TY - JOUR A1 - Hildebrandt, Jana A1 - Taubert, Andreas A1 - Thünemann, Andreas T1 - Synthesis and Characterization of Ultra‐Small Gold Nanoparticles in the Ionic Liquid 1‐Ethyl‐3‐methylimidazolium Dicyanamide, [Emim][DCA] N2 - AbstractWe report on gold clusters with around 62 gold atoms and a diameter of 1.15±0.10 nm. Dispersions of the clusters are long‐term stable for two years at ambient conditions. The synthesis was performed by mixing tetrachloroauric acid (HAuCl4 ⋅ 3 H2O) with the ionic liquid 1‐ethyl‐3‐methylimidazolium dicyanamide ([Emim][DCA]) at temperatures of 20 to 80 °C. Characterization was performed with small‐angle X‐ray scattering (SAXS), UV‐Vis spectroscopy, and MALDI‐TOF mass spectrometry. A three‐stage model is proposed for the formation of the clusters, in which cluster growth from gold nuclei takes place according to the Lifshitz‐Slyozov‐Wagner (LSW) model followed by oriented attachment to form colloidal stable clusters. KW - Reference materials KW - SAXS KW - Gold KW - Nanoparticle KW - Small-angle X-ray scattering KW - Ionic liquid PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-588203 DO - https://doi.org/10.1002/open.202300106 SN - 2191-1363 VL - 44 SP - 1 EP - 19 PB - Wiley AN - OPUS4-58820 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Guerra, M.F. A1 - Neri, E. A1 - Radtke, Martin T1 - Gold leaf tesserae: tracing the origins of gold using synchrotron-based techniques N2 - To gain insight into the possible origin of the gold used in the production of tesserae containing gold leaf less than 0.5 μm thick placed between two layers of glass, we propose a non-destructive synchrotron radiation (SR) XRF protocol based on sequential analysis under optimised analytical conditions. Using this protocol, trace element analysis is achieved with detection limits of 1–6 mg/kg. As Pt and Au have adjacent fluorescence energies, we tested the most challenging situation, when Pt is present in very low concentrations in gold. Data obtained by double-dispersive XRF (D2XRF) and μXRF for fourth–ninth-century mosaics decorating nine Eastern and Western religious buildings show that the Eastern and Western tesserae are made from different alloys. However, these alloys are identical to those used to make gold leaf for gilding, because plastic deformation requires the use of gold alloys with high ductility and malleability. Although trace element composition of gold used in the concerned period is only available for coins, by comparing the amounts of Pt contained in the tesserae and in the coins we show that Roman tesserae are made from Roman gold, as described in the documentary sources. We observe for the Byzantine period the use of a Byzantine gold and of gold supposedly from different stages of recycling, and we suggest the use of Umayyad and Abbasid gold for the production of Islamic tesserae. KW - Gold KW - XRF KW - Synchrotron KW - BAMline KW - D2XRF KW - Tesserae PY - 2023 DO - https://doi.org/10.1140/epjp/s13360-022-03638-y SN - 2190-5444 VL - 138 IS - 2 SP - 1 EP - 15 AN - OPUS4-57208 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bertorelle, F. A1 - Wegner, Karl David A1 - Berkulic, M. P. A1 - Fakhouri, H. A1 - Comby-Zerbino, C. A1 - Sagar, A. A1 - Bernadó, P. A1 - Resch-Genger, Ute A1 - Bonacic-Koutecký, V. A1 - Le Guével, X. A1 - Antoine, R. T1 - Tailoring the NIR-II Photoluminescence of Single Thiolated Au25 Nanoclusters by Selective Binding to Proteins N2 - Atomically precise gold nanoclusters are a fascinating class of nanomaterials that exhibit molecule-like properties and have outstanding photoluminescence (PL). Their ultrasmall size, molecular chemistry, and biocompatibility make them extremely appealing for selective biomolecule labeling in investigations of biological mechanisms at the cellular and anatomical levels. In this work, we report a simple route to incorporate a preformed Au25 nanocluster into a model bovine serum albumin (BSA) protein. A new approach combining small-angle X-ray scattering and molecular modeling provides a clear localization of a single Au25 within the protein to a cysteine residue on the gold nanocluster surface. Attaching Au25 to BSA strikingly modifies the PL properties with enhancement and a redshift in the second near-infrared (NIR-II) window. This study paves the way to conrol the design of selective sensitive probes in biomolecules through a ligand-based strategy to enable the optical detection of biomolecules in a cellular environment by live imaging. KW - Fluorescence KW - Aggregation KW - Signal enhancement KW - Cluster KW - Nano KW - Metal KW - NIRII KW - SWIR KW - Sensor KW - Quantum yield KW - Lifetime KW - Photophysics KW - Synthesis KW - Protein KW - Imaging KW - Bioimaging KW - Ligand KW - Gold PY - 2022 DO - https://doi.org/10.1002/chem.202200570 SN - 1521-3765 VL - 28 IS - 39 SP - 1 EP - 8 PB - Wiley-VCH CY - Weinheim AN - OPUS4-55077 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Le Guevel, X. A1 - Wegner, Karl David A1 - Würth, Christian A1 - Baulin, V. A. A1 - Musnier, B. A1 - Josserand, V. A1 - Resch-Genger, Ute A1 - Koll, J-C T1 - Tailoring the SWIR emission of gold nanoclusters by surface ligand rigidification and their application in 3D bioimaging N2 - The influence of solvent polarity and surface ligand rigidification on the SWIR emission profile of gold nanoclusters with an anistropic surface was investigated. A strong enhancement of the SWIR emission band at 1200 nm was observed when measuring in different local environments: in solution, in polymer composites, and in solids. SWIR in vivo imaging of mice assisted by deep learning after intravenous administration of these gold nanoclusters provides high definition pseudo-3D views of vascular blood vessels. KW - Nano KW - Nanomaterial KW - Metal cluster KW - Photoluminescence KW - Quantum yield KW - Photophysics KW - Lifetime KW - Sensor KW - NIR KW - SWIR KW - Ligand KW - Gold KW - Mechanism KW - Charge transfer KW - Enhancement strategy KW - Imaging KW - Application KW - Contrast agent PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-543582 DO - https://doi.org/10.1039/D1CC06737K VL - 58 IS - 18 SP - 2967 EP - 2970 PB - RSC AN - OPUS4-54358 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Liebig, F. A1 - Sarhan, R. M. A1 - Schmitt, C. N. Z. A1 - Thünemann, Andreas A1 - Prietzel, C. A1 - Bargheer, M. A1 - Koetz, J. T1 - Gold Nanotriangles with Crumble Topping and their Influence on Catalysis and Surface‐Enhanced Raman Spectroscopy N2 - By adding hyaluronic acid (HA) to dioctyl sodium sulfosuccinate (AOT)‐stabilized gold nanotriangles (AuNTs) with an average thickness of 7.5±1 nm and an edge length of about 175±17 nm, the AOT bilayer is replaced by a polymeric HA‐layer leading to biocompatible nanoplatelets. The subsequent reduction process of tetrachloroauric acid in the HA‐shell surrounding the AuNTs leads to the formation of spherical gold nanoparticles on the platelet surface. With increasing tetrachloroauric acid concentration, the decoration with gold nanoparticles can be tuned. SAXS measurements reveal an increase of the platelet thickness up to around 14.5 nm, twice the initial value of bare AuNTs. HRTEM micrographs show welding phenomena between densely packed particles on the platelet surface, leading to a crumble formation while preserving the original crystal structure. Crumbles crystallized on top of the platelets enhance the Raman signal by a factor of around 20, and intensify the plasmon‐driven dimerization of 4‐nitrothiophenol (4‐NTP) to 4,4′‐dimercaptoazobenzene in a yield of up to 50 %. The resulting crumbled nanotriangles, with a biopolymer shell and the absorption maximum in the second window for in vivo imaging, are promising candidates for biomedical sensing. KW - SAXS KW - Small-angle X-ray scattering KW - Nanoparticle KW - Gold PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-503977 DO - https://doi.org/10.1002/cplu.201900745 VL - 85 IS - 3 SP - 519 EP - 526 PB - Wiley-VCH Verlag CY - Weinheim AN - OPUS4-50397 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Nolze, Gert A1 - Saliwan Neumann, Romeo A1 - Reith, F. A1 - Etschmann, B. A1 - Kilburn, M. R. A1 - Brugger, J. T1 - Unravelling the formation histories of placer gold and platinum-group mineral particles from Corrego Bom Successo, Brazil: A window into noble metal cycling N2 - Gold and platinum-group-metals (PGM) are cycled through Earth's environments by interwoven geological, physical, chemical and biological processes leading to the trans/neoformation of metallic particles in placers. The placer deposit at Corrego Bom Successo (CBS, Brazil) is one of the few localities worldwide containing secondary gold- and PGM-particles. Placer gold consists of detrital particles from nearby hydrothermal deposits that were transformed in the surface environment. Processes that have affected these particles include shortdistance transport, chemical de-alloying of the primary Gold silver, and (bio)geochemical dissolution/reprecipitation of Gold leading to the formation of pure, secondary gold and the Dispersion of gold nanoparticles. The latter processes are likely mediated by non-living organic matter (OM) and bacterial biofilms residing on the particles. The biofilms are largely composed of metallophillic β- and γ-Proteobacteria. Abundant mobile gold and platinum nanoparticles were detected in surface waters, suggesting similar mobilities of these metals. Earlier hydrothermal processes have led to the formation of coarsely-crystalline, arborescent dendritic potarite (PdHg). On potarite surfaces, biogeochemical processes have then led to the formation of platinum- and palladium-rich micro-crystalline layers, which make up the botryoidal platinum palladium aggregates. Subsequently potarite was dissolved from the core of many aggregates leaving voids now often filled by secondary anatase (TiO2) containing biophilic elements. The presence of fungal structures associated with the anatase suggests that fungi may have contributed to ist formation. For the first time a primary magmatic PGM-particle comprising a mono-crystalline platinum palladium-alloy with platinum iridium osmium inclusions was described from this locality, finally defining a possible primary source for the PGM mineralisation. In conclusion, the formation of modern-day placer gold- and PGM-particles at CBS began 100s ofmillions of years ago bymagmatic and hydrothermal processes. These provided the metal sources for more recent biogeochemical cycling of PGEs and gold that led to the trans/neoformation of gold- and PGM-particles. KW - Gold KW - Platinum-group-metals KW - Biogeochemical cycling KW - Magmatic and hydrothermal processes KW - Biomineralisation PY - 2019 DO - https://doi.org/10.1016/j.gr.2019.07.003 SN - 1342-937X VL - 76 SP - 246 EP - 259 PB - Elsevier AN - OPUS4-48657 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zutta Villate, J. M. A1 - Hahn, Marc Benjamin T1 - Radioactive gold nanoparticles for cancer treatment N2 - Dose enhancement by gold nanoparticles (AuNP) was shown to increase the biological effectiveness of radiation damage in biomolecules and tissue. Most of the current studies focus on external beam therapy on combination with AuNP. Here we present a Monte-Carlo study (Geant4) to characterise radioactive AuNP. Radioactive 198 Au emits beta and gamma rays and is considered for applications with solid tumours. To effectively apply 198 AuNP their energy deposit characteristics have to be determined in terms of intrinsic and extrinsic properties e.g. AuNP diameter, AuNP density, and their clustering behaviour. After each decay process, the energy deposit, inelastic scattering events, kinetic energy spectrum of secondary particles within the AuNP themselves and in a spherical target volume of water up to 1 μm radius were determined. Simulations were performed for AuNP radii ranging from 2.5 nm to 20 nm radius, different cluster sizes and densities. The results show an increase of the energy deposit in the vicinity of the AuNP up to 150 nm. This effect nearly vanishes for distances up to one micron. For the case of AuNP clusters and the same activity, the enhancement of the energy deposit increases with the relative gold mass percentage and therefore can be adjusted by changing AuNP radius or clustering behaviour. KW - Gold KW - Nanoparticle KW - Cancer KW - Monte-Carlo KW - Simulation KW - Cluster PY - 2019 DO - https://doi.org/10.1140/epjd/e2019-90707-x SN - 1434-6060 SN - 1434-6079 VL - 73 IS - 95 SP - 1 EP - 7 PB - Springer CY - Berlin AN - OPUS4-47964 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Reith, F. A1 - Rea, M.A.D. A1 - Sawley, P. A1 - Zammit, C.M. A1 - Nolze, Gert A1 - Reith, T. A1 - Rantanen, K. A1 - Bissett, A. T1 - Biogeochemical cycling of gold: Transforming gold particles from arctic Finland N2 - (Bio)geochemical cycling of gold (Au) has been demonstrated in present-day (semi)-arid, (sub)-tropical and temperate environment. Hereby biofilms on Au-bearing mineral- and Au-particle surfaces drive Au dispersion and reconcentration, thereby (trans)forming the particles. However, it is unknown if biogeochemical cycling of Au occurs in polar environments, where air temperatures can reach −40 °C and soils remain frozen for much of the year. Therefore, placer Au-particles, soils and waters were collected at two placer mining districts in arctic Finland, i.e., the Ivalojoki and Lemmenjoki goldfields. Sites were chosen based on contrasting settings ((glacio)-fluvial vs. glacial-till deposits) and depths (surface to 5m below current surface). Gold particles were studied using a combination of tagged 16S rRNA gene next generation sequencing and electron microscopic/microanalytical techniques. Across all sites a range of Au-particle morphologies were observed, including morphotypes indicative of Au dissolution and aggregation. Elevated Au concentrations indicative of Au mobility were detected in placer particle bearing soils at both districts. Typically Au-particles were coated by polymorphic biofilm layers composed of living and dead cells embedded in extracellular polymeric substances. Intermixed were biominerals, clays and iron-sulfides/oxides and abundant secondary Au morphotypes, i.e., nano-particles, microcrystals, sheet-like Au, branched Au networks and overgrowths and secondary rims. Biofilms communities were composed of Acidobacteria (18.3%), Bacteroidetes (15.1%) and Proteobacteria (47.1%), with β-Proteobacteria (19.5%) being the most abundant proteobacterial group. Functionally, biofilms were composed of taxa contributing to biofilm establishment, exopolymer production and nutrient cycling, abundant taxa capable of Au mobilization, detoxification and biomineralization, among them Cupriavidus metallidurans, Acinetobacter spp. and Pseudomonas spp., were detected. In conclusion, these results demonstrate that placer Au-particle transformation and Au dispersion occur in cold, arctic environments. This corroborates the existence of biogeochemical Au cycling in present-day cold environments. KW - Gold KW - Bacteria KW - Biogeochemistry KW - Mobility KW - Finland KW - Cupriavidus metallidurans KW - NGS PY - 2018 DO - https://doi.org/10.1016/j.chemgeo.2018.03.021 SN - 0009-2541 VL - 483 SP - 511 EP - 529 PB - Elsevier AN - OPUS4-44805 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Guerra, M. F. A1 - Fischer, M. A1 - Radtke, Martin A1 - Reinholz, Uwe T1 - Inca figurines from the Ethnologisches Museum in Berlin: an analytical study of some typical and atypical productions N2 - Fourteen hollow and one cast anthropomorphic and zoomorphic figurines produced in Incan times for ritual offerings from the Ethnologisches Museum in Berlin were selected to investigate the technologies and alloys used for their fabrication with portable optical microscopy and non-destructive XRF elemental analysis. This group of gold and silver figurines includes typical specimens of the Inca production, such as the four silver figurines from the Island Coati in Lake Titicaca and the two gold figurines from Pachacamac, as well as specimens that are seldom present in collections, which makes them atypical. In addition to the tall figurines with atypical hair or standing pose, one bicolour figurine half silver, half gold) and another with coloured inlays were included in this study for comparison. The large majority of the silver specimens are made from very high quality alloys and the gold figurines are made from alloys containing low copper contents and silver ranging from 30wt% to 52wt%. KW - Gold KW - pXRF KW - Inca PY - 2017 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-436015 DO - https://doi.org/10.4000/bifea.8232 SN - 0303-7495 VL - 46 IS - 1 SP - 221 EP - 251 PB - Institut Français d'Études Andines AN - OPUS4-43601 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Niemeyer, B. A1 - Schwarzmaier, A. A1 - Radtke, Martin A1 - Hahn, Oliver T1 - Archaische Goldarbeiten aus Kleinasien in der Berliner Antikensammlung – Herstellungstechnik, Materialanalytik und der Fundkomplex »aus Ephesos« N2 - Ein Konvolut einzelner Schmuckstücke und die Goldbeigaben eines angeblichen Grabfundes wurden technologisch und analytisch untersucht. Die meisten Objekte sind Blecharbeiten, die aus einer Vielzahl von Einzelteilen mit metallischem Goldlot zusammengefügt und mit Granulation oder granulations-imitierendem Perl- oder Kerbdraht verziert wurden. Nur vier kleine Ohrringe sind massiv gegossen. Zwei Zierbleche dürften über Patrizen (Positivmodeln), die Deckel der Astragale in Matrizen (Negativmodeln) geformt worden sein. Alle Objekte wurden mit Synchrotron- und atmosphärischer Röntgenfluoreszenz analysiert. Die Daten zeigen das breite Spektrum an Goldlegierungen, die im 7./6. Jahrhundert v. Chr. in Kleinasien verarbeitet wurden: vom natürlichen Seifengold (Elektrum) bis zu geläutertem, fast reinem Gold. Eine Korrelation zwischen Goldqualität und Verarbeitungsmethode konnte nicht festgestellt werden. Sowohl hochreines als auch mit viel Silber und Kupfer legiertes Gold wurde zum Schmieden von Blecharbeiten, aber auch zum Massivguss verwendet. Aus der Goldfarbe kann wegen des Phänomens der oberflächlichen Goldanreicherung nicht auf eine Legierungszusammensetzung geschlossen werden. Der 1963 angekaufte Fundkomplex aus lydischen Metallarbeiten und ostionischen Salbgefäßen aus Ton dürfte einen Grabfund des frühen 6. Jahrhunderts v. Chr. darstellen, dessen Herkunft aus Ephesos jedoch nicht zu sichern ist. KW - Gold KW - Synchrotron KW - XRF PY - 2017 SN - 1866-7007 VL - 9 SP - 57 EP - 83 PB - RGZM. Archäologische Staatssammmlung München CY - München AN - OPUS4-42986 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -