TY - JOUR A1 - Hao, Ning A1 - Böhning, Martin A1 - Goering, Harald A1 - Schönhals, Andreas T1 - Nanocomposites of Polyhedral Oligomeric Phenethylsilsesquioxanes and Poly(bisphenol A carbonate) as Investigated by Dielectric Spectroscopy JF - Macromolecules N2 - Nanocomposites were prepared by solution blending of polyhedral oligomeric silsesquioxane with phenethyl substituents (PhenethylPOSS) into poly(bisphenol A carbonate) (PBAC). The nanocomposites were investigated by dielectric spectroscopy, differential scanning calorimetry (DSC) and density measurements. PhenethylPOSS shows one relaxation process, the α-relaxation, confirmed by DSC investigations. PBAC shows a β-relaxation at lower and an α-relaxation at higher temperatures. With increasing PhenethylPOSS content the α-relaxation of the composites shifts to lower temperatures. Thus, incorporation of PhenethylPOSS leads to a plasticization of PBAC due to a decrease of the packing density which is rationalized by density measurements. For higher concentrations of PhenethylPOSS (>10 wt %) the α-relaxation of the polycarbonate matrix splits into two peaks. Moreover, close to the α-relaxation of PhenethylPOSS a third process is observed. These results indicate a phase separation into a PBAC matrix with a few percents of molecularly solved POSS and POSS-rich domains. These POSS-rich domains are surrounded by an interfacial layer of PBAC having a higher concentration of POSS than the matrix. A phase diagram is deduced providing a miscibility criterion. For the phase separated nanocomposites an interfacial polarization phenomena is observed. Using a simplified model the time constant of this process is correlated with the size of the PhenethylPOSS-rich domains and theire increasing size with the increase of the concentration of POSS. KW - Polyhedral oligomeric silsesquioxane (POSS) KW - Polymer-based nanocomposites KW - Broadband dielectric spectroscopy KW - Interfacial polarisation PY - 2007 SN - 0024-9297 SN - 1520-5835 VL - 40 IS - 8 SP - 2955 EP - 2964 PB - American Chemical Society CY - Washington, DC AN - OPUS4-14768 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hao, Ning A1 - Böhning, Martin A1 - Schönhals, Andreas T1 - Dielectric Properties of Nanocomposites Based on Polystyrene and Polyhedral Oligomeric Phenethyl-Silsesquioxanes JF - Macromolecules N2 - Nanocomposites were prepared by solution blending of polyhedral oligomeric silsesquioxane with phenethyl substituents (PhenethylPOSS) into polystyrene (PS). The prepared materials were investigated by dielectric spectroscopy, differential scanning calorimetry (DSC), and density measurements. Additional FTIR investigations were carried out. Pure polystyrene shows two relaxation processes, an intermediate β*-process at lower and the α-relaxation at higher temperatures, the latter corresponding to segmental dynamics (dynamic glass transition). The molecular assignment of the β*-process needs further investigation. PhenethylPOSS can be incorporated into PS up to about 40 wt % without any indication of phase separation. With increasing PhenethylPOSS content, the α-relaxation of the composites shifts to lower temperatures and the loss peak broadens. Thus, the main effect of the nanofiller in the polystyrene matrix is to enhance the segmental dynamics, i.e., plasticization. The incorporation of approximately 40 wt % (approximately 5 mol %) PhenethylPOSS shifts the glass transition temperature Tg by 50 K to lower temperatures. The obtained results for polystyrene are discussed together with those reported recently for polycarbonate where a phase-separated morphology is observed for higher concentrations of PhenethylPOSS. The different behavior of PhenethylPOSS in polystyrene and polycarbonate is interpreted in terms of the different interaction of the phenyl rings within the POSS substituents with the phenyl rings of the polymers. For polystyrene, the interaction is stronger than for polycarbonate which probably leads to the enhanced miscibility of PhenethylPOSS into polystyrene. A detailed analysis of the temperature dependence of the dielectric relaxation strengths points also to additional interactions in the nanocomposites when compared to pure polystyrene. The broadening of the loss peak with increasing concentration is discussed in the framework of composition fluctuations. KW - Polyhedral oligomeric silsesquioxane (POSS) KW - Polymer-based nanocomposites KW - Broadband dielectric spectroscopy KW - Polystyrene PY - 2007 DO - https://doi.org/10.1021/ma071777g SN - 0024-9297 SN - 1520-5835 VL - 40 IS - 26 SP - 9672 EP - 9679 PB - American Chemical Society CY - Washington, DC AN - OPUS4-16492 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Leng, Jing A1 - Szymoniak, Paulina A1 - Kang, N.-J. A1 - Wang, D-Y A1 - Wurm, A. A1 - Schick, C. A1 - Schönhals, Andreas T1 - Influence of interfaces on the crystallization behavior and the rigid amorphous phase of poly(l-lactide)-based nanocomposites with different layered doubled hydroxides as nanofiller JF - Polymer N2 - Based on the three-phase model of semi-crystalline polymers, we determined all phase fractions of the NiAl-LDH/PLLA nanocomposites in dependence on the concentration of the nanofiller. Moreover, the rigid amorphous fraction (RAF) was separated into the RAFcrystal and the RAFfiller unbiasedly. A detailed comparison to the related nanocomposite system MgAl-LDH/PLLA was made considering that Mg and Ni have different atomic weights. As a first result is was found that NiAl-LDH/PLLA displays a higher crystallization rate compared to MgAl-LDH/PLLA, which is related to the different morphologies of the two nanocomposite systems. For both systems RAFcrystal increases with increasing concentration of the nanofiller. This means in the case of the nanocomposite not each crystal produces the same amount of RAF, as often assumed. Also, RAFfiller increases with the concentration for both systems but in a different way. This is discussed considering again the different morphologies of both nanocomposites. KW - Polymer-based nanocomposites KW - Temperature modulated differential scanning calorimetry PY - 2019 DO - https://doi.org/10.1016/j.polymer.2019.121929 VL - 184 SP - 121929 PB - Elesevier Ltd. AN - OPUS4-49557 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -