<?xml version="1.0" encoding="utf-8"?>
<export-example>
  <doc>
    <id>44405</id>
    <completedYear/>
    <publishedYear>2018</publishedYear>
    <thesisYearAccepted/>
    <language>eng</language>
    <pageFirst>787</pageFirst>
    <pageLast>795</pageLast>
    <pageNumber/>
    <edition/>
    <issue>6</issue>
    <volume>20</volume>
    <type>article</type>
    <publisherName>Royal Society of Chemistry</publisherName>
    <publisherPlace/>
    <creatingCorporation/>
    <contributingCorporation/>
    <belongsToBibliography>1</belongsToBibliography>
    <completedDate>--</completedDate>
    <publishedDate>--</publishedDate>
    <thesisDateAccepted>--</thesisDateAccepted>
    <title language="eng">Oriented surface nucleation and crystal growth in a 18BaO·22CaO·60SiO2 mol% glass used for SOFC seals</title>
    <abstract language="eng">A glass of the composition 37BaO·16CaO·47SiO2 wt% produced on an industrial scale is crystallized at 970 °C for times ranging from 15 min to 2 h. The crystallization at the immediate surface as well as the crystal growth into the bulk are analyzed using scanning electron microscopy (SEM) including energy dispersive X-ray spectroscopy (EDXS) and electron backscatter diffraction (EBSD) as well as X-ray diffraction in the Θ–2Θ setup (XRD). The immediate surface shows the oriented nucleation of walstromite as well as the formation of wollastonite and an unknown phase of the composition BaCaSi3O8. All three phases also grow into the bulk where walstromite ultimately dominates the kinetic selection and grows throughout the bulk due to a lack of bulk nucleation. Walstromite shows systematic orientation changes as well as twinning during growth. A critical analysis of the XRD-patterns acquired from various crystallized samples indicates that their evaluation is problematic and that phases detected by XRD in this system should be verified by another method such as EDXS.</abstract>
    <parentTitle language="eng">CrystEngComm</parentTitle>
    <identifier type="doi">10.1039/c7ce02008b</identifier>
    <enrichment key="date_peer_review">07.03.2018</enrichment>
    <author>W. Wisniewski</author>
    <author>C. Thieme</author>
    <author>Ralf Müller</author>
    <author>Stefan Reinsch</author>
    <author>S.-M. Groß-Barsnick</author>
    <author>C. Rüssel</author>
    <subject>
      <language>eng</language>
      <type>uncontrolled</type>
      <value>Glass</value>
    </subject>
    <subject>
      <language>eng</language>
      <type>uncontrolled</type>
      <value>Surface nucleation</value>
    </subject>
    <subject>
      <language>eng</language>
      <type>uncontrolled</type>
      <value>Orientation</value>
    </subject>
    <subject>
      <language>eng</language>
      <type>uncontrolled</type>
      <value>EBSD</value>
    </subject>
    <collection role="ddc" number="620">Ingenieurwissenschaften und zugeordnete Tätigkeiten</collection>
    <collection role="literaturgattung" number="">Verlagsliteratur</collection>
    <collection role="fulltextaccess" number="">Datei im Netzwerk der BAM verfügbar ("Closed Access")</collection>
  </doc>
  <doc>
    <id>62399</id>
    <completedYear/>
    <publishedYear>2025</publishedYear>
    <thesisYearAccepted/>
    <language>eng</language>
    <pageFirst>2462</pageFirst>
    <pageLast>2468</pageLast>
    <pageNumber/>
    <edition/>
    <issue>1</issue>
    <volume>17</volume>
    <type>article</type>
    <publisherName>ACS Publications</publisherName>
    <publisherPlace/>
    <creatingCorporation/>
    <contributingCorporation/>
    <belongsToBibliography>1</belongsToBibliography>
    <completedDate>--</completedDate>
    <publishedDate>--</publishedDate>
    <thesisDateAccepted>--</thesisDateAccepted>
    <title language="eng">Tracing the Formation of Femtosecond Laser-Induced Periodic Surface Structures (LIPSS) by Implanted Markers</title>
    <abstract language="eng">The generation of laser-induced periodic surface structures (LIPSS) using femtosecond lasers facilitates the engineering of material surfaces with tailored functional properties. Numerous aspects of their complex formation process are still under debate, despite intensive theoretical and experimental research in recent decades. This particularly concerns the challenge of verifying approaches based on electromagnetic effects or hydrodynamic processes by experiment. In the present study, a marker experiment is designed to conclude on the formation of LIPSS. Well-defined concentration depth profiles of 55Mn+- and 14N+-ions were generated below the polished surface of a cast Mn- and Si-free stainless steel AISI 316L using ion implantation. Before and after LIPSS generation, marker concentration depth profiles and the sample microstructure were evaluated by using transmission electron microscopy techniques. It is shown that LIPSS predominantly formed by material removal through locally varying ablation. Local melting and resolidification with the redistribution of the material occurred to a lesser extent. The experimental design gives quantitative access to the modulation depth with a nanometer resolution and is a promising approach for broader studies of the interactions of laser beams and material surfaces. Tracing LIPSS formation enables to unambiguously identify governing aspects, consequently guiding the path to improved processing regarding reproducibility, periodicity, and alignment.</abstract>
    <parentTitle language="eng">ACS Applied Materials &amp; Interfaces</parentTitle>
    <identifier type="issn">1944-8244 (Print)</identifier>
    <identifier type="issn">1944-8252 (Online)</identifier>
    <identifier type="doi">10.1021/acsami.4c14777</identifier>
    <identifier type="urn">urn:nbn:de:kobv:b43-623990</identifier>
    <enrichment key="opus.source">publish</enrichment>
    <enrichment key="date_peer_review">15.01.2025</enrichment>
    <enrichment key="opus.doi.autoCreate">false</enrichment>
    <enrichment key="opus.urn.autoCreate">true</enrichment>
    <licence>Creative Commons - CC BY - Namensnennung 4.0 International</licence>
    <author>R. Wonneberger</author>
    <author>S. Gräf</author>
    <author>Jörn Bonse</author>
    <author>W. Wisniewski</author>
    <author>K. Freiberg</author>
    <author>M. Hafermann</author>
    <author>C. Ronning</author>
    <author>F. A. Müller</author>
    <author>A. Undisz</author>
    <subject>
      <language>eng</language>
      <type>uncontrolled</type>
      <value>Laser-induced periodic surface structures (LIPSS)</value>
    </subject>
    <subject>
      <language>eng</language>
      <type>uncontrolled</type>
      <value>Femtosecond laser processing</value>
    </subject>
    <subject>
      <language>eng</language>
      <type>uncontrolled</type>
      <value>Ion implantation</value>
    </subject>
    <subject>
      <language>eng</language>
      <type>uncontrolled</type>
      <value>Transmission Electron Microscopy (TEM)</value>
    </subject>
    <subject>
      <language>eng</language>
      <type>uncontrolled</type>
      <value>Stainless steel</value>
    </subject>
    <collection role="ddc" number="620">Ingenieurwissenschaften und zugeordnete Tätigkeiten</collection>
    <collection role="institutes" number="">6 Materialchemie</collection>
    <collection role="institutes" number="">6.2 Material- und Oberflächentechnologien</collection>
    <collection role="themenfelder" number="">Material</collection>
    <collection role="literaturgattung" number="">Verlagsliteratur</collection>
    <collection role="fulltextaccess" number="">Datei für die Öffentlichkeit verfügbar ("Open Access")</collection>
    <collection role="unnumberedseries" number="">Wissenschaftliche Artikel der BAM</collection>
    <collection role="themenfelder" number="">Advanced Materials</collection>
    <thesisPublisher>Bundesanstalt für Materialforschung und -prüfung (BAM)</thesisPublisher>
    <file>https://opus4.kobv.de/opus4-bam/files/62399/2025-Wonneberger_ACSAMI17_2462.pdf</file>
  </doc>
</export-example>