TY - JOUR A1 - Costa e Silva, A. A1 - Coelho, D. A1 - Kranzmann, Axel A1 - Rizzo, Fernando T1 - Simulation of Fe-Cr-X Alloy Exposed to an Oxyfuel Combustion Atmosphere at 600°C JF - Journal of Phase Equilibria & Diffusion N2 - In coal-fired power plants using oxyfuel combustion process with carbon capture and sequestration, instead of air, a mixture of oxygen and recirculated flue gas is injected in the boiler. A series of steels were exposed to CO2-SO2-Ar-H2O gas mixtures at 600 °C for 1000 h to compare their high temperature corrosion behavior. During the corrosion process, carburization, decarburization and recrystallization were observed underneath the oxide scale depending on the gas mixture and alloy composition. The conditions that lead to carburization are not yet completely understood, but decarburization can be simulated using thermodynamic and kinetic models. In this work, the results of these simulations are compared with measured values for one of the alloys that displayed a decarburized region. Since the mobility of carbon in the scale is not known, two strategies were adopted: simulation of alloy-atmosphere contact; and estimation of the carbon flux to produce the observed decarburization. The second approach might give an insight on how permeable to carbon the scale is. KW - CALPHAD approach KW - Corrosion KW - Decarburization KW - DICTRA modeling KW - Experimental kinetics PY - 2016 DO - https://doi.org/10.1007/s11669-015-0421-3 SN - 1547-7037 VL - 37 IS - 1 SP - 19 EP - 24 PB - ASTM International AN - OPUS4-50612 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Costa e Silva, A. A1 - Coelho, D. A1 - Rizzo, F. A1 - Kranzmann, Axel T1 - Simulation of Fe-Cr-X alloy exposed to an oxyfuel combustion atmosphere at 600 °C JF - Journal of Phase Equilibria and Diffusion N2 - In coal-fired power plants using oxyfuel combustion process with carbon capture and sequestration, instead of air, a mixture of oxygen and recirculated flue gas is injected in the boiler. A series of steels were exposed to CO2-SO2-Ar-H2O gas mixtures at 600 °C for 1000 h to compare their high temperature corrosion behavior. During the corrosion process, carburization, decarburization and recrystallization were observed underneath the oxide scale depending on the gas mixture and alloy composition. The conditions that lead to carburization are not yet completely understood, but decarburization can be simulated using thermodynamic and kinetic models. In this work, the results of these simulations are compared with measured values for one of the alloys that displayed a decarburized region. Since the mobility of carbon in the scale is not known, two strategies were adopted: simulation of alloy-atmosphere contact; and estimation of the carbon flux to produce the observed decarburization. The second approach might give an insight on how permeable to carbon the scale is. KW - CALPHAD approach KW - Corrosion KW - Decarburization KW - DICTRA modeling KW - Experimental kinetics KW - Iron alloys KW - Kinetics KW - Multicomponent diffusion KW - Steel PY - 2016 DO - https://doi.org/10.1007/s11669-015-0421-3 SN - 1547-7037 SN - 1863-7345 VL - 37 IS - 1 SP - SI, 19 EP - 24 PB - Springer US AN - OPUS4-40110 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ewert, Uwe T1 - Progress in digital industrial radiology - Part 1: Radiographic techniques-film replacement and backscatter imaging JF - Badania Nieniszczące i Diagnostyka N2 - Similar to the success story of digital photography a major upheaval has been observed in digital industrial radiology. This paper is split into 3 parts: Part 1: Film Replacement and Backscatter Imaging: Computed radiography with phosphor imaging plates substitutes film applications. Digital Detector Arrays enable an extraordinary increase of contrast sensitivity in comparison to film radiography. The increased sensitivity of digital detectors enables the efficient usage for dimensional measurements and functionality tests substituting manual maintenance. The digital measurement of wall thickness and corrosion status is state of the art in petrochemical industry. Photon counting and energy discriminating detectors are applied up to 300 Kv provide increased thickness dynamic and material discrimination by synchronously acquisition of images of the high and low energy part of the spectrum. X-ray back scatter techniques have been applied in safety and security relevant applications with single sided access of source and detector. First inspections of CFRP in aerospace industry were successfully conducted with newly designed back scatter cameras. Numeric modeling is used to design X-Ray optics and inspection scenarios as well as conducting RT training. Part 2: Computed tomography (CT) Part 3: Micro Radiography and Micro CT. KW - Digital radiography KW - Computed tomography KW - Laminography KW - Imaging plates KW - Digital detector arrays KW - Photon counting detectors KW - Back scatter KW - Numeric modelling KW - CFRP KW - Welding KW - Corrosion PY - 2016 VL - 1-2 SP - 37 EP - 43 AN - OPUS4-39163 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rütters, H. A1 - Stadler, S. A1 - Bäßler, Ralph A1 - Bettge, Dirk A1 - Jeschke, S. A1 - Kather, A. A1 - Lempp, C. A1 - Lubenau, U. A1 - Ostertag-Hennig, C. A1 - Schmitz, S. A1 - Schütz, S. A1 - Waldmann, S. T1 - Towards an optimization of the CO2 stream composition - A whole-chain approach JF - International Journal of Greenhouse Gas Control N2 - CO2 streams captured from power stations or industrial plants may contain impurities that impact the consecutive steps of the CO2 capture and storage (CCS) chain. As the basis for an optimization of CO2 purity over the whole CCS chain, impacts of different impurities were investigated at key steps including studies on (i) corrosion of metallic materials in CO2 streams and brine, (ii) fluid and interfacial properties as a function of pressure, temperature and CO2 stream composition and their implications for CO2 transport, injection and geological storage, (iii) costs of different pipeline design options, (iv) geochemical alterations at typical reservoir conditions and their implications for geomechanical rock properties. Major findings are synthesized for two exemplary single source-single sink CCS chain scenarios involving CO2 stream compositions typical for pre-combustion capture and oxyfuel combustion. Recommendations for material selection for compression, transport and injection were derived for various CO2 stream compositions. To reliably control corrosion, a limitation of water contents to 50 ppmv is recommended for pipeline transportation of all CO2 streams. At geological storage conditions, the presence of either O2, NOx or SO2 only weakly affected fluid-mineral/rock interactions that still impacted geomechanical rock properties. KW - CCS KW - Impurities KW - Associated incidental substances KW - Pipeline design KW - Corrosion KW - Fluid-rock interactions PY - 2016 UR - http://www.sciencedirect.com/science/article/pii/S1750583616305047 DO - https://doi.org/10.1016/j.ijggc.2016.08.019 SN - 1750-5836 SN - 1878-0148 VL - 54 IS - 2 SP - 682 EP - 701 PB - Elsevier AN - OPUS4-38401 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pohl, K. A1 - Özcan Sandikcioglu, Özlem A1 - Voigt, M. A1 - Grundmeier, G. T1 - Adhesion and corrosive delamination of epoxy films on chemically etched ZnMgAl-alloy coatings JF - Materials and Corrosion N2 - The effect of alkaline and acidic pretreatment steps on the surface chemical composition and adhesion properties of ZnMgAl-alloy coated steel was investigated by means of spectroscopic methods, scanning Kelvin probe (SKP) and peel test measurements.The spectroscopic results indicate that the surface film composition can be adjusted by the wet-chemical treatment. To study the corresponding surface adhesive properties, the samples were coated with an epoxy amine adhesive. Peel tests under humid conditions indicated an increased interaction between the acidic pre-treated surface and the adhesive. The results of the SKP analysis show that the acidic cleaned substrates have the highest resistance to delamination, which can be explained by the shift of the interfacial electrode potential. KW - Corrosion KW - ZnMgAl-alloy coatings KW - XPS KW - Scanning Kelvin probe PY - 2016 DO - https://doi.org/10.1002/maco.201608968 SN - 0947-5117 SN - 1521-4176 VL - 67 IS - 10 SP - 1020 EP - 1026 AN - OPUS4-38196 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Quiroz, V. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Saldabilita di lamiere in acciaio inossidabile austenico ed austeno-ferritico ad alto contenuto di manganese con processo laser JF - Rivista Italiana della Saldatura N2 - Manganese alloyed stainless steels represent a cost-effective alternative to conventional CrNi- stainless steels due to strong fl uctuations of the market prices for nickel seen during the last years. In CrMnNi steels, nickel is partially replaced by lower-cost manganese and small amounts of nitrogen for stabilization of the austenitic phase. This also brings benefi ts regarding the mechanical properties, as it results in an increased material strength. Laser beam welding of such materials was investigated for direct comparison with Standard CrNi steels. Main emphasis was laid on fi nding adequate process parameters to achieve a stable welding process and obtain a good weld quality. Two different laser sources, a 4.4 kW Nd:YAG and a 5 kW CO2 laser, were used to weld 1.5 mm stainless steel sheets in continuous wave mode. A high-Mn austenitic (1.4376) and a lean duplex (1.4162) steel, as well as the standard austenitic (1.4301) and duplex (1.4362) grades were selected as test materials. Both butt and lap joint confi gurations were studied. Experiments were carried out systematically, varying the welding speed, laser power and focal point position in order to determine adequate process windows. The infl uence of the shielding gas type and fl ow rate on the process stability and the weld quality were investigated. The effects of weld edge preparation on the weld appearance and quality levels attained were also examined. The obtained welded joints were subjected to radiographic tests for detection of internal imperfections. Also a metallurgical characterization of the samples regarding the resulting phase composition or balance and hardness depending on the welding process parameters was conducted. Furthermore, tensile and potentiodynamic tests were performed to evaluate the mechanical and corrosion properties, respectively. The results provide an insight into the advantages and limitations of the laser beam welding process for joining high-manganese alloyed stainless steels. Conditions for the production of defect-free and corrosion-resistant welds having good mechanical properties could be determined. KW - Weldability KW - Austenitic stainless steels KW - Corrosion KW - CO2 lasers KW - Duplex stainless steels KW - Laser welding KW - Manganese KW - Mechanical properties KW - Shielding gases KW - YAG lasers PY - 2016 SN - 0035-6794 VL - 68 IS - 1 SP - 33 EP - 43 AN - OPUS4-38100 LA - ita AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ebell, Gino A1 - Burkert, Andreas A1 - Fischer, Joachim A1 - Lehmann, Jens A1 - Müller, Thoralf A1 - Meinel, Dietmar A1 - Paetsch, O. T1 - Investigation of chloride-induced pitting corrosion of steel in concrete with innovative methods JF - Materials and Corrosion N2 - The combination of electrochemical and 3D computed tomography (CT) investigations offers the possibility of verifying electrochemical measurements non-destructively. Determining the steel surfaces damaged by pitting corrosion allows developing specimens having damage pattern corresponding to practice. Corrosion phenomena like decoupled pitting corrosion cannot be verified by electrochemical measurements only, but with the combination of those two kinds of investigations it is possible. Another advantage is the minimization of the number of samples. The classical experimental procedure requires the destruction of samples after each damage step.This can be avoided by the use of 3D computed tomography. As long as the corrosion phenomena are completely within the examination zone shown by the 3D computed tomography, the electrochemical measurements can be calculated on an area basis to get the specific corrosion rate or polarization resistance. KW - Corrosion KW - Concrete KW - 3D x-ray KW - Corrosion rate PY - 2016 DO - https://doi.org/10.1002/maco.201608969 SN - 1521-4176 SN - 0947-5117 SN - 0043-2822 VL - 67 IS - 6 SP - 583 EP - 590 PB - Wiley-VCH Verlag GmbH & Co. KGaA CY - Weinheim AN - OPUS4-36341 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sobol, Oded A1 - Straub, F. A1 - Wirth, Thomas A1 - Holzlechner, G. A1 - Böllinghaus, Thomas A1 - Unger, Wolfgang T1 - Real Time Imaging of Deuterium in a Duplex Stainless Steel Microstructure by Time-of-Flight SIMS JF - Nature - Scientific Reports N2 - For more than one century, hydrogen assisted degradation of metallic microstructures has been identified as origin for severe technical component failures but the mechanisms behind have not yet been completely understood so far. Any in-situ observation of hydrogen transport phenomena in microstructures will provide more details for further elucidation of these degradation mechanisms. A novel experiment is presented which is designed to elucidate the permeation behaviour of deuterium in a microstructure of duplex stainless steel (DSS). A hydrogen permeation cell within a TOF-SIMS instrument enables electrochemical charging with deuterium through the inner surface of the cell made from DSS. The outer surface of the DSS permeation cell exposed to the vacuum has been imaged by TOF-SIMS vs. increasing time of charging with subsequent chemometric treatment of image data. This in-situ experiment showed evidently that deuterium is permeating much faster through the ferrite phase than through the austenite phase. Moreover, a direct proof for deuterium enrichment at the austenite-ferrite interface has been found. KW - Characterization and analytical techniques KW - Corrosion KW - Imaging technique KW - Mass spectrometry PY - 2016 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-353872 UR - http://www.nature.com/articles/srep19929 DO - https://doi.org/10.1038/srep19929 SN - 2045-2322 VL - 6 IS - 19929 SP - 1 EP - 7 PB - nature publishing group CY - London, United Kingdom AN - OPUS4-35387 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Glenn, A.M. A1 - Hughes, A.E. A1 - Torpy, A. A1 - Nolze, Gert A1 - Birbilis, N. T1 - Defect density associated with constituent particles in AA2024-T3 and its role in corrosion JF - Surface and interface analysis N2 - Electron backscatter diffraction (EBSD) and scanning electron microscopy were combined to study the effect of residual defect density on corrosion initiation in aluminium alloy AA2024-T3. EBSD was used to determine the level of misorientation (MO), from pixel to pixel, within individual grains. The MO can be determined with respect to either the average orientation angle of the grain or with respect to the average orientation angle of the surrounding pixels (in this instance, a matrix of 7×7 surrounding pixels has been applied). Herein, the MO, determined using the surrounding pixels, was used as the means for the assessing the level of defect density within a grain. It was found that there was a noteworthy, but not definitive, correlation of MO with corrosion initiation after 1 min exposure to 0.1 M NaCl solution. Additionally, the S and θ-phase particles were also identified using EBSD, displaying a range of MO and therefore defect density. KW - Al-alloy KW - S-phase KW - EBSD KW - Corrosion KW - AA2024-T3 KW - Defect density PY - 2016 DO - https://doi.org/10.1002/sia.5813 SN - 0142-2421 SN - 1096-9918 VL - 48 IS - 8 (SI) SP - 780 EP - 788 PB - Wiley CY - Chichester AN - OPUS4-34476 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -