TY - THES A1 - Aristia, Gabriela T1 - Polyaniline/Silicon Dioxide Composite-Based Coating for Corrosion Protection in Geothermal Systems N2 - Geothermal energy is one of the cleanest renewable alternatives to reduce the dependency on fossil fuel [1, 2]. Despite its promising future, its implementation faces various challenges, one of them being corrosion processes. To implement this energy, hot fluids are pumped from a geothermal well. These hot fluids originate from deep within the earth, so consist of different ionic species and gases in a wide range of temperatures, which lead to their corrosive nature. In terms of geothermal energy resources, Indonesia is at the forefront, with the highest preserved geothermal energy in the world of about 29 GWe and 312 potential geothermal locations [3]. Geothermal wells in Sibayak (North Sumatera), Indonesia, belong to young stratovolcanoes and have operating temperatures varying from 36 °C at the near ground surface to 310 °C at the bottom of the well, which is liquid-dominated with acidic and saline properties [4, 5]. Therefore, this geothermal fluid creates an aggressive environment that is conducive to corrosion of the powerplant infrastructure. Parts of the geothermal powerplant infrastructure, such as pipelines and heat exchangers, are commonly made of metals, e.g. carbon steel and stainless steel. Consequently, they may undergo corrosion and scaling when exposed to the geothermal fluid, especially for carbon steel. To ensure the safety and longevity of a geothermal powerplant, the infrastructure is constructed of expensive corrosion resistant alloys [6–10], e.g., titanium and Ni-Cr based alloys, or carbon steel which needs to be protected by coatings or inhibitors. To address the corrosion of carbon steel in the geothermal environment, artificial geothermal water was used to simulate a geothermal well in Sibayak, Indonesia, with pH 4 and a saline composition of 1,500 mg/l Cl-, 20 mg/l SO42-, 15 mg/l HCO3-, 200 mg/l Ca2+, 250 mg/l K+, and 600 mg/l Na+. Carbon steel underwent the most severe corrosion at 150°C in an oxygen-containing solution with a corrosion rate of 0.34 mm/year, which is approximately ten times higher than that in the absence of dissolved oxygen. In all conditions, pitting corrosion was observed, which necessitate a protection strategy on carbon steel. In order to promote a cost effective and locally available option, this work focused on an easily applicable coating which utilized local resources. Toward developing such protective coating based on the locally available resources in Indonesia which can yield good corrosion resistance and thermal stability in geothermal environment, two additional components, i.e. polyaniline (PANI) and silicon dioxide, were used to modify an alkyd-based commercial coating. The selection of the alkyd-based coating as a matrix focused on the industrial convenience basis, where the coating application procedure should be simple and easy to apply within reasonable costs. The alkyd-based coating underwent severe blistering when exposed to the artificial geothermal water at 70 and 150°C due to the reaction between CaCO3 (as one of its components) and the artificial geothermal water, as well as a possible alkyd hydrolysis in the initial stage of exposure. In the oxygen-free solution, the degradation was controlled by chemical and thermal reactions, whereas in the aerated condition, oxidization at the coating surface further accelerated polymer degradation. PANI was chosen as one of the anticorrosion pigments which was widely developed over the past decades. To investigate the interaction between PANI and the artificial geothermal water, PANI film was electrochemically deposited on the carbon steel surface and exposed to the artificial geothermal water. Electrochemically synthesized oxalate-doped PANI was protective against corrosion of carbon steel in artificial geothermal water at room temperature. The mechanism involved an exchange of electroactive species within the coating layer, as confirmed by electrochemical impedance spectra. Interaction of ionic species, such as Cl-, Na+, Ca2+ from the artificial geothermal water, with the outer layer of PANI is suggested both at 25°C and 150°C, based on the EDX spectra of the coating surface after exposure to the artificial geothermal water. Thus, the protection mechanism of PANI is not solely based on the physical barrier layer properties, but rather associated with the redox mediated properties of PANI, which selectively allow ionic species intrusion from the electrolyte into the PANI layer. Although PANI is a promising candidate as an anticorrosion coating, its morphological characterization reveals that electrochemically deposited PANI is not stable for an application at 150°C. Therefore, another approach was used to promote better protective behavior of PANI by dispersing chemically synthesized PANI in the alkyd-based coating. To enhance the thermal stability of the coating, silicon dioxide (SiO2) was added, which was able to prolong the sustainability of coated metals until 28 days compared to the unmodified alkyd-based coating, which underwent a change in color to brown/orange only within 7 days of exposure. This improvement might be associated with the role of SiO2 to proportionate the thermal expansion coefficient of the coating system to be compatible with that of carbon steel. Although the coating is thermally enhanced, the electrolyte might still intrude through the coating resulting in the change of coating color after 28 days of exposure in the artificial geothermal water. When PANI was added, the coating system provided an active corrosion protection on the carbon steel surface. The chemical and morphological characterization of the PANI-alkyd and SiO2-alkyd coating system showed that coatings were improved, and no blisters were observed, albeit the degradation continued. Based on the results of exposure tests, the combined coating system was further investigated. The combinational coating of PANI/SiO2-alkyd was used with 2 wt% of PANI and 15 wt% of SiO2. Electrochemical tests indicated cathodic protection at 150°C, as the Ecorr of PANI/SiO2 remained approximately 400 mV lower than the carbon steel potential. The impedance spectra of the combinational coating of PANI/SiO2 showed a continuous decrease in the absolute impedance value over time. A significant decrease was observed within one day of exposure, followed by a slow gradual decrease, which might be associated with water absorption in the coating. FTIR spectra revealed that several peaks associated with the organic portion of the coatings were reduced after the specimens were exposed for 6 months. However, the absorption peaks related to the inorganic portion of the coatings remained stable until 6 months. Morphological characterization of the combinational coating of PANI/SiO2 showed that there were no blisters or significant discoloration of coatings after long-term exposure for 6 months in artificial geothermal water at 150°C, indicating that the chemical degradation does not significantly affect the functionality of the coating. This clearly shows the durability of PANI/SiO2 coating in the geothermal condition, suggesting that this coating can be used for such geothermal application. However, further testing of this coating should be conducted in a real geothermal environment on-site to ensure safety and viability. KW - Geothermal KW - Corrosion KW - Coating KW - Polyaniline KW - Electrochemical impedance spectroscopy PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:188-refubium-26704-6 UR - https://refubium.fu-berlin.de/handle/fub188/26704 DO - https://doi.org/10.17169/refubium-26461 SP - 1 EP - 175 CY - Berlin AN - OPUS4-51281 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hille, Falk A1 - Sowietzki, D. A1 - Makris, R. T1 - Luminescence-based early detection of fatigue cracks JF - Materials Today: Proceedings N2 - Classic non-destructive fatigue crack detection methods reveal the state of the fatigue damage evolution at the moment of application, generally not under operational conditions. The here introduced crack luminescence method realizes a clear visibility of the occurred and growing crack in loaded components during operation. Different established experiments show that due to the sensitive coating a crack Formation can be detected even in early stage under the premise the crack reached the surface. The coating consists of two layers with different properties and functions. The bottom layer emits light as fluorescence under UV radiation. The top layer covers the fluorescing one and prevents the emitting of light in case of no damage at the surface. In case of surface crack occurrence, the luminescent light is clearly noticeable by visual observations and also by standard camera equipment which makes automated crack detection possible as well. It is expected that crack luminescence can increase structural safety as well as reduce costs and time for inspections and preventive maintenance. KW - Coating KW - Fatigue KW - Crack damage detection KW - Luminescence PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-510517 DO - https://doi.org/10.1016/j.matpr.2020.02.338 SN - 2214-7853 SP - 1 EP - 5 PB - Elsevier CY - Amsterdam AN - OPUS4-51051 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Bäßler, Ralph T1 - Review: Corrosion‐Resistant Linings and Coatings T2 - Materials and Corrosion N2 - This book introduces to aspects to be considered when dealing with coatings and linings. Philip A. Schweitzer covers and compares a variety of specific coatings and their applications. In 18 chapters he divided the content into two main parts: linings and coatings. All professionals involved in design and maintenance processes get by this book a compact survey of necessary considerations which needs to be done when applying surface protection measures. The literature references at the end of some chapters support the readers finding additional information about the special topic, mainly written by the author himself. Since this newly issued paperback edition is a 1:1 re‐print of the 2001 hardcover version, neither current publications are referenced, nor revisions were made. KW - Corrosion KW - Lining KW - Coating KW - Elastomer PY - 2020 DO - https://doi.org/10.1002/maco.202070094 SN - 1521-4176 SN - 0947-5117 VL - 71 IS - 9 SP - 1592 EP - 1593 PB - WILEY‐VCH Verlag GmbH & Co. KGaA CY - Weinheim AN - OPUS4-51167 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Bäßler, Ralph T1 - Review: Corrosion of Linings and Coatings: Cathodic and Inhibitor Protection and Corrosion Monitoring T2 - Materials and Corrosion N2 - This paperback issue of the 2007 hardcover version within the “Corrosion Engineering Handbook” series presents various materials and methods for controlling and protecting against corrosion instead of using expensive alloys to construct a tank or processing vessel. This book is a very comprehensive collection of the current knowledge about applied linings and coatings. So, it fulfills its intension, “that regardless of what is being built, … information for … whoever is responsible for the selection of material of construction will be found in this book to enable them to avoid unnecessary loss of material through corrosion”, to a very large extent. KW - Corrosion KW - Coating KW - Lining KW - Cathodic protection PY - 2020 DO - https://doi.org/10.1002/maco.202070104 SN - 1521-4176 SN - 0947-5117 VL - 71 IS - 10 SP - 1756 EP - 1757 PB - WILEY‐VCH Verlag GmbH & Co. KGaA CY - Weinheim AN - OPUS4-51414 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Bäßler, Ralph T1 - Review: Advanced Coating Materials T2 - Materials and Corrosion N2 - This book by Scrivener Publishing contains 14 chapters written by 82 leading scientists, experienced in the field of coatings. They demonstrate mechanisms, usage and manipulation of cutting‐edge coating methods. Each chapter is well structured and ends with a conclusion, highlighting the content. The book is divided into 3 parts: “Materials and Methods”, “Coating Materials Nanotechnology” and “Advanced Coating Technology and Applications”. Finally, this book provides a comprehensive insight into innovative research in advanced coating materials and state‐of‐the‐art technologies, without being a real textbook. It fulfills its intension of being beneficial both for technicians and scientists. KW - Corrosion KW - Coating KW - Protection PY - 2020 DO - https://doi.org/10.1002/maco.202070044 SN - 1521-4176 SN - 0947-5117 VL - 71 IS - 4 SP - 675 EP - 676 PB - WILEY‐VCH Verlag GmbH & Co. KGaA CY - Weinheim AN - OPUS4-50629 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Bäßler, Ralph T1 - Review: Polymer Coatings ‐ A Guide to Chemistry, Characterization, and Selected Applications T2 - Materials and Corrosion N2 - This book grew out of a course on polymer coatings held by the author at the university. It shall serve as an introduction to the wide field of polymer coatings. It is not intended to cover completely all facts on polymer coatings. All chapters are well structured. Selected figures and formulas illustrate the content and contribute to a good understandability. At the end of each chapter some hints for further reading are provided. Finally, the book fulfills its intention to introduce into the topic by providing basics on science and technology of polymer coatings, suitable for chemists in industry, materials scientists, polymer chemists and physical chemists. KW - Corrosion KW - Coating KW - Polymer PY - 2020 DO - https://doi.org/10.1002/maco.202070024 SN - 1521-4176 SN - 0947-5117 VL - 71 IS - 2 SP - 321 EP - 322 PB - WILEY‐VCH Verlag GmbH & Co. KGaA CY - Weinheim AN - OPUS4-50374 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Morys, Michael A1 - Häßler, Dustin A1 - Krüger, Simone A1 - Schartel, Bernhard A1 - Hothan, Sascha T1 - Beyond the standard time-temperature curve: Assessment of intumescent coatings under standard and deviant temperature curves JF - Fire Safety Journal N2 - Nowadays there are intumescent coatings available for diverse applications. There is no established assessment of their protection performance besides the standard time-temperature curve, but natural fire scenarios often play an important role. A reliable straightforward performance-based assessment is presented. The effective thermal conductivity per thickness is calculated based on intermediate-scale fire tests. The optimum thermal insulation, the time to reach it, and the time until contingent failure of the coating are used for an assessment independent of the heating curve. The procedure was conducted on four different commercially intumescent coatings for steel construction, one solvent-based, one waterborne, one epoxy-based, and a bandage impregnated with a waterborne coating. The performance was studied under four different but similar shaped heating curves with different maximum temperatures (standard time-temperature curve, hydrocarbon curve and two self-designed curves with reduced temperature). The thermal protection performance is crucially affected by the residue morphology. Therefore, a comprehensive morphology analysis, including micro-computed tomography and scanning electron microscopy, was conducted on small-scale residues (7.5 x 7.5 cm2). Two different types of inner structures and the residue surface after different heat exposures were discussed in terms of their influence on thermal protection performance. KW - Intumescence KW - Coating KW - Computed tomography KW - Small scale KW - Heating curves KW - Residue morphology PY - 2020 DO - https://doi.org/10.1016/j.firesaf.2020.102951 SN - 0379-7112 VL - 112 SP - 102951 PB - Elsevier Ltd. AN - OPUS4-50334 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -