. A1 - Martinelli, L. A1 - Mol, A. A1 - Neff, D. A1 - Nilsson, J.-O. A1 - Odnevall, I. A1 - Paterson, S. A1 - Paul, S. A1 - Prošek, T. A1 - Raupach, M. A1 - Revilla, R. I. A1 - Ropital, F. A1 - Schweigart, H. A1 - Szala, E. A1 - Terryn, H. A1 - Tidblad, J. A1 - Virtanen, S. A1 - Volovitch, P. A1 - Watkinson, D. A1 - Wilms, M. A1 - Winning, G. A1 - Zheludkevich, M. T1 - Corrosion challenges towards a sustainable society N2 - A global transition towards more sustainable, affordable and reliable energy systems is being stimulated by the Paris Agreement and the United Nation's 2030 Agenda for Sustainable Development. This poses a challenge for the corrosion industry, as building climate‐resilient energy systems and infrastructures brings with it a long‐term direction, so as a result the long‐term behaviour of structural materials (mainly metals and alloys) becomes a major prospect. With this in mind “Corrosion Challenges Towards a Sustainable Society” presents a series of cases showing the importance of corrosion protection of metals and alloys in the development of energy production to further understand the science of corrosion, and bring the need for research and the consequences of corrosion into public and political focus. This includes emphasis on the limitation of greenhouse gas emissions, on the lifetime of infrastructures, implants, cultural heritage artefacts, and a variety of other topics. KW - Corrosion KW - Corrosion costs KW - Corrosion protection KW - Preventive strategies PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-554801 DO - https://doi.org/10.1002/maco.202213140 SN - 1521-4176 VL - 73 IS - 11 SP - 1730 EP - 1751 PB - Wiley-VCH CY - Weinheim AN - OPUS4-55480 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Babutzka, Martin A1 - Grabowski, Sven A1 - Sahrhage, H. A1 - Lampke, T. T1 - Electrochemical corrosion investigations on binary and ternary zinc alloy coatings using gel electrolytes N2 - Novel agar-based test electrolytes are used to perform electrochemical corrosion investigations on ZnFe and ZnNi binary as well as ZnFeMo ternary zinc coatings. The objectives of the electrochemical investigations include the characterization of the corrosion behavior, the description of the protective effect of the coatings as well as the investigation of the layer formation and degradation under artificial aging. ZnFe and ZnFeMo coatings are applied with varying iron content as well as an additional passivation layer, respectively, to study the effect on corrosion resistance. The results show that the protective effect of the coatings is not negatively influenced by different iron contents or the addition of molybdenum. Additional passivation of the ZnFe-containing coatings by means of a passivating agent leads to a significant improvement in the protective effect. Artificial aging leads to slight degradation of the additional passivation layer whereas coatings without post-treatment enhance their protective effect by the formation of corrosion product layers. KW - Binary zinc alloys KW - Ternary zinc alloys KW - Corrosion testing KW - Gel electrolytes KW - Corrosion PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-543013 DO - https://doi.org/10.1002/adem.202101336 SN - 1438-1656 SP - 1 EP - 14 PB - Wiley-VCH CY - Weinheim AN - OPUS4-54301 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Aristia, Gabriela A1 - Bäßler, Ralph A1 - Nofz, Marianne A1 - Sojref, Regine A1 - Kohl, Anka T1 - Short-term exposure tests of ɣ-Al2O3 Sol-gel coating on X20Cr13 in artificial geothermal waters with different pH N2 - The suitability of an Al2O3 coating for corrosion protection on X20Cr13 was evaluated in various artificial geothermal brines, focusing on the influence of different pH (4, 6 and 8) and their chemical compositions on the coating properties. All experiments were performed in the laboratory using autoclaves at 150 ◦C and 1 MPa in deaerated condition for 1 and 7 days. Results showed that the pH of geothermal waters is the most detrimental factor in the transformation of ɣ-Al2O3 and its protective abilities. Delaminations were found in the Coating exposed to geothermal brines with pH 4. FTIR spectra indicated a transformation of ɣ-Al2O3 to boehmite AlOOH after exposure to pH 4 and 6, and bayerite Al(OH)3 was formed after exposure to pH 8. Different Crystal structures of the hydrated Al2O3 also contribute to the stability of the coatings, observed by the SEM- EDX of the surface and cross-section of coatings. This study indicated that ɣ-Al2O3 sol-gel coating presents a promising aspect of corrosion protection in geothermal environment with a neutral pH. KW - Al2O3 KW - Corrosion KW - Coating KW - Martensitic steel PY - 2021 DO - https://doi.org/10.1016/j.geothermics.2021.102193 SN - 0375-6505 VL - 96 SP - 102193 PB - Elsevier Ltd. CY - Amsterdam AN - OPUS4-52931 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Valet, Svenja A1 - Burkert, Andreas A1 - Ebell, Gino A1 - Babutzka, Martin T1 - Determination of the corrosion product layer resistance on zinc and electrolytically galvanized steel samples by using gel electrolytes N2 - Although zinc and zinc coatings have been widely used for corrosion protection for decades new zinc coatings are constantly being developed. Characterizing the corrosion protectiveness of these new coatings, however, should not be underestimated. While exposure tests are time intensive, cyclic tests can only be used for a very limited field of application. Thus, electrochemical measurements provide both an efficient and an effective alternative. Conventional aqueous bulk electrolytes influence the surface layers of a tested zinc coating and are therefore not reliable. Gel electrolytes, however, have evolved over the last few years, are minimally invasive and provide reliable results. This work describes experiments with gel electrolytes made of agar. Unlike previous work, it proposes a composition of gel electrolyte for minimally invasive description of the protective power of naturally formed oxide layers on zinc and zinc coatings. Therefore, as a first part, the gel electrolyte made of agar is verified as a method for zinc and zinc-coated samples. Afterwards, this paper introduces the corrosion product layer resistance RL as a promising parameter to evaluate the protective power of zinc coatings. Results are verified with EIS and FTIR measurements. An example on a representative zinc coating demonstrates the practical application. KW - Gel electrolytes KW - Agar KW - Zinc coatings KW - Atmospheric exposure KW - Corrosion PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-526053 DO - https://doi.org/10.1016/j.electacta.2021.138191 SN - 0013-4686 VL - 385 SP - 138191 PB - Elsevier Ltd. AN - OPUS4-52605 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Aristia, Gabriela A1 - Le, Quynh Hoa A1 - Nofz, Marianne A1 - Sojref, Regine A1 - Bäßler, Ralph T1 - Study of Al2O3 Sol-Gel Coatings on X20Cr13 in Artificial North German Basin Geothermal Water at 150 °C N2 - Al2O3 has been widely used as a coating in industrial applications due to its excellent chemical and thermal resistance. Considering high temperatures and aggressive mediums exist in geothermal systems, Al2O3 can be a potential coating candidate to protect steels in geothermal applications. In this study, γ-Al2O3 was used as a coating on martensitic steels by applying AlOOH sol followed by a heat treatment at 600 °C. To evaluate the coating application process, one-, two-, and three-layer coatings were tested in the artificial North German Basin (NGB), containing 166 g/L Cl−, at 150 °C and 1 MPa for 168 h. To reveal the stability of the Al2O3 coating in NGB solution, three-layer coatings were used in exposure tests for 24, 168, 672, and 1296 h, followed by surface and cross-section characterization. SEM images show that the Al2O3 coating was stable up to 1296 h of exposure, where the outer layer mostly transformed into boehmite AlOOH with needle-like crystals dominating the surface. Closer analysis of cross-sections showed that the interface between each layer was affected in long-term exposure tests, which caused local delamination after 168 h of exposure. In separate experiments, electrochemical impedance spectroscopy (EIS) was performed at 150 °C to evaluate the changes of coatings within the first 24 h. Results showed that the most significant decrease in the impedance is within 6 h, which can be associated with the electrolyte penetration through the coating, followed by the formation of AlOOH. Here, results of both short-term EIS measurements (up to 24 h) and long-term exposure tests (up to 1296 h) are discussed. KW - Al2O3 KW - Geothermal KW - Martensitic steels KW - Behmite KW - Corrosion PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-525551 DO - https://doi.org/10.3390/coatings11050526 SN - 2079-6412 VL - 11 IS - 5 SP - 526 PB - MDPI CY - Basel AN - OPUS4-52555 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Le, Quynh Hoa A1 - Bäßler, Ralph A1 - Bettge, Dirk A1 - Buggisch, E. A1 - Schiller, Bernadette Nicole A1 - Beck, M. T1 - Corrosion Study on Wellbore Materials for the CO2 Injection Process N2 - For reliability and safety issues of injection wells, corrosion resistance of materials used needs to be determined. Herein, representative low-cost materials, including carbon steel X70/1.8977 and low alloyed steel 1.7225, were embedded in mortar to mimic the realistic casing-mortar interface. Two types of cement were investigated: (1) Dyckerhoff Variodur commercial Portland cement, representing a highly acidic resistant cement and (2) Wollastonite, which can react with CO2 and become stable under a CO2 stream due to the carbonation process. Exposure tests were performed under 10 MPa and at 333 K in artificial aquifer fluid for up to 20 weeks, revealing crevice corrosion and uniform corrosion instead of expected pitting corrosion. To clarify the role of cement, simulated pore water was made by dispersing cement powder in aquifer fluid and used as a solution to expose steels. Surface analysis, accompanied by element mapping on exposed specimens and their crosssections, was carried out to trace the chloride intrusion and corrosion process that followed. KW - Carbon capture storage KW - CCS KW - Carbon dioxide KW - Corrosion KW - Carbon steel KW - Aquifer fluid KW - Cement KW - Casing KW - Pitting PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-519774 DO - https://doi.org/10.3390/pr9010115 SN - 2227-9717 VL - 9 IS - 1 SP - 115 PB - MDPI CY - Basel AN - OPUS4-51977 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Stoljarova, A. A1 - Regenspurg, S. A1 - Bäßler, Ralph A1 - Mathiesen, T. A1 - Braüner Nielsen, J. T1 - Effect of lead and copper containing brine on steel materials for geothermal applications – A corrosion study N2 - Geothermal brines often contain high amounts of lead and copper ions that can precipitate as native Cu and Pb as consequence of galvanic corrosion when brines react with carbon steel materials. This contribution evaluates which materials could overcome the problem of galvanic corrosion at geothermal environment. The behavior of these materials in water containing high chloride concentration (> 100 g/L NaCl) as well as various amounts of dissolved bCl2 and/or CuCl2 was characterized by electrochemical and exposure measurements. Both methods reveal carbon steel suffers corrosion susceptibility, accompanied by Cu◦ and/or Pb◦ precipitation on the surface. Electrochemical measurements on stainless steels result in significant difference in corrosion and repassivation potentials (Ecorr = -189 mV, Erep = 70 mV), indicating a good corrosion resistance. KW - Copper KW - Lead KW - Corrosion KW - Steel KW - Geothermal energy PY - 2021 DO - https://doi.org/10.1016/j.geothermics.2020.102024 SN - 0375-6505 VL - 91 SP - NIL_75 EP - NIL_85 PB - Elsevier CY - Amsterdam AN - OPUS4-51976 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bäßler, Ralph T1 - Review: Science, Technology and Applications of Metals in Additive Manufacturing N2 - Often 3D‐printing and additive manufacturing are mentioned as the 3rd industrial revolution. In this conjunction this book provides a brief overview on additively manufactured metal pieces. This book fulfills its intension to serve as an educational guide, providing a holistic picture encompassing science, technology and applications for the real‐life use of Metal Additive Manufacturing. KW - Additive manufacturing KW - Corrosion KW - Material properties PY - 2020 DO - https://doi.org/10.1002/maco.202070114 SN - 1521-4176 SN - 0947-5117 VL - 71 IS - 11 SP - 1929 EP - 1930 PB - WILEY‐VCH Verlag GmbH & Co. KGaA CY - Weinheim AN - OPUS4-51514 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Seifert, Lando T1 - Review: Steel‐Reinforced Concrete Str‐uctures: Assessment and Repair of Corrosion N2 - In 2019 CRC Press published the "Steel‐Reinforced Concrete Structures" as a paperback. This book does not vary in terms of content from the hardback publication of 2008. But it is first reviewed here in corrosion news. The book provides eight of nine chapters in which the author discusses technical aspects of assessment and repair of steel‐reinforced concrete structures. To sum up, this book is recommended for students and people involved with the assessment and repair of reinforced‐concrete structures, who want to get a quick introduction into the different aspects of the field. Readers also learn much about the economic interactions besides the topic. However, for experienced technicians and corrosion experts, this book may not be exact enough in both the electrochemical description of deterioration processes and the practical aspects of repair and control methods. Despite that, the discussions of the author are scientifically correct. KW - Concrete KW - Corrosion PY - 2020 DO - https://doi.org/10.1002/maco.202070084 SN - 1521-4176 SN - 0947-5117 VL - 71 IS - 8 SP - 1408 EP - 1409 PB - WILEY‐VCH Verlag GmbH & Co. KGaA CY - Weinheim AN - OPUS4-51075 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Boschmann Käthler, C. A1 - Angst, U. A1 - Ebell, Gino A1 - Elsener, B. T1 - Chloride-induced reinforcement corrosion in cracked concrete: the influence of time of wetness on corrosion propagation N2 - Literature data on the influence of concrete cracks on corrosion propagation of reinforcing steel are contradictory. This might be due to very different exposure and test conditions but also to a lack of time-resolved data in cyclic wetting–drying exposure. Here, the influence of the environmental conditions on the corrosion rates in cracked concrete is studied experimentally. The results show that the corrosion rate in cracked concrete depends on the duration of wetting and drying phases and the relative humidity (RH) during the drying phase. The lower the ambient RH in the drying phase, the faster the cracks dry, which depresses the corrosion rate in the periods between the wetting events. A model is proposed to estimate corrosion rates in cracked concrete cyclic wetting/drying exposure. KW - Korrosion KW - Corrosion KW - Concrete PY - 2020 DO - https://doi.org/10.1080/1478422X.2020.1789371 SP - 1 EP - 11 PB - Taylor Francis Online CY - London AN - OPUS4-50986 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Babutzka, Martin A1 - Müller, Thoralf A1 - Mietz, Jürgen A1 - Burkert, Andreas T1 - Investigation of the influence of iron‐containing abrasives on the corrosion behaviour of the aluminium alloy AlSi1.2Mg0.4 N2 - The corrosion resistance of aluminium surfaces is closely linked to the surfacecstate after a grinding process. For years, iron‐containing abrasive materials were suspected to lead to increased corrosion susceptibility after processing of aluminium surfaces. To prove a possible correlation between the iron content of an abrasive and the corrosion behaviour of aluminium components, scientific investigations and experimentally practical corrosion tests are necessary. For the current investigation, specimens of a technical Al‐Si alloy from the same batch were used. The test specimens were mechanically ground with various resin‐bonded model abrasives containing different iron contents. The performed corrosion tests did not reveal a negative influence of the different iron‐containing abrasives on the corrosion behaviour of the Al–Si alloy. However, the most sensitive measuring method (electrochemical noise) showed differences in the surface activity depending on the type of abrasive. KW - Aluminium KW - Corrosion KW - Corrosion testing KW - Grinding PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-506762 DO - https://doi.org/10.1002/maco.202011657 SN - 0947-5117 SN - 1521-4176 VL - 71 IS - 10 SP - 1667 EP - 1679 PB - Wiley‐VCH Verlag GmbH & Co. KGaA CY - Weinheim AN - OPUS4-50676 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kratzig, A. A1 - Le, Quynh Hoa A1 - Bettge, Dirk A1 - Menneken, M. A1 - Bäßler, Ralph T1 - Early Stage of Corrosion Formation on Pipeline Steel X70 Under Oxyfuel Atmosphere at Low Temperature N2 - The early stage of corrosion formation on X70 pipeline steel under oxyfuel atmosphere was investigated by applying a simulated gas mixture (CO2 containing 6700 ppmv O2, 100 ppmv NO2, 70 ppmv SO2 and 50 ppmv H2O) for 15 h at 278 K and ambient pressure. Short-term tests (6 h) revealed that the corrosion starts as local spots related to grinding marks progressing by time and moisture until a closed layer was formed. Acid droplets (pH 1.5), generated in the gas atmosphere, containing a mixture of H2SO4 and HNO3, were identified as corrosion starters. After 15 h of exposure, corrosion products were mainly X-ray amorphous and only partially crystalline. In-situ energy-dispersive X-ray diffraction (EDXRD) results showed that the crystalline fractions consist primarily of water-bearing iron sulfates. Applying Raman spectroscopy, water-bearing iron nitrates were detected as subordinated phases. Supplementary long-term tests exhibited a significant increase in the crystalline fraction and formation of additional water-bearing iron sulfates. All phases of the corrosion layer were intergrown in a nanocrystalline network. In addition, numerous globular structures have been detected above the corrosion layer, which were identified as hydrated iron sulphate and hematite. As a type of corrosion, shallow pit formation was identified, and the corrosion rate was about 0.1 mma−1. In addition to in-situ EDXRD, SEM/EDS, TEM, Raman spectroscopy and interferometry were used to chemically and microstructurally analyze the corrosion products. KW - Corrosion KW - CCUS KW - In-situ ED-XRD KW - CO2 pipeline transport KW - Oxyfuel KW - Carbon steel KW - Impurities PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-506303 DO - https://doi.org/10.3390/pr8040421 SN - 2227-9717 VL - 8 IS - 4 SP - 421-1 EP - 421-19 PB - MDPI CY - Basel AN - OPUS4-50630 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -