TY - JOUR A1 - Chaudry, Mohsin A1 - Mohr, Gunther A1 - Hilgenberg, Kai T1 - Experimental and numerical comparison of heat accumulation during laser powder bed fusion of 316L stainless steel JF - Progress in Additive Manufacturing N2 - Heat accumulation during laser powder bed fusion (LPBF) of metallic build parts can adversely affect their microstructure and mechanical properties. To study the heat accumulation during 316L steel based parts manufactured by LPBF, a finite element method (FEM) based numerical study is carried out. For the investigation, a computationally efficient FEM based model, where the whole layer is simultaneously exposed to a heat source, is used. The simulation results are compared with experimental results to validate the numerical model. While considering different influencing factors such as volumetric energy density (VED) and inter-layer time (ILT), the FEM model is shown to successfully simulate the process of heat accumulation during LPBF based manufacturing of a cuboidal shaped geometry. It is shown that ILT and VED have a significant effect on heat accumulation. The validated numerical model provides a good basis for the optimization of processing parameters and geometries for a future investigation of a reduction of heat accumulation effects. Furthermore, it can be used to quickly provide preheating boundary conditions for detailed investigations by different model approaches at a finer scale for future studies. KW - Laser powder bed fusion KW - Finite element method KW - Heat accumulation KW - Inter-layer time PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-545115 DO - https://doi.org/10.1007/s40964-022-00282-x SP - 1 EP - 13 PB - Springer AN - OPUS4-54511 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Drendel, Jan A1 - Logvinov, Ruslan A1 - Heinrichsdorff, Frank A1 - Hilgenberg, Kai T1 - Simulation-based controlling of local surface temperature in laser powder bed fusion using the process laser JF - Additive Manufacturing N2 - State-of-the-art laser powder bed fusion (PBF-LB/M) machines allow pre-heating of the substrate plate to reduce stress and improve part quality. However, two major issues have been shown in the past: First, with increasing build height the apparent pre-heat temperature at the surface can deviate drastically from the nominal pre-heat temperature in the substrate plate. Second, even within a single layer the local surface pre-heat temperature can show large gradients due to thermal bottlenecks in the part geometry underneath the top surface. Both lead to unwanted changes in microstructure or defects in the final parts. In this study, a first attempt is taken to show the feasibility of pre-heating the top surface with the onboard laser beam to overcome the mentioned issues. A single layer of a group of three parts built from IN718 to a height of 33.5 mm is pre-heated in a commercially available PBF-LB/M machine to an average steady state surface temperature of 200 °C using the onboard laser beam. The parts are continuously heated, omitting powder deposition and melting step. Temperatures are measured by thermocouples underneath the surface. The experiments are supported by a thermal finite element (FE) model that predicts the temperature field in the parts. When heating the parts uniformly with the laser beam, differences in surface temperatures as large as 170 K are observed. To overcome this inhomogeneity, the heat flux supplied by the laser beam is modulated. An optimized, spatial heat flow distribution is provided by the thermal FE model and translated into a scan pattern that reproduces the optimized heat distribution on the PBF-LB/M machine by locally modulating hatch distance and scan velocity. This successfully reduces the differences in surface temperature to 20 K. Thermographic imaging shows that a homogeneous surface temperature can be achieved despite the localized heat input by the beam. The potential for industrial application of the optimized laser-heating technique is discussed. KW - Additive Manufacturing KW - Simulation KW - Surface temperature KW - Laser powder bed fusion PY - 2023 DO - https://doi.org/10.1016/j.addma.2023.103854 SN - 2214-8604 VL - 78 SP - 1 EP - 16 PB - Elsevier B.V. AN - OPUS4-58825 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ehlers, Henrik A1 - Pelkner, Matthias A1 - Thewes, R. T1 - Heterodyne Eddy Current Testing Using Magnetoresistive Sensors for Additive Manufacturing Purposes JF - IEEE Sensors Journal N2 - In recent years additive manufacturing technologies have become widely popular. For complex functional components or low volume production of workpieces, laser powder bed fusion can be used. High safety requirements, e.g. in the aerospace sector, demand extensive quality control. Therefore, offline non-destructive testing methods like computed tomography are used after manufacturing. Recently, for enhanced profitability and practicality online non-destructive testing methods, like optical tomography have been developed. This paper discusses the applicability of eddy current testing with magnetoresistive sensors for laser powder bed fusion parts. For this purpose, high spatial resolution giant magnetoresistance arrays are utilized for testing in combination with a single wire excitation coil. A heterodyne principle minimizes metrology efforts. This principle is compared to conventional signal processing in an eddy current testing setup using an aluminum test sample with artificial surface defects. To evaluate the influence of the powder used in the manufacturing process on eddy current testing and vice versa, a laser powder bed fusion mock-up made from stainless steel powder (316L) is used with artificial surface defects down to 100 µm. This laser powder bed fusion specimen was then examined using eddy current testing and the underlying principles. KW - Eddy current testing KW - Heterodyning KW - Laser powder bed fusion KW - Giant magnetoresistance KW - Additive manufacturing KW - 316L PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-506140 DO - https://doi.org/10.1109/JSEN.2020.2973547 SN - 1530-437X VL - 20 IS - 11 SP - 5793 EP - 5800 PB - IEEE AN - OPUS4-50614 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ehlers, Henrik A1 - Thewes, R. A1 - Pelkner, Matthias T1 - Online Process Monitoring for Additive Manufacturing Using Eddy Current Testing With Magnetoresistive Sensor Arrays JF - IEEE Sensors Journal N2 - The rising popularity of additive manufacturing processes leads to an increased interest in possibilities and methods for related process monitoring. Such methods ensure improved process quality and increase the understanding of the manufacturing process, which in turn is the basis for stable component quality, e.g., required in the aerospace industry or in the medical sector. For laser powder bed fusion, a handful of process monitoring tools already exist, such as optical tomography, thermography, pyrometry, imaging, or laser power monitoring. Although these tools provide helpful information about the process, more information is required for an accurate in-depth understanding. In this article, advanced approaches in eddy current testing (ET) are combined, such as single wire excitation, magnetoresistive (MR) sensor arrays, and heterodyning to build up a system that can be used for online process monitoring of laser powder bed fusion. In addition to detailed information about the developed ET system and underlying signal processing, the first results of magnetoresistance-basedonline ET during the laser powder fusion process are presented. While producing a step-shaped cuboid, each layer is tested during recoating. Test results show that not only the contours of the topmost layer are detected but also the contours of previous layers covered by powder. At an excitation frequency of 1 MHz, a penetration depth of approx. 400 μm is obtained. To highlight the possibilities of ET for online process monitoring of laser powder bed fusion, results are compared with postexposure images of the integrated layer control system (LCS). KW - Process monitoring KW - Eddy current testing KW - Giant magneto resistance (GMR) KW - Additive manufacturing KW - Laser powder bed fusion PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-560881 DO - https://doi.org/10.1109/JSEN.2022.3205177 VL - 22 IS - 20 SP - 19293 EP - 19300 PB - IEEE CY - New York, NY AN - OPUS4-56088 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Fritsch, Tobias A1 - Farahbod-Sternahl, L. A1 - Serrano Munoz, Itziar A1 - Léonard, F. A1 - Haberland, C. A1 - Bruno, Giovanni T1 - 3D Computed Tomography Quantifies the Dependence of Bulk Porosity, Surface Roughness, and Re-Entrant Features on Build Angle in Additively Manufactured IN625 Lattice Struts JF - Advanced Engineering Materials N2 - Layer-by-layer additive manufacturing (AM) by means of laser-powder bed Fusion (L-PBF) offers many prospects regarding the design of lattice structures used, for example, in gas turbines. However, defects such as bulk porosity, Surface roughness, and re-entrant features are exacerbated in nonvertical structures, such as tilted struts. The characterization and quantification of these kinds of defects are essential for the correct estimation of fracture and fatigue properties. Herein, cylindrical struts fabricated by L-PBF are investigated by means of X-ray computed tomography (XCT), with the aim of casting light on the dependence of the three kinds of defects (bulk porosity, surface roughness, and re-entrant features) on the build angle. Innovative analysis methods are proposed to correlate shape and position of pores, to determine the angular-resolved Surface roughness, and to quantify the amount of re-entrant surface features, q. A meshing of the XCT surface enables the correlation of q with the classical Surface roughness Pa. This analysis leads to the conclusion that there is a linear correlation between q and Pa. However, it is conjectured that there must be a threshold of surface roughness, below which no re-entrant features can be build. KW - Additive manufacturing KW - Laser powder bed fusion KW - Computed tomography KW - Surface roughness analysis KW - Re-entrant surface feature PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-534728 DO - https://doi.org/10.1002/adem.202100689 IS - 2100689 SP - 1 EP - 8 PB - Wiley-VCH Verlag AN - OPUS4-53472 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Fritsch, Tobias A1 - Sprengel, Maximilian A1 - Evans, Alexander A1 - Farahbod-Sternahl, L. A1 - Saliwan Neumann, Romeo A1 - Hofmann, M. A1 - Bruno, Giovanni T1 - On the determination of residual stresses in additively manufactured lattice structures JF - Journal of Applied Crystallography N2 - The determination of residual stresses becomes more complicated with increasing complexity of the structures investigated. Additive manufacturing techniques generally allow the production of ‘lattice structures’ without any additional manufacturing step. These lattice structures consist of thin struts and are thus susceptible to internal stress-induced distortion and even cracks. In most cases, internal stresses remain locked in the structures as residual stress. The determination of the residual stress in lattice structures through nondestructive neutron diffraction is described in this work. It is shown how two difficulties can be overcome: (a) the correct alignment of the lattice structures within the neutron beam and (b) the correct determination of the residual stress field in a representative part of the structure. The magnitude and the direction of residual stress are discussed. The residual stress in the strut was found to be uniaxial and to follow the orientation of the strut, while the residual stress in the knots was more hydrostatic. Additionally, it is shown that strain measurements in at least seven independent directions are necessary for the estimation of the principal stress directions. The measurement directions should be chosen according to the sample geometry and an informed choice on the possible strain field. If the most prominent direction is not measured, the error in the calculated stress magnitude increases considerably. KW - Additive manufacturing KW - Laser powder bed fusion KW - Residual stress KW - Principal stress components KW - Neutron diffraction KW - Lattice structures PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-520663 DO - https://doi.org/10.1107/S1600576720015344 SN - 1600-5767 VL - 54 SP - 228 EP - 236 AN - OPUS4-52066 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kempf, A. A1 - Hilgenberg, Kai T1 - Influence of heat treatments on AlSi10Mg specimens manufactured with different laser powder bed fusion machines JF - Materials Science & Engineering A N2 - Mechanical properties such as ultimate tensile strength, yield strength, and tensile elongation of parts manufactured with Laser Powder Bed Fusion (L-PBF) can differ significantly after the building process limiting the advantage of production flexibility of that technology. At this background, the present work investigated the influence of post process heat treatments (HT) on microstructure, hardness, and tensile properties of AlSi10Mg specimens in different As-built (AB) conditions. For this purpose, two superordinate aspects were covered within this study. Firstly, various HTs were performed on specimens built-up with the same L-PBF machine applying the same parameter set-up. Results of tensile tests and hardness measurements were discussed considering the microstructural changes examined with scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy as well as X-ray diffraction, and gathered in a material data map. Based on the observed microstructural changes and a calculated quality index which comprises strength and ductility properties, three HTs were selected for the second part of this work. Therein, the effect of these HTs on specimens fabricated with overall three L-PBF machines working with different raw materials, process parameters, and build-up strategies was studied. Specimens characterization included porosity measurements, the evaluation of material defects, microstructure analysis via SEM, hardness measurements, and tensile tests. It was found that strength properties in the AB condition revealed appreciable deviations: Values of yield strength and ultimate tensile strength were from 228 to 292 MPa and from 346 to 484 MPa, respectively. Whereas heat treated specimens at 300 °C for 0.5 as well as 2 h only exhibited slight differences in strength, a complete homogenization of strength properties was obtained after conducting a T6 HT. Nevertheless, ductility was not homogenized after heat treating caused by the presence of material defects such as keyhole pores and lack of fusion defects. It was shown that even slight differences in porosity determined in cross-sections can significantly affect ductility properties. KW - Laser powder bed fusion PY - 2021 DO - https://doi.org/10.1016/j.msea.2021.141371 SN - 0921-5093 VL - 818 SP - 141371 PB - Elsevier B.V. CY - Berlin AN - OPUS4-52741 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kempf, A. A1 - Hilgenberg, Kai T1 - Influence of sub-cell structure on the mechanical properties of AlSi10Mg manufactured by laser powder bed fusion JF - Materials Science & Engineering A N2 - AlSi10Mg is one of the most applied alloys for laser powder bed fusion (LPBF) technology, due to its great possibilities for implementing new lightweight concepts such as in automotive industries. For the component design it is necessary to know about the mechanical properties and the mechanical behaviour. The many published strength properties of LPBF processed AlSi10Mg show significant differences up to approximately 225 MPa in ultimate tensile strength (UTS) and 195 MPa in yield strength (YS). To understand these varying properties, a ring trial was carried out manufacturing specimens on 6 LPBF machines with different parameters and build-up strategies. They were studied in the as-built (AB) condition and after heat treatment at 300 °C for 30 min, respectively. For examining the mechanical properties, tensile tests and hardness measurements were carried out. The microstructure was characterized by optical light microscopy (OM), field emission scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDX), X-ray diffraction (XRD) and electron backscatter diffraction (EBSD). The identified differences in strength properties were discussed based on the 4 strengthening mechanism known for metallic materials and at the background of material defects. It was found that the size of the typical sub-cell structure of LPBF AlSi10Mg affected substantially the mechanical properties in the AB condition, in which with decreasing sub-cell size strength increased. If heat treatment was applied, the strength properties decreased and did not differ anymore. Since annealing led to coarsened sub-cells, whereas the grains itself did not change in size, the influence of sub-cell structure on strength was further confirmed. In addition, acicular precipitates in the AB condition were observed at specimens from one LPBF machine showing the lowest tensile elongation. KW - Laser powder bed fusion KW - AlSi10Mg KW - Mechanical properties KW - Microstructure PY - 2020 DO - https://doi.org/10.1016/j.msea.2020.138976 VL - 776 SP - Paper 138976, 12 PB - Elsevier B.V. AN - OPUS4-50316 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kempf, Andreas A1 - Kruse, Julius A1 - Madia, Mauro A1 - Hilgenberg, Kai T1 - Correlation between quasistatic und fatigue properties of additively manufactured AlSi10Mg using Laser Powder Bed Fusion JF - Procedia Structural Integrity N2 - In order to find a resource efficient approach for the fatigue lifetime prediction of laser powder bed fusion (L-PBF) processed AlSi10Mg material, results of tensile and fatigue tests were compared. The specimens were manufactured with three different L-PBF machines and studied in different heat treatment conditions (as-built, annealed, T6 heat treated). The investigations showed that the high attainable tensile strength properties after the manufacturing process are not beneficial in the high cycle fatigue (HCF) regime. In contrast, the applied heat treatments, which lead typically to a decrease of ultimate tensile strength, improved dramatically the fatigue behavior. Additionally, a clear correlation between the elongation at fracture and HCF resistance has been found for individual heat treatment conditions. This empiric relationship provides an estimation of the fatigue resistance in the presence of material defects and can be implemented in part and process approvals. T2 - FATIGUE DESIGN 2021 CY - Online meeting DA - 17.11.2021 KW - Additive Manufacturing KW - Laser powder bed fusion KW - AlSi10Mg KW - Tensile properties KW - Fatigue properties PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-544921 DO - https://doi.org/10.1016/j.prostr.2022.03.009 SN - 2452-3216 VL - 38 SP - 77 EP - 83 PB - Elsevier B.V. AN - OPUS4-54492 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Khimich, M. A. A1 - Prosolov, K. A. A1 - Mishurova, Tatiana A1 - Evsevleev, Sergei A1 - Monforte, X. A1 - Teuschl, A. H. A1 - Slezak, P. A1 - Ibragimov, E. A. A1 - Saprykin, A. A. A1 - Kovalevskaya, Z. G. A1 - Dmitriev, A. I. A1 - Bruno, Giovanni A1 - Sharkeev, Y. P. T1 - Advances in Laser Additive Manufacturing of Ti-Nb Alloys: From Nanostructured Powders to Bulk Objects JF - Nanomaterials N2 - The additive manufacturing of low elastic modulus alloys that have a certain level of porosity for biomedical needs is a growing area of research. Here, we show the results of manufacturing of porous and dense samples by a laser powder bed fusion (LPBF) of Ti-Nb alloy, using two distinctive fusion strategies. The nanostructured Ti-Nb alloy powders were produced by mechanical alloying and have a nanostructured state with nanosized grains up to 90 nm. The manufactured porous samples have pronounced open porosity and advanced roughness, contrary to dense samples with a relatively smooth surface profile. The structure of both types of samples after LPBF is formed by uniaxial grains having micro- and nanosized features. The inner structure of the porous samples is comprised of an open interconnected system of pores. The volume fraction of isolated porosity is 2 vol. % and the total porosity is 20 vol. %. Cell viability was assessed in vitro for 3 and 7 days using the MG63 cell line. With longer culture periods, cells showed an increased cell density over the entire surface of a porous Ti-Nb sample. Both types of samples are not cytotoxic and could be used for further in vivo studies. KW - Additive manufacturing KW - Biomaterials KW - Ti-Nb alloy KW - Nanostructured powder KW - Laser methods KW - Powder methods KW - Laser powder bed fusion PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-525344 DO - https://doi.org/10.3390/nano11051159 VL - 11 IS - 5 SP - 1159 PB - MDPI AN - OPUS4-52534 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Merz, Benjamin A1 - Nilsson, R. A1 - Garske, C. A1 - Hilgenberg, Kai T1 - Camera-based high precision position detection for hybrid additive manufacturing with laser powder bed fusion JF - The International Journal of Advanced Manufacturing Technology (JAMT) N2 - Additive manufacturing (AM) in general and laser powder bed fusion (PBF-LB/M) in particular are becoming increasingly important in the field of production technologies. Especially the high achievable accuracies and the great freedom in design make PBF-LB/M interesting for the manufacturing and repair of gas turbine blades. Part repair involves building AM-geometries onto an existing component. To minimise the offset between component and AM-geometry, a precise knowledge of the position of the component in the PBF-LB/M machine is mandatory. However, components cannot be inserted into the PBF-LB/M machine with repeatable accuracy, so the actual position will differ for each part. For an offset-free build-up, the actual position of the component in the PBF-LB/M machine has to be determined. In this paper, a camera-based position detection system is developed considering PBF-LB/M constraints and system requirements. This includes finding an optimal camera position considering the spatial limitations of the PBF-LB/M machine and analysing the resulting process coordinate systems. In addition, a workflow is developed to align different coordinate systems and simultaneously correct the perspective distortion in the acquired camera images. Thus, position characteristics can be determined from images by image moments. For this purpose, different image segmentation algorithms are compared. The precision of the system developed is evaluated in tests with 2D objects. A precision of up to 30μm in translational direction and an angular precision of 0.021∘ is achieved. Finally, a 3D demonstrator was built using this proposed hybrid strategy. The offset between base component and AM-geometry is determined by 3D scanning and is 69μm. KW - Laser powder bed fusion KW - Additive manufacturing KW - Hybrid repair KW - Machine vision KW - Image processing KW - Position detection PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-568583 DO - https://doi.org/10.1007/s00170-022-10691-5 SP - 1 EP - 16 PB - Springer AN - OPUS4-56858 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mishurova, Tatiana A1 - Artzt, K. A1 - Haubrich, J. A1 - Evsevleev, Sergei A1 - Evans, Alexander A1 - Meixner, M. A1 - Serrano Munoz, Itziar A1 - Sevostianov, I. A1 - Requena, G. A1 - Bruno, Giovanni T1 - Connecting Diffraction-Based Strain with Macroscopic Stresses in Laser Powder Bed Fused Ti-6Al-4V JF - Metallurgical and Materials Transactions A N2 - The laser powder bed fusion (LPBF) production process often results in large residual stress (RS) in the parts. Nondestructive techniques to determine RS are badly needed. However, a reliable quantification of macro-RS (i.e., stress at the component level) by means of diffraction-based techniques is still a great challenge, because the link between diffraction-based strain and macro-RS is not trivial. In this study, we experimentally determine (by means of in-situ synchrotron radiation diffraction) this link for LPBF Ti-6Al-4V. We compare our results with commonly used models to determine the so-called diffraction elastic constants (DECs). We show that LPBF materials possess different DECs than wrought alloys, simply because their microstructural and mechanical properties are different. We also show that the existing models can be used to calculate DECs only if high accuracy of the RS values is not required. If the peculiarities of the microstructure have to be taken into account (as is the case of additively manufactured materials), a radically new approach is desirable. KW - Tiatanium KW - Synchrotron X-ray diffraction KW - Macroscopic stress KW - Laser powder bed fusion KW - Texture KW - Diffraction elastic constants PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-506483 DO - https://doi.org/10.1007/s11661-020-05711-6 VL - 51 IS - 6 SP - 3194 EP - 3204 PB - Springer AN - OPUS4-50648 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mishurova, Tatiana A1 - Evsevleev, Sergei A1 - Piault, Pierre A1 - King, Andrew A1 - Henry, Laura A1 - Bruno, Giovanni T1 - Understanding the hot isostatic pressing efectiveness of laser powder bed fusion Ti‑6Al‑4V by in‑situ X‑ray imaging and difraction experiments JF - Scientific reports N2 - In the present study, in-situ observation of Hot Isostatic Pressure (HIP) procedure of laser powder bed fusion manufactured Ti-6Al-4V parts was performed to quantitatively estimate the densifcation rate of the material and the infuence of the defect initial size and shape on such rate. The observations were performed in-situ using the Ultrafast Tomography Paris-Edinburgh Cell and the combination of fast phase-contrast synchrotron X-ray tomography and energy dispersive difraction. With this strategy, we could quantify how the efectiveness of HIP depends on the characteristics of a defect. Smaller defects showed a higher densifcation rate, while the defect shape did not have signifcant efect on such rate. KW - Additive manufacturing KW - Laser powder bed fusion KW - X-ray computed tomography KW - Hot isostatic pressing PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-587702 DO - https://doi.org/10.1038/s41598-023-45258-1 SN - 2045-2322 VL - 13 IS - 1 SP - 1 EP - 11 AN - OPUS4-58770 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mohr, Gunther A1 - Sommer, Konstantin A1 - Knobloch, Tim A1 - Altenburg, Simon A1 - Recknagel, Sebastian A1 - Bettge, Dirk A1 - Hilgenberg, Kai T1 - Process Induced Preheating in Laser Powder Bed Fusion Monitored by Thermography and Its Influence on the Microstructure of 316L Stainless Steel Parts JF - Metals N2 - Undetected and undesired microstructural variations in components produced by laser powder bed fusion are a major challenge, especially for safety-critical components. In this study, an in-depth analysis of the microstructural features of 316L specimens produced by laser powder bed fusion at different levels of volumetric energy density and different levels of inter layer time is reported. The study has been conducted on specimens with an application relevant build height (>100 mm). Furthermore, the evolution of the intrinsic preheating temperature during the build-up of specimens was monitored using a thermographic in-situ monitoring set-up. By applying recently determined emissivity values of 316L powder layers, real temperatures could be quantified. Heat accumulation led to preheating temperatures of up to about 600 °C. Significant differences in the preheating temperatures were discussed with respect to the individual process parameter combinations, including the build height. A strong effect of the inter layer time on the heat accumulation was observed. A shorter inter layer time resulted in an increase of the preheating temperature by more than a factor of 2 in the upper part of the specimens compared to longer inter layer times. This, in turn, resulted in heterogeneity of the microstructure and differences in material properties within individual specimens. The resulting differences in the microstructure were analyzed using electron back scatter diffraction and scanning electron microscopy. Results from chemical analysis as well as electron back scatter diffraction measurements indicated stable conditions in terms of chemical alloy composition and austenite phase content for the used set of parameter combinations. However, an increase of the average grain size by more than a factor of 2.5 could be revealed within individual specimens. Additionally, differences in feature size of the solidification cellular substructure were examined and a trend of increasing cell sizes was observed. This trend was attributed to differences in solidification rate and thermal gradients induced by differences in scanning velocity and preheating temperature. A change of the thermal history due to intrinsic preheating could be identified as the main cause of this heterogeneity. It was induced by critical combinations of the energy input and differences in heat transfer conditions by variations of the inter layer time. The microstructural variations were directly correlated to differences in hardness. KW - Additive manufacturing KW - Laser powder bed fusion KW - In-situ process monitoring KW - Thermography KW - Heat accumulation KW - Inter layer time KW - Cellular substructure PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-529240 DO - https://doi.org/10.3390/met11071063 VL - 11 IS - 7 SP - 1063 PB - MDPI CY - Basel, Schweiz AN - OPUS4-52924 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Nadammal, Naresh A1 - Mishurova, Tatiana A1 - Fritsch, Tobias A1 - Serrano Munoz, Itziar A1 - Kromm, Arne A1 - Haberland, C. A1 - Portella, Pedro Dolabella A1 - Bruno, Giovanni T1 - Critical role of scan strategies on the development of microstructure, texture, and residual stresses during laser powder bed fusion additive manufacturing JF - Additive Manufacturing N2 - Laser based powder bed fusion additive manufacturing offers the flexibility to incorporate standard and userdefined scan strategies in a layer or in between the layers for the customized fabrication of metallic components. In the present study, four different scan strategies and their impact on the development of microstructure, texture, and residual stresses in laser powder bed fusion additive manufacturing of a nickel-based superalloy Inconel 718 was investigated. Light microscopy, scanning electron microscopy combined with electron backscatter diffraction, and neutron diffraction were used as the characterization tools. Strong textures with epitaxially grown columnar grains were observed along the build direction for the two individual scan strategies. Patterns depicting the respective scan strategies were visible in the build plane, which dictated the microstructure development in the other planes. An alternating strategy combining the individual strategies in the successive layers and a 67◦ rotational strategy weakened the texture by forming finer microstructural features. Von Mises equivalent stress plots revealed lower stress values and gradients, which translates as lower distortions for the alternating and rotational strategies. Overall results confirmed the scope for manipulating the microstructure, texture, and residual stresses during laser powder bed fusion additive manufacturing by effectively controlling the scan strategies. KW - Additive manufacturing KW - Laser powder bed fusion KW - Nickel-based superalloys KW - Scan strategies KW - Residual stresses KW - Microstructure and texture PY - 2021 DO - https://doi.org/10.1016/j.addma.2020.101792 VL - 38 SP - 1792 PB - Elsevier B.V. AN - OPUS4-51944 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pauzon, C. A1 - Mishurova, Tatiana A1 - Fischer, M. A1 - Ahlström, J. A1 - Fritsch, Tobias A1 - Bruno, Giovanni A1 - Hryha, Eduard T1 - Impact of contour scanning and helium-rich process gas on performances of Alloy 718 lattices produced by laser powder bed fusion JF - Materials & Design N2 - Contour scanning and process gas type are process parameters typically considered achieving second order effects compared to first order factors such as laser power and scanning speed. The present work highlights that contour scanning is crucial to ensure geometrical accuracy and thereby the high performance under uniaxial compression of complex Alloy 718 lattice structures. Studies of X-ray computed tomography visualizations of as-built and compression-strained structures reveal the continuous and smooth bending and compression of the walls, and the earlier onset of internal contact appearance in the denser lattices printed with contour. In contrast, the effect of addition of He to the Ar process gas appears to have limited influence on the mechanical response of the lattices and their microstructure as characterized by electron backscattered diffraction. However, the addition of He proved to significantly enhance the cooling rate and to reduce the amount of the generated spatters as evidenced by in situ monitoring of the process emissions, which is very promising for the process stability and powder reusability during laser powder bed fusion. KW - Additive manufacturing KW - Laser powder bed fusion KW - Gyroid lattice KW - Process atmosphere PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-546632 DO - https://doi.org/10.1016/j.matdes.2022.110501 SN - 0264-1275 VL - 215 SP - 110501 PB - Elsevier Ltd. AN - OPUS4-54663 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Poka, Konstantin A1 - Ali, Sozol A1 - Saeed, Waleed A1 - Merz, Benjamin A1 - Epperlein, Martin A1 - Hilgenberg, Kai T1 - Design and implementation of a machine log for PBF-LB/M on basis of IoT communication architectures and an ETL pipeline JF - Progress in Additive Manufacturing N2 - AbstractPowder Bed Fusion with Laser Beam of Metals (PBF-LB/M) has gained more industrial relevance and already demonstrated applications at a small series scale. However, its widespread adoption in various use cases faces challenges due to the absence of interfaces to established Manufacturing Execution Systems (MES) that support customers in the predominantly data-driven quality assurance. Current state-of-the-art PBF-LB/M machines utilize communication architectures, such as OPC Unified Architecture (OPC UA), Message Queuing Telemetry Transport (MQTT) and Representational State Transfer Application Programming Interface (REST API). In the context of the Reference Architecture Model Industry 4.0 (RAMI 4.0) and the Internet of Things (IoT), the assets, particularly the physical PBF-LB/M machines, already have an integration layer implemented to communicate data such as process states or sensor values. Missing is an MES component acting as a communication and information layer. To address this gap, the proposed Extract Transform Load (ETL) pipeline aims to extract relevant data from the fabrication of each build cycle down to the level of scan vectors and additionally to register process signals. The suggested data schema for archiving each build cycle adheres to all terms defined by ISO/TC 261—Additive Manufacturing (AM). In relation to the measurement frequency, all data are reorganized into entities, such as the AM machine, build cycle, part, layer, and scan vector. These scan vectors are stored in a runtime-independent format, including all metadata, to be valid and traceable. The resulting machine log represents a comprehensive documentation of each build cycle, enabling data-driven quality assurance at process level. KW - FAIR data KW - Data-driven quality assurance KW - Laser powder bed fusion PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-601256 DO - https://doi.org/10.1007/s40964-024-00660-7 SN - 2363-9512 SP - 1 EP - 12 PB - Springer Science and Business Media LLC AN - OPUS4-60125 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Jakob A1 - Evans, Alexander A1 - Polatidis, E. A1 - Čapek, J. A1 - Mohr, Gunther A1 - Serrano Munoz, Itziar A1 - Bruno, Giovanni T1 - Understanding the impact of texture on the micromechanical anisotropy of laser powder bed fused Inconel 718 JF - Journal of materials science N2 - The manufacturability of metallic alloys using laser-based additive manufacturing methods such as laser powder bed fusion has substantially improved within the last decade. However, local melting and solidification cause hierarchically structured and crystallographically textured microstructures possessing large residual stress. Such microstructures are not only the origin of mechanical anisotropy but also pose metrological challenges for the diffraction-based residual stress determination. Here we demonstrate the influence of the build orientation and the texture on the microstructure and consequently the mechanical anisotropy of as-built Inconel 718. For this purpose, we manufactured specimens with [001]/[011]-, [001]- and [011]/[111]-type textures along their loading direction. In addition to changes in the Young’s moduli, the differences in the crystallographic textures result in variations of the yield and ultimate tensile strengths. With this in mind, we studied the anisotropy on the micromechanical scale by subjecting the specimens to tensile loads along the different texture directions during in situ neutron diffraction experiments. In this context, the response of multiple lattice planes up to a tensile strain of 10% displayed differences in the load partitioning and the residual strain accumulation for the specimen with [011]/[111]-type texture. However, the relative behavior of the specimens possessing an [001]/[011]- and [001]-type texture remained qualitatively similar. The consequences on the metrology of residual stress determination methods are discussed. KW - Laser powder bed fusion KW - Additive manufacturing KW - Electron backscatter diffraction KW - Tensile testing KW - Diffraction PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-555840 DO - https://doi.org/10.1007/s10853-022-07499-9 SN - 1573-4803 VL - 2022 IS - 57 SP - 15036 EP - 15058 PB - Springer Science + Business Media B.V. CY - Dordrecht AN - OPUS4-55584 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Serrano Munoz, Itziar A1 - Evans, Alexander A1 - Mishurova, Tatiana A1 - Sprengel, Maximilian A1 - Pirling, T. A1 - Kromm, Arne A1 - Bruno, Giovanni T1 - The importance of subsurface residual stress in laser powder bed fusion IN718 JF - Advanced engineering materials N2 - The residual stress (RS) in laser powder bed fusion (LPBF) IN718 alloy samples produced using a 67°-rotation scan strategy is investigated via laboratory X-ray diffraction (XRD) and neutron diffraction (ND). The location dependence of the strain-free (d₀) lattice spacing in ND is evaluated using a grid array of coupons extracted from the far-edge of the investigated specimen. No compositional spatial variation is observed in the grid array. The calculated RS fields show considerable non-uniformity, significant stress gradients in the region from 0.6 to 2 mm below the surface, as well as subsurface maxima that cannot be accounted for via XRD. It is concluded that failure to determine such maxima would hamper a quantitative determination of RS fields by means of the stress balance method. KW - Laser powder bed fusion KW - Neutron and X-ray diffraction KW - Residual stress analysis KW - Strain-free lattice references KW - Stress balance PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-532707 DO - https://doi.org/10.1002/adem.202100895 SN - 1615-7508 SN - 1527-2648 VL - 24 IS - 6 SP - 1 EP - 7 PB - Wiley-VCH CY - Weinheim AN - OPUS4-53270 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sonntag, Nadja A1 - Piesker, Benjamin A1 - Ávila Calderón, Luis Alexander A1 - Mohr, Gunther A1 - Rehmer, Birgit A1 - Agudo Jácome, Leonardo A1 - Hilgenberg, Kai A1 - Evans, Alexander A1 - Skrotzki, Birgit T1 - Tensile and Low‐Cycle Fatigue Behavior of Laser Powder Bed Fused Inconel 718 at Room and High Temperature JF - Advanced Engineering Materials N2 - This study investigates the room‐ and high‐temperature (650 °C) tensile and low‐cycle‐fatigue behavior of Inconel 718 produced by laser powder bed fusion (PBF‐LB/M) with a four‐step heat treatment and compares the results to the conventional wrought material. The microstructure after heat treatment is characterized on different length scales. Compared to the wrought variant, the elastic and yield properties are comparable at both test temperatures while tensile strength, ductility, and strain hardening capacity are lower. The fatigue life of the PBF‐LB/M variant at room temperature is slightly lower than that of the wrought material, while at 650 °C, it is vice versa. The cyclic stress response for both material variants is characterized by cyclic softening, which is more pronounced at the higher test temperature. High strain amplitudes (≥0.7%) at room temperature and especially a high testing temperature result in the formation of multiple secondary cracks at the transitions of regions comprising predominantly elongated grain morphology and columns of stacked grains with ripple patterns in the PBF‐LB/M material. This observation and pronounced crack branching and deflection indicate that the cracks are controlled by sharp micromechanical gradients and local crystallite clusters. KW - Additive manufacturing KW - Fatigue damage KW - Heat treatment KW - Inconel 718 KW - Laser powder bed fusion KW - Low-cycle fatigue KW - Tensile strength PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-599316 DO - https://doi.org/10.1002/adem.202302122 SN - 1527-2648 SP - 1 EP - 17 PB - Wiley AN - OPUS4-59931 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -