TY - JOUR A1 - Bücker, Michael A1 - Böcker, Wolfgang D. G. A1 - Reinsch, Stefan A1 - Unger, Brita T1 - Alternativer Holzschutz KW - Holzschutz KW - Kieselsol KW - Biozide KW - Sol-Gel-Prozess PY - 2004 SN - 1435-1854 IS - 11 SP - 77 EP - 80 PB - Verl. f. Fachpublizistik CY - Stuttgart AN - OPUS4-6333 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Dreßler, Martin A1 - Nofz, Marianne A1 - Malz, Frank A1 - Pauli, Jutta A1 - Jäger, Christian A1 - Reinsch, Stefan A1 - Scholz, G. T1 - Aluminum speciation and thermal evolution of aluminas resulting from modified Yoldas sols N2 - Aluminas resulting from sols prepared via a modified Yoldas procedure were studied with differential thermal analysis (DTA), differential thermal gravimetrie (DTG), 27Al nuclear magnetic resonance (27Al MAS NMR) and X-ray diffraction (XRD) concerning their thermal properties, aluminum speciation and phase content. Hydrolysis of aluminum-sec-butoxide in aluminum nitrate solutions allowed to prepare stable sols with varying NO3-/Al molar ratios, solids contents and pH values. Resulting sols contained different aluminum species including also Al13 polycations. Sol preparation conditions also determined aluminum speciation in solid products obtained after thermal treatments of gels obtained from these sols. Al13 polycations and AlO5 species were found to play an important role for thermally induced transformation from amorphous products via eta-Al2O3 to alpha-Al2O3. Intermediately formed eta-Al2O3 promotes the phase transformation to alpha-Al2O3. KW - Alumina KW - Modified Yoldas sols KW - 27Al nuclear magnetic resonance KW - Differential thermal analysis KW - X-ray diffraction PY - 2007 U6 - https://doi.org/10.1016/j.jssc.2007.06.018 SN - 0022-4596 SN - 1095-726X VL - 180 IS - 9 SP - 2409 EP - 2419 PB - Elsevier CY - San Diego, Calif. AN - OPUS4-16189 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Scholz, Philipp A1 - Wachtendorf, Volker A1 - Elert, Anna Maria A1 - Falkenhagen, Jana A1 - Becker, Roland A1 - Hoffmann, Katrin A1 - Resch-Genger, Ute A1 - Tschiche, Harald A1 - Reinsch, Stefan A1 - Weidner, Steffen ED - Scholz, Philipp T1 - Analytical toolset to characterize polyurethanes after exposure to artificial weathering under systematically varied moisture conditions N2 - Polyether and -ester urethanes (PU) were exposed to artificial weathering at 40 °C and artificial UV radiation in a weathering chamber. In 3 parallel exposures, humidity was varied between dry, humid, and wet conditions. Material alteration was investigated by various analytical techniques like size exclusion chromatography (SEC), liquid chromatography-infrared spectroscopy (LC-FTIR), thermal-desorption gas chromatography-mass spectrometry (TD-GC-MS), fluorescence mapping and dynamic mechanical analysis (DMA). Our results show that depending on the weathering conditions, different degradation effects can be observed. By means of SEC an initial strong decrease of the molar masses and a broadening of the mass distributions was found. After a material dependent time span this was followed by a plateau where molar mass changes were less significant. A minor moisture-dependent degradation effect was only found for polyester PU. Fluorescence measurements on two materials revealed an increase in the luminescence intensity upon weathering process reaching a saturation level after about 500 h. The changes in the optical properties observed after different exposure conditions and times were very similar. The TD-GC-MS data showed the fate of the stabilizers and antioxidant in the course of weathering. LC-FTIR measurements revealed a change in peak intensities and the ratio of urethane and carbonyl bands. KW - Polyurethane KW - Artificial weathering KW - Moisture KW - Crosslinking KW - Degradation PY - 2019 UR - https://www.sciencedirect.com/science/article/pii/S0142941819303708 U6 - https://doi.org/10.1016/j.polymertesting.2019.105996 SN - 0142-9418 VL - 78 SP - 105996, 1 EP - 9 PB - Elsevier CY - Amsterdam AN - OPUS4-48625 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kiefer, P. A1 - Maiwald, M. A1 - Deubener, J. A1 - Balzer, R. A1 - Behrens, H. A1 - Waurischk, Tina A1 - Reinsch, Stefan A1 - Müller, Ralf T1 - Automated Analysis of Slow Crack Growth in Hydrous Soda-Lime Silicate Glasses N2 - To explore the impact of ambient and structural water on static fatigue, the initiation and growth of 3279 Vickers induced median radial cracks were automatically recorded and analyzed. We find that humidity is more efficient in initiating cracks and promoting their growth than water, which is dissolved in the glass structure. In particular for slow crack growth (< 3x10-6 m s-1), tests in dry nitrogen showed a considerable decrease in the crack growth exponent with increasing water content of the glasses. On the other hand, if tests were performed in humid air, the crack growth exponent was independent of the water content of the hydrous glasses, while stress intensity decreased slightly. These observations indicate that water promotes the processes at the crack-tip regardless of its origin. However, ambient water is more efficient. KW - Indentation fracture toughness KW - Slow crack growth KW - Automated analysis KW - Hydrous glass KW - Vickers indentation PY - 2020 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-513085 VL - 7 SP - 268 AN - OPUS4-51308 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Dreßler, Martin A1 - Reinsch, Stefan A1 - Schadrack, Reinhard A1 - Benemann, Sigrid T1 - Burnout behavior of ceramic coated open cell polyurethane (PU) sponges N2 - Open cell rigid foams made from polyurethane (PU) are frequently used in ceramic processing for preparation of porous ceramics by the so-called replica technique. This work presents data regarding the PU burnout, shrinkage characteristics as well as the morphology of the ceramic coated PU sponges during heating up. Shrinkage of the ceramic coated PU sponges closely follows the mass loss due to PU decomposition. Two temperatures (i) 267 °C and (ii) 380 °C were identified at which PU decomposition reaches local maxima. Shrinkage measurements on ceramic coated PU sponges reveal that both PU decomposition stages lead to similar extends of shrinkage in the ceramic coated PU sponge. Differential thermal analysis (DTA) showed that the two decomposition related temperatures (267 and 380 °C) differ concerning the energy release. While the low-temperature signal is endothermic, an exothermic signal was detected at 380 °C. The morphology of the ceramic coated PU sponges was investigated with scanning electron microscopy (SEM) which gave insight into the formation of hollow ceramic struts-a well known feature of ceramics being prepared by the replica technique. KW - Polyurethane (PU) KW - Porous ceramics KW - Mass spectrometry KW - Thermal analysis PY - 2009 U6 - https://doi.org/10.1016/j.jeurceramsoc.2009.07.025 SN - 0955-2219 SN - 1873-619X VL - 29 IS - 16 SP - 3333 EP - 3339 PB - Elsevier CY - Oxford AN - OPUS4-20092 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Al-Terkawi, Abdal-Azim A1 - Scholz, G. A1 - de Oliveira Guilherme Buzanich, Ana A1 - Reinsch, Stefan A1 - Kemnitz, E. A1 - Emmerling, Franziska T1 - Ca- and Sr- tetrafluoroisophthalates: mechanochemical synthesis, characterization, and ab initio structure determination N2 - New fluorinated coordination polymers were prepared mechanochemically by milling the alkaline earth metal hydroxides MII(OH)2·xH2O (MII: Ca, Sr) with tetrafluoroisophthalic acid (H2mBDC-F4). The structures of [{Ca(mBDC-F4)(H2O)2}·H2O] and [{Sr(mBDC-F4)(H2O)2}·H2O] were determined based on ab initio calculations and their powder X-ray diffraction (PXRD) data. The compounds are isomorphous and crystallize in the orthorhombic space group P212121. The determined structures were validated by using extended X-ray absorption (EXAFS) data. The new materials were thoroughly characterized using elemental analysis, thermal analysis, magic angle spinning NMR, and attenuated total reflection-infrared spectroscopy. Further characterization methods such as BET, dynamic vapor sorption, and scanning electron microscopy imaging were also used. Our investigations indicate that mechanochemistry is an efficient method for preparing such materials. KW - Mechanochemistry KW - In situ KW - XRD KW - Coordination polymers PY - 2017 UR - http://pubs.rsc.org/-/content/articlehtml/2017/dt/c7dt00734e U6 - https://doi.org/10.1039/c7dt00734e VL - 46 IS - 18 SP - 6003 EP - 6012 AN - OPUS4-41516 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Unger, Brita A1 - Bücker, Michael A1 - Reinsch, Stefan A1 - Hübert, Thomas T1 - Chemical aspects of wood modification by sol-gel-derived silica N2 - It has been shown that tetraethoxysilane-derived precursors are suitable solutions for impregnating pine sapwood to improve its dimensional stability. Tailored sol–gel syntheses result in precursors with nano-scaled silica species which are able to penetrate into the cell walls of wood. The physical fixation of those species inside the cell walls was verified by ESEM/EDX investigations. There is evidence that the silica species are chemically bonded to wood components. Nonreacted alkoxy groups can exist in the wood composites after impregnation. The amount of these organic residues depends on the composition of the precursors, especially their condensation degree and reactivity. Treatments for finishing the composites after the impregnation step to get clean products and stable properties are discussed in this context. An explanation of the complex relationship between solids content in the impregnation solutions and percentage weight gain and bulking of the composites is given. It can be demonstrated that high WPG values (>20 %) are pre-conditions for an effective protection of the resulting composites but they only guarantee efficient improvements if connected with the incorporation of the inorganic component inside the cell walls. Therefore, the sol–gel syntheses have to be carried out in such a manner that very small (<2 nm) as well as reactive species are sufficiently available. This demands syntheses using sub-stoichiometric water contents (H2O/TEOS <4, better <2). KW - Silica-wood composites KW - Sol-gel derived precursors KW - Curing KW - Fixation of silica KW - Dimensional stability PY - 2013 U6 - https://doi.org/10.1007/s00226-012-0486-7 SN - 0043-7719 SN - 1432-5225 VL - 47 IS - 1 SP - 83 EP - 104 PB - Springer CY - Berlin AN - OPUS4-26258 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Waurischk, Tina A1 - Müller, Ralf A1 - Reinsch, Stefan A1 - Kiefer, P. A1 - Deubener, J. A1 - Balzer, R. A1 - Behrens, H. T1 - Crack Growth in Hydrous Soda-Lime Silicate Glass N2 - Stable crack growth was measured for nominal dry and water-bearing (6 wt%) soda-lime silicate glasses in double cantilever beam geometry and combined with DMA studies on the effects of dissolved water on internal friction and glass transition, respectively. In vacuum, a decreased slope of logarithmic crack growth velocity versus stress intensity factor is evident for the hydrous glass in line with an increase of b-relaxation intensity indicating more energy Dissipation during fracture. Further, inert crack growth in hydrous glass is found to be divided into sections of different slope, which indicates different water related crack propagation mechanism. In ambient air, a largely extended region II is observed for the hydrous glass, which indicates that crack growth is more sensitive to ambient water. KW - Internal friction KW - Soda-lime silicate glass KW - Water content KW - Stable crack growth KW - DCB geometry KW - Stress intensity factor PY - 2020 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-506829 VL - 7 SP - Articel 66 AN - OPUS4-50682 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Reinsch, Stefan A1 - Nascimento, M.L.F. A1 - Müller, Ralf A1 - Zanotto, E. D. T1 - Crystal growth kinetics in cordierite and diopside glasses in wide temperature ranges N2 - We measured and collected literature data for the crystal growth rate, u(T), of µ-cordierite (2MgO · 2Al2O3 · 5SiO2) and diopside (CaO · MgO · 2SiO2) in their isochemical glass forming melts. The data cover exceptionally wide temperature ranges, i.e. 800–1350 °C for cordierite and 750–1378 °C for diopside. The maximum of u(T) occurs at about 1250 °C for both systems. A smooth shoulder is observed around 970 °C for µ-cordierite. Based on measured and collected viscosity data, we fitted u(T) using standard crystal growth models. For diopside, the experimental u(T) fits well to the 2D surface nucleation model and also to the screw dislocation growth mechanism. However, the screw dislocation model yields parameters of more significant physical meaning. For cordierite, these two models also describe the experimental growth rates. However, the best fittings of u(T) including the observed shoulder, were attained for a combined mechanism, assuming that the melt/crystal interface growing from screw dislocations is additionally roughened by superimposed 2D surface nucleation at large undercoolings, starting at a temperature around the shoulder. The good fittings indicate that viscosity can be used to assess the transport mechanism that determines crystal growth in these two systems, from the melting point Tm down to about Tg, with no sign of a breakdown of the Stokes–Einstein/Eyring equation. KW - Crystal growth KW - Oxide glasses KW - Silicates KW - Kristallwachstumsgeschwindigkeit KW - Kinetik KW - Silikatgläser PY - 2008 U6 - https://doi.org/10.1016/j.jnoncrysol.2008.09.007 SN - 0022-3093 VL - 354 IS - 52-54 SP - 5386 EP - 5394 PB - North-Holland Publ. Co. CY - Amsterdam AN - OPUS4-18383 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Nagamine, K. A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Honma, T. A1 - Komatsu, T. T1 - Crystallization behavior of lithium iron phosphate glass powders in different atmospheres N2 - Crystallization behavior in different atmospheres (air, Ar, and 7% H2/Ar) of lithium iron phosphate glass (33Li2O–33Fe2O3–1Nb2O5–33P2O5 (LFNP)) powders with different sizes of 2–1000 µm was examined. The crystallization peak temperature (Tp) in Ar and 7% H2/Ar decreased with decreasing the particle size of glass powders, but the value of Tp in air was independent of particle size. The crystallized glass obtained by heating to Tp showed the formation of the α-Li3Fe2(PO4)3 and LiFePO4 crystalline phases. Fe2O3 crystals were formed only in the inside of crystallized glass plates in the heating in air. The crystallization of LiFePO4 was largely enhanced in the particle size of <2 µm during the heating in Ar and 7% H2/Ar atmospheres. The main crystallization mechanism in LFNP glass was found to be surface crystallization. Significant shrinkages were observed for glass compacts (pellets) in the heating in 7% H2/Ar. These results suggest that controlling particle sizes and atmospheres enables the design the morphology of LiFePO4 crystals in LFNP glass. KW - DTA KW - Kristallisation KW - Phasenentwicklung KW - Unterschiedliche Atmosphären KW - Lithiumionen-Batterie PY - 2011 U6 - https://doi.org/10.1111/j.1551-2916.2011.04579.x SN - 0002-7820 SN - 1551-2916 VL - 94 IS - 9 SP - 2890 EP - 2895 PB - Blackwell Publishing CY - Malden AN - OPUS4-24914 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -